• 제목/요약/키워드: Empress 2

검색결과 101건 처리시간 0.02초

열가압 및 열처리에 따른 IPS Empress 2 세라믹의 굴곡강도와 미세구조 (FLEXURE STRENGTH AND MICROSTRUCTURE OF IPS EMPRESS 2 GLASS-CERAMIC ON HEAT-PRESSING AND HEAT TREATMENTS)

  • 오상천;동진근
    • 대한치과보철학회지
    • /
    • 제38권5호
    • /
    • pp.575-582
    • /
    • 2000
  • This investigation was designed to determine whether heat-pressing and/or simulated heat treatments affected the flexure strength and the microstructure of the lithium disilicate glass-ceramic in the IPS Empress 2 system. Four groups of the specimens were prepared as follows: group 1 - as-received material, group 2 - heat-pressed material; group 3 - heat-pressed and simulated initial heat-treated material; group 4 - heat-pressed and the simulated heat-treated material with full firings for a final restoration. The three-point bending test and the scanning elec-tron microscope (SEM) analysis was conducted for the purpose of this study. The flexure strength of group 2 was significantly higher than that of group 1. However, there were no significant differences in strength among group 2, 3, and 4, and between group 1 and 4. The SEM micrographs of the lithium disilicate glass-ceramic showed the closely packed, multi-directionally interlocking microstructure of numerous lithium disilicate crystals protruding from the glass matrix. The crystals of the heat-pressed materials (group 2, 3, and 4) were a little denser and about two times bigger than those of the as-received material (group 1). This change of microstructure is more obviously exhibited particularly between group 1 and 2. However, there was no a marked difference among group 2, 3, and 4 after the heat-pressing procedure. Although there were significant increase of the strength and some changes of the microstructure after the heat-pressing operation, the combination of the heat-pressing and the simulated subsequent heat treatments did not produce the increase of strength of IPS Empress 2 glass-ceramic.

  • PDF

열가압 및 열처리에 따른 IPS Empress 2 Glass-Ceramic의 색 안정성 (Color Stability of IPS Empress 2 Glass-Ceramic after Heat-Pressing and Heat-Treatments)

  • 송기범;이상권;김유리;오상천
    • 구강회복응용과학지
    • /
    • 제18권2호
    • /
    • pp.93-99
    • /
    • 2002
  • This study was performed to investigate the color stability of IPS Empress 2 glass-ceramic after heat-pressing and/or heat-treatments. Three types of IPS Empress 2 ingots (shade 100, 300, 500) were tested. For this study, three groups were prepared as follows: group 1 is as-received material, group 2 is heat-pressed material, and group 3 is fully heat -treated material. The color of the specimens was measured with a colorimeter. The data were statistically evaluated with one-way ANOVA and Scheffe's multiple test. The results obtained were as follows: 1. IPS Empress 2 glass-ceramic demonstrated less color stability according as the shade is lighter. Namely, the shade 500 showed the lowest color shifts and the shade 100 showed the greatest color shifts after heat-pressing and heat-treatments. 2. In the cases of shade 100 and 300, the changes of ${\Delta}E^*$ were affected mostly by the changes of $L^*$ and $b^*$. 3. In ${\Delta}E^*$ of the shade 100, there were significant differences among the group 1, 2, and 3 (P<0.001). 4. In ${\Delta}E^*$ of the shade 300, there were significant differences between the group 1 and 2, and the group 1 and 3 (P<0.001). 5. In ${\Delta}E^*$ of the shade 500, there was significant difference only between the group 1 and 3 (P<0.001).

