• 제목/요약/키워드: Fundamental mass Concrete

검색결과 38건 처리시간 0.021초

기포제 혼입 단열형 경량모르타르의 물리적 특성 및 압축강도 추정에 관한 기초적 연구 (Fundamental Study on Estimating Compressive Strength and Physical Characteristic of Heat insulation Lightweight Mortar With Foam Agent)

  • 민태범;우영제;이한승
    • KIEAE Journal
    • /
    • 제10권3호
    • /
    • pp.89-96
    • /
    • 2010
  • In comparison with ordinary or heavy-weight concrete, light-weight air void concrete has the good aspects in optimizing super tall structure systems for the process of design considering wind load and seismic load by lightening total dead load of buildings and reducing natural resources used. Light-weight air void concrete has excellent properties of heat and sound insulating due to its high amount porosity of air voids. So, it has been used as partition walls and the floor of Ondol which is the traditional Korean floor heating system. Under the condition of which the supply of light-weight aggregates are limited, the development of light-weight concrete using air voids is highly required in the aspects of reduced manufacturing prices and mass production. In this study, we investigated the physical properties and thermal behaviors of specimens that applied different mixing ratios of foaming agent to evaluate the possibility of use in the structural elements. We proposed the estimating equation for compressive strength of each mix having different ratio of foaming agent. We also confirmed that the density of cement matrix is decreased as the mixing amount of foaming agent increase up to 0.6% of foaming agent mixing ratio which was observed by SEM. Based on porosity and compressive strength of control mortar without foaming agent, we built the estimating equations of compressive strength for mortars with foaming agent. The upper limit of use in foaming agent is about 0.6% of the binder amount. Each air void is independent, and size of voids range from 50 to $100{\mu}m$.

Evaluating the accuracy of mass scaling method in non-linear quasi-static finite element analysis of RC structures

  • A. Yeganeh-Salman;M. Lezgy-Nazargah
    • Structural Engineering and Mechanics
    • /
    • 제85권4호
    • /
    • pp.485-500
    • /
    • 2023
  • The non-linear static analysis of reinforced concrete (RC) structures using the three-dimensional (3D) finite element method is a time-consuming and challenging task. Moreover, this type of analysis encounters numerical problems such as the lack of convergence of results in the stages of growth and propagation of cracks in the structure. The time integration analysis along with the mass scaling (MS) technique is usually used to overcome these limitations. Despite the use of this method in the 3D finite element analysis of RC structures, a comprehensive study has not been conducted so far to assess the effects of the MS method on the accuracy of results. This study aims to evaluate the accuracy of the MS method in the non-linear quasi-static finite element analysis of RC structures. To this aim, different types of RC structures were simulated using the finite element approach based on the implicit time integration method and the mass scaling technique. The influences of effective parameters of the MS method (i.e., the allowable values of increase in the mass of the RC structure, the relationship between the duration of the applied load and fundamental vibration period of the RC structure, and the pattern of applied loads) on the accuracy of the simulated results were investigated. The accuracy of numerical simulation results has been evaluated through comparison with existing experimental data. The results of this study show that the achievement of accurate structural responses in the implicit time integration analyses using the MS method involves the appropriate selection of the effective parameters of the MS method.

온도응력 측정용 시험장치의 개발 (Development of Thermal Stress Measuring System)

  • 전상은;김국한;김진근
    • 콘크리트학회논문집
    • /
    • 제13권3호
    • /
    • pp.228-236
    • /
    • 2001
  • 매스콘크리트 구조물에서 발생하는 온도응력을 예측하기 위해 많은 연구가 해석적인 방법과 실험적인 방법을 통해 수행되어왔다. 그러나 이러한 해석적인 방법과 실험적인 방법으로 온도응력을 예측하는 것은 한계가 있다. 해석적인 방법은 콘크리트의 탄성계수, 열팽창계수와 같은 물성치를 정확히 알아야 한다. 그리고 실험적인 방법은 대부분이 실제 구조물이나 모형구조물을 통하여 직접 온도응력을 측정한다. 그러나 이와 같은 방법은 경제적인 문제뿐만 아니라 현장의 불확실한 조건들을 감수해야 한다. 본 연구에서는 온도응력을 실내에서 직접적으로 측정할 수 있는 시험장치를 개발하였다. 개발된 온도응력 시험장치는 콘크리트와 다른 열팽창계수를 갖는 재료를 이용하여 실제 구조물에서 발생할 수 있는 콘크리트의 내/외부 구속에 의한 온도응력의 변화를 구현할 수 있으며, 이를 정량적으로 예측할 수 있다. 실험은 해석을 통해 얻은 온도이력을 구현할 수 있는 항온항습조에서 수행하였고, 온도응력은 장비에 부착된 변형률게이지를 통해 얻은 변형률을 이용하여 계산하였다. 개발된 장비의 검증을 위해 매립게이지를 이용하여 온도응력을 측정하는 실험을 동시에 수행하였고, 이 결과에 의하면 개발된 시험장치는 불확실한 콘크리트의 초기재령 물성치를 고려하여 보다 정확하게 온도응력을측정할 수 있으며, 검증실험 결과에 의해 그 객관성과 타당성을 입증할 수 있었다.

