Electronic structure studies of Co-substituted FINEMET alloys by x-ray absorption spectroscopy

  • Chae, K.H.;Gautam, S.;Song, J.H.;Kane, S.N.;Varga, L.K.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.377-377
    • /
    • 2010
  • FINEMET type nanocrystalline materials synthesized by controlled crystallization of amorphous ribbons[1] exhibit excellent soft magnetic properties making them attractive for technological applications. Present work reports the electronic structure studies of Co-substituted FINEMET to get information on the effect of successive Co substitution on local environment around Fe and Co atom by using near edge x-ray absorption fine structure (NEXAFS) and x-ray magnetic circular dichroism (XMCD) measurements. NEXAFS spectroscopy and XMCD measurements have been carried out at Fe $L_{3,2}$ and Co $L_{3,2}$-edges to investigate the chemical states and electronic structure of FINEMET [$(Fe_{100-x}Co_x)_{78}Si_9Nb_3Cu_1Ba$](0$L_{3,2}$-edge reveal that Fe is in 2+ state and in tetrahedral symmetry with other elements. The magnetic properties exhibiting soft magnetic behavior[2] are discussed on the basis of the electronic structure studied through XMCD.

  • PDF

EFFECT OF THE MICROSTRUCTURE ON MAGNETIC PROPERTIES OF $Nd_{2}(Fe,Co)_{14}B_{1}Ga$-BASED ALLOYS DURING HDDR PROCESS

  • Jeung, W.Y.;Lee, S.H.;Vintaikin, B.E.
    • Journal of the Korean Magnetics Society
    • /
    • v.5 no.5
    • /
    • pp.408-411
    • /
    • 1995
  • Microstructure and magnetic properties of $Fe-Nd_{13.5}-Co_{15}-B_{6-8}Ga_{0-1}-Zr_{0.2-1}$ alloys during HDDR process were studied. $ZrB_{2}$ phase was detected and identified by X-Ray diffraction. Influence of Ga, Zr and Ga+Zr additions on phase relations at different stages of HDDR process was studied by X-ray diffraction and magnetic measurements.

  • PDF

A Study on the Magnetic Properties of Melt-Spun (Fe, T)-Nd-C Alloys (TAl, Ti, Co, Ni)

  • Jang, T.S.;Cho, D.H.
    • Journal of Magnetics
    • /
    • v.3 no.4
    • /
    • pp.116-119
    • /
    • 1998
  • Influence of small additions ($\leq$2.0 at.%) of Al, Ti, Co, and Ni on the microstructural development and the magnetic properties of melt-spun Fe-Bd-C alloys was investigated. Addition of these elements tended to stabilize the crystallization of as-spun ribbons. Especially, Al and Ti preferred to stabilize$ Fe_{17}Nd_2C_x.$ The average grain size of Fe17Nd2Cx (0.1~0.3 ${\mu}{\textrm}{m}$), obtained by a proper annealing, in the ribbon treated with 0.5 at.% additive was much smaller than that of additive-free ribbons, which would be the major source of large increase in coercivity. Among the additives, Ni was very effective to increase the coercivity whereas Co had beneficial effect on $T_c.$ By adding 0.5 at.% Ni, intrinsic coercivities of more than 1.4 T, 40~50% higher than that (~1.0T) of additive-free ribbons, can be obtained after annealing at 750~80$0^{\circ}C$.

  • PDF

Effects of heat treatment and Co addition on the magnetic properties of FeCoBSi thin film (FeCoSiB 자성박막의 자기적 특성에 미치는 Co 및 열처리의 영향)

  • 신현수;양성훈;장태석;박종완
    • Journal of the Korean Vacuum Society
    • /
    • v.9 no.4
    • /
    • pp.389-393
    • /
    • 2000
  • Effects of Co addition and heat treatment on the magnetic properties of Fe-Si-B thin films were investigated. The compositions of metalloids, i.e, B and Si, in the alloys were kept 10 at.% each. Heat treatments were carried out in the temperature range from 100 to $300^{\circ}C$ for up to 60 min. Amorphous thin films of FeCoSiB were deposited on the water-cooled substrates by dc magnetron sputtering. The composition of thin films was controlled by placing proper number of pellets of alloying elements and analyzed by ICP, resulting in $Fe_{80-X}Co_ XB_{10}Si_{10}$ (X=8~18 at.%). Saturation magnetization of the alloys increased as Co concentration increased up to 10 at.% and then decreased with further increase of Co concentration. However, coercive force of the films decreased with the increase of Co concentration. Furthermore, the coercive force was also reduced by the annealing due to the residual stress relief.

  • PDF

Crystal structures and Magnetic properties of Co-($Al_{1-X}Fe_X$) alloys (Co-($Al_{1-X}Fe_X$) 합금계의 결정구조 및 자기적 성질)

  • Koh, Kowan-Young;Yun, Seok-Gil
    • Korean Journal of Materials Research
    • /
    • v.2 no.2
    • /
    • pp.143-150
    • /
    • 1992
  • Crystal structures and magnetic properties of annealed Co-(Al-Fe) alloys have been investigated. Annealed specimens showed superparamagnetism when x=0.05 and ferromagnetism when $x{\geq}0.10$. Magnetization increased as x increased. X-ray diffraction data revealed that specimens were single-phase in B2(CsCl) structure with constant lattice parameter $2.87{\AA}$. The experimental results were analized on the point of view of the local environmental effect of magnetic atoms.

