A study on the characteristics of Pb free Sn-2%Ag-x%Bi solder alloys (Pb Free Sn-2%Ag-x%Bi계 Solder의 특성에 관한 연구)

  • 흥순국;박일경;강정윤
    • Journal of Welding and Joining
    • /
    • v.16 no.3
    • /
    • pp.148-156
    • /
    • 1998
  • The purpose of this study is to investigate the characteristics of Pb-Free Sn-2%Ag-Bi solder alloys. The solder alloys used in this study is Sn-2%Ag-(3,5,7,9%) Bi It is examined that their properties such as melting range, wettability, microstructure, microhardness, and tensile property. The addition of Bi(3,5,7,9%) lowered the melting point of the solder and the melting range was 196~203$^{\circ}C$. The wettability of the solder as equal to that of Sn-37% Pb solder. The morphology of structure did not change largely by addition of Bi. But the structure of cellular dendrite of linear type displayed. The tensile strength of the solder was superior to that of Sn-37%Pb solder. But the elongation was inferior to that of Sn-37%Pb solder. The hardness of Sn-2%Ag solder was tow times and that of Sn-2%Ag-Bi solder was three times of that in Sn-37%Pb solder. But the effect of increment of Bi content did not change largely.

  • PDF

A study on the characteristics of low Pb Sn-5%Pb-1.5%Ag-x%Bi solder alloys (저Pb Sn-5%Pb-1.5%Ag-x%Bi계 솔더 합금의 특성에 관한 연구)

  • 홍순국;주철홍;강정윤;김인배
    • Journal of Welding and Joining
    • /
    • v.16 no.3
    • /
    • pp.157-166
    • /
    • 1998
  • Recently as environmental pollution caused by Pb has posed a serious threat to the global environment, the trend to regulate the usage of Pb in electronic industry is one the rise. Currently, the solder alloy with high Pb content, Sn-37%Pb, is utilized in the electronic assembly therefore, the objective of this study is to develop an alternative solder alloy for the existing Sn-37%Pb solder alloy. First thing, this work choosed Sn-5%Pb-1.5%Ag, Sn-5%Pb-1.5%Ag-x%Bi(x=1~5%) for candidate solder alloys, and examined their properties such as melting range, wettability, microhardness, tensile property, oxidation behavior and microstructure. Wettability was on the same level of Sn-37%Pb. Dissolution of Pb ion in Sn-5%Pb solder was 0.46ppm. This solder alloy revealed cellular dendrite microstructure $\beta$-Sn matrix, Pb-rich phase, Ag/Sn, and Cu/Sn Intermetallic compounds. The range of solidification temperature was within 3$0^{\circ}C$. Also these alloy displayed higher tensile strength and lower elongation than Sn-37%Pb. The resistance of oxidation in Sn-5%Pb-1.5%Ag solder alloy was superior to that of Sn-37%Pb solder alloy. But that of Sn-5%Pb-1.5%Ag-5%Bi solder alloy was equal to that of Sn-37%Pb solder alloy.

  • PDF

A Study on Characteristics of Sn-37Pb and Sn-4.0Ag-0.5Cu Solder Joints as Various A:V Ratio (A:V Ratio 변화에 따른 Sn-37Pb, Sn-4.0Ag-0.5Cu Solder 접합부의 특성 연구)

  • Han, Hyun-Joo;Lim, Seok-Jun;Moon, Jung-Tak;Lee, Jin
    • Proceedings of the International Microelectronics And Packaging Society Conference
    • /
    • 2001.11a
    • /
    • pp.67-73
    • /
    • 2001
  • To investigate the relationships of solder joint characteristics with solder composition and A:V ratio (solder volume per pad area), Sn-37Pb and Sn-4.0Ag-0.5Cu solder balls with 330, 400, 450 and $457{\mu}{\textrm}{m}$ size were reflowed on same substrate. Sn-37Pb and Sn-4.0Ag-0.5Cu was reflowed at $220^{\circ}C$ and $240^{\circ}C$ respectively by IR-type soldering machine. As a result of reflowed solder- ball diameter(D) and height(H) measurement, D/H was decreased with solder ball size increment in range of 330~450 ${\mu}{\textrm}{m}$. But, D/H was increased in the solder joint for 457 ${\mu}{\textrm}{m}$ size, it was caused possibly by decrement of solder ball height increment compared with solder volume increment. As a result of shear and pull test, joint strength with A:V ratio was high. Joint strength of Sn-4.0Ag-0.5Cu was higher than Sn-37Pb. However, Sn-37Pb had more stable solder joint of small standard deviation. A thick and clean scallop type Ni-Cu-Sn intermetallic compound layer was formed in high A:V ratio and Sn-4.0Ag-0.5Cu solder joint interface.

