• 제목/요약/키워드: Iron Ion Effects

검색결과 63건 처리시간 0.02초

광택 니켈 도금속에 미치는 이가식 이온의 영향 (The Effects of Ferrous Ion on Properties of Bright Nickel Electordeposit)

  • 육기진;여운관;박룡진
    • 한국표면공학회지
    • /
    • 제15권4호
    • /
    • pp.218-225
    • /
    • 1982
  • The effects of ferrous ion on the properties of bright nickel electrodeposit were exa-mined. Iron exists as ferrous ion (Fe+2) and ferric ion (Fe+3) in the bath, a portion of the former tend to be oxidized to the somewhat harmful ferric ion. Iron was added to bath as the ferrous sulfate, ferrous ion prevented from the oxidation with citric acid. It was found that the hardness was increased as the concentration of ferrous ion, the ductility was slightly increased too. The appearance can obtain the wide bright deposits within 4g/$\ell$. The corrosion resistance drastically dropped from 5g/$\ell$ In the case of considering the effect of ferrous ion on the corrosion resistance and the appearance, the allowable limits is 4g/$\ell$, if the reductant is used.

  • PDF

Borate 완충용액에서 철의 부식에 대한 대기의 영향 (Atmospheric Effects on Corrosion of Iron in Borate Buffer Solution)

  • 김현철;김연규
    • 대한화학회지
    • /
    • 제56권6호
    • /
    • pp.673-678
    • /
    • 2012
  • 변전위법과 선형분극법을 이용하여 Borate 완충용액에서 철의 부식에 대한 대기의 영향을 조사하였다. 철의 부식은 용액 속에 녹아있는 산소의 양에 크게 영향을 받았다. 용액에 녹아 있는 산소의 환원반응으로 환원전류가 증가하여 부식전위가 양의 방향으로 이동하였다. 물 또는 산소의 환원 반응에 의하여 생성된 $OH^-$ 이온은 철 전극의 전기이중층에 $OH^-$ 이온의 농도를 증가시켜 철 전극에 $OH^-$ 이온의 흡착을 용이하게 하였다. 철 전극 표면에 $OH^-$ 이온의 흡착은 Langmuir isotherm 또는 Temkin logarithmic isotherm을 이용하여 설명할 수 있었다.

뱀장어 (Anguilla japonica) 추출물 중의 Carnosine, 단백질 및 철분 함량에 미치는 추출방법의 영향 (Effects of Extraction Method on the Carnosine, Protein, and Iron Contents of Eel (Anguilla japonica) Extracts)

  • 송호수;이근태;강옥주
    • 한국수산과학회지
    • /
    • 제39권5호
    • /
    • pp.384-390
    • /
    • 2006
  • To improve the extractability of carnosine and the levels of pro-oxidants such as iron in eel (Anguilla japonica) extracts, we examined the effects of extraction time, temperature, ion exchange chromatography and ultrafiltration (UF). The respective protein and total iron were reduced approximately 55 and 60% at 60$^{\circ}C$, 63 and 70% at 80$^{\circ}C$, 68 and 76% at 100$^{\circ}C$ and 82 and 48% with ion exchange chromatography, respectively, compared to the untreated extract. However, there was no significant difference in the carnosine levels in the eel extracts. Ultrafiltration reduced the protein content of the extract by 52% compared with the untreated extract. UF reduced the protein contents of the samples from 60, 80, and 100% heat treatment and ion exchange chromatography treatment by 27, 50, 46 and 47%, respectively. UF reduced the total iron contents of the identical four treatments by 14, 22, 23, and 43%, respectively, while UF increased the carnosine by 23, 17, 20, and 6%, respectively.

Effects of ATP and ADP on iron uptake in rat heart mitochondria

  • Kim, Mi-Sun;Song, Eun-Sook
    • Animal cells and systems
    • /
    • 제14권4호
    • /
    • pp.245-252
    • /
    • 2010
  • Iron uptake in mitochondria and fractionated mitochondria compartments was studied to understand iron transport in heart mitochondria. The inner membrane is most active in iron uptake. Mitochondrial uptake was dependent on iron concentration and the amount of mitochondria. Iron transport was inversely proportional to pH in the range of 6.0 to 8.0. Iron transport reached a maximum after 30 min of incubation at $37^{\circ}C$. Iron uptake was inhibited by 1 mM ATP and stimulated by 1 mM ADP. The oxidative phosphorylation inhibitor oligomycin inhibited iron uptake, but rotenone and antimycin A did not. The divalent ions $Mg^{2+}$, $Cu^{2+}$, $Mn^{2+}$, and $Zn^{2+}$ suppressed iron uptake at $10\;{\mu}M$ and stimulated it at 1 mM. The divalent ion $Ca^{2+}$ stimulated iron uptake at $10\;{\mu}M$ and suppressed it at 1 mM, competing with iron. The uptake of calcium was stimulated by 10 to $1000\;{\mu}M$ ATP, while iron uptake was stimulated reciprocally by 10 to $1000\;{\mu}M$ ADP, suggesting that these ions have movements similar to those of ATP and ADP.

