  • Experiments on the automatic control of NaOH concentration and on the spraying condition of NaOH solution in the alkaline degreasing process of a continuous hot-dip galvanizing line have been carried out in order to improve degreasing performance of a galvanizing sheet steel using laboratory degreasing and galvanizing simulators. The concentration of NaOH for the good degreasing has been determined to be 6.0% and more and this concentration has been able to be automatically well controlled within $\pm$0.1% by employing a solution electrical conductivity meter under a flow injection analysis condition rather than by employing a sodium ion selective electrode in the degreasing simulator. Frequent blocking of the spraying nozzles of the solution has been reduced considerably by the set-up and periodical operation of an automatic valve system in the nozzle system. By applying this automatic valve system and by automatic controlling the NaOH concentration and other ordinary variables in the degreasing process, the degreasing performance has been increased from the conventional 76% to the new 85%.

  • PDF

Minimizing Zinc Consumption In Hot-Dip Galvanizing Lines

  • Bright, Mark;Ellis, Suzanne
    • Corrosion Science and Technology
    • /
    • v.10 no.2
    • /
    • pp.43-46
    • /
    • 2011
  • Zinc consumption in a continuous galvanizing line is one of the highest operating cost items in the facility and minimizing zinc waste is a key economic objective for any operation. One of the primary sources of excessive loss of zinc is through the formation of top dross and skimmings in the coating pot. It has been reported that the top skimmings, manually removed from the bath, typically consist of more than 80% metallic zinc with the remainder being entrained dross particles ($Fe_2Al_5$) along with some oxides. Depending on the drossing practices and bath management, the composition of the removed top skimmings may contain up to 2 wt% aluminum and 1 wt% iron. On-going research efforts have been aimed at in-house recovery of the metallic zinc from the discarded top skimmings prior to selling to zinc recycling brokers. However, attempting to recover the zinc entrapped in the skimmings is difficult due to the complex nature of the intermetallic dross particles and the quality and volume of the recycled zinc is highly susceptible to fluctuations in processing parameters. As such, an efficient method to extract metallic zinc from top skimmings has been optimized through the use of a specialized thermo-mechanical process enabling a continuous galvanizing facility to conserve zinc usage on-site. Also, through this work, it has been identified that filtration of discrete dross particles has been proven effective at maintaining the cleanliness of the zinc. Future efforts may progress towards expanded utilization of filters in continuous galvanizing.

A STUDY ON THE FLOW CHARACTERISTICS OF AIR-KNIFE USING A CONSTANT EXPANSION RATE NOZZLE (팽창률이 일정한 노즐을 사용한 AIR-KNIFE 유동에 관한 연구)

  • Lee, Dong-Won;Kang, Nam-Cheol;Kim, Guen-Young;Kwon, Young-Doo;Kwon, Soon-Bum
    • Journal of computational fluids engineering
    • /
    • v.13 no.4
    • /
    • pp.1-7
    • /
    • 2008
  • In the process of continuous hot-dip galvanizing, it is well known that the gas wiping through an air knife system is most effective because of its uniformity in coating thickness, possibility of thin coating, workability in high speed, and simplicity of control. However, gas wiping used in the galvanizing process brings about a problem of splashing at the strip edge above a certain high speed of process. It is also known that the problem of edge splashing is more harmful than that at the mid strip surface. For a given liquid(of a certain viscosity and surface tension), the onset of splashing mainly depends upon the strip velocity, the gas-jet pressure, and the nozzle's stand-off distance. In these connections in the present study, we proposed three kinds of air knife system having nozzles of constant expansion rate, and compared the jet structures issuing from newly proposed nozzle systems with the result by a conventional one. In numerical analysis, the governing equations are consisted of two-dimensional time dependent Navier-Stokes equations, and the standard k-${\varepsilon}$ turbulence model is employed to solve turbulence stress and so on. As the result, it is found that we had better use the constant expansion-rate nozzle which can be interpreted from the point view of the energy saving for the same coating thickness. Also, we better reduce the size of separation bubble and enhance the cutting ability at the strip surface, by using an air-knife having constant expansion-rate nozzle.

Study of Characteristics of Hot Dip Galvanized Steel Strip by Oxygen-free Finishing (비산화성 분위기에 의한 용융아연도금의 특성 연구)

  • 진영구;김흥윤
    • Journal of the Korean institute of surface engineering
    • /
    • v.28 no.5
    • /
    • pp.300-308
    • /
    • 1995
  • The effect of nitrogen finishing for the control of coating weight in a nitrogen sealing box on the coating surface property in hot dip galvanizing process has been studied. The coated surface is free of oxide marks and edge overcoated. The coating uniformity is excellent ; the standard deviation of the coating thickness along width of the specimen was $1~1.2\mu\textrm{m}$ in the box whereas $2.5~3\mu\textrm{m}$ in the air. Considering surface quality of the coating such as oxide mark, edge overcoated and zinc dust, the oxygen content between 40 and 200 ppm was suggested in the box in addition the oxygen content of at least 40 ppm or the minimum dew point of $-27^{\circ}C$ is required to prevent a zinc vaporization.

  • PDF

The Development of Coating Weight Model and Control Logics in Continuous Galvanizing Line

  • Kook, Chae-Hong;Tae, Shin-Ki
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 2001.10a
    • /
    • pp.121.5-121
    • /
    • 2001
  • For the last decade, remarkable progress in the coating weight uniformity of hot dip galvanized product has been made to overcome the tightening quality constraints and produce cost-effective galvanized products. This progress results from research and development works for more efficient air knife, more accurate model of coating process, more precise measurement of coating weight and more efficient control logics. The activities for an efficient mathematical model to predict coating weight and several control logics which has been implemented on the No.1 CGL, No. 2 CGL, and PGL at KwangYang Steel Works are reviewed in this article.

