Preliminary Study on Rapid Measurement of Gross Alpha/Beta and 90Sr Activities in Surface Soil by Mobile ZnS(Ag)/PTV Array and Handheld PVT Rod with Gated Energy Channels

  • Lee, Chanki;Kim, Hee Reyoung
    • Journal of Radiation Protection and Research
    • /
    • 제46권4호
    • /
    • pp.194-203
    • /
    • 2021
  • Background: Surface soil radiation monitoring around nuclear facilities is important to classify and characterize the contaminated areas. A scanning and direct measurement technique can survey the sites rapidly before starting sampling analysis. Materials and Methods: Regarding this, we test and suggest a measurement technique for gross alpha/beta and 90Sr activities in surface soil based on a mobile ZnS(Ag)/PVT (polyvinyltoluene) array and a handheld PVT rod, respectively. To detect 90Sr selectively in soil mixed with naturally occurring radioactive materials, chosen energy channel counts from the multichannel analyzers were used instead of whole channel counts. Soil samples contaminated with exempt liquid 90Sr with 1 Bq·g-1, 3 Bq·g-1, and 10 Bq·g-1 were prepared and hardened by flocculation. Results and Discussion: The mobile ZnS(Ag)/PVT array could discriminate gross alpha, gross beta, and gamma radiation by the different pulse-shaped signal features of each sensor material. If the array is deployed on a vehicle, the scan minimum detectable concentration (MDC) range will be about 0.11-0.17 Bq·g-1 at 18 km·h-1 speed, highly sensitive to actual sites. The handheld PVT rod with 12 mm (Φ) × 20 mm (H) size can directly measure 90Sr selectively if channels on which energies are from 1,470 and 2,279 keV are gated, minimizing crossdetection of other radionuclides. These methods were verified by measuring soil samples fabricated with homogeneous 90Sr concentrations, showing static MDC of 2.16 Bq·g-1 at a measurement time of 300 seconds. Conclusion: Based on the results, comprehensive procedures using these detectors are suggested to optimize soil sites survey.

가속열 노화로 열화된 탄성받침 고무재료의 전단 특성(1): 천연고무 (Shear Characteristics of Elastomeric Bearing Rubber Deteriorated by Accelerated Heat Aging(1): Natural Rubber)

  • 선창호;김익현
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제25권6호
    • /
    • pp.95-102
    • /
    • 2021
  • 유연한 고무재료를 사용하는 탄성받침은 최근 교량의 내진보강용으로 많이 적용되고 있다. 그러나 다양한 요인에 의하여 고무재료의 노화가 진행되고 이로 인해 탄성받침의 전단강성에 변화가 생기고 이는 교량의 내진성능에 영향을 미친다. 천연고무를 대상으로 노화촉진시간과 노출시간을 변수로 하여 노화촉진시험을 수행하여 전단특성의 변화를 분석하였다. 노화가 진행될수록(노화촉진온도 및 노출시간이 증가할수록) 최대전단응력과 전단변형율은 감소한다. 또한 동일한 전단변형률에서 전단강성이 크게 증가한다. 이는 고무재료가 경화됨을 의미하며 탄성받침의 내진성능이 저하되는 것을 암시한다.

고로슬래그미분말 및 강섬유를 적용한 고유동 흙막이 벽체 재료의 성능 평가 (Performance of High-Flowable Retaining Wall Material Using Ground Granulated Blast-Furnace Slag and Steel Fiber)

  • 김동규;유강민;이승태
    • 한국지반환경공학회 논문집
    • /
    • 제23권11호
    • /
    • pp.5-11
    • /
    • 2022
  • 본 연구는 고로슬래그미분말(SG) 및 강섬유(SF)를 적용한 고유동 흙막이 벽체 재료(RWM)의 역학적 성능을 평가하기 위한 것으로써, 흙막이 벽체 재료의 재료분리저항성, 유동성, 연행공기량을 확보하기 위하여 고성능감수제, 공기연행제 및 증점안정화제를 굳지 않은 흙막이 벽체 재료에 적정량을 사용하였다. 흙막이 벽체 재료 경화체의 강도특성을 고찰하기 위하여 압축, 할열 인장 및 휨강도를 소정의 재령에서 측정하였으며, 표면전기저항, 흡수율 실험을 통하여 흙막이 벽체 재료의 역학적 성능을 평가하였다. 실험결과에 따르면 SGC 배합은 OPC 배합에 비하여 대체적으로 우수한 성능을 나타내었으며, SF는 흙박이 벽체 재료의 역학적 성능향상에 효과적인 것으로 조사되었다. 특히, SG의 사용은 흙막이 벽체 재료의 장기강도 발현 뿐만 아니라 차수성능 향상에 기여할 것으로 판단된다.