지진시 저층건물 면진구조의 비선형 동적 거동 (Dynamic Stability Analysis of Base-Isolated Low-level Nonlinear Structure Under Earthquake Excitation)

  • 문병영;강경주;강범수;김계수
    • 대한기계학회논문집A
    • /
    • 제25권11호
    • /
    • pp.1743-1750
    • /
    • 2001
  • This paper presents an analysis of nonlinear response of the seismically isolated structure against earthquake excitation to evaluate isolation performances of a rubber bearing. In the analysis of the vibration of building, the building is modeled by lumped mass system where the restoring force is considered as linear, bilinear and trilinear. Fundamental equations of motion are derived for the base isolated structure, and hysteretic and nonlinear-elastic characteristics are considered for a numerical calculation. The excitation levels are magnified fur the recorded strong earthquake motions in order to examine dynamic stability of the structure. Seismic responses (of the building are compared fur the each restoring force type. As a result, it is shown that the effect of the motion by the nonlinear response of the building is comparatively not so large from a seismic design standpoint. The responses of the isolated structures reduce sufficiently and controled the motion of the building well in a practical range. By increasing the acceleration of the earthquake, the yielding of the farce was occurred in the concrete and steel frame, which shows the necessity of the exact nonlinear dynamic analysis.

물-결합재비에 따른 알칼리 활성 슬래그 모르타르의 초기 재령 특성에 관한 연구 (A Study on Early Age Properties of Alkali Activated Slag Mortar According to Water/Binder Ratio)

  • 오상혁;김대왕;이광명
    • 한국건설순환자원학회논문집
    • /
    • 제7권2호
    • /
    • pp.63-69
    • /
    • 2012
  • 최근 시멘트 제조시 발생되는 다량의 이산화탄소로 인한 온난화 현상이 심각한 실정이며, 이러한 환경문제와 자원 고갈 문제를 동시에 해결하기 위해 고로슬래그와 같은 산업부산물을 콘크리트 배합에 사용하는 사례가 증가하고 있다. 일반적으로 고로슬래그는 대체율 20~50%의 범위에서 가장 많이 사용되고 있으나, 최근에는 고로슬래그를 100% 사용한 알칼리 활성 슬래그 콘크리트의 개발 및 실용화 연구가 활발히 진행되고 있다. 본 연구에서는 고강도 알칼리 활성 콘크리트의 구조 부재 적용을 위한 기초 자료를 확보하기 위해 알칼리 활성화 슬래그 모르타르의 초기 재령특성을 조사하였다. 물-결합재비(W/B)는 0.3, 0.4, 0.5의 3수준으로 하고 알칼리 활성화제인 NaOH를 슬래그 질량대비 4%, 8%, 12% 첨가한 AAS 모르타르의 압축강도, 플로우, 초결과 종결, 초음파속도를 측정하였다. 그 결과, 물-결합재비가 낮을수록 높은 압축강도가 발현되었으나 시간 경과에 따라 플로우가 저하하고 응결시간이 빨라지는 것으로 나타나 고강도 알칼리 활성 콘크리트를 제조하기 위해서는 적절한 유동화제의 사용이 필수적이라고 판단된다.

  • PDF

가열온도곡선 변화에 따른 고강도 콘크리트의 폭렬방지특성 (Spalling Prevention of High Strength concrete Corresponding to the Various Heating Curves)

  • 한천구;배장춘
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제13권3호통권55호
    • /
    • pp.127-134
    • /
    • 2009
  • 본 연구는 고강도 콘크리트의 복합유기섬유 혼입률 변화 및 ISO와 RABT의 가열온도곡선 변화에 따른 내화시험을 실시한 후 폭렬방지성상 및 잔존압축강도 특성 등을 분석한 것으로, 그 결과를 요약하면 다음과 같다. 복합유기섬유 혼입 콘크리트의 기초적 특성으로 유동성은 섬유혼입률이 증가할수록 직선적으로 저하하는 경향이었고, 공기량은 약간의 증가 또는 감소의 경향은 있었으나 큰 차이 없었으며, 28 일 압축강도는 완만한 감소경향을 나타내었다. 내화특성으로, RABT 가열온도곡선의 경우는 ISO 가열온도곡선에 비해 복합 유기섬유 혼입률이 많은 범위까지 폭렬양상을 나타내었으나, 주로 박리폭렬일뿐 내부까지 극심한 폭렬양상은 발생하지 않았다. 결국 W/B 25%인 고강도 콘크리트의 경우 ISO 가열온도곡선은 섬유의 혼입률 0.04%이상에서, RABT 가열온도곡선의 경우는 섬유의 혼입률 0.10%이상에서 폭렬이 방지되는 것으로 나타났다. 가열온도곡선 변화에 따른 질량감소율은 폭렬이 방지된 경우 ISO 가열온도곡선은 7%전후, RABT 가열온도 곡선은 9%전후로 나타났다. 가열온도곡선변화에 따른 잔존압축강도율은 폭렬이 방지된 경우 ISO 가열온도 곡선은 50%~60%, RABT 가열온도곡선은 30%~35%를 나타내었다.

