생불활성 질화물 이온도금된 티타늄 임프란트의 표면특성 및 생체적합성 (Surface characteristics and biocompatibility of bioinert nitrides ion plated titanium implant)

  • 장갑성;김흥중;박주철;김병옥;한경윤
    • Journal of Periodontal and Implant Science
    • /
    • 제29권1호
    • /
    • pp.209-231
    • /
    • 1999
  • Even though titanium(Ti) and its alloys are the most used dental implant materials, there are some problems that Ti wears easily and interferes normal osteogenesis due to the metal ions. Ti coated with bioactive ceramics such as hydroxyapatite has also such problems as the exfoliation or resorption of the coated layer, Recent studies on implant materials have been proceeding to improve physical properties of the implant substrate and biocompatibility of the implant surfaces. The purpose of the present study was to examine the physical property and bone tissue compatibility of bioinert nitrides ion plated Ti, Button type specimens(14mm in diameter, 2.32rrun in height) for the abrasion test and cytotoxicity test and thread type implants(3.75mm in diameter, 6mm in length) for the animal experiments were made from Ti(grade 2) and 316LVM stainless steel. Ti specimens were ion plated with TiN, ZrN by the low temperature arc vapor deposition, and the depth profile of the TiN/Ti, ZrN/Ti ion plated surface was examined by Auger Electron Spectroscopy. Three kind of button type specimens .of TiN/Ti, ZrN/Ti and Ti were used for abrasion test, and HEPAlClC7 cells and CCD cells were cultivated for 4 days with the specimens for cytotoxicity test. Thread type implants of TiN/Ti, ZrN/Ti, Ti, 316LVM were implanted on the femur of 6 adult dogs weighing 10kg-13kg. Two dogs were sacrified for histological examination after 45 days and 90 days, and four dogs were sacrified for the removal torque test of the implant') after 90 days. The removal torque force was measured by Autograph (Shimadzu Co., AGS-1000D series, Japan). Abrasion resistance of TiN/Ti was the highest, and that of ZrN/Ti and Ti were followed. The bioinert nitride ion plated Ti had much better abrasion resistance, compared with Ti, In the cytotoxicity test, the number of both cells were increased in all specimens, and there were no significant difference in cytotoxic reaction among all groups (p>0.1), In histological examination, 316LVM showed the soft tissue engagement in interface between the implant and bone, but the other materials after 45 days noted immature new bone formation in the medullary portion along the implant surface, and those after 90 days showed implant support by new bone formation in both the cortical and the medullary portion, The removal torque force of Tilv/Ti showed significantly higher than that of Ti(p(O,05). The difference in removal torque force between TiN/Ti and ZrN/Ti was not significant(p>0.05), and that of 316LVM was lowest among all groups(p<0.05). These results suggest that bioinert nitrides ion plated Ti can resolve the existing problems of Ti and bioactive ceramics, and it may be clinically applicable to human.

  • PDF

다양한 치은 연하 수복물에 대한 치은 섬유아 세포 부착 연구 (Attachment of Human Gingival Fibroblast to Various Subgingival Restorations;A Comparative Study in Vitro)

