MOD법을 이용한 BLT박막의 제초 및 특성에 관한 연구 (The Preparation and Characterization of BLT Thin Films by MOD Process)

  • 이진한;장건익
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.186.1-189
    • /
    • 2001
  • Ferroelectric $Bi_{4-x}$La$_{x}$Ti$_3$O$_{12}$ (BLT)thin films with various compositions(x=0.65, 0.70, 0.75) were prepared on Pt//Ti/SiO$_2$/Si(100) substrate by metal-organic deposition. The electrical and structural characteristics of BLT thin films were investigated to develop ferroelectric thin films for capacitor layers of FRAM. After spin coating, thin films were annealed at $650^{\circ}C$ for 1hour in oxygen atomosphere. Scanning electron micrographs showed uniform surfaces composed of rod-like grains. The $Bi_{4-x}$La$_{x}$Ti$_3$O$_{12}$ (x=0.70) thin film capacitors with a Pt top electrode showed better ferroelectric properties than other films. At the applied voltage of 5V, the dielectric constant($\varepsilon$$_{r}$), dissipation factor(tan$\delta$),remanent polarization(2Pr), and coercive field(2Ec) of the $Bi_{4-x}$La$_{x}$Ti$_3$O$_{12}$ (x=0.70)thin films were about 272.54, 0.059, 32.4 $\mu$C/cm$^2$, 2Ec=119.9kV/cm. Also the capacitor did not show any significant fatigue up to 4.8$\times$10$^{10}$ read/write switching cycles.hing cycles.s.

  • PDF

La 첨가량에 따른 Bi$_{4-x}La_x$Ti$_3O_12$ 강유전체의 주파수특성 (The Ferroelectric Frequency characteristics of Bi$_{4-x}La_x$Ti$_3O_12$ ceramics with the variation of Lanthanum additives)

  • 김응권;박복기;박기엽;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.463-466
    • /
    • 2001
  • In recent year, Ferroelectric BLT($Bi_{4-x}$La$_{x}$Ti$_3$O$_{12}$) is a promising candidate materials. This study was Practiced to make good conditions of BLT targets. In this study, calcination and sintering temperature were kept at 75$0^{\circ}C$, 110$0^{\circ}C$ for 2 hour respectively. the density obtained 7.612, 7.98, 7.877 g/㎤ as La$_2$O$_3$ contents were 0.0mol%, 0.25mo1%, 0.5mol%. Especially, the lanthanum content of 0.5 mol% measured C-axis (117) preferred orientation more than the others targets in the XRD. In $\varepsilon$$_{r}$-f relationship using by HP 4194 A impedance analyzer, the 0.5 mol% observed above 200 relative dielectric constant. but the dissipation factor was higher than others targets at 100Hz~13MHz range. SEM photograph with the content of La$_2$O$_3$ was observed like rod and plate types.types.s.

  • PDF

열처리 조건이 Bi1-xLaxTi3O12 (x=0.75) 박막의 특성에 미치는 효과 (Effects of Annealing Conditions on the Properties of Bi1-xLaxTi3O12 Thin Films)

  • 박문흠;김상수;강민주;하태곤
    • 한국재료학회지
    • /
    • 제14권10호
    • /
    • pp.701-706
    • /
    • 2004
  • Bismuth layered structure ferroelectric thin films, La-substituted $Bi_{4}Ti_{3}O_{12}$ ($Bi_{1-x}La_{x}Ti_{3}O_{12}$, x=0.75, BLT) were prepared on the $Pt(111)/Ti/SiO_2/Si(100)$ substrates by a sol-gel spin coating process. The thin films were annealed in various conditions, i.e., oxygen, nitrogen and vacuum atmospheres for various annealing time. We investigated the annealing condition effects on the grain orientation and ferroelectric properties. The measured XRD patterns revealed that the BLT thin films showed only $Bi_{4}Ti_{3}O_{12}$-type phase with random orientation. $La^{3+}$ ion substitution for $Bi^{3+}$ ion in perovskite layers of $Bi_{4}Ti_{3}O_{12}$ decreased the degree of c-axis orientation and increased the remanent polarization ($2P_{r}$). The remanent polarization ($2P_{r}$) and the coercive field ($2E_{c}$) of the BLT thin film annealed at $650^{\circ}C$ for 5 min in oxygen atmosphere were $87{\mu}C/cm^2$ and 182 kV/cm, respectively, at an applied electric field of 240 kV/cm. For all of the BLT thin films annealed in various conditions, the fatigue resistance was shown. The improvement of ferroelectric properties with La substitution in $Bi_{4}Ti_{3}O_{12}$ could be attributed to the changes in space charge densities and grain orientation in the thin film.

