Wet Etching Behaviors of Transparent Conducting Ga-Doped Zinc Oxide Thin Film by Organic Acid Solutions

  • Lee, Dong-Kyoon;Lee, Seung-Jung;Bang, Jung-Sik;Yang, Hee-Sun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2008년도 International Meeting on Information Display
    • /
    • pp.831-833
    • /
    • 2008
  • 150 nm thick Ga-doped ZnO thin film, which was deposited by a sputtering process, was wet-chemically etched by using various organic acids such as oxalic, citric and formic acid. Wet etch parameters including etchant concentration and temperature are investigated for each etchant, and their effects on the etch rate and the feature of edge line are compared.

  • PDF

Reduction of reflection from PET (polyethylene terephthalate) film surface by natural plasma etching

  • Oh, Hoon;Song, Yu-Jin;Whang, Ki-Woong
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2006년도 6th International Meeting on Information Display
    • /
    • pp.1419-1424
    • /
    • 2006
  • We could reduce the reflection from PET(polyethylene terephthalate) film surface by natural plasma etching which does not use etch masks. The plasma etched PET film showed lower reflectance and higher transmittance which is resulted by making subwavelength structure(SWS) on the film surface by the plasma etch rate difference between the amorphous and crystalline region in the surface of PET film.

  • PDF

A Study on the Plasma Etching of Ru Electrodes using $O_2/Cl_2$ Helicon Discharges

  • Kim, Hyoun-Woo;Hwang, Woon-Suk
    • Corrosion Science and Technology
    • /
    • 제2권4호
    • /
    • pp.189-193
    • /
    • 2003
  • The Ru etching using $O_2/C_{12}$ plasmas has been studied by employing the helicon etcher. The changes of Ru etch rate, Ru to $SiO_2$ etch selectivity and Ru electrode etching slope with varied process variables were investigated. The Ru etching slope at the optimized etching condition was measured to be $84^{\circ}$. We reveal that the Ru etching using $O_2/C_{12}$ plasma generates the $RuO_2$ thin film. Possible mechanism of Ru etching is discussed.

Ridge Formation by Dry-Etching of Pd and AlGaN/GaN Superlattice for the Fabrication of GaN Blue Laser Diodes

  • 김재관;이동민;박민주;황성주;이성남;곽준섭;이지면
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2012년도 제42회 동계 정기 학술대회 초록집
    • /
    • pp.391-392
    • /
    • 2012
  • In these days, the desire for the precise and tiny displays in mobile application has been increased strongly. Currently, laser displays ranging from large-size laser TV to mobile projectors, are commercially available or due to appear on the market [1]. In order to achieve a mobile projectors, the semiconductor laser diodes should be used as a laser source due to their size and weight. In this presentation, the continuous etch characteristics of Pd and AlGaN/GaN superlattice for the fabrication of blue laser diodes were investigated by using inductively coupled $CHF_3$ and $Cl_2$ -based plasma. The GaN laser diode samples were grown on the sapphire (0001) substrate using a metal organic chemical vapor deposition system. A Si-doped GaN layer was grown on the substrate, followed by growth of LD structures, including the active layers of InGaN/GaN quantum well and barriers layer, as shown in other literature [2], and the palladium was used as a p-type ohmic contact metal. The etch rate of AlGaN/GaN superlattice (2.5/2.5 nm for 100 periods) and n-GaN by using $Cl_2$ (90%)/Ar (10%) and $Cl_2$ (50%)/$CHF_3$ (50%) plasma chemistry, respectively. While when the $Cl_2$/Ar plasma were used, the etch rate of AlGaN/GaN superlattice shows a similar etch rate as that of n-GaN, the $Cl_2/CHF_3$ plasma shows decreased etch rate, compared with that of $Cl_2$/Ar plasma, especially for AlGaN/GaN superlattice. Furthermore, it was also found that the Pd which is deposited on top of the superlattice couldn't be etched with $Cl_2$/Ar plasma. It was indicating that the etching step should be separated into 2 steps for the Pd etching and the superlattice etching, respectively. The etched surface of stacked Pd/superlattice as a result of 2-step etching process including Pd etching ($Cl_2/CHF_3$) and SLs ($Cl_2$/Ar) etching, respectively. EDX results shows that the etched surface is a GaN waveguide free from the Al, indicating the SLs were fully removed by etching. Furthermore, the optical and electrical properties will be also investigated in this presentation. In summary, Pd/AlGaN/GaN SLs were successfully etched exploiting noble 2-step etching processes.