  • PDF

A Study on the Characteristics of Sn-Ag-X Solder Joint -The Wettability of Sn-Ag-Bi-In Solder to Plated Substrates- (Sn-Ag-X계 무연솔더부의 특성 연구 -기판 도금층에 따른 Sn-Ag-Bi-In 솔더의 젖음특성-)

  • 김문일;문준권;정재필
    • Journal of the Korean institute of surface engineering
    • /
    • v.35 no.1
    • /
    • pp.11-16
    • /
    • 2002
  • As environmental concerns increasing, the electronics industry is focusing more attention on lead free solder alternatives. In this research, we have researched wettability of intermediate solder of Sn3Ag9Bi5In, which include In and Bi and has similar melting temperature to Sn37Pb eutectic solder. We investigated the wetting property of Sn3Ag9Bi5In. To estimate wettability of Sn3Ag9Bi5In solder on various substrates, the wettability of Sn3Ag9Bi5In solder on high-pure Cu-coupon was measured. Cu-coupon that plated Sn, Ni and Au/Ni and Si-wafer adsorbed Ni/Cu under bump metallurgy on one side. As a result, the wetting property of Sn3Ag9Bi5In solder is a little better than that of Sn37Pb and Sn3.5Ag.

Characterization of the Sn-Ag-Cu and Sn-Cu Lead-free Solder by adding P (P의 함량에 따른 Sn-Ag-Cu 및 Sn-Cu 무연솔더의 특성평가)

  • 신영의;황성진
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.16 no.6
    • /
    • pp.549-554
    • /
    • 2003
  • The purpose of this paper is to investigate the solder properties by the change of P mass percentage. Tension test, wetting balance test, spread test, and analysis of intermetallic compound after isothermal aging of Sn-2.5Ag-0.7Cu-0.005P, Sn-2.5Ag-0.7Cu-0.01P, Sn-2.5Ag-0.7Cu-0.02P, Sn-0.7Cu-0.005P were performed. Adding P in the solder alloys resulted in improvement of tensile strength, reduction of intermetallic compound growth, reduction of oxidization in fusible solders under wave soldering. After comparing solder alloy containing P with tin-lead eutectic solder alloy, P contained solders alloys showed much better solder properties than eutectic solder alloy. Furthermore, this solder alloy presented remarkable properties than any other lead-free solder alloy.

A Study on the Characteristics of Low Pb Sn-5%Pb-1.5%Pb-1.5Ag-x%In Solder Alloys (저 Pb Sn-5%Pb-1.5%Ag-x%In계 솔도 합금의 특성에 관한 연구)

  • Hong, Sun-Guk;Ju, Cheol-Hong;Gang, Jeong-Yun;Kim, In-Bae
    • Korean Journal of Materials Research
    • /
    • v.8 no.11
    • /
    • pp.1011-1019
    • /
    • 1998
  • This work designed Sn-5%Pb-1.5%Ag-x%In solder alloy to develop the solder alloy with low Pb content. This solder alloy doesn't cause environmental pollution. and this study reviewed the probability of replacement of Sn-37%Pb solder as evaluation of melting range, wettability. microstructure, microhardne'ss, tensile strength, drossability of this new solder alloys. The level of international regulation in dissolution amount of Pb ion was 3ppm. But dissolution amount of Pb ion in Sn-5%Pb solder alloy confirmed not to threat the global environmental is 0.46ppm. The melting range of this solder alloy was $183-192^{\circ}C$. Also the range of solidification was very narrow within $5^{\circ}C$. The wettability was similar to Sn-37%Pb solder, and the effect of amount of In addition of wettability couldn't be founded. The probability of replacement in the melting range and wettability is very high. And microhardness of this solder alloy was 1.5 times of conventional type solder. Tensile strength of new solder alloys was a little high than that of conventional type solder. With increasing amount of In% addition, tensile strength was increased, but elongation was decreased. The solder alloy of l%In addition revealed AgSn and Pb on dendrite microstructure boundary, and $Ag_3Sn$, $Ag_3In$ and Pb were revealed on it at the solder alloy of 3% In addition. The drossability was superior to Sn-37%Pb solder alloy and the solder alloys of 2% In addition was not generated for 3hrs.

  • PDF

Effect of Sn Decorated MWCNT Particle on Microstructures and Bonding Strengths of the OSP Surface Finished FR-4 Components Assembled with Sn58%Bi Composite Solder Joints (OSP 표면처리된 FR-4 PCB기판과 Sn58%Bi 복합솔더 접합부의 미세조직 및 접합강도에 미치는 Sn-MWCNT의 영향)