La 첨가량에 따른 $Bi_{4-x}La_{x}Ti_{3}O_{12}$ 강유전체의 주파수특성 (The Ferroelectric Frequency characteristics of $Bi_{4-x}La_{x}Ti_{3}O_{12}$ ceramics with the variation of Lanthanum additives)

  • 김응권;박복기;박기엽;박춘배
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.463-466
    • /
    • 2001
  • In recent year, Ferroelectric $BLT(Bi_{4-x}La_{x}Ti_{3}O_{12})$ is a promising candidate materials. This study was practiced to make good conditions of BL T targets. In this study, calcination and sintering temperature were kept at $750^{\circ}C$, $1100^{\circ}C$ for 2 hour respectively. the density obtained 7.612, 7.98, $7.877g/cm^{3}$ as $La_{2}O_{3}$ contents were 0.0mol%, 0.25mol%, 0.5mol%. Especially, the lanthanum content of 0.5 mol% measured C-axis (117) preferred orientation more than the others targets in the XRD. In $\varepsilon_{r}-f$ relationship using by HP 4194 A impedance analyzer, the 0.5 mol% observed above 200 relative dielectric constant. but the dissipation factor was higher than others targets at 100Hz~13MHz range. SEM photograph with the content of $La_{2}O_{3}$ was observed like rod and plate types.

  • PDF

FRAM 응용을 위한 BLT박막의 제작 및 특성 (A Fabrication and ferroelectric properties of BLT Thin Films for FRAM)

  • 김경태;권지운;심일운;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.565-568
    • /
    • 2001
  • We have fabricated $Bi_{3.25}$$La_{0.75}$ti$_3$O$_{12}$ (BLT) thin(200nm) films on the Pt/Ti/SiO$_2$/Si substrates using a MOD(Metalorganic decomposition) method with annealing temperature from 55$0^{\circ}C$ to 75$0^{\circ}C$. The structural properties of the films examined by x-ray diffraction. The layered-perovskite phase obtained above $600^{\circ}C$. Scanning electron micrographs showed uniform surface composed of rodlike grains. The grain size increased with increasing annealing temperature. The BLT thin films showed little polarization fatigue test up to 3.5x10$^{9}$ bipolar cycling at a 5V and 100kHz.kHz.

  • PDF

FRAM 응용을 위한 BLT 박막의 제작 및 특성 (A Fabrication and ferroelectric properties of BLT Thin Films for FRAM)

  • 김경태;권지운;심일운;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집 Vol.14 No.1
    • /
    • pp.565-568
    • /
    • 2001
  • We have fabricated $Bi_{3.25}La_{0.75}Ti_{3}O_{12}(BLT)$ thin(200nm) films on the $Pt/Ti/SiO_{2}/Si$ substrates using a MOD(Metalorganic decomposition) method with annealing temperature from $550^{\circ}C$ to $750^{\circ}C$. The structural properties of the films examined by x-ray diffraction. The layered-perovskite phase obtained above $600^{\circ}C$. Scanning electron micrographs showed uniform surface composed of rodlike grains. The grain size increased with increasing annealing temperature. The BLT thin films showed little polarization fatigue test up to $3.5{\times}10^{9}$ bipolar cycling at a 5V and 100kHz.

  • PDF

Electrical Properties of Metal-Ferroelectric-Insulator-Semiconductor Field-Effect Transistor Using an Au/$(Bi,La)_4Ti_3O_{12}/LaZrO_x$/Si Structure

  • Jeon, Ho-Seung;Lee, Gwang-Geun;Kim, Joo-Nam;Park, Byung-Eun;Choi, Yun-Soo
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.171-172
    • /
    • 2007
  • We fabricated the metal-ferroelectric-insulator-semiconductor filed-effect transistors (MFIS-FETs) using the $(Bi,La)_4Ti_3O_{12}\;and\;LaZrO_x$ thin films. The $LaZrO_x$ thin film had a equivalent oxide thickness (EOT) value of 8.7 nm. From the capacitance-voltage (C-V) measurements for an Au/$(Bi,La)_4Ti_3O_{12}/LaZrO_x$/Si MFIS capacitor, a hysteric shift with a clockwise direction was observed and the memory window width was about 1.4 V for the bias voltage sweeping of ${\pm}9V$. From drain current-gate voltage $(I_D-V_G)$ characteristics of the fabricated Fe-FETs, the obtained threshold voltage shift (memory window) was about 1 V due to ferroelectric nature of BLT film. The drain current-drain voltage $(I_D-V_D)$ characteristics of the fabricated Fe-FETs showed typical n-channel FETs current-voltage characteristics.