유동화제가 알칼리 활성 슬래그 모르타르의 유동 특성 및 압축 강도에 미치는 영향 (Influence of Superplasticizers on Fluidity and Compressive Strength of Alkali Activated Slag Mortar)

  • 김대왕;오상혁;이광명
    • 한국건설순환자원학회논문집
    • /
    • 제8권1호
    • /
    • pp.33-40
    • /
    • 2013
  • 최근 시멘트 생산 시에 발생하는 다량의 $CO_2$로 인한 환경문제가 심각한 실정이며, 이러한 환경문제를 해결하기 위해 고로슬래그 미분말과 같은 산업부산물을 시멘트 대체 재료로 사용한 알칼리 활성 슬래그 콘크리트에 대한 연구가 활발히 진행되고 있다. AAS 콘크리트는 상온에서 고강도 발현이 가능하지만 알칼리 반응으로 인한 빠른 응결시간과 유동성 손실로 인해 작업시간 확보에 어려움이 있는 것으로 알려져 있다. 본 연구에서는 알칼리 활성 콘크리트의 구조 부재 적용을 위한 기초 자료 확보를 위해 AAS 모르타르의 압축강도 및 유동 특성에 시멘트용 유동화제가 미치는 영향을 분석하였다. 물-결합재비(W/B)는 0.35로 고정하고 알칼리 활성화제로 수산화나트륨과 물유리를 사용하여 AAS 모르타르를 제조하였으며, 유동성 확보를 위해 4종의 유동화제인 나프탈렌(N), 리그닌(L), 멜라민(M), PC(P) 계를 각각 슬래그 질량대비 최대 2%까지 첨가하여 압축강도, 플로우, 초음파 속도를 측정하였다. 실험결과, 멜라민계 유동화제를 첨가한 경우 AAS 모르타르의 압축 강도 저하 현상 없이 유동성이 증진되는 것으로 나타났으며, 나프탈렌계와 PC계의 경우에는 유동성 개선효과가 미미한 것으로 나타났다.

  • PDF

SC구조의 내진설계를 위한 감쇠비 (Damping Ratios for Seismic Design of SC Structures)

  • 이승준;김원기
    • 한국강구조학회 논문집
    • /
    • 제22권5호
    • /
    • pp.487-496
    • /
    • 2010
  • 미국의 NRC(United States Nuclear Regulatory Commission)에서 발간된 "Regulatory Guide 1.61 of United States NRC(2007)"는 원전구조물의 내진설계에 적용되는 구조감쇠비를 철근콘크리트(이하 RC)구조의 경우 4%(OBE)와 7%(SSE), 강구조의 경우 3%(OBE)와 4%(SSE)를 규정하고 있다. 그러나 최근 개발된 강판-콘크리트(이하 SC)구조의 경우 구조감쇠비에 대한 규정이 없다. 본 연구의 목적은 RC구조와 SC구조의 감쇠비의 상대적 차이를 비교함으로서 SC구조의 감쇠비를 조사하는 것이다. 4개의 실험체, RC-S, RC-M, SC-S 그리고 SC-M에 대한 실험적 연구가 수행되었다. 뒷 글자 S와 M은 실험체의 거동이 전단에 의해 지배되는 것과 휨에 의해 지배되는 것을 의미한다. 실험방법은 엑츄에이터와 실험체의 질량사이를 연결하는 인장시험편이 파단되면서 실험체의 자유진동을 발생하게 하는 방법을 적용하였다. 가속도계를 이용하여 측정된 실험데이타를 분석하여 하중의 크기에 따른 기본진동수와 감쇠비를 결정하였다. 4개 실험체의 감쇠비를 비교분석하여 SC구조의 감쇠비는 OBE해석에 RC구조와 동일하게 4%를 제안하였으며 SSE해석의 경우 RC구조의 감쇠비보다 1% 적은 6%를 제안하였다.