  • PDF

Effect of Ni Addition Interfacial Reaction and Corrosion Resistance in Hot Dip Galvanizing (용융안연 도금욕의 Ni첨가가 도금강판의 게면반응 및 내식성에 미치는 영향)

  • 이경구;시희봉;이도재
    • Journal of the Korean institute of surface engineering
    • /
    • v.31 no.6
    • /
    • pp.379-388
    • /
    • 1998
  • The iron-zinc interfacial reaction and corrosin properties in galvanizing bath containning Ni have been intestigated. The substrate steel plates were galvanized in Zn or Zn-0.018Al baths with various Ni contents. The corrosion resistance of galvanized specimens was also evaluated by $60^{\circ}$bending test for galvannealing speaaimens. The corrosion resistance was improved with Ni addition in pure Zn bath, while deteriorated with Ni addition in Zn-0.18Al bath. The anti-powdering property, on thhe otherhand, was improved with Ni addition in Zn-0.18Al bath, while deteriorated with Ni addition in pure Zn. It was found that the anti-powdering property was improved with increasing $\xi$ phase ratio in reaction layer.

  • PDF

Influence of Coating Conditions on Fe Dissolution and Dross Formation in Continuous Hot-dip Galvanizing Process (연속 용융아연도금 공정에서 Fe용출 및 드로스 발생에 미치는 도금조건의 영향)

  • 전선호;김상헌
    • Journal of the Korean institute of surface engineering
    • /
    • v.36 no.5
    • /
    • pp.364-372
    • /
    • 2003
  • In continuous galvanizing process, dissolution of iron into molten zinc results in a fairly great amount of dross. In order to decrease dross, the amount of dissolved iron of strip in molten zinc was investigated in the range of 0∼0.22%Al content, 440∼$470^{\circ}C$ strip temperature and 3∼60 sec dipping time. Uniform Fe-Al-Zn inhibition layer was formed in the coating layer/strip interface not only in the grain boundary but also in the grain of substrate with the increase of Al content in the zinc pot, while the amount of iron dissolution was decreased. Inhibition layer was unstable as the dipping time and strip temperature increased and the amount of iron dissolution increased.

Influence of Selective Oxidation Phenomena in CGLs on Galvanized Coating Defects Formation

  • Gong, Y.F.;Birosca, S.;Kim, Han S.;De Cooman, B.C.
    • Corrosion Science and Technology
    • /
    • v.7 no.1
    • /
    • pp.1-5
    • /
    • 2008
  • The gas atmosphere in continuous annealing and galvanizing lines alters both composition and microstructure of the surface and sub-surface of sheet steel. The formation and morphology of the oxides of alloying elements in High Strength Interstitial Free (HS-IF), Dual Phase (DP) and Transformation-Induced Plasticity (TRIP) steels are strongly influenced by the furnace dew point, and the presence of specific oxide may result in surface defects and bare areas on galvanized sheet products. The present contribution reviews the progress made recently in understanding the selective formation of surface and subsurface oxides during annealing in hot dip galvanizing and conventional continuous annealing lines. It is believed that the surface and sub-surface composition and microstructure have a pronounced influence on galvanized sheet product surface quality. In the present study, it is shown that the understanding of the relevant phenomena requires a combination of precise laboratory-scale simulations of the relevant technological processes and the use of advanced surface analytical tools.

Corrosion Analysis of Materials by High Temperature and Zn Fume (고온 및 Zn Fume에 의한 소재들의 부식성 분석)

  • Baek, Min Sook
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.5
    • /
    • pp.551-556
    • /
    • 2018
  • The material normally used in hot dip galvanizing facilities is SM45C (carbon steel for mechanical structure, KS standard), mainly because of its price. During this process, the oxidation of the plating facility occurs due to the heat of the Zn fumes coming from the molten zinc. Since the cycle time of the current facilities is 6 months, much time and money are wasted. In this study, the corrosive properties of various materials (Inconel625, STS304, SM45C) were investigated by oxidation in a high temperature and Zn fumes environment. The possibility of applying the hot-dip galvanizing equipment was investigated for each material. The Zn fumes were generated by directly bubbling Ar gas into Zn molten metal in a 650 degree furnace. High-temperature, Zn fumes corrosion was conducted for 30 days. The sample was removed after 30 days and the oxidation of the surface was confirmed with EDS and SEM, and the corrosion properties were examined using potentiodynamic polarization tests.

Corrosion analysis for application of CCO thin films to industrial equipment materials (산업 설비 재료에 CCO박막의 적용을 위한 부식성 분석)

  • Baek, Min Sook
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.19 no.6
    • /
    • pp.98-103
    • /
    • 2018
  • Many coating technologies have been developed so far to improve the corrosion resistance, strength, abrasion resistance and other surface properties of materials and equipment. Among them, the formation of CCO (CaCoO, then CCO) thin films has been studied and used in the electronic material field. One of the characteristics of CCO thin films is that it is resistant to high temperature heat. Particularly, the method of forming the CCO thin film is relatively simple, and it was judged that it could be introduced into the existing equipment. Therefore, in this study, an experiment and analysis were carried out to determine whether the coating of CCO thin films can be applied to hot dip galvanizing facilities. A CCO thin film was formed on the surface of STS304 base material and oxidized in a Zn fume atmosphere in a $650^{\circ}C$ furnace with an air atmosphere. Oxidation was carried out for 30 days, after which the shape of the CCO thin film was confirmed by SEM and its corrosivity was analyzed through a potentiodynamic polarization experiment.