Elevated Temperature Strength and Microstructure of Atomized and Ball-milled Al-xFe-yCr Alloys

  • Kim, Kyeong-Hwan;Chun, Byong-Sun
    • 한국분말재료학회지
    • /
    • 제7권4호
    • /
    • pp.197-204
    • /
    • 2000
  • Gas atomization mechanical alloying and hot pressing have successfully made high temperature Al-9.45Fe-4.45Cr alloy. The microstructure and mechanical properties of this alloy has been studied by using optical microscope, scanning electron microscope, transmission electron microscope, X-ray diffractometer and compressive tester. It contains high concentration of transition elements of Fe and Cr, which form thermally stable dispersoids in the aluminum matrix. Proper oxidation of powders during ball milling strengthens the bulk extrudates by providing the obstacle particles. The oxide particles are very chemically and thermally stable and prevent the coarsening of the intermediate compounds.

  • PDF

내황화성 비정질 Nb-Ni-Al-Si 코팅층의 개발 (Development of Sulfidation Resistant Amorphous Nb-Ni-Al-Si Coating Layer)

  • 이동복;김종성;백종현
    • 한국표면공학회지
    • /
    • 제30권4호
    • /
    • pp.248-254
    • /
    • 1997
  • The sulfidation behavior of a sputter-deposited amorphous coating of 69.0%Nb-16.9Ni-11.9%Al-2.2%Si (at.%) has been investigated as a funtion of temperature.(973-1173K) in pure sulfur pressure of 0.01atm. The sulfidation kinetics of the casting obyed the parabolic rate low over the whole temperature ranges studied. The stlfidation rate increased with the temperature, as expected. The sulfide scale, the composition of which was $Al_2S_3,\;NbS_2,\;Ni_{3-x}S_2\;and\;FeCrS_4$, formed on the amorphous coating was primarily bilayered. Both the outer fastgrowing non-protective 4Al_2S_3$scale and the inner slowly-growing protective $NbS_2$,/TEX> scale and the inner slowly-growing protective $NbS_2$ scale had some Fe and Cr dissolution, which evidently came from the base substrate alloy of stainless steel type 304. Belows the coating, Kirkendall void formation was noticed. Nevertheless, a dramatic improvement of sulfidation resistance was achieved by sputter-depositing Nb-2 Ni-Al-Si layer on the stainless steel 304.

  • PDF

중간층 증착에 의한 CrAlN 코팅의 기계적 물성 및 내열성 향상에 관한 연구 (Enhanced Mechanical Properties and Thermal Stability of CrAlN Coatings by Interlayer Deposition)