  • PDF

Random-Oriented (Bi,La)4Ti3O12 Thin Film Deposited by Pulsed-DC Sputtering Method on Ferroelectric Random Access Memory Device

  • Lee, Youn-Ki;Ryu, Sung-Lim;Kweon, Soon-Yong;Yeom, Seung-Jin;Kang, Hee-Bok
    • Transactions on Electrical and Electronic Materials
    • /
    • 제12권6호
    • /
    • pp.258-261
    • /
    • 2011
  • A ferroelectric $(Bi,La)_4Ti_3O_{12}$ (BLT) thin film fabricated by the pulsed-DC sputtering method was evaluated on a cell structure to check its compatibility to high density ferroelectric random access memory (FeRAM) devices. The BLT composition in the sputtering target was $Bi_{4.8}La_{1.0}Ti_{3.0}O_{12}$. Firstly, a BLT film was deposited on a buried Pt/$IrO_x$/Ir bottom electrode stack with W-plug connected to the transistor in a lower place. Then, the film was finally crystallized at $700^{\circ}C$ for 30 seconds in oxygen ambient. The annealed BLT layer was found to have randomly oriented and small ellipsoidal-shaped grains (long direction: ~100 nm, short direction: ~20 nm). The small and uniform-sized grains with random orientations were considered to be suitable for high density FeRAM devices.

Sol-gel법에 의해 제조된 강유전체 $Bi_{3.15}La_{0.85}Ti_3O_{12}$ 박막의 결정 배향성 조절 (Crystallographic orientation modulation of ferroelectric $Bi_{3.15}La_{0.85}Ti_3O_{12}$ thin films prepared by sol-gel method)

  • 이남열;윤성민;이원재;신웅철;류상욱;유인규;조성목;김귀동;유병곤
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.851-856
    • /
    • 2003
  • We have investigated the material and electrical properties of $Bi_{4-x}La_xTi_3O_{12}$ (BLT) ferroelectric thin film for ferroelectric nonvolatile memory applications of capacitor type and single transistor type. The 120nm thick BLT films were deposited on $Pt/Ti/SiO_2/Si$ and $SiO_2/Nitride/SiO_2$ (ONO) substrates by the sol-gel spin coating method and were annealed at $700^{\circ}C$. It was observed that the crystallographic orientation of BLT thin films were strongly affected by the excess Bi content and the intermediate rapid thermal annealing (RTA) treatment conditions regardeless of two type substrates. However, the surface microstructure and roughness of BLT films showed dependence of two different type substrates with orientation of (111) plane and amorphous phase. As increase excess Bi content, the crystallographic orientation of the BLT films varied drastically in BLT films and exhibited well-crystallized phase. Also, the conversion of crystallographic orientation at intermediate RTA temperature of above $450^{\circ}C$ started to be observed in BLT thin films with above excess 6.5% Bi content and the rms roughness of films is decreased. We found that the electrical properties of BLT films such as the P-V hysteresis loop and leakage current were effectively modulated by the crystallographic orientations change of thin films.

  • PDF

FRAM 응용을 위한 건조온도에 따른 BLT 박막의 강유전 특성 (Ferroelectric Properties of Bi3.25La0.75Ti3O12 Thin Films with Various Drying Temperature for FRAM Applications)

  • 김경태;김동표;김창일;김태형;강동희;심일운
    • 한국전기전자재료학회논문지
    • /
    • 제16권4호
    • /
    • pp.265-271
    • /
    • 2003
  • Ferroelectric lanthanum-substituted Bi$_4$Ti$_3$O$_{12}$(BLT) thin films were fabricated by spin-coating onto a Pt/Ti/SiO$_2$/Si substrate by metalorganic decomposition technique. The grain size in BLT thin films were prepared with controlled by various drying process. The effect of grain size on the crystallization and ferroelectric properties were investigated by x-ray diffraction and field emission scanning electron microscope. The dependence of crystallization and electrical properties are related to the grain size in BLT thin films with different drying temperature. The remanent polarization of BLT thin film increases with the increasing grain size. The value of 2P$_{r}$ and E$_{c}$ of BLT thin film dried at 45$0^{\circ}C$ were 25.9 $\mu$C/$\textrm{cm}^2$ and 85 kV/cm, respectively. The BLT thin film with larger grain size has better fatigue properties. The fatigue properties revealed that small grained film showed more degradation of switching charge than large grained films.lms.s.