  • 이은숙;송인택;임정수;김형섭
    • Journal of Periodontal and Implant Science
    • /
    • 제29권3호
    • /
    • pp.621-636
    • /
    • 1999
  • When mucoperiosteal flaps are positioned and sutured to desirable position, the wound contains several interface between tissues which differ fundamentally in composition & biological reaction. Thus the C-T surface of the flap will, on one hand, oppose another vascularized surface, and on the other, the avascular dental material for example, when root resoptions, fractured root, endodontic perforation, deep root carious lesions were filled with amalgam, glass ionomer, resin etc. Recently, a number of case report described the successful treatment of a subgingival root lesion with restorative material & free gingival graft, open flap surgery, but more objective research was needed . Most of study on restorative materials were concerned for cytotoxicity not for actual healing event on that materials and its influencing factors such as biocompatibility, surface wettability, surface topography . The aim of this in vitro study was to evaluate the effect of amalgam, resin modified glass ionomer, composite resin per se, and their surface roughness on the growth of human gingival fibroblast. The cells were obtained and placed on culture flask and incubated for 3 days with the prepared test materials. Then count the attached cell number with hemocytometer,(n=12) and 2 samples were examined with SEM about attachment cell morphology . Another 4 samples were evaluated on their surface roughness with Talysurf and average surface roughness value(Ra) were obtained. Statistical difference in attached cell number, roughness value were analyzed using ANOVA. The number of attached cell was as follows, for root dentin specimen 16.7${\pm}$4.41, resin modified glass ionomer 14.0${\pm}$4.15, resin 8.13${\pm}$3.63, amalgam 0.72${\pm}$3.33(${\times}10^3$). Between root dentin and resin-modified glass ionomer, no significant difference was observed, but resin, amalgam showed a significant less cell numbers than for root dentin, resin modified glass ionomer cement. SEM examination expressed many cell surface attachment apparatus in root dentin and resin modified glass ionomer specimens. For resin specimen, cell attachment was observed but exposed less appratus. The average surface roughness value are following results. Dentin specimen 0.6972${\pm}$ 0.104, resin modified glass ionomer 0.0822${\pm}$0.009, resin 0.0875${\pm}$0.005, amalgam 4.2145${\pm}$0.985(${\mu}m$). Between root dentin, resin-modified glass ionomer, and resin, no significant difference was observed, but amalgam showed a significant more rough surface than other groups. When evlauated the interrelationship between cell attachment and surface roughness, therefore, there was weak reverse correlation.(pearson correlation : - 0.593) These results suggest that resin modified glass ionomer have the favorable healing potential when used for subgingival restoration. And for relationship between cell attachment and surface characteristics, further investigations were needed.

  • PDF

브레이징 접합공정 조건이 SiN4/S.S. 316 접합체의 기계적 특성 및 신뢰도에 미치는 영향 (Effects of Brazing Processing Condition on Mechanical Properties and Reliability of Si3N/S.S. 316 Joints)

  • 장희석;박상환;최성철
    • 한국세라믹학회지
    • /
    • 제39권10호
    • /
    • pp.955-962
    • /
    • 2002
  • 활성 금속 브레이징법의 공정변수인 브레이징 온도 및 시간의 변화가 Cu buffer layer를 사용한 $Si_3N_4$Stainless steel 316 접합체의 기계적 특성 및 신뢰도에 미치는 영향을 규명하기 위하여 브레이징 조건 변화에 따른 접합계면 미세구조 변화를 조사하였다. 900${\circ}C$ 이상의 온도에서 브레이징 된 접합체에서는 Cu buffer layer가 브레이징 합금에 용해되어 연속 Cu층을 유지하지 못하였으며, $Si_3N_4$/brazing alloy 계면에서 계면 반응물 층의 두계도 급격히 증가하였다. 950${\circ}C$에서 브레이징된 Cu buffer layer를 사용한 $Si_3N_4$/Stainless steel 316 접합체의 파괴강도는 접합체 내 잔류응력의 증가로 급격히 감소하였다. 950${\circ}C$ 이하의 온도에서 브레이징 시간의 변화는 Cu buffer layer를 사용한 $Si_3N_4$/Stainless steel 316 접합체의 파괴강도 및 파괴경로에 큰 영향을 미치지 못하였다.

저온동시소성(LTCC)을 위한 결정화 유리(La2O3-B2O3-TiO2계)와 BaNd2Ti5O14 세라믹을 이용한 마이크로파 유전체 특성 (Microwave Dielectric Properties of La2O3-B2O3-TiO2 Glass-Ceramic and BaNd2Ti5O14Ceramic System for LTCC Application)

  • 황성진;김유진;김형순
    • 한국세라믹학회지
    • /
    • 제41권8호
    • /
    • pp.599-604
    • /
    • 2004
  • 무선 이동통신 산업에서 소형화와 RF모듈을 구현하기 위해 저온 동시 소성 세라믹(LTCC)기술이 부각되고 있다. LTCC용 재료는 90$0^{\circ}C$ 이하의 온도에서 소성이 되어야 한다 본 연구는 BaO-N $d_2$ $O_3$-Ti $O_2$ (BNT:20∼40wt%) 세라믹과 L $a_2$ $O_3$- $B_2$ $O_3$-Ti $O_2$ (LBT:80∼60wt%) 유리를 혼합하여 유리를 결정화시킴으로, 나타나는 부수적인 효과를 얻고자 하였다. 이에 소결 거동, 결정상 분석, 상대밀도 그리고 유전특성을 평가하였다 80wt% 유리의 첨가는 90%에 가까운 상대밀도를 갖는 복합체로서 15에 가까운 유전율과 10000GHz의 품질계수와 같은 우수한 유전특성을 보였다. 이와 같은 결과는 유리 결정화를 이용하여 LTCC용 유전체에 적용될 수 있는 가능성을 부여하였다.