  • 김회근;라정현;송면규;이상율
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.100-100
    • /
    • 2016
  • 물리기상증착방법 (Physical vapor deposition)에 의하여 합성된 천이금속 질화물 박막은 경도, 내마모성 등 절삭공구의 성능을 향상시키며, Ti-Al-N, Ti-Zr-N, Zr-Al-N, Cr-Si-N 등의 3원계 경질 박막에 대한 연구가 지속적으로 이루어지고 있다. 이중에서도 CrAlN 코팅은 높은 경도, 낮은 표면 조도 등의 우수한 기계적 특성 이외에 고온에서 안정한 합금상 형성으로 인하여 우수한 내열성을 보유하여 공구 코팅으로의 적용 가능성이 크다. 그러나 최근 공구사용 환경의 가혹화로 인하여 코팅의 내마모성 및 내열성 등의 물성 향상을 통한 공구의 수명 향상이 필요시 되고 있으며, 코팅에 적합한 중간층을 합성함으로써 공구 코팅으로의 적용 가능성을 높이는 연구들이 진행되고 있다. 본 연구에서는 CrAlN 코팅의 물성을 향상시키기 위해 CrAlN 코팅과 WC-Co 6wt.% 모재 사이에 CrN, CrZrN, CrN/CrZrSiN 등의 다양한 중간층을 합성하였으며, 중간층을 포함한 모든 코팅의 두께는 $3{\mu}m$ 로 제어하였다. 합성된 코팅의 미세조직, 경도 및 탄성계수, 내모성을 분석하기 위해 field emission scanning electron microscopy(FE-SEM), nano-indentation, ball-on-disk 마모시험기 및 ${\alpha}-step$을 사용하였다. 코팅의 내열성을 확인하기 위해 코팅을 furnace에 넣어 공기중에서 500, 600, 700, 800, 900, $1,000^{\circ}C$로 30분 동안 annealing 한 후에 nano-indentation을 사용하여 경도를 측정하였다. CrAlN 코팅을 나노 인덴테이션으로 분석한 결과, 모든 코팅의 경도(35.5-36.2 GPa)와 탄성계수(424.3-429.2 GPa)는 중간층의 종류에 상관없이 비슷한 값을 보인 것으로 확인됐다. 그러나, 코팅의 마찰계수는 중간층의 종류에 따라 다른 값을 보였으며, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅의 마찰계수는 0.34로 CrZrN 중간층을 증착한 CrAlN 코팅의 마찰계수(0.41)에 비해 낮은 값을 보였다. 또한, 코팅의 마모율 및 마모폭도 비슷한 경향을 보인 것으로 보아, CrN/CrZrSiN 중간층을 합성한 CrAlN 코팅의 내마모성이 상대적으로 우수한 것으로 판단된다. 이것은 중간층의 H/E ratio가 코팅의 내마모성에 미치는 영향에 의한 결과로 사료된다. H/E ratio는 파단시의 최대 탄성 변형율로써, 모재/중간층/코팅의 H/E ratio 구배에 따라 코팅 내의 응력의 완화 정도가 변하게 된다. WC 모재 (H/E=0.040)와 CrAlN 코팅(H/E=0.089) 사이에서 CrN, CrZrSiN 중간층의 H/E ratio 는 각각 0.076, 0.083 으로 모재/중간층/코팅의 H/E ratio 구배가 점차 증가함을 확인 할 수 있었고, 일정 응력이 지속적으로 가해지면서 진행되는 마모시험중에 CrN과 CrZrSiN 중간층이 WC와 CrAlN 코팅 사이에서 코팅 내부의 응력구배를 완화시키는 역할을 함으로써 CrAlN 코팅의 내마모성이 향상된 것으로 판단된다. 모든 코팅을 열처리 후 경도 분석결과, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅은 $1,000^{\circ}C$까지 약 28GPa의 높은 경도를 유지한 것으로 확인 되었고, 이는 CrZrSiN 중간층 내에 존재하는 $SiN_x$ 비정질상의 우수한 내산화성에 의한 결과로 판단된다.

  • PDF

급속응고 Al-20wt%Si-5wt%Fe 합금분말 압출재의 강도에 관한 연구 (Fabrication of Rapidly Solidified Al-20wt%Si-5wt%Fe Alloy Powder and Mechanical Properties of its Extrudates)

  • 김택수
    • 한국분말재료학회지
    • /
    • 제1권1호
    • /
    • pp.66-71
    • /
    • 1994
  • Optical microstructures and mechanical properties of Na gas atomized Al-20Si-5Fe alloying powder and its hot extrudates were studied on 3 different types of powder size distribution. This powder showed the size distribution of 10~210 $\mu\textrm{m}$. Also the microstructures of $\alpha$-Al, primary and eutectic Si and needle shaped intermetallic compounds were observed by optical microscope. These needle shaped intermetallic compounds were identified as ${\delta}Al_4FeSi_2$- by XRD and EDX analysis. The ultimate tensile strength(UTS) of these alloy extrudates was increased from 324 to 390 MPa with decreasing powder size range from 120~210 $\mu\textrm{m}$ to 10~64 $\mu\textrm{m}$. A value of Micro-vic-kers hardness was simillar to the result of UTS. These extrudates showed better wear resistance than those of Al-20Si-2X(X : Ni, Cr, Zr), although they are insensitive to the size distribution. These results indicate that the presentation of ${\delta}Al_4FeSi_2$ intermetallic compounds contributed to the wear resistance improvement.

  • PDF

CuFeAlOx 촉매상에서의 황산분해 반응 (Sulfuric Acid Decomposition on CuFeAlOx Catalysts)

  • 전동근;이관영;공경택;유계상;김홍곤;정광덕;이병권;김창수
    • 한국수소및신에너지학회논문집
    • /
    • 제19권1호
    • /
    • pp.71-76
    • /
    • 2008
  • CuFeOx/$Al_2O_3$ catalysts are developed for the use in sulfuric acid decomposition which is a subcycle in thermochemical iodine-sulfur cycle to split water into hydrogen and oxygen. Both Cu and Fe components are co-precipitated with Al component to enhance distribution of active components. Developed catalysts are improved in the capability of sulfuric acid decomposition and endurance under highly acidic environment compared to commercial catalysts such as Pt/$Al_2O_3$ and $2CuO{\cdot}Cr_2O_3$. Developed CuFeAlOx catalysts exhibited higher sulfuric acid decomposition ability than $2CuO{\cdot}Cr_2O_3$ and longer endurance trends than Pt/$Al_2O_3$ maintaining comparable performance, respectively.