  • PDF

PECVD TEOS $SiO_2$막의 특성에 관한 연구 (Studies on the Properties of the Plasma TEOS $SiO_2$ Film)

  • 이수천;이종무
    • 한국세라믹학회지
    • /
    • 제31권2호
    • /
    • pp.206-212
    • /
    • 1994
  • Effects of the film deposition process parameters on the properties such as deposition rate, etch rate, refractive index, stress and step coverage of plasma enhanced chemical vapor deposited (PECVD) tetraethylorthosilicate glass (TEOS) SiO2 film were investigated and analysed using SEM, FTIR and SIMS techniques. Increasing TEOS flow or decreasing O2 flow increased the deposition rate and the compressive stress of the oxide film but produced a less denser film. The deposition rate decreased owing to the decrease in the sticking coefficient of the TEOS and the O2 molecules onto the substrate Si with increasing the substrate temperature. Increasing the substrate temperature produced a denser film with a lower etch rate and the higher refractive index by lowering SiOH and moisture contents. Increasing the rf power increases the ion bombardment energy. This increase in energy, in turn, increases the deposition rate and tends to make the film denser. No appreciable changes were found in the deposition rate but the refractive index and the stress of the film decreased with increasing the deposition pressure. The carbon content in the plasma TEOS CVD oxide film prepared under our standard deposition conditions were very low according to the SIMS analysis results.

  • PDF

The Development of Cl-Plasma Etching Procedure for Si and SiO$_2$

  • Kim, Jong-Woo;Jung, Mi-Young;Park, Sung-Soo;Boo, Jin-Hyo
    • 한국표면공학회지
    • /
    • 제34권5호
    • /
    • pp.516-521
    • /
    • 2001
  • Dry etching of Si wafer and $SiO_2$ layers was performed using He/Cl$_2$ mixture plasma by diode-type reactive ion etcher (RIE) system. For Si etching, the Cl molecules react with the Si molecules on the surface and become chemically stable, indicating that the reactants need energetic ion bombardment. During the ion assisted desorption, energetic ions would damage the photoresist (PR) and produce the bad etch Si-profile. Moreover, we have examined the characteristics of the Cl-Si reaction system, and developed the new fabrication procedures with a $Cl_2$/He mixture for Si and $SiO_2$-etching. The developed novel fabrication procedure allows the RIE to be unexpensive and useful a Si deep etching system. Since the etch rate was proved to increase linearly with fHe and the selectivity of Si to $SiO_2$ etch rate was observed to be inversely proportional to fHe.

  • PDF

Cl2/Ar 플라즈마를 이용한 Al2O3 박막의 식각 (Dry Etching of Al2O3 Thin Film by Cl2/Ar Plasma)

  • 양설;엄두승;김관하;송상헌;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제22권12호
    • /
    • pp.1005-1008
    • /
    • 2009
  • In this study, adaptively coupled plasma (ACP) source was used for dry etching of $Al_2O_3$ thin film. During the etching process, the wafer surface temperature is an important parameter to influent the etching characteristics. Therefore, the experiments were carried out in ACP to measuring the etch rate, the selectivities of $Al_2O_3$ thin film to mask materials and the etch profile as functions of $Cl_2$/Ar gas ratio and substrate temperature. The highest etch rate of $Al_2O_3$ was 65.4 nm/min at 75% of $Cl_2/(Cl_2+Ar)$ gas mixing ratio. The etched profile was characterized using field effect scanning electron microscopy (FE-SEM). The chemical states of $Al_2O_3$ thin film surfaces were investigated with x-ray photoelectron spectroscopy (XPS).

