• Title/Summary/Keyword: Flowable resin

Search Result 110, Processing Time 0.022 seconds

EFFECT OF INCREMENTAL FILLING TECHNIQUE ON THE POLYMERIZATION SHRINKAGE OF COMPOSITE RESIN (적층충전법이 복합레진의 중합수축에 미치는 영향)

  • Kim, Hyo-Suk;Lee, Nan-Young;Lee, Sang-Ho;Oh, You-Hyang
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.32 no.3
    • /
    • pp.481-490
    • /
    • 2005
  • The aim of this study was to investigate the relationship between the C-factor and shrinkage strain values of composite resin and examine the strain values in different incremental filling techniques. The strain gauge method was used for measurement of polymerization shrinkge strain. Experiment was divided two step. In a first experiment, we compared with strain value in three different depth (2mm, 3mm, 4mm) and microhardness of each samples after 24hours were measured. In a second experiment, we examined the strain values in five different filling techniques(Group 1: bulk filling, Group 2: oblique incremental filling, Group 3: horizontal incremental filling, Group 4: vertical incremental filling, Group 5: lining of flowable resin and bulk filling) The results of the present study can be summarized as follows: 1. Composite resin in acrylic molds showed the initial expansion at the early phase of polymerization. 2. Contraction stress was not revealed significant difference between depth of 2mm and 3mm(P>0.05). 3. Contraction stress in sample of 4mm was showed the lowest value(P<0.05). 4. Microhardness of specimen was revealed more difference between upper and lower surface in depth of 4mm than 2 and 3mm(P<0.05). 5. Lining of flowable resin and bulk filling (Group 5) was showed the lowest contraction stress, Group 2 and 3 was showed the highest contraction stress(P<0.05). On the basis above results, the stress that result from the polymerization shrinkage, when incremental curing techniques are used, showed that there is no advantage in incremental placement and curing.

  • PDF

THE EFFECT OF RESTORATIVE MATERIALS ON THE STRESS DISTRIBUTION OF CLASS V COMPOSITE RESIN RESTORATIONS - A 3D FINITE ELEMENT INVESTIGATION (수복재료가 5급 복합레진 수복물의 응력분포에 미치는 영향에 관한 3차원유한요소법적 연구)

  • Ahn, Hyoung-Ryoul;Kim, Hyeon-Cheol;Hur, Bock;Park, Jeong-Kil
    • Restorative Dentistry and Endodontics
    • /
    • v.31 no.1
    • /
    • pp.20-29
    • /
    • 2006
  • The purpose of this study was to analyze the stress distribution aspect of unrestored and restored combined shape (wedge shape occulusally and saucer shape gingivally) class V cavity, which found frequently in clinical cases. A maxillary second permolar restored with a combined shape class V composite restorations were modeled using the three dimensional finite element method. Static occlusal load of 170 N was applied on lingual incline of buccal cusp at the angle of $45^{\circ}$ with the longitudinal axis of the tooth. And three dimensional finite element analysis was taken by ANSYS (Version 6.0, Swanson Analysis System Co., Houston, U.S.A) program which represent the stress distribution on unrestored and restored cavity wall and margin. The conclusions were as follows. 1. Compared to the unrestored cavity, Von Mises stress at the cementoenamel junction and line angle of the cavity base were reduced and in restored cavity. 2. Von Mises stress at the occlusal and cervical cavity margin and wall were increased in restored cavity in comparison with the unrestored cavity. 3. In the hybrid and hybrid/flowable composite resin restoration, Von Mises stress at the cementoenamel junction and line angle of the cavity base were reduced more than in the flowable restoration. 4. In the hybrid and hybrid/flowable composite resin restoration, Von Mises stress at the occlusal and cervical cavity margin and wall were increased more than in the flowable restoration.