Fe-30Al-5Cr 합금의 미세조직 및 $D0_3{\leftrightarrow}B2$ 천이온도에 미치는 Ti, Hf 및 Zr의 첨가효과 (Effects of Titanium, Hafnium and Zircornium Alloying Elements on Microstructures and $D0_3{\leftrightarrow}B2$ Transition Temperature of Fe-30Al-5Cr Alloys)

  • 김성수;주성민;오선훈;김관휴;최답천
    • 한국주조공학회지
    • /
    • 제21권1호
    • /
    • pp.15-23
    • /
    • 2001
  • The changes in the microstructures and $D0_3{\leftrightarrow}B2$ transition temperature were investigated for Fe-30at.%AI-5at.%Cr alloy with the ordered $D0_3$, structure when Ti, Hf and Zr were added respectively. The addition of Cr has no effect on the microstructure. However, as the amount of Ti addition increased, the grain size became smaller. Addition of Ti+Hf, Ti+Zr and Ti+Hf+Zr also showed the similar effect. When 20at.% of Ti was added, the second phase precipitates on the substrate. The addition of Cr, Hf and Zr alone has no effect on $D0_3{\leftrightarrow}B2$ transition temperature. However, as the amount of Ti addition increased by 5, 10, 15 and 20at.%, the transition temperatures showed 929, 930, 960 and $930^{\circ}C$ respectively.

  • PDF

정전 분무법을 이용하여 제조된 Fe-Cr-Al 분말 다공체 금속의 고온 산화에 미치는 소결 온도의 영향 (Effect of Sintering Temperature on the High Temperature Oxidation of Fe-Cr-Al Powder Porous Metal Manufactured by Electrospray Process)

  • 오재성;공영민;김병기;이기안
    • 한국분말재료학회지
    • /
    • 제19권6호
    • /
    • pp.435-441
    • /
    • 2012
  • A new manufacturing process of Fe-Cr-Al powder porous metal was attempted. First, ultra-fine fecralloy powders were produced by using the submerged electric wire explosion process. Evenly distributed colloid (0.05~0.5% powders) was dispersed on PU (Polyurethane) foam through the electrospray process. And then degreasing and sintering processes were conduced. In order to examine the effect of sintering temperature in process, pre-samples were sintered for two hours at temperatures of $1350^{\circ}C$, $1400^{\circ}C$, $1450^{\circ}C$, and $1500^{\circ}C$, respectively, in $H_2$ atmospheres. A 24-hour TGA (thermo gravimetric analysis) test was conducted at $1000^{\circ}C$ in a 79% $N_2$+21% $O_2$ to investigate the high temperature oxidation behavior of powder porous metal. The results of the high temperature oxidation tests showed that oxidation resistance increased with increasing sintering temperature (2.57% oxidation weight gain at $1500^{\circ}C$ sintered specimen). The high temperature oxidation mechanism of newly manufactured Fe-Cr-Al powder porous metal was also discussed.

The Electrochemical Behavior of Ni-base Metallic Glasses Containing Cr in H2SO4 Solutions

