Combustion Characteristics of Bamboo Charcoal Boards (대나무숯 성형보드의 연소특성)

  • Park, Sang-Bum;Park, Joo-Saeng
    • Journal of the Korean Wood Science and Technology
    • /
    • v.40 no.1
    • /
    • pp.19-25
    • /
    • 2012
  • The fire retardant bamboo charcoal (BC) boards were manufactured for interior building materials in this study, The BC boards were manufactured by mixing and pressing of the bamboo charcoal, expanded vermiculite, and inorganic binder. The combustion behaviors of the BC boards were investigated using a cone calorimeter at an incident heat flux of 50 kW/$m^2$. Three building materials (plywood, BC board of Japan, and gypsum board) were used to observe the burning behaviors of weight loss, total heat release rate, and maximum heat release rate. Surface test and toxicity evaluation of the BC board were also conducted. The weight loss of the BC board (12.0%) was lower than the nonflammable gypsum board (15.6%) after burning of 10 min. Total heat release of the BC was 3 MJ/$m^2$ (KS standard 8 MJ/$m^2$) and total heat release rate of the BC was 20 kW/$m^2$ (KS standard 200 kW/$m^2$). Therefore, the BC boards were adjustable for the third-grade flame retardant building materials. External appearance change and mouse toxicity were not found in the BC boards after the combustion test.

Analysis on Material Characteristics of Restored Areas with Mortar and Basis of Surface Deterioration on the Stupa of State Preceptor Jigwang from Beopchensaji Temple Site in Wonju, Korea (원주 법천사지 지광국사탑 복원부 모르타르 재료학적 특징 및 표면손상 기초 해석)

  • Chae, Seung A;Cho, Ha Jin;Lee, Tae Jong
    • Journal of Conservation Science
    • /
    • v.37 no.5
    • /
    • pp.411-425
    • /
    • 2021
  • The Stupa of State Preceptor Jigwang from Beopcheonsa Temple Site in Wonju (National Treasure) is a representative stupa of the Goryeo Dynasty, with outstanding Buddhist carvings and splendid patterns, clearly indicating its honoree and year of construction. However, it was destroyed by bombing during the Korean War (1950-1953) and repaired and restored with cement and reinforcing bars in 1957. The surface condition of the original stone shows long-term deterioration due to the m ortar used in past restorations. In order to identify the exact causes of deterioration, the m ortar and surface contaminants on the original stone were analyzed. Portlandite, calcite, ettringite, and gypsum from the mortar were identified, and its ongoing deterioration was observed through pH measurements and the neutralization reaction test. Analysis of surface contaminants identified calcite and gypsum, both poorly water-soluble substances, and their growth in volume among rock-forming minerals was observed by microscopy. Based on those results, semi-quantitative analysis of Ca and S contents significantly influencing the formation of salt crystals was conducted using P-XRF to analyze the basis of surface deterioration, and cross-validation was performed by comparing the body stone affected by the mortar and the upper stylobate stone unaffected by the mortar. Results indicate that the elements are directly involved in the surface deterioration of the body stone.

A study on the asperity degradation of rock joint surfaces using rock-like material specimens (유사 암석 시편을 사용한 암석 절리면 돌출부 손상 연구)

  • Hong, Eun-Soo;Kwon, Tae-Hyuk;Cho, Gye-Chun
    • Journal of Korean Tunnelling and Underground Space Association
    • /
    • v.11 no.3
    • /
    • pp.303-314
    • /
    • 2009
  • Image analyses for sheared joint specimens are performed to study asperity degradation characteristics with respect to the roughness mobilization of rock joints. Four different types of joint specimens, which are made of high-strength gypsum materials, are prepared by replicating the three-dimensional roughness of rock joints. About twenty jointed rock shear tests are performed at various normal stress levels. The characteristic and scale of asperity degradation on the sheared joint specimens are analyzed using the digital image analysis technique. The results show that the asperity degradation characteristic mainly depends on the normal stress level and can be defined by asperity failure and wear. The asperity degradation develops significantly around the peak shear displacement and the average amount of degraded asperities remains constant with further displacement because of new degradation of small scale asperities. The shear strength results using high-strength gypsum materials can not fully represent physical properties of each mineral particles of asperities on the natural rock joint surface. However the results of this quantitative estimation for the relationship between the peak shear displacement and the asperity degradation suggest that the characterization of asperity degradation provides an important insight into mechanical characteristics and shear models of rock joints.