광산배수 처리를 위한 세멘테이션 공정 중 구리제거효율에 대한 철분 응집의 영향 (The Effects of Iron Powder Agglomeration on the Copper Removal Efficiency during Cementation Process for Treating Mine Drainages)

  • 나현진;엄유익;홍승관;유경근
    • 자원리싸이클링
    • /
    • 제28권5호
    • /
    • pp.74-79
    • /
    • 2019
  • 구리이온농도를 117.15 mg/L로 조절한 모의 광산배수용액 제조하고, 세멘테이션제로서 철분을 투입하여 세멘테이션 공정 중 구리이온제거효율에 대한 철분당량, 철분크기, 교반속도의 영향을 조사하였다. 교반속도가 200 rpm의 경우, 온도 $20^{\circ}C$에서 2 당량의 철분을 투입하면 90분에 51 %의 구리가 제거되었으나 16 당량의 철분을 투입하면 60분에 99 % 이상의 구리가 제거되었다. $48{\mu}m$ 이하와 $150{\mu}m$ 크기의 철분을 2당량 투입하여 구리제거율을 관찰한 결과 200 rpm에서는 큰 차이를 나타내지 않았으나 교반속도를 400 rpm으로 증가시킨 경우 두 입도 모두에서 구리제거효율을 크게 증가하였으며, 이는 200 rpm에서 철분의 입자가 응집되어 비표면적이 감소된 것이 원인으로 SEM분석을 통해 확인하였다. 교반속도 600 rpm, 반응온도 $20^{\circ}C$, $48{\mu}m$ 이하 철분 2 당량의 조건에서 60 분에 99 % 이상의 구리가 제거된 것을 확인하였다.

Effect of trace amount of ferrous and ferric ions on the dissolution of iron plate in magnetically treated 3% sodium chloride solution

  • Chiba, Atsushi;Ohki, Tomohiro;Wu, Wen-Chang
    • Corrosion Science and Technology
    • /
    • 제4권2호
    • /
    • pp.45-50
    • /
    • 2005
  • A 3% NaCl solution of 1 $dm^3$ circulated with 1.5 $dm^3/min$ by a pump for 24 h in the presence of magnetic field. An iron plate immersed in a $100cm^3$ of test solution for 24 h. The rest potential and pH on surface fixed after 3 h. Containing 0~120 ppm of Fe(II) ion, the dissolution in the magnetically treated solution rose comparing with that in the non-magnetically treated solution. The dissolution amount reached to maximum at 50 ppm, then fixed in the non-magnetically treated solution. When Fe(II) ion existed in the magnetically treated solution, dissolution accelerated a little. In the non-magnetic treated solution containing 10~125 ppm of Fe(III) ion existed, the dissolution accelerated. The dissolution amounts reached to maximum at 50 ppm, then decreased from maximum value. In the magnetically treated solution, the dissolution amounts reached to minimum until 50 ppm, then increased from minimum value. The dissolution amounts affected larger with increasing of magnetic flux density. Fe(II), Fe(III) ions and magnetic treatment affected to formation of $Fe(OH)_2$ and/or $Fe_3O_4$ films. The magnetically treated effects memorized about one month.

$CaCO_3$침전능 조절에 의한 금속시편에서의 부식방지 (The Corrosion Control Using CCPP(Calcium Carbonate Precipitation Potential )Index in Metallic Coupons)

  • 이재인;임진경;서상훈;김동윤;신춘환
    • 한국환경과학회지
    • /
    • 제9권6호
    • /
    • pp.505-509
    • /
    • 2000
  • The purpose of this study was to evaluate the effects of $Ca(OH)_2$ and $CO_2$ additions on the corrosion of metal coupons(ductile iron, galvanized steel, copper and stainless steel). Corrosion rate and released metal ion concentration of ductile iron and galvanized steel decreased by adjusting alkalinity, calcium hardness and pH with $Ca(OH)_2$ & $CO_2$ additions on copper and stainless steel were less than those on ductile iron and galvanized steel. When ductile iron coupon was exposed to water treated with Ca(OH)$_2$&$CO_2$, additions, the main components of corrosion product formed on its surface were $CaCO_3$ and $Fe_2 O_3 or Fe_2 O_4$ which often reduce the corrosion rate by prohibiting oxygen transport to the metal surface.

