Effect of dehydride atmosphere on Hydrogen concentration of Tantalum (탈수소화 분위기가 탄탈륨 분말 수소농도에 미치는 영향 연구)

  • Lee, Ji-eun;Yoon, Jin-Ho;Lee, Chan Gi
    • Journal of Industrial Technology
    • /
    • v.41 no.1
    • /
    • pp.25-30
    • /
    • 2021
  • Hydride-dehydride process for efficient recycling of tantalum (Ta) is used for manufacturer of Ta powder. In case of metal powder, Impurities as like nitride, oxygen, hydrogen is decreased of physical properties. For manufacture of Ta powder, control of theses impurities is important. In this study, to decreased of impurities on Ta powder using HDH process optimize dehydride condition. Dehydration behavior of Ta is depended on temperature, time, and atmosphere. Phase transition of Ta hydride is analyzed by X-ray diffraction (XRD). Concentration of hydrogen is decreased with temperature increased. At high temperature, concentration of hydrogen in Ta is similar according to time increased. Size and morphology of powder is not observed after dehydride. Ta powder, which is less than 20 um, concentration of hydrogen under 800 ppm is obtain.

Study on Manufacture of Tantalum Powder from Tantalum Scrap using Hydride-Dehydride Process (HDH Process) (수소화-탈수소화법을 이용한 탄탈륨 스크랩으로부터 탄탈륨 분말 제조 연구)

  • Lee, Ji-eun;Lee, Chan Gi;Park, Ji Hwan;Yoon, Jin-Ho
    • Resources Recycling
    • /
    • v.27 no.5
    • /
    • pp.30-37
    • /
    • 2018
  • For recylcing of high purity tantalum (Ta) scrap, We investigated manufacture of tantalum powder using hydride-dehydride (HDH) process. Tantalum had excellent properties such as ductile, hardness and high melting point. Usually these properties made difficult to make a powder. In this study, Tantalum powder was manufactured using Tantalum hydride via hydridation. Tantalum hydride was formed at $500^{\circ}C$, 5 hr/$700^{\circ}C$, 3 hr and it is easy to make a tantalum hydride powder because hydrogen in the tantalum act as a defect dislocation and lattice expansion. The powder was pulverized to a size of less than $10{\mu}m$ under a condition of 1300 rpm, 30 min using a ring mill, and tantalum powder with less than 50 ppm hydrogen was prepared through dehydridation in an Ar and low vacuum atmosphere.

Establishment of Process of Manufacture of Ti-6Al-4V Alloy Sintering Body by MIM

  • Otsuka, A.;Suzuki, K.;Achikita, M.
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.759-760
    • /
    • 2006
  • Ti-6Al-4V has low specific gravity, high corrosion resistance and superior mechanical properties but it is very difficult to control oxygen content in MIM process. It is necessary to use powders with coarse particle size to decrease oxygen content of powders, so feedstocks with poor fluidity and sintered bodies with lower density are obtained in such cases. Fine titanium hydride-dehydride powders were blended with atomized powders to accomplish higher fluidity and sintered density. Sintered bodies had higher sintered density and mechanical properties equivalent to those of wrought materials by controlling oxygen content less than 0.35mass%.

  • PDF

Getter Properties of Ti80-XZr20VX Alloy Powders (Ti80-XZr20VX 합금분말의 게터 특성)

  • Park, Je-Shin;Kim, Won-Baek;Soh, Chang-Youl;Cho, Sung-Wook
    • Journal of Powder Materials
    • /
    • v.16 no.1
    • /
    • pp.28-32
    • /
    • 2009
  • The activation temperatures and hydrogen sorption rates of $Ti_{80-X}Zr_{20}V_X$ alloys were evaluated at room temperature. The alloy powders were prepared by arc melting and then hydride-dehydride(HDH) process. The alloy powders were apt to activate by increase of vanadium in Ti-Zr-V alloys. The easy activation was explained in terms of surface oxygen content which decreased with increase of vanadium on Ti-Zr-V alloys.