  • PDF

Effect of Cobalt Contents on the Biocompatibility and Corrosion Properties of Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N Alloy (Fe-31Cr-27Ni-1.6Mo-1.5W-0.26N계 초내식성 스테인리스강의 생체적합성 및 부식특성에 미치는 Co함량의 영향)

  • Jang, Soon Geun;Yoo, Young Ran;Nam, Hee Soo;Shim, Gyu Tae;Kim, Jung Gu;Kim, Young Sik
    • Korean Journal of Metals and Materials
    • /
    • v.46 no.4
    • /
    • pp.209-216
    • /
    • 2008
  • Super austenitic stainless steels shows the high PRE (Pitting Resistance Equivalent) number and the good corrosion resistance. This work controlled the Co contents in Fe-31Cr-1.7Mo-27Ni-0.25N alloys to elucidate the effect of cobalt contents on the biocompatibility and corrosion resistance. Increasing Co contents, the hardness of the annealed alloys tends to be reduced. In aged alloys, cobalt decreased the increments of hardness by aging treatment. Cobalt decreased the critical pitting temperature (CPT) in 6% $FeCl_3$ + 1% HCl solution, but improved the anodic polarization behavior in Hanks' balanced salt solution and artificial saliva solution. Repassivation rate in artificial body solutions was improved by increasing cobalt contents, but didn't show the linear relationship to PRE number of the alloys. The experimental alloys showed the non-cytotoxicity because of its high corrosion resistance.

Synthesis and Characterization of Fe-Co/mesoHZSM-5 : Effect of Desilication Agent and Iron-cobalt Composition

  • Jimmy, Jimmy;Roesyadi, Achmad;Suprapto, Suprapto;Kurniawansyah, Firman
    • Korean Chemical Engineering Research
    • /
    • v.58 no.1
    • /
    • pp.163-169
    • /
    • 2020
  • Synthesis of Fe-Co/meso-HZSM5 catalyst, intended to be applied in Fischer-Tropsch (FT) reaction was investigated. The study emphasized the effect of desilication agents, NaOH and KOH, on the catalyst materials properties. Impregnation composition of active metal (Fe and Co) was also examined. HZSM-5, converted from ammonium ZSM-5 through calcination, was treated with NaOH and KOH for desilication, followed by impregnation with 10% metal loading. Fe composition in the initial mixture was varied at 10-50% from total composition. After impregnation, reduction was applied by flowing hydrogen gas at 400 ℃ for 10 hours. The use of KOH solution induced greater mesoporous volumes; however, it had a detrimental effect on zeolite crystal structure. NaOH solutions, on the other hand, increased mesopore area as high as 100%, indicated from surface area increase from 266.28 m2/g of HZSM-5, to 526.03 m2/g of NaOH-desilicated HZSM-5. In addition, the application of NaOH solution increased pore volume from 0.14 cc/g to 0.486 cc/g. Further, more Fe-Co alloys and less oxide of iron (Fe2O3) as well cobalt (Co3O4) had been commonly observed in the produced catalysts. The largest Fe-Co alloys could be found in 50Fe-50Co/HZSM-5

Preparation of TiCoxFe1-x(x=0.50~1.00) System Metal Membrane for Hydrogen Separation (수소분리용 TiCoxFe1-x(x=0.50~1.00)계 금속막 제조)

  • Jang, Kyu-young;Kang, Tae Beom
    • Membrane Journal
    • /
    • v.25 no.2
    • /
    • pp.191-201
    • /
    • 2015
  • We have studied on the preparation of $TiCo_xFe_{1-x}$(x=0.50~1.00) system alloy, the characteristics of $TiCo_xFe_{1-x}$(x=0.50~1.00) system alloy by X-ray diffractometer (XRD), pressure composition temperature (PCT) curve, scanning electron microscopy (SEM) and the $H_2-N_2$ gas mixture separation of $TiCo_xFe_{1-x}$(x=0.50~1.00)- stainless steel (SS) composite membranes. The formation of $TiCo_xFe_{1-x}$(x=0.50~1.00) system alloys with cubic crystal same as TiCo was confirmed by X-ray diffractometer. $TiCo_xFe_{1-x}$(x=0.50~1.00) system alloys showed the hysteresis at $120^{\circ}C$. As the Fe content of $TiCo_xFe_{1-x}$(x=0.50~1.00) system alloys increased, the hysteresis was increased both range x=0.90~1.00 and x=0.55~0.60, and the range x=0.55~0.90 gave decreased hysteresis. $TiCo_{0.55}Fe_{0.45}$ alloy was the one showed the lowest hysteresis among them. The lowest value of hydrogen permeation pressure of $TiCo_xFe_{1-x}$(x=0.50~1.00)-SS composite membrane was $TiCo_{0.55}Fe_{0.45}$-SS composite membrane with the value of 2.5 atm at $120^{\circ}C$; otherwise, $TiCo_{0.90}Fe_{0.10}$-SS composite had the highest pressure value among the membranes with the value of 10 atm. $TiCo_{0.55}Fe_{0.45}$-SS composite membrane was the best to separate the $H_2-N_2$ gas mixture excellently among the $TiCo_xFe_{1-x}$(x=0.50~1.00)-SS composite membranes since $TiCo_{0.55}Fe_{0.45}$ had the least hysteresis, and hydrogen permeation pressure was the lowest with value of 2.5 atm.