  • Park, Hyun-Joon;Lee, Choong-Jae;Min, Kyung Deuk;Jung, Seung-Boo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.26 no.4
    • /
    • pp.163-169
    • /
    • 2019
  • Sn-Pb solder alloys in electronics rapidly has been replaced to Pb free solder alloys because of various environmental regulations such as restriction of hazardous substances directive (RoHS), European Union waste electrical, waste electrical and electronic equipment (WEEE), registration evaluation authorization and of chemicals (REACH) etc. Because Sn58%Bi (in wt.%) solder alloy has low melting point and higher mechanical properties than that of Sn-Pb solder, it has been studied to manufacture electronic components. However, the reliability of Sn58%Bi solder could be lowered because of the brittleness of Bi element included in the solder alloy. Therefore, we observed the microstructures of Sn58%Bi composite solders with various contents of Sn-decorated multiwalled carbon nanotube (Sn-MWCNT) particles and evaluated bonding strength of the FR-4 components assembled with Sn58%Bi composite solder. Also, microstructures and bonding strengths of the Sn58%Bi composite solder joints were evaluated with the number of reflows from 1 to 7 times, respectively. Bonding strengths and fracture energies of the Sn58%Bi composite solder joints were measured by die shear test. Microstructures and fracture modes were observed with scanning electron microscope (SEM). Microstructures in the Sn58%Bi composite solder joints were finer than that of only Sn58%Bi solder joint. Bonding strength and fracture energy of Sn58%Bi composite solder including 0.1 wt.% of Sn-decorated MWCNT particles increased up to 20.4% and 15.4% at 5 times in reflow, respectively.

Thermal Fatigue Life Prediction of ${\mu}BGA$ Solder Joint Using Sn-37mass%Pb Solder and Sn-3.5mass%Ag Lead-free Solder (Sn-37mass%Pb 솔더 및 Sn-3.5mass%Ag 무연솔더를 이용한 ${\mu}BGA$ 솔더접합부의 열피로수명 예측)

  • 신영의;이준환;하범용;정승부;정재필
    • Journal of Welding and Joining
    • /
    • v.19 no.4
    • /
    • pp.406-412
    • /
    • 2001
  • This study is focussed on the numerical prediction of the thermal fatigue life of a ${\mu}BGA$(Micro Ball Grid Array) solder joint. Numerical method is used to perform three-dimensional finite element analysis for Sn-37mass%Pb. Sn-3.5mass%Ag solder alloys during the given thermal cycling. Strain values, along with the result of mechanical fatigue tests for solder alloys were then used to predict the solder joint fatigue life using the Coffin-Manson equation. In this study, a practical correlation for the prediction of the thermal fatigue life is suggested by using the dimensionless variable $\gamma$. As a result. it could be found that Sn-3.5mass%Ag has longer fatigue life than Sn-37mass%Pb in low cycle fatigue. In addition. the result with ${\gamm}ashow$a good agreement with the FEA results.

  • PDF

A Study on the Characteristics of Sn-Ag-X Solder Joint (Sn-Ag-X계 무연솔더 접합부의 미세조직 및 전단강도에 관한 연구)

  • 김문일;문준권;정재필
    • Journal of Welding and Joining
    • /
    • v.20 no.2
    • /
    • pp.77-81
    • /
    • 2002
  • Many kinds of Pb-free solder have been investigated because of the environmental concerns. Sn-Ag-Cu system is well blown as most competitive Pb-free solder. However, since Sn-Ag-Cu system has relatively high melting point compared to Sn-Pb eutectic, it may a limitation, the some application. In this study, Bi and In contained solder of $Sn_3Ag_8Bi_5In$ which has relatively lower melting point, $188~204^{\circ}C$, was investigated. $Sn_3Ag_8Bi_5In$ solder ball of $500\mu\textrm{m}$ diameter was set on the Ni/Cu/Cr-UBM and reflow soldered in the range of $220~240^{\circ}C$ for 5~15s. The maximum shear strength of the solder ball was around 170mN by reflowing at $240^{\circ}C$ for 10s. Intermetallic compound formed on the UBM of Si-wafer was analysed by SEM(scanning electron microscope) and XRD(X-ray diffractometer).

Prediction of Thermal Fatigue Life on $\mu$BGA Solder Joint Using Sn-3.5Ag, Sn-3.5Ag-0.7Cu, and Sn-3.5Ag-3.0In-0.5Bi Solder Alloys (Sn-3.5Ag, Sn-3.5Ag-0.7Cu, Sn-3.5Ag-3.0In-0.5Bi Solder를 이용한 $\mu$BGA Solder접합부의 열피로 수명예측)

  • 김연성;김형일;김종민;신영의
    • Journal of Welding and Joining
    • /
    • v.21 no.3
    • /
    • pp.92-98
    • /
    • 2003
  • This paper describes the numerical prediction of the thermal fatigue life of a $\mu$BGA(Micro Ball Grid Array) solder joint. Finite element analysis(FEA) was employed to simulate thermal cycling loading for solder joint reliability. Strain values, along with the result of mechanical fatigue tests for solder alloys were then used to predict the solder joint fatigue life using the Coffin-Manson equation. The results show that Sn-3.5mass%Ag solder had the longest thermal fatigue life in low cycle fatigue. Also a practical correlation for the prediction of the thermal fatigue life was suggested by using the dimensionless variable ${\gamma}$, which was possible to use several lead free solder alloys for prediction of thermal fatigue life. Furthermore, when the contact angle of the ball and chip has 50 degrees, solder joint has longest fatigue life.