Reactivity of aluminosilicate materials and synthesis of geopolymer mortar under ambient and hot curing condition

  • Zafar, Idrees;Tahir, Muhammad Akram;Hameed, Rizwan;Rashid, Khuram;Ju, Minkwan
    • Advances in concrete construction
    • /
    • 제13권1호
    • /
    • pp.71-81
    • /
    • 2022
  • Aluminosilicate materials as precursors are heterogenous in nature, consisting of inert and partially reactive portion, and have varying proportions depending upon source materials. It is essential to assess the reactivity of precursor prior to synthesize geopolymers. Moreover, reactivity may act as decisive factor for setting molar concentration of NaOH, curing temperature and setting proportion of different precursors. In this experimental work, the reactivities of two precursors, low calcium (fly ash (FA)) and high calcium (ground granulated blast furnace slag (GGBS)), were assessed through the dissolution of aluminosilicate at (i) three molar concentrations (8, 12, and 16 M) of NaOH solution, (ii) 6 to 24 h dissolution time, and (iii) 20-100℃. Based on paratermeters influencing the reactivity, different proportions of ternary binders (two precursors and ordinary cement) were activated by the combined NaOH and Na2SiO3 solutions with two alkaline activators to precursor ratios, to synthesize the geopolymer. Reactivity results revealed that GGBS was 20-30% more reactive than FA at 20℃, at all three molar concentrations, but its reactivity decreased by 32-46% with increasing temperature due to the high calcium content. Setting time of geopolymer paste was reduced by adding GGBS due to its fast reactivity. Both GGBS and cement promoted the formation of all types of gels (i.e., C-S-H, C-A-S-H, and N-A-S-H). As a result, it was found that a specified mixing proportion could be used to improve the compressive strength over 30 MPa at both the ambient and hot curing conditions.

Effect of GGBS and fly ash on mechanical strength of self-compacting concrete containing glass fibers

  • Kumar, Ashish;Singh, Abhinav;Bhutani, Kapil
    • Advances in concrete construction
    • /
    • 제12권5호
    • /
    • pp.429-437
    • /
    • 2021
  • In the era of building engineering the intensification of Self Compacting Concrete (SCC) is world-shattering magnetism. It has lot of rewards over ordinary concrete i.e., enrichment in production, cutback in manpower, brilliant retort to load and vibration along with improved durability. In the present study, the mechanical strength of CM-2 (SCC containing 10% of rice husk ash (RHA) as cement replacement and 600 grams of glass fibers per cubic meter) was investigated at various dosages of cement replacement by fly ash (FA) and GGBS. A total of 17 SCC mixtures including two control SCC mixtures (CM-1 and CM-2) were developed for investigating fresh and hardened properties in which, ten ternary cementitious blends of SCC by blending OPC+RHA+FA, OPC+RHA+GGBS and five quaternary cementitious blends (OPC+RHA+FA+GGBS) at different replacement dosages of FA and GGBS were developed with reference to CM-2. For constant water-cement ratio (0.42) and dosage of SP (2.5%), the addition of glass fibers (600 grams/m3) in CM-1 i.e., CM-2 shows lower workability but higher mechanical strength. While fly ash based ternary blends (OPC+RHA+FA) show better workability but lower mechanical strength as FA content increases in comparison to GGBS based ternary blends (OPC+RHA+GGBS) on increasing GGBS content. The pattern for mixtures appeared to exhibit higher workablity as that of the concentration of FA+GGBS rises in quaternary blends (OPC+RHA+FA+GGBS). A decrease in compressive strength at 7-days was noticed with an increase in the percentage of FA and GGBS as cement replacement in ternary and quaternary blended mixtures with respect to CM-2. The highest 28-days compressive strength (41.92 MPa) was observed for mix QM-3 and the lowest (33.18 MPa) for mix QM-5.