  • Arab, Sanaa.T.;Emran, Khadijah.M.;Al-Turaif, Hamad A.
    • 대한화학회지
    • /
    • 제56권4호
    • /
    • pp.448-458
    • /
    • 2012
  • In order to develop alloy resistance in aggressive sulphat ion, the corrosion behavior of metallic glasses $Ni_{92{\cdot}3}Si_{4.5}B_{32}$, $Ni_{82,3}Cr_7Fe_3Si_{4.5}B_{3.2}$ and $Ni_{75.5}Cr_{13}Fe_{4.2}Si_{4.5}B_{2.8}$ (at %) at different concentrations of $H_2SO_4$ solutions was examined by electrochemical methods and Scanning Electron Microscope (SEM) and X-ray Photoelectron Microscopy (XPS) analyses. The corrosion kinetics and passivation behavior was studied. A direct proportion was observed between the corrosion rate and acid concentration in the case of $Ni_{92{\cdot}3}Si_{4.5}B_{32}$ and $Ni_{75.5}Cr_{13}Fe_{4.2}Si_{4.5}B_{2.8}$ alloys. Critical concentration was observed in the case of $Ni_{82,3}Cr_7Fe_3Si_{4.5}B_{3.2}$ alloy. The influence of the alloying element is reflected in the increasing resistance of the protective film. XPS analysis confirms that the protection film on the $Ni_{92{\cdot}3}Si_{4.5}B_{32}$ alloy was NiS which is less protective than that formed on Cr containing alloys. The corrosion rate of $Ni_{82,3}Cr_7Fe_3Si_{4.5}B_{3.2}$ and $Ni_{75.5}Cr_{13}Fe_{4.2}Si_{4.5}B_{2.8}$. alloys containing 7% and 13% Cr are $7.90-26.1{\times}10^{-3}$ mm/y which is lower about 43-54 times of the alloy $Ni_{92{\cdot}3}Si_{4.5}B_{32}$ (free of Cr). The high resistance of $Ni_{75.5}Cr_{13}Fe_{4.2}Si_{4.5}B_{2.8}$ alloy at the very aggressive media may due to thicker passive film of $Cr_2O_3$ which hydrated to hydrated chromium oxyhydroxide.

두께 비율과 기판 바이어스 전압이 AlCrN/AlCrSiN 이중층 코팅의 기계적 특성에 미치는 영향 (Influence of thickness ratio and substrate bias voltage on mechanical properties of AlCrN/AlCrSiN double-layer coating)

  • 김회근;라정현;이상율;한희덕
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.162-162
    • /
    • 2017
  • AlCrN 코팅은 높은 경도, 낮은 표면 조도 등의 상온에서의 우수한 기계적 특성 이외에 고온에서 안정한 합금상의 형성으로 인하여 우수한 내열성을 보이는 코팅이며, Si을 첨가하여 나노복합구조를 갖는 AlCrSiN 코팅은 고경도 특성을 나타내는 나노결정립과 고내열성을 나타내는 $Si_3N_4$ 비정질이 동시에 존재함으로써 뛰어난 고온 특성까지 보유하여 공구 코팅으로의 적용 가능성이 크다. 본 연구에서는, 가혹화된 공구사용 환경 대응 하는 더욱 우수한 내마모성 및 내열성을 보이는 코팅막을 개발하기 위해 AlCrN/AlCrSiN 이중층 코팅을 합성하였다. 합성된 코팅의 구조 및 물성을 분석하기 위해 field emission scanning electron microscopy(FE-SEM), nano-indentation, atomic force microscopy(AFM) 및 ball-on-disk wear tester를 사용하였다. 내열성을 확인하기 위하여 코팅을 furnace에 넣어 500, 600, 700, 800, 900도에서 30분 동안 annealing한 후에 nano-indentation을 사용하여 경도를 측정을 하였다. 5:5, 7:3, 9:1의 두께 비율로 AlCrN/AlCrSiN 이중층 코팅을 합성하였으며 모든 코팅의 두께는 $3{\mu}m$로 제어되었다. AlCrN 코팅층의 두께가 증가할수록, 이중층 코팅의 경도 및 내마모성은 점차 향상되었지만 코팅의 밀착력은 감소하였다. 일반적으로 AlCrN 코팅은 상대적으로 높은 잔류응력을 갖고 있으므로, AlCrN 층의 두께비율이 증가함에 따라 코팅내의 잔류응력이 높아져 코팅의 경도는 증가하고 밀착특성은 낮아진 것으로 판단된다. AlCrSiN 상부층 공정시 기판 바이어스 전압을 -50 ~ -200V 로 증가시키면서 이중층 코팅을 합성하였다. XRD 분석 결과, 공정 바이어스 전압이 증가함에 따라 AlCrSiN 상부층은 점차 비정질화 되었고, 코팅의 경도와 표면 특성이 향상되는 것을 확인하였다. 이러한 특성 향상은 높은 바이어스 인가가 이온 충돌효과의 증가를 야기시켰으, 이로 인해 치밀한 코팅층 합성에 의한 결과로 판단된다. AlCrN/AlCrSiN 이중층 코팅을 어닐링 한 후 경도 분석 결과, -150, -200V에서 합성한 코팅은 900도 이상에서 26GPa 이상의 높은 경도를 보인 것으로 보아 우수한 내열성을 갖는 것으로 확인 되었다. 이는 AlCrSiN 상부층의 높은 Si 함량 (11at.%) 으로 인한 충분한 $Si_3N_4$ 비정질상의 형성과, 고바이어스 인가로 인한 AlCrN 결정상과 $Si_3N_4$ 비정질상의 고른 분배가 코팅의 내열성을 향상시키는데 기여를 한 결과로 판단된다.