Cl2/BCl3/Ar 플라즈마에서 반응성 이온들에 의해 식각된 ZnO 박막 표면 연구 (A Study of the Etched ZnO Thin Films Surface by Reactive Ion in the Cl2/BCl3/Ar Plasma)

  • 우종창;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제23권10호
    • /
    • pp.747-751
    • /
    • 2010
  • In the study, the characteristics of the etched Zinc oxide (ZnO) thin films surface, the etch rate of ZnO thin film in $Cl_2/BCl_3/Ar$ plasma was investigated. The maximum ZnO etch rate of 53 nm/min was obtained for $Cl_2/BCl_3/Ar$=3:16:4 sccm gas mixture. According to the x-ray diffraction (XRD) and atomic force microscopy (AFM), the etched ZnO thin film was investigated to the chemical reaction of the ZnO surface in $Cl_2/BCl_3/Ar$ plasma. The field emission auger electron spectroscopy (FE-AES) analysis showed an elemental analysis from the etched surfaces. According to the etching time, the ZnO thin film of etched was obtained to The AES depth-profile analysis. We used to atomic force microscopy to determine the roughness of the surface. So, the root mean square of ZnO thin film was 17.02 in $Cl_2/BCl_3/Ar$ plasma. Based on these data, the ion-assisted chemical reaction was proposed as the main etch mechanism for the plasmas.

OES 를 이용한 SBT 박막의 식각 메카니즘 연구 (The Study of Etching Mechanism in $SrBi_2Ta_2O_9$ thin film by Optical Emission Spectroscopy)

  • 신성욱;김창일;장의구;이원재;유병곤;김태형
    • 한국항해항만학회:학술대회논문집
    • /
    • 한국항해항만학회 2000년도 추계학술대회논문집
    • /
    • pp.40-44
    • /
    • 2000
  • In this paper, since the research on the etching of SrBi$_2$Ta$_2$O$_{9}$ (SBT) thin film was few (specially Cl$_2$-base ), we had studied the surface reaction of SBT thin films using the OES in high density plasma etching as a function of rf power, dc bias voltage, and Cl$_2$/(C1$_2$+Ar) gas mixing ratio. It had been found that the etch rate of SBT thin films appeared to be more affected by the physical sputtering between Ar ions and surface of the SBT compared to the chemical reaction in our previous papers$^{1.2}$ . The change of Cl radical density that is measured by the OES as a function of gas combination showed the change of the etch rate of SBT thin films. Therefore, the chemical reactions between Cl radical in plasma and components of the SBT enhance to increase the etch rates of SBT thin films and these results were confirmed by XPS analysis.

  • PDF

BCl3/Ar 플라즈마에 Cl2 가스 첨가에 따른 TiN 박막의 식각 특성 (Etch Characteristics of TiN Thin Film with Addition Cl2 Gas in BCl3/Ar Plasma)

  • 엄두승;우종창;김동표;김창일
    • 한국전기전자재료학회논문지
    • /
    • 제21권12호
    • /
    • pp.1051-1056
    • /
    • 2008
  • In this study, the investigations of the TiN etching characteristics were carried out with addition of $Cl_2$ gas in an inductively coupled $BCl_3$-base plasma system. Dry etching of the TiN was studied by varying the etching parameters including $Cl_2$ gas addition ratio, RF power, DC-bias voltage and pressure. The etch rate of TiN thin film was maximum when the $Cl_2$ gas addition flow was 2 sccm with fixed other conditions. As the RF power DC-bias voltage were increased, the etch rate of TiN thin film showed increasing tendency. $BCl_3/Cl_2$/Ar plasmas were characterized by optical emission spectroscopy (OES) analysis. The chemical reaction on the surface of the etched TiN films was investigated with X-ray photoelectron spectroscopy (XPS).