• 제목/요약/키워드: Implant stability test

검색결과 109건 처리시간 0.036초

$Smartpeg^{TM}$의 고압멸균소독 및 재사용이 임플랜트 안정성 지수(ISQ) 측정에 미치는 영향 (THE EFFECT OF AUTOCLAVE STERILIZATION AND REUSE OF $SMARTPEG^{TM}$ ON THE IMPLANT STABILITY QUOTIENT (ISQ) MEASUREMENT)

  • 강인호;김명주;임영준;김창회
    • 대한치과보철학회지
    • /
    • 제45권5호
    • /
    • pp.644-652
    • /
    • 2007
  • Statement of problem: Resonance frequency analysis is evaluated as the non-invasive and objective method for the evaluation of implant stability and has been increasingly used. It is necessary to evaluate the factors affect the ISQ measurement stability. Purpose: This study was performed to evaluate the effect of the autoclave sterilization and reuse of $Smartpeg^{TM}$ on ISQ measurement. Material and methods: $SmartPeg^{TM}$ (Integration Diagnostics Ltd., $G\ddot{o}teborg$, Sweden) of autoclave group (A) was autoclave sterilized 9 times and $Smartpeg^{TM}$ of reuse group (R) was reused 9 times. Ten $SmartPeg^{TM}s$ were allocated to each group and after each autoclave sterilization and reuse, implant stability quotient (ISQ) values were measured 3 times from the two directions a and b at a right angle. $Osstell^{TM}$ mentor (Integration Diagnostics Ltd. $G\ddot{o}teborg$, Sweden) was used and type 1 (article no. 100353) $Smartpeg^{TM}$ was selected according to $Smartpeg^{TM}$ reference list. Osstem Implant US II future (Osstem Co., Seoul, Korea) in $4.0mm{\times}11.5mm$ was embedded in the self-curing acrylic resin ($Orthojet^{(R)}$, Lang Dental, U.S.A.). Data was statistically analyzed by one-way ANOVA $({\alpha}=.05)$ and scheffe test was done where a significant difference exist. Correlation test was also done between ISQ value and the number of autoclave sterilization or reuse. Results: 1. In autoclave group, the means and sd. of ISQ value before autoclave sterilization were $84.97{\pm}0.41,\;84.93{\pm}0.74$ at direction a and b. There was significant differences between autoclave groups at direction a and b (P=.000). 2. In reuse group, the means and sd. of ISQ value before reuse were $85.40{\pm}0.62,\;85.50{\pm}0.57$ at direction a and b. There was no significant difference between reuse groups at direction a and b (P>.05). 3. There was a weak positive correlation between the number of reuse and ISQ value at direction a and b (${\gamma}=.207$ and .246, P<.01). Conclusion: Within the limitations of this study, the following conclusions were drawn. Till ninth reuse of $Smartpeg^{TM}$, the ISQ measurement stability did not be affected. After twice autoclave sterilization of $Smartpeg^{TM}$ the ISQ measurement stability was affected.

Micro-CT를 이용한 맞춤형 CAD-CAM 지대주의 적합성 분석 (Fit analysis of CAD-CAM custom abutment using micro-CT)

  • 민광석;정재헌;김희중
    • 대한치과보철학회지
    • /
    • 제54권4호
    • /
    • pp.370-378
    • /
    • 2016
  • 목적: Biomet 3i 시스템과 Astra 시스템의 내측 연결형 임플란트 고정체에 국내에서 제작된 맞춤형 CAD-CAM 지대주를 체결하여 구성 성분 간의 적합성과 나사의 안정성을 평가하고자 하였다. 재료 및 방법: 24개 3i 임플란트 중 12개의 임플란트에 기성 지대주를 연결하고, 나머지 임플란트에는 맞춤형 CAD-CAM 지대주를 연결하여 각각 Group 1과 Group 2로 분류하였다. 동일 개수와 동일한 방법으로 Astra 임플란트를 각각 Group 3와 Group 4로 분류하였다. 각각의 고정체에 지대주를 장착하여 각 계면 사이의 적합성을 micro-CT로 관찰하고 초기 풀림 토크를 측정한 후 평가하였다. 결과: 고정체-지대주의 접촉길이는 Group 1과 Group 2 사이 뿐만 아니라 Group 3와 Group 4 사이에도 유의한 차이가 없었다(Mann-Whitney test, P>.05). 하지만, 지대주와 나사의 계면 및 고정체와 나사의 계면에서 Group 2와 Group 4가 Group 1와 Group 3에 비해 각기 더 큰 접촉양상을 보여주었다(Mann-Whitney test, P<.05). 또한, Group 2와 Group 4가 Group 1과 Group 3에 비해 각기 더 낮은 나사의 초기 풀림 토크를 기록하였다(Student t-test, P<.05). 결론: CAD-CAM지대주는 임상에 적용할 만한 적합성을 지니고 있으나, 광범위한 임상 적용을 위해서는 풀림 토크가 향상되어야 할 것으로 사료된다.