Analysis of mechanical properties of secondary concrete products using CO2 captured material (이산화탄소 고정 탄산화물을 적용한 콘크리트 2차 제품의 기초 특성 분석)

  • Hye-Jin Yu;Sung-Kwan Seo;Kuem-Dan Park;Hyuk-Joon Kwon;Jeong-Hwan Kim
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.34 no.2
    • /
    • pp.66-72
    • /
    • 2024
  • In this study, the applicability of CCMs (Carbondioxide conversion capture materials) manufactured by reacting carbon dioxide gas with DG (Desulfurization gypsum) as a cement substitute for secondary concrete products were evaluated and the basic physical properties of CCMs-mixed mortar and concrete specimens were measured to derive the optimal mixing ratio. The main chemical oxides of CCMs were CaO and SO3, and the main crystalline phases were CaSO4·2H2O, Ca(OH)2, CaCO3, and CaSO4. In addition, by the results of particle size analysis and heavy metal measurement, the applicability of CCMs as a cement substitute for secondary concrete products was confirmed. As a result of measuring the strength behavior using mortar and concrete specimens with CCMs, the compressive and flexural strength decreased as the mix ratio of CCMs increased, but requirements by the standards for interlocking blocks and retaining wall blocks, which are target products in this study, were satisfied up to the optimal mixing ratio of 10 wt.% substitution. Therefore, its applicability as a cement substitute for secondary concrete products was confirmed.

A Study on the Review of Repair Methods and Repair Materials for the Prevention of Fire spread of Building Exterior Materials (건축물 외장재의 화재확대방지를 위한 보수구법 및 보수재료 검토에 관한 연구)

  • Lee, Byeong-Heun;Jin, Seung-Hyeon;Park, Sung-Ha;Kwon, Young-Jin
    • Fire Science and Engineering
    • /
    • v.33 no.3
    • /
    • pp.105-111
    • /
    • 2019
  • In Korea, the results of a field survey on the construction of flammable exterior materials implemented in 2018 revealed that 147,559 buildings belong to this category. It was found that the fire spreading cases in upper and adjacent constructions are about 3,500 per year, the fires of starting in flammable exterior material are about 1,500 per year. In this study, we investigated the repair method of buildings constructed by flammable exterior material and conducted performance verification of each repair materials for prevention of similar fire. In the case of the repair method, a method of reinforcing with a repair material after removing the existing building finishing material and a method of attaching the repair material after performing the face finishing are proposed. In addition, we conducted cone calorimeter tests of 6 materials such as fireproof gypsum board, mineral wool, hard urethane foam, ceramic board and ALC panel as dryvit and repairing materials, and investigated basic combustion performance of that materials.

Improvement of Blast Furnace Slag Mortar Using the Recycled Fine Aggregates Depending on Improvement Material Type and Replacement Ratio (품질향상재 종류 및 치환율 변화에 따른 순환잔골재 사용 고로슬래그 모르타르의 품질향상)

  • Han, Cheon-Goo;Kim, Dae-Gun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.1
    • /
    • pp.76-83
    • /
    • 2012
  • In this study, the research examined the effect on FC, WG, RP replacement ratio on the quality improvement of BS mortar using the RA. First of all, the flow value increased as the FC contents increased, and decreased as the WG and RP contents increased. The air contents was reduced as the FC and RP contents increased, but was increased as the WG contents went up While the compressive strength of 1 : 7 mix proportion increased with the increase of the FC and WG contents, it decreased as there was more RP contents. The compressive strength of RP could increase as the mix proportion increased, but the difference depending on the improvement material type and replacement ratio decreased gradually. The absorption deteriorated as the FC and RP contents increased in all the mix proportions, but improved a little when WG was used. Meanwhile, the absorption decreased as the compressive strength improved in all the mix proportions as a correlation, but the order was FC, RP and WG depending on the quality improvement material types. The FC and WG were most favorable in terms of quality improvement as a total analysis, and the RP and WG was most effective in terms of economical efficiency and resource recycling.

  • PDF

The Initiation of Slip on Frictional Fractures (마찰 전단면의 전단거동과 에너지방출률)

  • Park, Chi-Hyun
    • Tunnel and Underground Space
    • /
    • v.20 no.5
    • /
    • pp.344-351
    • /
    • 2010
  • Slip along a frictional fracture can be approached as initiation and propagation of a mode II crack along its own plane. Fracture mechanics theories predict that under pure mode II loading initiation will occur when the energy release rate of the fracture attains a critical value ($G_{IIC}$), which is generally taken as a material property. For the past few years the rock mechanics group at Purdue University has investigated experimentally the dependence of $G_{IIC}$ on normal stress and on the frictional characteristics of a fracture. A number of experiments has been conducted first on acrylic, a material that, using photoelastic methods, allows visualization of the stress field ahead of the fracture tip; and later on gypsum, a rock model material with relatively low unconfined compression strength. The experimental investigation has been expanded to include other frictional materials with higher unconfined compression strength. Direct shear tests have been conducted on specimens made with cement paste. New observations together with previous experiments indicate that $G_{IIC}$ can only be considered a material property when the peak friction angle of the discontinuity is similar to the residual friction angle; otherwise the critical energy release rate increases with normal stress.