철강산업부산물을 사용한 방조제용 그라우트 재료 및 그 특성 (Properties of Grout Material for Seawall Using Slags from Steel Making Industry)

  • 김하석;김기석 ;백봉현;육심훈
    • 한국건설순환자원학회논문집
    • /
    • 제10권4호
    • /
    • pp.523-530
    • /
    • 2022
  • 해수의 흐름이 존재하는 방조제 제체 보강공사 시 가장 큰 문제는 재료의 유출로, 콘크리트의 중력식 타설은 원활히 공극을 채우기 어렵고 굳지 않은 콘크리트의 시멘트는 해수에 분산될 확률이 높기 때문에 경화 후 품질의 신뢰성이 저하될 뿐만 아니라, 인근 환경에 악역향을 끼칠 수 있다. 이에 주입이 가능한 겔형태의 주입재가 필요하다, 본 연구에서는 급결성을 띠는 전기로환원슬래그 및 고로슬래그를 활용하여 초기 강도와 해수 침지에 따른 내구성 향상 효과를 평가하였다, 실험 결과 실리카계 약액과의 반응을 통해 흐름성을 갖는 겔형태의 주입재 제조가 가능하였으며 겔의 흐름성은 배합에 따라 105~143 mm 수준으로 현장모사 시험을 통해 외부 유출 없이 공극을 채울 수 있어 현장 적용성을 확인하였다.

The effects of limestone powder and fly ash as an addition on fresh, elastic, inelastic and strength properties of self-compacting concrete

  • Hilmioglu, Hayati;Sengul, Cengiz;Ozkul, M. Hulusi
    • Advances in concrete construction
    • /
    • 제14권2호
    • /
    • pp.93-102
    • /
    • 2022
  • In this study, limestone powder (LS) and fly ash (FA) were used as powder materials in self-compacting concrete (SCC) in increasing quantities in addition to cement, so that the two powders commonly used in the production of SCC could be compared in the same study. Considering the reduction of the maximum aggregate size in SCC, 10 mm or 16 mm was selected as the coarse aggregate size. The properties of fresh concrete were determined by slump flow (including T500 time), V-funnel and J-ring experiments. The experimental results showed that as the amount of both LS and FA increased, the slump flow also increased. The increase in powder material had a negative effect on V-funnel flow times, causing it to increase; however, the increase in FA concretes was smaller compared to LS ones. The increase in the powder content reduced the amount of blockage in the J-ring test for both aggregate sizes. As the hardened concrete properties, the compressive and splitting strengths as well as the modulus of elasticity were determined. Longitudinal and transverse deformations were measured by attaching a special frame to the cylindrical specimens and the values of Poisson's ratio, initiation and critical stresses were obtained. Despite having a similar W/C ratio, all SCC exhibited higher compressive strength than NVC. Compressive strength increased with increasing powder content for both LS and FA; however, the increase of the FA was higher than the LS due to the pozzolanic effect. SCC with a coarse aggregate size of 16 mm showed higher strength than 10 mm for both powders. Similarly, the modulus of elasticity increased with the amount of powder material. Inelastic properties, which are rarely found in the literature for SCC, were determined by measuring the initial and critical stresses. Crack formation in SCC begins under lower stresses (corresponding to lower initial stresses) than in normal concretes, while critical stresses indicate a more brittle behavior by taking higher values.

Coconut shell waste as an alternative lightweight aggregate in concrete- A review