다양한 가상 골 결함에 따른 공진 주파수의 비교 분석 (A COMPARATIVE ANALYSIS WITH RESONANCE FREQUENCY ACCORDING TO VARIOUS SIMULATED BONE DEFECTS)

  • 김상미;박찬진;이양진;장범석;조리라
    • 대한치과보철학회지
    • /
    • 제43권4호
    • /
    • pp.487-497
    • /
    • 2005
  • Purpose: Resonance frequency analysis (RFA) , a non-invasive technique for the clinical measurement of implant stability, was investigated. Peri-implant bony defect may contribute to implant failure. This in vitro study evaluated the resonance frequencies according to various bony defects and determined whether the directional bone defect can affect the value of frequency analysis. Material and Method: Fifteen 3.75 mm in diameter and 10 mm in length, machined self-tapping implant future were used. Twelve types of bone defects that have different horizontal and vertical dimensions were simulated. Embedded implants were attached to the dental surveyor. Then, the transducer was connected with the implant fixture and the ISQ value was measured at four different directions. Two-way analysis of variance and post hoc $Sch\`{e}ffe'$ test were performed at the 95% significance level. Results: The control group showed the highest ISQ value and 5 thread-$360^{\circ}$ group had the lowest one. As the vertical exposure of implants in each angle was increased, the ISQ value was decreased. Although the horizontal exposure in each thread was increased, the ISQ value was not significantly decreased. Conclusion : Although the simulated defect type was different from each other, the ISQ value was similar among groups.

Comparison of mechanical and biological properties of zirconia and titanium alloy orthodontic micro-implants

  • Choi, Hae Won;Park, Young Seok;Chung, Shin Hye;Jung, Min Ho;Moon, Won;Rhee, Sang Hoon
    • 대한치과교정학회지
    • /
    • 제47권4호
    • /
    • pp.229-237
    • /
    • 2017
  • Objective: The aim of this study was to compare the initial stability as insertion and removal torque and the clinical applicability of novel orthodontic zirconia micro-implants made using a powder injection molding (PIM) technique with those parameters in conventional titanium micro-implants. Methods: Sixty zirconia and 60 titanium micro-implants of similar design (diameter, 1.6 mm; length, 8.0 mm) were inserted perpendicularly in solid polyurethane foam with varying densities of 20 pounds per cubic foot (pcf), 30 pcf, and 40 pcf. Primary stability was measured as maximum insertion torque (MIT) and maximum removal torque (MRT). To investigate clinical applicability, compressive and tensile forces were recorded at 0.01, 0.02, and 0.03 mm displacement of the implants at angles of $0^{\circ}$, $10^{\circ}$, $20^{\circ}$, $30^{\circ}$, and $40^{\circ}$. The biocompatibility of zirconia micro-implants was assessed via an experimental animal study. Results: There were no statistically significant differences between zirconia micro-implants and titanium alloy implants with regard to MIT, MRT, or the amount of movement in the angulated lateral displacement test. As angulation increased, the mean compressive and tensile forces required to displace both types of micro-implants increased substantially at all distances. The average bone-to-implant contact ratio of prototype zirconia micro-implants was $56.88{\pm}6.72%$. Conclusions: Zirconia micro-implants showed initial stability and clinical applicability for diverse orthodontic treatments comparable to that of titanium micro-implants under compressive and tensile forces.

치과 임플란트용 골융합 측정기의 설계 및 평가 (Design and Evaluation of Osseointegration Analysis System for Dental Implant)

  • 이주희;김창일;백종후;조정호;전명표;정영훈;이영진;이정배;이승대
    • 한국전기전자재료학회논문지
    • /
    • 제24권3호
    • /
    • pp.188-193
    • /
    • 2011
  • The osseointegration of dental implant is influenced by many factors such as surface geometry, loading and the amount of bone. Thus, stability of the dental implant should be checked periodically. In order to test the stability of dental implant by using resonance frequency analysis, we designed a structure of transducers and fabricated a piezoelectric devices. Using finite element analysis, the thickness and length of piezoelectric device and transducers were tailorized and the optimized frequency of 10 kHz was obtained. The resonance frequency from simulation analysis and evaluation was estimated to be similar as 10 kHz. The osseointegration was further enhanced with increasing frequency from the evaluation result of the finite element analysis.