$MoSi_2$ 금속간화합물 복합재료의 미세구조와 방전가공특성 (Microstructure and EDM Processing of $MoSi_2$ Intermetallic Composite)

  • 윤한기;이상필;윤경욱;김동현
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.23-28
    • /
    • 2002
  • This paper describes the machining characteristics of the $MoSi_2$ based composites by electric discharge drilling with various tubular electrodes, besides, Hardness characteristics and microstructures of $Nb/MoSi_2$ laminate composites were evaluated from the variation of fabricating conditions such as preparation temperature, applied pressure and pressure holding time. $MoSi_2$ -based composites has been developed in new materials for jet engine of supersonic-speed airplanes and gas turbine for high- temperature generator. Achieving this objective may require new hard materials with high strength and high temperature-resistance. However, With the exception of grinding, traditional machining methods are not applicable to these new materials. Electric discharge machining (EDM) is a thermal process that utilizes a spark discharge to melt a conductive material, the tool electrode being almost non-unloaded, because there is no direct contact between the tool electrode and the workpiece. By combining a nonconducting ceramics with more conducting ceramic it was possible to raise the electrical conductivity. From experimental results, it was found that the lamination from Nb sheet and $MoSi_2$ powder was an excellent strategy to improve hardness characteristics of monolithic $MoSi_2$. However, interfacial reaction products like (Nb, Mo)$SiO_2$ and $Nb_2Si_3$ formed at the interface of $Nb/MoSi_2$ and increased with fabricating temperature. $MoSi_2$ composites which a hole drilling was not possible by the conventional machining process, enhanced the capacity of ED-drilling by adding $NbSi_2$ relative to that of SiC or $ZrO_2$ reinforcements.

  • PDF

Cr을 첨가한 ZnO-Bi2O3-Sb2O3계의 소결과 전기적 특성 (Sintering and Electrical Properties of Cr-doped ZnO-Bi2O3-Sb2O3)

  • 홍연우;신효순;여동훈;김진호
    • 한국전기전자재료학회논문지
    • /
    • 제23권12호
    • /
    • pp.942-948
    • /
    • 2010
  • In this study we aims to examine the effects of 0.5 mol% $Cr_2O_3$ addition on the reaction, microstructure development, resultant electrical properties, and especially the bulk trap and interface state levels of ZnO-$Bi_2O_3-Sb_2O_3$ (Sb/Bi=0.5, 1.0, and 2.0) systems (ZBS). The samples were prepared by conventional ceramic process, and characterized by XRD, density, SEM, I-V, impedance and modulus spectroscopy (IS & MS) measurement. The sintering and electrical properties of Cr-doped ZBS (ZBSCr) systems were controlled by Sb/Bi ratio. Pyrochlore ($Zn_2Bi_3Sb_3O_{14}$) was decomposed more than $100^{\circ}C$ lowered on heating in ZBS (Sb/Bi=1.0) by Cr doping. The densification of ZBSCr (Sb/Bi=0.5) system was retarded to $800^{\circ}C$ by unknown Bi-rich phase produced at $700^{\circ}C$. Pyrochlore on cooling was reproduced in all systems. And $Zn_7Sb_2O_{12}$ spinel ($\alpha$-polymorph) and $\delta-Bi_2O_3$ phase were formed by Cr doping. In ZBSCr, the varistor characteristics were not improved drastically (non-linear coefficient $\alpha$ = 7~12) and independent on microstructure according to Sb/Bi ratio. Doping of $Cr_2O_3$ to ZBS seemed to form $Zn_i^{..}$(0.16 eV) and $V^{\bullet}_o$ (0.33 eV) as dominant defects. From IS & MS, especially the grain boundaries of Sb/Bi=0.5 systems were divided into two types, i.e. sensitive to oxygen and thus electrically active one (1.1 eV) and electrically inactive intergranular one (0.95 eV) with temperature.

