• Title/Summary/Keyword: FSW Parts

Search Result 6, Processing Time 0.02 seconds

New technology Trends on Friction Stir Welding Based on Milling Process in terms of Tools, Machine and Applied Parts (밀링기반 마찰교반접합 신기술동향: 공구, 장비 및 응용부품)

  • Noh, Joong-Suk;Kim, Ju-Ho;Go, Gun-Ho;Kang, Myung-Chang
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.12 no.6
    • /
    • pp.37-44
    • /
    • 2013
  • Friction stir welding (FSW) is a solid state joining technique that has expanded rapidly since its development in 1991 and has numerous applications in a wide variety of industries. This paper introduces the basic principles of friction stir welding (FSW) and presents a survey of the latest technologies and applications in the field. The basic principles that are discussed include the terminology, tool/workpiece processes, FSW merits and process variants. In particular, the process variants including the rotation speed and traveling speed are discussed, which include the defect-free zone in an oxygen free copper and Al alloy, respectively. Multiple aspects of the FSW machine are developed, including a horizontal 2D FSW machine and a hybrid complex FSW machine. The latest applications are introduced, with an emphasis on the recent advances in the aerospace, automotive, and IT display industries. Finally, the direction for future research and potential applications are examined.

Development of the Two-piece Aluminum Wheels Using the Friction Stir Welding (마찰교반용접법을 이용한 2피스 알루미늄 휠의 개발)

  • Choi, In-Young;Kang, Young-June;Kim, Andrey;Ahn, Kyu-Saeng
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.22 no.4
    • /
    • pp.700-707
    • /
    • 2013
  • Owing to high oil prices and environmental issues, the automobile industry has conducted considerable research and made large investments to manufacture a high-efficiency automobiles. In the case of automobile wheels in which a lightweight material is used to increase the fuel efficiency a mold is used to increase the production efficiency; however, the use of the molding method for this purpose is very expensive. Therefore an automobile wheel consists of two parts. In this study a two-piece automobile wheel is manufactured by the friction stir welding(FSW) of Al6061-T6 to reduce the manufacturing cost and process complexity. The FSW welding tool geometry and rotational speed, and the feed rate are key factors that significantly affect the weld strength. Therefore tensile tests were conducted on specimens produced using various welding conditions, and the optimal FSW welding conditions were applied to manufacture aluminum wheels. To ensure reliability, prototype aluminum wheels were manufactured and their mechanical reliability and safety were evaluated using a durability test, fatigue durability test, and impact test. Through this study, aluminum wheel production was made possible using the FSW method.

Evaluation of mechanical properties on friction stir lap jointed Al6061/HT590 alloys (겹치기 마찰교반접합 된 Al6061/HT590 합금의 기계적 특성 평가)

  • Kim, Eun-Hye;Lee, Kwang-Jin;Song, Kuk-Hyun
    • Journal of Welding and Joining
    • /
    • v.33 no.2
    • /
    • pp.8-13
    • /
    • 2015
  • This study was carried out to evaluate mechanical properties of the jointed Al6061/HT590 alloys by friction stir welding (FSW). FSW was conducted under the conditions with tool rotating speed of 500 RPM and traveling speed of 300 mm/min., where Ar gas was introduced to prevent the materials from corrosion during the welding process. Electron back-scattering diffraction (EBSD) was used to characterize microstructures such as grain size, misorientation angle and crystal orientation. Evolution of intermetallic compounds in Al6061 during the process were examined in terms of morphology, size and aspect ratio at three distinct zones Al base material, heat affected zone and stir zone, where transmission electron microscope (TEM) was used. It was revealed that FSW gave rise to refinement of grains as well as growth of intermetallic compounds in Al6061. The morphological changes of intermetallic compounds exerted an influence on mechanical properties, resulting in occurrence of fracture in the part of the base material instead of the jointed parts (heat affected zone and stir zone). This study systematically evaluated the microstructural evolutions during the FSW for joining Al6061 with HT590 and their effect on mechanical properties.

Spacecraft Bus Initial Activation and Checkout of a LEO Satellite (저궤도 위성의 본체 초기 점검)

  • Jeon, Moon-Jin;Kwon, Dong-Young;Kim, Day-Young
    • Aerospace Engineering and Technology
    • /
    • v.11 no.2
    • /
    • pp.33-38
    • /
    • 2012
  • A LEO Satellite performs automatic initial operations by FSW after separation from a launch vehicle. After initial operation by FSW is finished, preparation for normal operation is performed by ground during bus initial activation and checkout phase. First of all, we check state of health of the satellite including solar array deployment status. After then, each unit of spacecraft bus is activated and checked. After activation and checkout of every units used for normal operation, we check maneuver performance for imaging mission and orbit maintenance performance. Because the Bus IAC is performed during limited ground contact time, every detailed procedure must be designed considering ground contact. Therefore, the Bus IAC procedure is separated into several parts based on ground contact duration. In addition, the procedures for every possible operation including expected situation as results of IAC procedures and unexpected contingency situation must be prepared. The contingency operation is also designed based on ground contact duration. The LEO satellite was successfully launched and the Bus IAC was successfully performed. In this paper, we explain design concepts and execution results of Bus IAC.

Technologies for Robotized Welding of Big Aluminium Structures with Tolerances for High Speed Trains (고속 열차용 대형 알루미늄 부품의 GAP 대응 로봇 자동화 용접 기술)

  • Lee, Sang Chul
    • Journal of Welding and Joining
    • /
    • v.31 no.1
    • /
    • pp.33-37
    • /
    • 2013
  • Robotized MIG welding of large aluminium components for high speed trains is state-of-the-art. The implementation of online laser cameras enables seam tracking and adoptive modification of welding parameters. A constant fill is achieved regardless of the gap tolerances. Friction Stir Welding has been introduced to the market as a reliable and fast joining technology. The advantages of high welding speeds and the elimination of arc light, fumes and liquefaction in the welding spot lead to economical realisation of heavy-duty gantry systems. FSW robots offer a high flexibility with regard to welding of curved parts, and can be equipped with laser cameras for exact joint tracking.

STUDY ON WELDABILITY OF CU (OFC) BY FRICTION STIR WELDING

  • Bang, Keuk-saeng;Lee, Won-bae;Yeon, Yun-mo;Jung, Seung-boo
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.522-527
    • /
    • 2002
  • The microstructure and mechanical properties of friction stir welded OFC plates with 2mm in thickness were examined with the changing welding parameters such as welding speed, rotation speed in this study. The sounding welding conditions was acquired at the optimum welding conditions of the 41mm/min to 61mm/min of welding speed at 1250 rpm of rotation speed. The microstructure of weld zone was divided into four parts such as the base metal region (EM), thermal mechanical affected zone (TMAZ), heat affected zone (HAZ), stir zone (SZ). The grain size in the SZ and the width of weld nugget were increased with increasing welding speed. The hardness profiles of the base metal were distributed about 80HV. The HAZ is a slightly softened region of about 60~75 HV relative to the base metal. The hardness profiles of the SZ were higher than that of base metal. The tensile strength was increased with increasing welding speed. In case increasing rotation speed, tensile strength was decreased. The maximum tensile strength was about 220:MPa which was 110% of joint efficience of that of base metal at 41mm/min of welding speed, 1250rpm of rotation speed.

  • PDF