Biomechanical behavior of CAD/CAM cobalt-chromium and zirconia full-arch fixed prostheses

  • Barbin, Thais;Silva, Leticia Del Rio;Veloso, Daniele Valente;Borges, Guilherme Almeida;Presotto, Anna Gabriella Camacho;Barao, Valentim Adelino Ricardo;Groppo, Francisco Carlos;Mesquita, Marcelo Ferraz
    • The Journal of Advanced Prosthodontics
    • /
    • 제12권6호
    • /
    • pp.329-337
    • /
    • 2020
  • PURPOSE. To verify the influence of computer-aided design/computer-aided manufacturing (CAD/CAM) implant-supported prostheses manufactured with cobalt-chromium (Co-Cr) and zirconia (Zr), and whether ceramic application, spark erosion, and simulation of masticatory cycles modify biomechanical parameters (marginal fit, screw-loosening torque, and strain) on the implant-supported system. MATERIALS AND METHODS. Ten full-arch fixed frameworks were manufactured by a CAD/CAM milling system with Co-Cr and Zr (n=5/group). The marginal fit between the abutment and frameworks was measured as stated by single-screw test. Screw-loosening torque evaluated screw stability, and strain analysis was explored on the implant-supported system. All analyses were performed at 3 distinct times: after framework manufacturing; after ceramic application in both materials' frameworks; and after the spark erosion in Co-Cr frameworks. Afterward, stability analysis was re-evaluated after 106 mechanical cycles (2 Hz/150-N) for both materials. Statistical analyses were performed by Kruskal-Wallis and Dunn tests (α=.05). RESULTS. No difference between the two materials was found for marginal fit, screwloosening torque, and strain after framework manufacturing (P>.05). Ceramic application did not affect the variables (P>.05). Spark erosion optimized marginal fit and strain medians for Co-Cr frameworks (P<.05). Screw-loosening torque was significantly reduced by masticatory simulation (P<.05) regardless of the framework materials. CONCLUSION. Co-Cr and Zr frameworks presented similar biomechanical behavior. Ceramic application had no effect on the biomechanical behavior of either material. Spark erosion was an effective technique to improve Co-Cr biomechanical behavior on the implant-supported system. Screw-loosening torque was reduced for both materials after masticatory simulation.

마그네슘 양극산화 임플란트의 성공률에 관한 전향적 임상연구 (A Prospective Clinical Trial on the Mg Oxidized Clinical Implants)

  • 임소민;김대곤;박찬진;조리라;엄흥식;이재관
    • 구강회복응용과학지
    • /
    • 제27권1호
    • /
    • pp.25-39
    • /
    • 2011
  • 마그네슘 양극산화 임플란트는 동물실험에서 우수한 골반응을 나타내었지만 이에 대한 임상 연구는 전무하다. 본 연구에서는 마그네슘 양극산화 임플란트의 단기간 성공률 및 안정성, 변연골 흡수량을 평가하고자 하였다. 강릉원주대학교 치과병원의 임상시험위원회의 승인을 거쳐 건강한 부분 무치악 환자에게 마그네슘 양극산화 임플란트를 식립한 후 일반적인 프로토콜에 따라 보철 치료를 시행하였다. 1차 수술, 2차 수술, 보철물 시적, 하중 후 1개월, 3개월, 6개월 평가를 시행하였으며, 매회 내원 시 임플란트 안정지수(Implant stability quotient, ISQ)를 측정하고 구내 치근단 방사선 사진에서 변연골 흡수량을 산출하였다. 반복측정이 있는 분산분석법을 이용하여 통계적 분석을 시행하였다. 총 50명에게 식립된 101개의 임플란트 중 골유착에 실패한 임플란트는 없었으며, 하중 후 6개월 성공률은 100%였다. 평균 ISQ는 시간이 경과함에 따라 증가하였으며 여성보다 남성에서, 상악보다 하악에서 높게 나타났다 (P<.05). 하중 6개월 후 골질이 양호할수록, 고정체 직경이 클수록 높은 ISQ 값을 보였다 (P<.05). 하중 후 6개월간 평균 변연골 흡수량은 0.26 mm로 관찰되었으며 하악보다 상악에서, 여성보다 남성에서 더 많은 흡수가 관찰되었다. 본 연구의 마그네슘 양극산화 임플란트의 6개월 성공률은 100%이며, 낮은 골질에서도 우수한 골유착이 관찰되었다. 안정성과 변연골 수준 또한 만족스러운 결과를 보였지만 더욱 장기적인 임상연구가 필요하다고 사료된다.