Identification of the Environmentally Problematic Input/Environmental Emissions and Selection of the Optimum End-of-pipe Treatment Technologies of the Cement Manufacturing Process (시멘트 제조공정의 환경적 취약 투입물/환경오염물 파악 및 최적종말처리 공정 선정)

  • Lee, Joo-Young;Kim, Yoon-Ha;Lee, Kun-Mo
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.39 no.8
    • /
    • pp.449-455
    • /
    • 2017
  • Process input data including material and energy, process output data including product, co-product and its environmental emissions of the reference and target processes were collected and analyzed to evaluate the process performance. Environmentally problematic input/environmental emissions of the manufacturing processes were identified using these data. Significant process inputs contributing to each of the environmental emissions were identified using multiple regression analysis between the process inputs and environmental emissions. Optimum combination of the end-of-pipe technologies for treating the environmental emissions considering economic aspects was made using the linear programming technique. The cement manufacturing processes in Korea and the EU producing same type of cement were chosen for the case study. Environmentally problematic input/environmental emissions of the domestic cement manufacturing processes include coal, dust, and $SO_x$. Multiple regression analysis among the process inputs and environmental emissions revealed that $CO_2$ emission was influenced most by coal, followed by the input raw materials and gypsum. $SO_x$ emission was influenced by coal, and dust emission by gypsum followed by raw material. Optimization of the end-of-pipe technologies treating dust showed that a combination of 100% of the electro precipitator and 2.4% of the fiber filter gives the lowest cost. The $SO_x$ case showed that a combination of 100% of the dry addition process and 25.88% of the wet scrubber gives the lowest cost. Salient feature of this research is that it proposed a method for identifying environmentally problematic input/environmental emissions of the manufacturing processes, in particular, cement manufacturing process. Another feature is that it showed a method for selecting the optimum combination of the end-of-pipe treatment technologies.

Engineering Research on the Burial Ground Materials of the Buried Cultural Assets in Andong (안동지역 매장문화재 중 매장지반재료의 공학적 특성)

  • Park, Hyeong-Dong;Hwang, Ji-Ho;Kim, Sung-Soo
    • Journal of Conservation Science
    • /
    • v.8 no.1 s.11
    • /
    • pp.51-57
    • /
    • 1999
  • Although the mummies of Lee, Myeong-Jung and his wife whose family name is Moon, were buried in similar sites in 1560's, the degree of decay of the dead bodies and antiquities between two people were quite different. This study was focused on the cause of those differences in the view of engineering concept. Granular soil around the study site shows good drainage and such characteristic could be a factor of excellent conservation of dead body. From the physical characteristics of the material containing lime that is considered to be a barrier from water and air, it was observed that the material around dead body of the wife was more compact and denser than that of the husband. This may suggest that the former is better than the latter in keeping away from the water and air. To understand those differences of physical characteristics between two materials containing lime, minerals had to be identified from the two materials. It was revealed that material containing lime around dead body of the wife contains gypsum and more calcite, which could be the reason for better barrier Preventing from water and air than that around the husband.

  • PDF

The Mineral Carbonation Using Steelmaking Reduction Slag (제강 환원슬래그의 광물탄산화)

  • Ryu, Kyoung-Won;Choi, Sang-Hoon
    • Economic and Environmental Geology
    • /
    • v.50 no.1
    • /
    • pp.27-34
    • /
    • 2017
  • Mineral carbonation for the storage of carbon dioxide is a CCS option that provides an alternative for the more widely advocated method of geological storage in underground formation. Carbonation of magnesium- or calcium-based minerals, especially the carbonation of waste materials and industrial by-products is expanding, even though total amounts of the industrial waste are too small to substantially reduce the $CO_2$ emissions. The mineral carbonation was performed with steelmaking reduction slag as starting material. The steelmaking reduction slag dissolution experiments were conducted in the $H_2SO_4$ and $NH_4NO_3$ solution with concentration range of 0.3 to 1 M at $100^{\circ}C$ and $150^{\circ}C$. The hydrothermal treatment was performed to the starting material via a modified direct aqueous carbonation process at the same leaching temperature. The initial pH of the solution was adjusted to 12 and $CO_2$ partial pressure was 1MPa for the carbonation. The carbonation rate after extracting $Ca^^{2+}$ under $NH_4NO_3$ was higher than that under $H_2SO_4$ and the carbonation rates in 1M $NH_4NO_3$ solution at $150^{\circ}C$ was dramatically enhanced about 93%. In this condition well-faceted rhombohedral calcite, and rod or flower-shaped aragonite were appeared together in products. As the concentration of $H_2SO_4$ increased, the formation of gypsum was predominant and the carbonation rate decreased sharply. Therefore it is considered that the selection of the leaching solution which does not affect the starting material is important in the carbonation reaction.