• Title/Summary/Keyword: GTAW

Search Result 147, Processing Time 0.019 seconds

A Development of Overlay GTAW Welding System for Pipe Inside Straight Process (직선형 프로세스 파이프 내면 오버레이 GTAW 용접시스템 개발)

  • Eun, Jong-Mok;Lee, Young-Kyu
    • Journal of Welding and Joining
    • /
    • v.32 no.2
    • /
    • pp.4-8
    • /
    • 2014
  • In this research, GTA overlay welding system is developed for inside of straight pipes in various diameter. It can be applied to oil, ship building and plant industry, especially pipes connected to pressure vessels, for the purpose of cost reduction by cladding inside of pipes with corrosion and heat resistant alloys such as stainless steel or Inconel. Developed system consists of GTA power source, torch, wire feeding system, automatic arc length adjusting device, CCD camera and cooling unit. Two types of pipe inside overlay welding system are developed. One is for maximum 3m pipe length with 3 inch ~ 12 inch pipe outer diameter. Another type can be applied to maximum 12m pipe length with 7 ~ 24 inch OD. Developed system successfully produced inside cladded pipe and the results are shown through cross sectional images of the pipes.

S-N Fatigue Strength of Small Diameter Branch Welded Pipe with Variation of Welding Shapes and Welding Procedures (용접부의 형상과 공정변화에 따른 소구경 분기배관의 피로강도 특성평가)

  • 백종현;김우식
    • Journal of Welding and Joining
    • /
    • v.22 no.3
    • /
    • pp.50-55
    • /
    • 2004
  • S-N fatigue tests were conducted to investigate the fatigue strength of small diameter socket and butt welded joints made of carbon steels. Experimental parameters were pipe diameter, throat depth, shape of socket welds and welding procedure. Filler metals used in SMAW and GTAW procedure were E9016-G with diameter of 4.0 m and ER70S-G with diameter of 2.4 m. API 5L Gr.B pipes were adopted as a small diameter branch pipes. All socket fittings were machined from ASTM A105 carbon steel. Tensile strength was not affected by the welding procedure. Fatigue strength in socket weld joints increased with increasing pipe diameter, area of weld metal and weld leg length of pipe side.

A Study of Characteristics on the Dissimilar Metals (STS 316L - Carbon Steel: ASTM A516-70) Welds made with GTAW (스테인리스강 STS 316L과 탄소강 A516-70의 이종금속 GTA 용접부 특성에 대한 연구)

  • Kim, Se Cheol;Shin, Tae Woo;Moon, In Joon;Jang, Bok Su;Koh, Jin Hyun
    • Journal of Welding and Joining
    • /
    • v.33 no.4
    • /
    • pp.37-43
    • /
    • 2015
  • Characteristics of dissimilar metal welds between STS 316L and carbon steel ASTM A516 Gr.70 made with GTAW have been evaluated in terms of microstructure, ferrite content, chemical analysis, hardness and corrosion resistance. Three heat inputs of 9.00, 11.25, 13.00kJ/cm were employed to make joints of dissimilar metals with ER309 wire. Based on microstructural examination, the amount of vermicular type of ${\delta}$-ferrite was increased with increasing heat input due to the increase of Creq/Nieq in the second layer of welds. Based on the EDX analysis of weld metals, Cr and Ni content in the 2nd layer increased while those content in the first layer of welds decreased with heat inputs. Cellular solidification mode in the 1st layer and dendritic solidification mode in the 2nd layer due to different cooling rates were prevailed, respectively. Heat affected zone which formed hard microstructure showed higher hardness than the weld metal. The salt spray test of dissimilar metals weld joints showed that the carbon steel surfaces only corroded. The weight loss rate due to corrosion increased up to 100hours but it decreased above 100 hours. There was little difference in the weight loss caused by corrosion regardless of heat inputs.