  • PDF

The effects of chitosan complex on the various bacteria

  • Lee, Hyun-Joo
    • 대한약학회:학술대회논문집
    • /
    • 대한약학회 2003년도 Proceedings of the Convention of the Pharmaceutical Society of Korea Vol.1
    • /
    • pp.227.1-227.1
    • /
    • 2003
  • To assess the effect of chitosan complex with metal ion on various pathogenic bacteria, the antibacterial activities were investigated. Arsenic, bismuth, calcium, iodine, iron, mercury, platinum, and silver were used as a metal ion. Staphylococcus aureus. Streptococcus mutans, Helicobacter pylori, Propionibacterium acnes and human saliva were examined. It was demonstrated that metal ions associated chitosan showed aggregation activities on various pathogens.

  • PDF

담자균류의 효소에 관한 연구(I) -표고버섯 중의 광감응성 Mitochondrial $F_0F_1-ATPase$의 철이온 효과- (Study on the Enzyme of Basidiomycetes(I) -The Effects of Iron Ions on the Light-Induced Mitochondrial $F_0F_1-ATPase$ of Lentinus edodes-)

  • 민태진;이미애;배강규
    • 한국균학회지
    • /
    • 제21권3호
    • /
    • pp.165-171
    • /
    • 1993
  • 표고버섯 중의 광감응성 mitochondrial ATP synthase는 0.1 mM $Fe^{2+}$ 단독 이온에 의하여 그 활성이 대조구에 비해 102%, 증가되었으며, 반면 $Fe^{3+}$$Mg^{2+}$ 이온은 효소의 활성을 억제시켰다. 0.5 mM $Mg^{2+}$ 존재하에서 0.1 mM $Fe^{2+}$ 이온에 의한 이 효소의 활성은 32% 증가되었으며 0.5 mM $Mg^{2+}$ 존재하에서 $Fe^{3+}$ 이온효과는 단독 $Fe^{3+}$ 이온의 효과와 유사한 경향으로 효소의 활성을 저해하였다. 0.5 mM $Mg^{2+}$과 0.1 mM, 0.5 mM 및 1.0 mM $Fe^{3+}$ 이온의 공존하에서$Fe^{2+}$ 이온에 의한 효소의 활성은 모두 억제되었으며, 특히 0.5 mM $Mg^{2+}$과 0.1 mM $Fe^{3+}$ 이온의 공존하에서 5.0 mM $Fe^{2+}$ 이온에 의하여 53%의 억제현상을 나타내었다. 따라서 표고버섯 중의 광감응성 mitochondrial ATP synthase의 활성은 $Fe^{2+}$ 이온에 의하여 특이적으로 크게 증가되며, 이 효소에 대한 $Fe^{2+}$ 이온의 활성화 효과가 $Mg^{2+}$ 이온에 의하여 크게 영항을 받지 않으나, $Fe^{3+}$ 이온의 공존하에서는 억제됨을 알았다. 활성화 금속이온인 $Fe^{2+}$ 존재하에서 이 효소의 최적 pH는 7.6이며, 최적 온도는 $63^{\circ}C$이었다. 또한 이 효소는 금속 chelating agent인 EDTA에 의하여 효소의 활성이 상실됨으로써 metalloenzyme의 가능성을 제시하였다.

  • PDF

The Effect of Iron Catalysts on the Formation of Alcohol and Ketone in the Biomimetic Oxidation of Cyclohexane

  • Kim Seong-Bo;Lee Kyu-Wan;Kim, Yong-Joon;Hong Seog-In
    • Bulletin of the Korean Chemical Society
    • /
    • 제15권6호
    • /
    • pp.424-427
    • /
    • 1994
  • Effects of iron compounds in known biomimetic oxidation systems (Gif IV and GoAgg II) have been studied on activity and ketone/alcohol selectivity of cyclohexane oxidation. Both ketone/alcohol ratio and cyclohexane conversion were affected by counter-ion Z of iron compounds Z-Fe. When Z has a more electron withdrawing property, the reactivity is increased and the formation of ketone is favored. From these experimental results, a new mechanism is proposed for the biomimetic oxidation system.