Abstract
We have fabricated $Bi_{3.25}$$La_{0.75}$ti$_3$O$_{12}$ (BLT) thin(200nm) films on the Pt/Ti/SiO$_2$/Si substrates using a MOD(Metalorganic decomposition) method with annealing temperature from 55$0^{\circ}C$ to 75$0^{\circ}C$. The structural properties of the films examined by x-ray diffraction. The layered-perovskite phase obtained above $600^{\circ}C$. Scanning electron micrographs showed uniform surface composed of rodlike grains. The grain size increased with increasing annealing temperature. The BLT thin films showed little polarization fatigue test up to 3.5x10$^{9}$ bipolar cycling at a 5V and 100kHz.kHz.