Effect of tribochemical silica coating on the shear bond strength of rebonded monocrystalline ceramic brackets (단결정형 세라믹 브라켓의 재접착 시 tribochemical silica coating이 전단접착강도에 미치는 영향)

  • Jeon, Young-Mi;Son, Woo-Sung;Kang, Sang-Wook
    • The korean journal of orthodontics
    • /
    • v.40 no.3
    • /
    • pp.184-194
    • /
    • 2010
  • Objective: The purpose of this study was to investigate the effect of tribochemical silica coating on the shear bond strength (SBS) of rebonded ceramic brackets using nano-filled flowable composite resin. Methods: A total of 60 premolars were prepared and divided into 4 equal groups as follows: Tribochemical silica coating (TC) + Transbond XT (XT), TC + Transbond supreme LV (LV), Sandblast treatment (SA) + XT, SA + LV. Treated ceramic brackets were rebonded on the premolars using each adhesive. All samples were tested in shear mode on a universal testing machine. Results: SBS of silica coated groups were high enough for clinical usage (TCLV: 10.82 $\pm$ 1.82 MPa, TCXT: 11.50 $\pm$ 1.72 MPa). But, SBS of the sandblast treated groups had significantly lower values than the tribochemical silica coated groups (SALV, 1.23 $\pm$ 1.16 MPa; SAXT, 1.76 $\pm$ 1.39 MPa; p < 0.05). There was no difference between the shear bond strength by type of adhesive. In the silica coated groups, 77% of the samples showed bonding failure in the adhesive. In the sandblast treated group, all bonding failures occurred at the bracket-adhesive interface. Conclusions: The result of this study suggest that newly introduced nano-filled flowable composite resin and tribochemical silica coating application on debonded ceramic bracket bases can produce appropriate bond strengths for orthodontic bonding.

Erosive Effect of Salad Dressing on Flowable Composite Resin Surfaces

  • Na-Hyun Kwon;Im-Hee Jung;Ye-Jin Kim;Jin-Yeong Lee;Na-Sun Jung;Hyun-Woong Jeong;Do-Seon Lim
    • Journal of dental hygiene science
    • /
    • v.23 no.1
    • /
    • pp.29-38
    • /
    • 2023
  • Background: The purpose of this study was to investigate the effect of salad dressings on the flowable composite resin surface and the erosion-inhibitory effect of calcium. Methods: The experiment included six groups: oriental dressing, balsamic dressing, lemon-garlic dressing, lemon-garlic dressing supplemented with 3% calcium, mineral water as a negative control group, and orange juice as a positive control group. pH and titratable acidity were measured. The prepared specimens were immersed in the experimental solutions for 1, 3, 5, 15, and 30 minutes. The surface microhardness was measured using the Vickers hardness number before and after the treatment, and the surface of the specimens was observed using a scanning electron microscope (SEM). Results: The pH values of the experimental groups in increasing order were as follows: lemon-garlic dressing (2.49±0.03), balsamic dressing (3.12±0.06), lemon-garlic dressing +3% calcium (3.27±0.09), oriental dressing (3.75±0.03), orange juice (3.82±0.02), and mineral water (7.32±0.16). The largest surface hardness reduction value was shown in lemon-garlic dressing (-9.61±1.16), followed by balsamic dressing (-9.17±1.63), oriental dressing (-8.62±1.09), orange juice (-8.19±1.36), lemon-garlic dressing +3% calcium (-6.76±1.23), and mineral water (-1.63±2.47). According to the SEM findings, the experimental and positive control groups showed rough surfaces and micropores, whereas the negative control group showed a smooth surface. Moreover, the lemon-garlic dressing with +3% calcium showed fewer micropores and a smoother surface than the lemon-garlic dressing. Conclusion: The intake of salad dressings at a low pH could weaken the surface microhardness of the flowable composite resin. However, adding calcium to these salad dressings can reduce the risk of microhardness reduction on the flowable composite resin surface.