Girth Welding Procedure and Mechanical Properties of Gas Pipeline (가스배관 원주자동용접 공정 개발 및 기계적 특성 평가)

  • Kim, Woo-Sik;Kim, Young-Pyo;Kim, Choel-Man
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.84-84
    • /
    • 2009
  • 파이프라인을 건설함에 있어 가장 중요한 기술이 배관 용접기술이다. 즉 파이프와 파이프를 연결하는 작업이 공사 진척도를 결정하기 때문에, 이를 얼마나 경제적으로 신속하게 수행해 나가느냐하는 것은 건설기간 및 건설비용을 결정하는 핵심 요소이다. 가스배관 시공 원주용접 방법은 여러 가지 있는데, 현재 국내에서는 전량 수동용접을 채택하고 있다. 이 방법은 국내 가스배관을 건설한 초기부터 적용해온 것으로 우수한 품질을 확보할 수 있으며, 취약한 국내 자동화기술과 열악한 도로 매설 시공여건에서 적용하기 용이한 방안이다. 그러나 우수한 용접기량을 보유한 용접사가 점차 부족해지고, 배관시공 시간을 단축하고 비용을 줄이기 위한 필요성이 점차 커지면서 이를 해결할 수 있는 기술로서 자동원주용접방안이 있다. 이 기술들은 해외 가스배관에 이미 오래전부터 적용되어 용접부위 신뢰성과 품질 우수성을 확보하고 시공비용절감을 달성하고 있다. 자동용접을 적용하기 위해서는 용접절차를 수립하여 절차인증시험을 수행하고, 기존방안과 동일이상의 품질이 확보되며 효율성을 겸비해야만 한다. 국가 기본에너지의 안정적인 공급을 위해 적기 시공이 필요하고, 1 km당 10 억원 이상이 소요되는 배관시공비용 중 약 1/3이 용접비파괴검사 비용인 점을 감안할 때 품질이 확보되면서 경제적인 시공방안이 있다면 이를 적용하는 것이 국가 산업 경제적 측면에서 필요한 일이다. 이와 관련된 연구에서는 국내 가스배관 원주용접에 적용 가능한 용접공정을 검토하고, 용접절차를 수립하여 절차인증시험을 수행하였으며, 추가로 배관 원주 자동용접부위에 대한 기계적 특성 평가를 실시하였다. 현재 국내 건설여건과 비파괴검사 기준을 만족시키고 안전성과 효율성을 겸비한 방법으로는 초층과 2층은 수동 GTAW를 적용하고 나머지 층은 반자동 FCAW를 적용하는 방안이 적절한 것으로 판단된다. 전 층을 자동 GTAW로 용접하는 방안은 품질은 확보되지만 효율성측면에서 대형배관에는 적용하기 어려울 것으로 보이며, 해외에서 많이 사용되는 자동 GMAW 방안은 국내 비파괴검사기준을 만족시키기 어려워 검토대상에서 제외하였다. 본 논문에서는 두 가지 용접방법에 대한 용접공정개발과정과 원주용접부위 기계적 특성을 검토하여 최적방안을 제시하고자 한다.

  • PDF

Mechanical Properties Evaluation of Gas Tungsten Arc Welding for INCONEL 718 alloy apply to Cryogenic Condition (극저온 환경에 적용되는 INCONEL 718합금의 Gas Tungsten Arc Welding 기계적 특성 평가)

  • Kim, Ki-Hong;Moon, In-Sang;Moon, Il-Yoon;Rhee, Byung-Ho
    • Korean Journal of Materials Research
    • /
    • v.19 no.12
    • /
    • pp.692-698
    • /
    • 2009
  • Inconel 718 alloy has excellent mechanical properties at room temperature, high temperature and cryogenic conditions. UTS of base metal is about 900MPa at room temperature; this is increased up to 1300MPa after heat treatment & aging-hardening. Mechanical properties of Inconel 718 Alloy were similar to those shown in the the results for tensile test; mechanical properties of Inconel 718 alloy's GTAW were similar to those of base metal's properties at room temperature. Mechanical properties at cryogenic conditions were better than those at room temperature. Heat-treated Inconel 718, non- filler metal GTAW on Inconel 718 and GTAW used filler metal on Inconel 718's UTS was 1400MPa at cryogenic condition. As a result, the excellent mechanical properties of Inconel 718 alloy under cryogenic conditions was proved through tensile tests under cryogenic conditions. In addition, weldability of Inconel 718 alloy under cryogenic conditions was superior to that of its base-metal. In this case, UTS of hybrid joint (IS-G) at -100$^{\circ}C$ was 900MPa. Consequently, UTS of Inconel 718 alloy is estimated to increase from -100$^{\circ}C$ to a specific temperature below -100$^{\circ}C$. Therefore, Inconel 718 alloy is considered a pertinent material for the production of Lox Pipe under cryogenic conditions.