유기산, 산화음이온 및 금속 산화물 간의 근권 내 상호작용 연구를 위한 계산화학과 적외선 분광학에 관한 총설: 기본적인 원리와 스펙트럼 처리 (Reviews in Infrared Spectroscopy and Computational Chemistry to Reveal Rhizospheric Interactions among Organic Acids, Oxyanions and Metal oxides: Fundamental Principles and Spectrum Processing)

  • 한준호;노희명
    • 대한환경공학회지
    • /
    • 제39권7호
    • /
    • pp.426-439
    • /
    • 2017
  • 이 총설은 근권에서 일어나는 유기산, 산화음이온, 그리고 금속 산화물 간의 상호작용을 이해하는데 활용하고 있는 적외선 분광학과 계산화학에 대한 기본적 원리, 역사, 적용 분야, 장점, 그리고 단점에 대해 최근 연구들을 바탕으로 요약하였다. 식물의 유기산과 금속 산화물은 토양 환경에서 산화음이온의 유효도와 이동성을 결정하기 때문에, 산화음이온의 환경 내 거동을 이해하기 위해서는 계면에서 이들의 상호작용을 이해하는 것이 중요하다. 적외선 분광학의 감쇠 전반사 기법은 계면에서 일어나는 화학적인 반응을 측정하는 강력한 도구이지만, 광학적 특성들이 실험 설계와 대상에 따라 매우 다르게 나타날 수 있으므로 이를 이용한 측정은 까다롭다. 전반사에 의해 발생하는 소멸파의 침투 깊이가 가장 중요한 매개 변수인데, 침투 깊이는 적외선의 입사각과 대상 파장, 그리고 매질의 굴절률에 따라 결정된다. 또한, 적외선을 이용하여 계면에서의 화학반응을 분석할 때 겹쳐서 발생하는 스펙트럼을 해석하는 것 역시 큰 문제이기 때문에, 겹쳐 나타나는 스펙트럼을 해석하여 밴드를 검출하고, 이 스펙트럼을 deconvolution하는 것이 필수적이다. 본 총설에서는 적외선스펙트럼을 처리하는 기본적인 절차와, 밴드 검출에 사용하는 네가지 방법인 도함수 분광학과 이차 상관 분광학, multivariate curve resolution, 계산 화학을 액체상에 존재하는 인산염 종분화로 설명하였다. 스펙트럼 처리와 계산 화학을 조합하였을 때 간단한 계에서 측정한 겹쳐진 스펙트럼 결과는 해석할 수 있었지만, 자연과 같은 복잡계에서 측정한 겹쳐진 스펙트럼을 해석하는 것은 여전히 불가능한 상황이다. 그러나 향후 분석 및 신호 처리 기술 발달에 따라 복잡계뿐만 아니라 자연계에서 일어나는 계면 반응을 해석할 수 있을 것으로 기대한다.

$RuO_2$박막의 미세 구조가 박막형 마이크로 슈퍼캐패시터의 특성에 미치는 영향 (Effect of RuO$_2$ Thin Film Microstructure on Characteristics of Thin Film Micro-supercapacitor)

  • 김한기;윤영수;임재홍;조원일;성태연;신영화
    • 한국재료학회지
    • /
    • 제11권8호
    • /
    • pp.671-678
    • /
    • 2001
  • $RuO_2$ 박막을 전극으로 하여 Pt/Ti/Si 기판 위에 $RuO_2$ /LiPON/$RuO_2$의 다층 구조로 이루어진 전고상의 박막형 마이크로 슈퍼캐패시터를 제작하였다. 전극용 $RuO_2$박막은 반응성 dc 마그네트론 스퍼터를 이용하여 $O_2$/[Ar+$O_2$]비를 증가시키며 성장시켰고, 비정질 LiPON 고체전해질 박막은 순수한 질소분위기 하에서 rf 스퍼터링으로 성장시켰다. 상온에서의 충-방전 측정을 통해 $RuO_2$ 박막의 미세구조에 따라 슈퍼캐패시터의 사이클 특성이 영향을 받는 것을 알 수 있었다. Glancing angle x-ray diffraction(GXRD)과 transmission electron microscopy (TEM) 분석을 통해 산소 유량의 증가가 $RuO_2$박막의 미세 구조의 영향을 주는 것을 알 수 있었고, X-ray photoelectron spectroscopy (XPS) 분석을 통해 산소 유량 비의 증가가 Ru과 산소간의 결합에도 영향을 줌을 알 수 있었다. 또한 사이클 후 슈퍼캐패시터의 TEM 및 AES depth profiling 분석을 통해, 충-방전 시 $RuO_2$와 LiPON과의 계면반응에 의해 형성된 계면 층이 사이클 특성에 영향을 줌을 알 수 있었다.