  • Muhammad Fahad, Ejaz;Muhammad ,Aslam;Waqas, Aziz;M. Jahanzaib, Khalil;M. Jahanzaib, Ali;Muhammad, Raheel;Aayzaz, Ahmed
    • Advances in materials Research
    • /
    • 제11권4호
    • /
    • pp.299-330
    • /
    • 2022
  • This review article highlights the physical, mechanical, and chemical properties of coconut shells, and the fresh and hardened properties of the coconut shell concrete are summarized and were compared with other types of aggregates. Furthermore, the structural behavior in terms of flexural, shear, and torsion was also highlighted, with other properties including shrinkage, elastic modulus, and permeability of the coconut shell concrete. Based on the reviewed literature, concrete containing coconut shell as coarse aggregate with normal sand as fine showed the 28-day compressive strength between 2 and 36 MPa with the dried density range of 1865 to 2300 kg/m3. Coconut shell concretes showed a 28-day modulus of rupture and splitting tensile strength values in the ranges of 2.59 to 8.45 MPa and 0.8 to 3.70 MPa, respectively, and these values were in the range of 5-20% of the compressive strength. The flexural behavior of CSC was found similar to other types of lightweight concrete. There were no horizontal cracks on beams which indicate no bond failure. Whereas, the diagonal shear failure was prominent in beams with no shear reinforcements while flexural failure mode was seen in beams having shear reinforcement. Under torsion, CSC beams behave like conventional concrete. Finally, future recommendations are also suggested in this study to investigate the innovative lightweight aggregate concrete based on the environmental and financial design factors.

A Study on Ability of Cognitive Impairment According for Decreased Balance Function of Pneumoconiosis Patients

  • Tae Hoon Lee;Sang Seok Yeo
    • The Journal of Korean Physical Therapy
    • /
    • 제35권4호
    • /
    • pp.111-116
    • /
    • 2023
  • Purpose: Pneumoconiosis is a chronic lung disease in which the lungs become hardened due to the accumulation of fine mineral dust that has been breathed in at industrial sites. The lungs are unable to function properly, resulting in complications of several respiratory diseases. Methods: The subjects were 36 elderly adults (pneumoconiosis patients 18, healthy elderly 18) over the age of 65 years. The respiratory function was assessed using a spirometer to measure forced vital capacity (FVC), first second of forced expiration (FEV1), FEV1/FVC, and peak expiratory flow n(PEF). The static balance function test was determined by the center of mass (COM), ankle angle range, hip angle range, sway parameters, and reciprocal compensatory index (RCI). Cognitive function was measured by applying MoCA-k. Results: Comparison of respiration functions between the two groups showed statistically significant differences in FVC, FEV1, FEV1/FVC, and PEFs (p<0.05). Cognitive abilities showed statistically significant differences due to higher cognitive skills in the control group as compared to the patient group (p<0.05). Most results of the static balance capability measurements showed statistically significant differences between the groups (p<0.05). However, no statistically significant differences were obtained for COM AP Range, Angle AP Range, RCI ML Range, and AP Range (p>0.05). Conclusion: The results of the current study indicate that patients suffering from pneumoconiosis have less cognitive ability and balance function as compared to healthy elderly people. Therefore, we expect an improvement in the balance ability and cognitive function through systematic management and strengthening lung function training to improve the quality of life of pneumoconiosis patients.

Effects of heat and gamma radiation on the degradation behaviour of fluoroelastomer in a simulated severe accident environment

  • Inyoung Song ;Taehyun Lee ;Kyungha Ryu ;Yong Jin Kim ;Myung Sung Kim ;Jong Won Park;Ji Hyun Kim
    • Nuclear Engineering and Technology
    • /
    • 제54권12호
    • /
    • pp.4514-4521
    • /
    • 2022
  • In this study, the effects of heat and radiation on the degradation behaviour of fluoroelastomer under simulated normal operation and a severe accident environment were investigated using sequential testing of gamma irradiation and thermal degradation. Tensile properties and Shore A hardness were measured, and thermogravimetric analysis was used to evaluate the degradation behaviour of fluoroelastomer. Fourier transform infrared spectroscopy and X-ray photoelectron spectroscopy were used to characterize the structural changes of the fluoroelastomer. Heat and radiation generated in nuclear power plant break and deform the chemical bonds, and fluoroelastomer exposed to these environments have decreased C-H and functional groups that contain oxygen and double bonds such as C-O, C=O and C=C were generated. These functional groups were formed by auto oxidation by reacting free radicals generated from the cleaved bond with oxygen in the atmosphere. In this auto oxidation reaction, crosslinks were generated where bonded to each other, and the mobility of molecules was decreased, and as a result, the fluoroelastomer was hardened. This hardening behaviour occurred more significantly in the severe accident environment than in the normal operation condition, and it was found that thermal stability decreased with the generation of unstable structures by crosslinking.