A STUDY ON PHYSICAL PROPERTIES OF FLOWABLE COMPOSITE RESINS (유동성 복합레진의 물리적 성질에 대한 연구)

  • Kim, Ji-Young;Jeong, Byung-Cho;Yang, Kyu-Ho
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.29 no.3
    • /
    • pp.423-429
    • /
    • 2002
  • Recently, the clinical uses of flowable composite resins have increased because of fast, convenient and excellent accessibility, but little has been reported about physical properties of flowable resins. The purpose of this study was to measure and compare the physical properties(compressive strength, relative flowability, relative radiopacity) of 4 contemporary flowable composite resins(Filtek flow, Tetric Flow, Revolution Palfique Estelite LV high flow). The results were as follows; 1. There were no significant differences between 4 flowable composite resins in compressive strength, but all were lower than that of traditional hybrid composite resin(p<0.001). 2. The relative flowability were increased in order of Palfique Estelite LV high flow, Revolution, Filtek flow, Tetric Flow and sealant(p<0.001), but there were no significant differences between Filtek flow and Tetric Flow. 3. There were significant differences between flowable composite resins in relative radiopacity and they showed similar or higher radiopacity than dentin(p<0.001), especially Tetric Flow and Filtek Flow showed higher radiopacity than enamel(p<0.001). This results suggested that the stress of application area have to be considered since flowable composite resins have lower compressive strength than hybrid composite, and the differences of flowability between these flowable composite resins can be considered when they are selected. All tested flowable composite resins showed optimal radiopacity to ISO's recommend.

  • PDF

AN IN VITRO STUDY OF MICROLEAKAGE OF COMPOSITE RESINS (복합레진의 미세누출에 관한 연구)

  • Lee, Sun-Young;Yang, Yeon-Mi;Baik, Byeong-Ju;Jeon, Cheol-Wan;Kim, Jae-Gon
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.30 no.4
    • /
    • pp.593-599
    • /
    • 2003
  • The purposes of this study were to evaluate the microleakage of class V composite resin restorations utilizing the different curing lights, to assess the flowable resin, $Filtek^{TM}Flow$(3M Dental Products, USA) and composite resin, $Filtek^{TM}Z250$(3M Dental Products, USA) which need 20s curing time for halogen light could replace $Z100^{TM}$ Restorative(3M Dental Products, USA) for the microleakage, and to evaluate the effect of adhesive resin on marginal microleakage. Light curing units used in this study were conventional halogen light, XL3000(3M Dental Products, USA) and plasma arc light, Flipo(Lokki, France). Class V cavities were prepared and each cavity was filled with each composite resin. After being filled, the teeth were stored in distilled water, polished, thermocycled and soaked in 1% methylene blue solution. Following results were obtained from evaluation of the sectioned surface. 1. There was no statistically significant difference in microleakage of $Filtek^{TM}Flow$ and $Filk^{TM}Z250$ between two kinds of curing units(p>0.05). 2. Flowable resin, $Filtek^{TM}Flow$ showed more microleakage than Z100 and $Filtek^{TM}Z250$ regardless of curing units(p<0.05). 3. Adhesive resin reduced the microleakage of composite resin in both halogen light and plasma arc light(p<0.05).

  • PDF

Polymerization Shrinkage and Stress of Silorane-based Dental Restorative Composite (Silorane-기질 치아 수복용 복합레진의 중합수축과 중합수축응력)

  • Lee, In-Bog;Park, Sung-Hwan;Kweon, Hyun-Jeong;Gu, Ja-Uk;Choi, Nak-Sam
    • Composites Research
    • /
    • v.26 no.3
    • /
    • pp.182-188
    • /
    • 2013
  • The purpose of this study was to measure the volumetric polymerization shrinkage kinetics and stress of a silorane-based dental restorative composite and compare it with those of conventional methacrylate-based dental composites. Two methacrylate-based composites (Z250, Z350 flowable) and one silorane-based composite (P90) were investigated. The volumetric polymerization shrinkage of the composites during light curing was measured using a laboratory-made volume shrinkage measurement instrument based on the Archimedes' principle, and the polymerization stress was also determined with the strain gage method. The shrinkage of silorane-based composites (P90) was the lowest, and that of Z350 flowable was the highest. Peak polymerization shrinkage rate was the lowest in P90 and the highest in Z350 flowable. The time to reach peak shrinkage rate of P90 was longer than those of the methacrylate-based composites. The polymerization shrinkage stress of P90 was lower than those of the methacrylate-based composites.