  • PDF

계면 화학반응과 무전해 니켈 금속층에서 나타나는 취성파괴와의 연관성에 관한 연구 (Correlation between Interfacial Reaction and Brittle Fracture Found in Electroless Ni(P) Metallization)

  • 손윤철;유진
    • 마이크로전자및패키징학회지
    • /
    • 제12권1호
    • /
    • pp.41-46
    • /
    • 2005
  • 무전해 Ni(P)과 솔더와의 반응 중 발견되는 취성파괴 현상과 계면 화학반응시의 금속간화합물 spalling과의 연관성을 전단 파괴실험을 통하여 체계적으로 연구하였다. 취성파괴는 무전해 Ni(P)과 Sn-3.5Ag 솔더와의 반응 후에만 나타났고 Sn-3.0Ag-0.5Cu 솔더와의 반응시에는 연성파괴만이 관찰되었다. Sn-3.0Ag-0.5Cu 솔더와의 반응시 $(Ni,Cu)_3Sn_4$$(Cu,Ni)_6Sn_5$의 삼성분계 금속간화합물이 생성되었고 spatting은 발생하지 않았다. 반면, Sn-3.5Ag 솔더와의 반응시에는 $Ni_3Sn_4$ 금속간화합물이 spatting된 솔더패드에서 취성파괴가 발생하였다. 파괴표면을 면밀히 분석한 결과 취성파괴는 $Ni_3Sn_4$ 금속간화합물과 Ni(P) 금속층 사이에 형성된 $Ni_3SnP$ 층에서 발생하는 것을 알 수 있었다. $Ni_3SnP$ 금속간화합물 층은 $Ni_3Sn_4$ 금속간화합물이 spatting되는 과정 중에 두껍게 성장하므로 무진해 Ni(P) 사용시 기계적 신뢰성을 보장하기 위해서는 금속간화합물의 spatting을 방지하는 것이 매우 중요하다.

  • PDF

Pt/SBT/Si, Pt/SBT/Pt 강유전체 게이트 구조에서 수소 열화 현상 및 Ir 게이트 전극에 의한 열화 방지 방법 (Hydrogen Degradation of Pt/SBT/Si, Pt/SBT/Pt Ferroelectric Gate Structures and Degradation Resistance of Ir Gate Electrode)

  • 박전웅;김익수;김성일;김용태;성만영
    • 마이크로전자및패키징학회지
    • /
    • 제10권2호
    • /
    • pp.49-54
    • /
    • 2003
  • 본 연구에서는 Pt/SrBi$_2$Ta$_2$O$_{9}$(SBT)/Si (MFS)와 Pt/SBT/Pt (MFM) 각각의 구조에서 수소 열처리에 의한 SBT박막의 물리, 전기적 영향에 대해 연구하였다. SBT 박막의 미세구조 및 전기적 특성은 수소 열처리 후에 SBT 박막의 손상으로 열화된다. 특히, Pt 전극에 의한 SBT 박막의 열화 현상을 연구하기 위해 각각 Si 와 Pt 위에 SBT 를 증착하여 같은 조건으로 열처리를 하였다. XRD, XPS, P-V, C-V 측정을 통해 Pt 전극 없이 SBT자체로도 수소 열처리 후에 열화 됨을 확인 할 수 있었다. 또한, 수소 열화현상이라고 하는 촉매 반응으로 SBT 열화 현상이 Pt로 가속화되었다. 이러한 현상을 방지하기 위해서 새로운 Ir 전극을 제안하여 $Ir/IrO_2/SBT/IrO_2$ 구조에서의 수소 열처리 전후 및 회복 열처리를 통해 SBT 박막의 전기적 특성을 연구하였다. P-V측정을 통해 SBT박막을 이용한 MFM구조에서 Ir이 열화 방지용 전극 물질로의 활용 가능성을 확인하였다.

  • PDF