Factors Associated with the Stability of Two-part Mini-implants for Intermaxillary Fixation

  • Kim, Seong-Hun;Seo, Woon-Kyung;Lee, Won;Kim, In-Soo;Chung, Kyu-Rhim;Kook, Yoon-Ah
    • Journal of Korean Dental Science
    • /
    • 제2권2호
    • /
    • pp.24-30
    • /
    • 2009
  • Two component orthodontic C-implants have been introduced as intermaxillary fixation (IMF) screws in cases of periodontal problems with bone loss, severely damaged teeth, or short roots. This retrospective research sought to investigate the complications and risk factors associated with the failure of two-part C-implants for IMF cases and to show the possible indications compared to one-component mini-implants. The study sample consisted of 46 randomly selected patients who had a total of 203 implants. Pearson chi-square tests of independence were used to test for associations among categorical variables. At least 19 of the total 203 implants failed (9.3%). There was no significant difference in implant failure due to gender, oral hygiene, and placement, although a significant difference due to soft tissue characteristics and root contact was observed. The two-component design of the mini-implant is reliable for difficult IMF cases. Note, however, that the factors influencing implant failure were found to be age, root damage, and condition of soft tissues.

  • PDF

임플란트 지대주나사 코팅이 결합안정성에 미치는 영향 (Influence of the Dental Implant Abutment Screw Coating Materials on Joint Stability)

  • 임현필;박영선;방몽숙;양홍서;박상원;윤숙자
    • 구강회복응용과학지
    • /
    • 제25권2호
    • /
    • pp.157-169
    • /
    • 2009
  • 본 논문의 목적은 코팅처리의 기계적 성질과 임플란트 지대주나사의 코팅처리가 고정체와의 결합안정성에 미치는 영향을 연구하고자 함이다. 이를 위해 Megagen 임플란트 시스템과 직경 15 mm, 높이 1 mm의 티타늄원판을 사용하였다. 지대주 나사와 원판에 TiN, TiCN, 및 TiC를 코팅하여 실험군으로, 코팅처리하지 않은 것을 대조군으로 하였다. 실험군은 지대주나사를 32 Ncm로 체결한 후 풀림회전력과 조임회전각을 측정하고, 10만 번씩 저작 모방 시험을 실시하여 풀림회전력의 변화를 관찰하였다. 조임회전각은 TiCN, TiC코팅나사에서 코팅하지 않은 나사보다 크게 나타났다(p<0.05). 그러나 풀림회전력은 TiCN, TiC코팅나사에서 코팅하지 않은 나사보다 낮게 나타났다(p<0.05). 저작 모방 시험후 코팅한 나사에서 코팅하지 않은 나사보다 풀림 회전력이 더 높게 나타났으며 풀림회전력은 건조상태와 습윤상태 사이에 유의한 차이가 없었다. 이상의 결과로 TiC 코팅군은 저작 모방 시험 전에는 풀림회전력이 낮았지만 저작 모방 시험 후에는 낮은 마찰계수로 인한 높은 풀림회전력과 조임회전각을 가져 임플란트 지대주나사의 결합안정성에 영향을 미치는 효율적인 방법임을 시사한다.

Influence of the implant-abutment connection design and diameter on the screw joint stability

  • Shin, Hyon-Mo;Huh, Jung-Bo;Yun, Mi-Jeong;Jeon, Young-Chan;Chang, Brian Myung;Jeong, Chang-Mo
    • The Journal of Advanced Prosthodontics
    • /
    • 제6권2호
    • /
    • pp.126-132
    • /
    • 2014
  • PURPOSE. This study was conducted to evaluate the influence of the implant-abutment connection design and diameter on the screw joint stability. MATERIALS AND METHODS. Regular and wide-diameter implant systems with three different joint connection designs: an external butt joint, a one-stage internal cone, and a two-stage internal cone were divided into seven groups (n=5, in each group). The initial removal torque values of the abutment screw were measured with a digital torque gauge. The postload removal torque values were measured after 100,000 cycles of a 150 N and a 10 Hz cyclic load had been applied. Subsequently, the rates of the initial and postload removal torque losses were calculated to evaluate the effect of the joint connection design and diameter on the screw joint stability. Each group was compared using Kruskal-Wallis test and Mann-Whitney U test as post-hoc test (${\alpha}$=0.05). RESULTS. The postload removal torque value was high in the following order with regard to magnitude: two-stage internal cone, one-stage internal cone, and external butt joint systems. In the regular-diameter group, the external butt joint and one-stage internal cone systems showed lower postload removal torque loss rates than the two-stage internal cone system. In the wide-diameter group, the external butt joint system showed a lower loss rate than the one-stage internal cone and two-stage internal cone systems. In the two-stage internal cone system, the wide-diameter group showed a significantly lower loss rate than the regular-diameter group (P<.05). CONCLUSION. The results of this study showed that the external butt joint was more advantageous than the internal cone in terms of the postload removal torque loss. For the difference in the implant diameter, a wide diameter was more advantageous in terms of the torque loss rate.