A 3-year retrospective study of clinical durability of bulk-filled resin composite restorations

  • Muhittin Ugurlu;Fatmanur Sari
    • Restorative Dentistry and Endodontics
    • /
    • v.47 no.1
    • /
    • pp.5.1-5.11
    • /
    • 2022
  • Objectives: This study aimed to assess the clinical longevity of a bulk-fill resin composite in Class II restorations for 3-year. Materials and Methods: Patient record files acquired from the 40 patients who were treated due to needed 2 similar sizes Class II composite restorations were used for this retrospective study. In the experimental cavity, the flowable resin composite SDR was inserted in the dentinal part as a 4 mm intermediate layer. A 2 mm coverage layer with a nano-hybrid resin composite (CeramX) was placed on SDR. The control restoration was performed by an incremental technique of 2 mm using the nano-hybrid resin composite. The restorations were blindly assessed by 2 calibrated examiners using modified United States Public Health Service criteria at baseline and 1, 2, and 3 years. The data were analyzed using non-parametric tests (p = 0.05). Results: Eighty Class II restorations were evaluated. After 3-years, 4 restorations (5%) failed, 1 SDR + CeramX, and 3 CeramX restorations. The annual failure rate (AFR) of the restorations was 1.7%. The SDR + CeramX group revealed an AFR of 0.8%, and the CeramX group an AFR of 2.5% (p > 0.05). Regarding anatomical form and marginal adaptation, significant alterations were observed in the CeramX group after 3-years (p < 0.05). The changes in the color match were observed in each group over time (p < 0.05). Conclusions: The use of SDR demonstrated good clinical durability in deep Class II resin composite restorations.

Effect of dentin roughening and type of composite material on the restoration of non-carious cervical lesions: an in vivo study with 18 months of follow-up

  • Sanjana Verma;Rakesh Singla;Gurdeep Singh Gill;Namita Jain
    • Restorative Dentistry and Endodontics
    • /
    • v.48 no.4
    • /
    • pp.35.1-35.14
    • /
    • 2023
  • Objectives: The purpose of this study was to evaluate the impact of dentin roughening and the type of composite resin used (either bulk-fill flowable or nanohybrid) on the restoration of non-carious cervical lesions (NCCLs) with an 18-month follow-up period. Materials and Methods: This prospective split-mouth study included 36 patients, each with a minimum of 4 NCCLs. For each patient, 4 types of restorations were performed: unroughened dentin with nanohybrid composite, unroughened dentin with bulk-fill flowable composite, roughened dentin with nanohybrid composite, and roughened dentin with bulk-fill flowable composite. A universal bonding agent (Tetric N Bond Universal) was applied in self-etch mode for all groups. The restorations were subsequently evaluated at 6, 12, and 18 months in accordance with the criteria set by the FDI World Dental Federation. Inferential statistics were computed using the Friedman test, with the level of statistical significance established at 0.05. Results: The 4 groups exhibited no significant differences in relation to fracture and retention, marginal staining, marginal adaptation, postoperative hypersensitivity, or the recurrence of caries at any follow-up point. Conclusions: Within the limitations of the present study, over an 18-month follow-up period, no significant difference was present in the clinical performance of bulk-fill flowable and nanohybrid composite restorations of non-carious cervical lesions. This held true regardless of whether dentin roughening was performed.

The influence of different base materials on marginal adaptation of direct class I composite resin restorations

  • Cho, Yong-Sik;Park, Sung-Ho
    • Proceedings of the KACD Conference
    • /
    • 2003.11a
    • /
    • pp.619-619
    • /
    • 2003
  • This study was intended to evaluate the influence of different base materials on the marginal integrity of posterior direct composite resin restorations. Large conventional butt-joint MOD cavity preparations, with margins in enamel and dentin, were prepared in vitro in 24 extracted human mandibular molars and randomly divided into four equal groups. One of three base materials(RMGI, compomer, flowable resin) was placed on the pulpal floors, of the teeth of the groups. One group of teeth, which served as the control group, was not given any base mterial.(중략)

  • PDF