  • PDF

다양한 중간층 증착이 CrAlN 코팅의 상온 및 고온 특성에 미치는 효과에 관한 연구 (Effect of Various Interlayer Deposition on Room Temperature and High Temperature Properties of CrAlN Coatings)

  • 김회근;라정현;이상율
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.143-143
    • /
    • 2017
  • CrAlN 코팅은 높은 경도, 낮은 표면 조도 등의 상온에서의 우수한 기계적 특성 이외에 고온에서 안정한 합금상의 형성으로 인하여 우수한 내산화성 및 내열성을 보유하여 공구 코팅으로의 적용 가능성이 크다. 그러나 최근 공구사용 환경의 가혹화로 인하여 코팅의 내마모성 및 내열성 등의 물성 향상을 통한 공구의 수명 향상이 필요시 되고 있으며, 다양한 코팅 물질을 활용하여 다층 코팅을 합성함으로써 난삭재용 공구 코팅의 물성을 높이는 연구들이 진행되고 있다. 본 연구에서는 CrAlN 코팅과 WC-Co 6wt.% 모재 사이에 CrZrN, CrN, CrN/CrZrSiN 등의 중간층을 합성하여 CrAlN 코팅의 상온 및 고온 특성을 향상시키는 연구가 진행되었다. 합성된 코팅의 구조 및 물성을 분석하기 위해 field emission scanning electron microscopy(FE-SEM), nano-indentation, atomic force microscopy(AFM) 및 ball-on-disk wear tester를 사용하였다. 코팅의 고온 특성을 확인하기 위해 코팅을 furnace에 넣어 공기중에서 30분 동안 annealing 한 후에 nano-indentation을 사용하여 경도를 측정하였고, $500^{\circ}C$ annealing 코팅의 표면 조도 분석 및 $500^{\circ}C$에서 마찰마모시험을 실시하였다. CrAlN 코팅의 상온 특성을 분석한 결과, 모든 코팅의 경도(35.5-36.2 GPa)와 탄성계수(424.3-429.2 GPa)는 중간층의 종류에 상관없이 비슷한 값을 보인 것으로 확인됐다. 그러나, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅의 마찰계수는 0.33로 CrZrN 중간층을 증착한 CrAlN 코팅의 마찰계수(0.41)에 비해 향상된 값 보였으며, 코팅의 마모율 및 마모폭도 비슷한 경향을 보인 것으로 보아 코팅의 내마모성이 향상된 것으로 판단된다. 이것은 중간층의 H/E ratio가 코팅의 내마모성에 미치는 영향에 의한 결과로 사료된다. H/E ratio는 파단시의 최대 탄성 변형율로써, 모재/중간층/코팅의 H/E ratio 구배에 따라 코팅 내의 응력의 완화 정도가 변하게 된다. WC 모재 (H/E=0.040)와 CrAlN 코팅(H/E=0.089) 사이에서 CrN, CrZrSiN 중간층의 H/E ratio는 각각 0.076, 0.083 으로 모재/중간층/코팅의 H/E ratio 구배가 점차 증가함을 확인 할 수 있었고, 일정 응력이 지속적으로 가해지면서 진행되는 마모시험중에 CrN과 CrZrSiN 중간층이 WC와 CrAlN 코팅 사이에서 코팅 내부의 응력구배를 완화시키는 역할을 함으로써 CrAlN 코팅의 내마모성이 향상된 것으로 판단된다. 내열성 시험 결과, CrN/CrZrSiN 중간층을 증착한 코팅은 $1,000^{\circ}C$까지 약 28GPa의 높은 경도를 유지한 것으로 확인 되었다. $500^{\circ}C$ annealing 후 진행된 표면 조도와 마모시험 결과, 모든 코팅의 조도 값 및 마찰계수는 상온 값에 비해 증가하였으며 CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅의 변화량이 가장 낮은 값을 보였다. 이는 CrZrSiN 중간층 내에 존재하는 $SiN_x$ 비정질상이 고온 annealing시에 산소 차폐막 역할을 하여, 코팅내의 잔류 산소에 의한 산화작용을 효과적으로 방지함으로써 코팅의 고온 특성이 향상된 것으로 판단된다.

  • PDF