A study on the Application Effect of Friction Stir Processing for Enhanced Pitting Corrosion Resistance of Stainless Steel Welds in Chloride Environment (염화물 환경에서 스테인리스강 용접부의 공식저항성 향상을 위한 마찰교반공정 적용효과에 관한 연구)

  • Jong Moon Ha;Deog Nam Shim;Seung Hyun Kim
    • Transactions of the Korean Society of Pressure Vessels and Piping
    • /
    • v.19 no.2
    • /
    • pp.84-92
    • /
    • 2023
  • As temporary storage facilities for spent nuclear fuels in domestic nuclear power plants are expected to be saturated, external intermediate storage facilities would be required in the future. Spent nuclear fuels are stored in metal canisters and then placed in a dry environment within concrete or metal casing for operation. In the United States, the dry storage method for spent nuclear fuels has been operated for an extended period. Based on the corrosion experiences of dry storage canisters in chloride environments, numerous studies have been conducted to reduce corrosion in welds. With the construction of intermediate storage facilities in Korea for spent nuclear fuels expected near coastal areas adjacent to nuclear power plants, there is a need for research on the corrosion occurrence of welds and mitigation methods for canisters in chloride environments. In this paper, we measured and compared the residual stresses in the Heat-Affected Zones (HAZ) after electron beam welding (EBW) and gas tungsten arc welding (GTAW) processes for candidate materials such as 304L, 316L, and duplex stainless steel(DSS). We investigated the possibility of microstructure control through the application of surface modification processes using friction stir processing (FSP). Corrosion tests on each welded specimen revealed a higher corrosion rate in EBW welds compared to GTAW. Furthermore, it was confirmed that corrosion resistance improved due to phase refinement and redistribution of precipitates when FSP was applied.

Effect of weldability in shielding gases on the GTAW process of austenitic stainless steel (스테인레스강의 GTAW 기법에서 보호가스가 용접성에 미치는 영향)

  • Kim, Dae-Ju;Baek, Ho-Seong;Ryu, Seung-Hyeop;Go, Seong-Hun;Kim, Gyeong-Ju;Kim, Dae-Sun
    • Proceedings of the KWS Conference
    • /
    • 2006.10a
    • /
    • pp.63-65
    • /
    • 2006
  • The paper deals with the effect of hydrogen or helium in argon as a shielding gas on GTA welding of austenitic stainless steel. The studies were carried out in GTA(Gas Tungsten Arc) welding with a non-consumable electrode in case with different volume additions of hydrogen or helium to the argon shielding gas, i.e $5%H_2,\;10%H_2$, 30%He and 67%He. The penetration, welding voltage, microstructure and mechanical property were examined. The deepest penetration was obtained from the sample which was welded under shielding gas of $10%H_2$. The studies showed that hydrogen or helium addition to argon changes the static characteristic of the welding arc. The hydrogen or helium addition to argon increases arc power and the quantity of the material melted. The weld metal penetration depth and its width increased with increasing hydrogen or helium content. Additionally, welding voltage increased with increasing hydrogen or helium content.

  • PDF

Effect of Welding variables on White Spots Formation on the autogeneous GTA Welds of 36% Nickel-Iron alloy (36% Nickel-Iron 합금의 자동 GTA 용접부 반점 형성에 미치는 용접 변수의 영향)

  • Lee, Hee-Keun;Park, Jong-Min;Kim, Jin-Yong;Huh, Man-Ju
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.38-38
    • /
    • 2009
  • 36 percent nickel-iron alloy possesses a useful combination of low thermal expansion, moderately high strength and good toughness at temperatures down to that of liquid helium, $-269^{\circ}C$. These propeties coupled with good weldability and desirable physical properties make this alloy attractive for many cryogenic applications such as the cargo containment system in Liquefied Natural Gas carriers and pipes for low temperature. Generally, welding method of the 36% nickel-iron is applied with the manual and autogeneous GTAW. Lately white spots have been observed on the some autogeneous GTA welds of them. But the white spot formation have not been studied yet. This paper covers the analysis results of the white spots formation as changing welding variables.

  • PDF