In vitro study of compressive fracture strength of Empress 2 crowns cemented with various luting agents

  • Kim Min-Ho;Yang Jae-Ho;Lee Sun-Hyung;Chung Hun-Young;Chang Ik-Tae
    • 대한치과보철학회지
    • /
    • 제39권3호
    • /
    • pp.260-272
    • /
    • 2001
  • All-ceramic restorations have had a more limited life expectancy than metal ceramic restorations because of their low strength. Their relatively lower strength and resistance to fracture have restricted the use of all-ceramic crowns to anterior applications where occlusal loads are lower. But there has been increasing interest in all-ceramic restorations because patients are primarily concerned with improved esthetics. Many efforts have been made to in prove the mechanical properties of dental ceramics. This study was designed to elucidate the influence of the luting agent on the strength of the Empress 2 crown (staining technique) cemented on human teeth. Seventy extracted human permanent molar teeth were chosen. Teeth were prepared for Empress 2 crowns with milling machine on a surveyor. A dental bur was placed in the mandrel that was positioned so that the long axis of the bur was perpendicular to the surveyor base. Dimensions of the Empress 2 crown preparation were $6^{\circ}$ taper on each side, $1.5{\pm}0.1mm$ shoulder margin, and 4mm crown height. The luting cements used in this study were as follow: 1. Uncemented 2. Zinc phosphate cements (Confi-Dental) 3. Conventional glass ionomer cement : Fuji 1 (GC) 4. Resin-modified glass ionomer cements : Fuji plus (GC) 5. Adhesive cements : Panavia F (Kuralay), Variolink II (Vivadent), Choice (Bisco). Fracture test using Instron. The crowns were loaded in compressive force to evaluate the effect of these cements on the breaking strength of these all-ceramic crowns. A steel ball with a diameter of 4mm was placed on the occlusal surface and load was applied to the steel ball by a cylindrical bolt with a crosshead speed of 0.5mm per minute until fracture occurred. The fractured surface was examined using Scanning Electron Microscopic Image (SEM) to discover the correlation between fracture strength and bonding capacity. Within the limitation of this in vitro study design, the results were as follows : 1. fomentations significantly increased the fracture resistance of Empress ceramic crowns compared to control. Uncemented (206.9 N): ZPC (812.9 N): Fuji 1 (879.5 N): Fuji Plus (937.7 N): Choice (1105.4 N): Variolink II (1221.1 N): Panavia F (1445.2 N). 2. Resin luting agent, treated by a silane bond enhancing agents, yielded a significant increase in fracture resistance. In some of the Panavia F group, a fracture extended into dentin. 3. According to SEM images of fractured Empress crowns, the stronger the bond at both interfaces(crown and die), the more fracture strength was acquired.

  • PDF

MARGINAL FIDELITY AND FRACTURE STRENGTH OF IPS EMPRESS $2^{(R)}$ CERAMIC CROWNS ACCORDING TO DIFFERENT CEMENT TYPES

  • Cho Hyun-Ok;Kang Dong-Wan
    • 대한치과보철학회지
    • /
    • 제40권6호
    • /
    • pp.545-559
    • /
    • 2002
  • There has been increasing use of IPS Empress $2^{(R)}$ owing to easy fabrication method, high esthetics similar to natural teeth, good marginal accuracy, and sufficient fracture strength. However, in clinical application, although a luting agent and the tooth cementation bonding procedure influence the marginal accuracy and fracture strength restoration, there has been a controversy in the selection of proper luting agent. This study was to measure the marginal fidelites and fracture strength of IPS Empress crowns according to three cement types, Protec $cem^{(R)}$, Variolink $II^{(R)}$ and Panavia $21^{(R)}$. After construction of 12 experimental dies for each group, IPS Empress $2^{(R)}$ crowns were fabricated and luted the metal master die prepartion of the maxillary right premolar. Marginal gaps before cementation and after cementation were measured. Buccal incline on the functional cusp of specimens were loaded until the catastrophic failure and fracture strength was measured. The results of this study were as follows: 1. The range of gap was $34.04{\pm}4.84{\mu}m$ before cementation and $37.88{\pm}5.00{\mu}m$ after cementation, which showed significant difference by paired t-test (p<0.05). The difference in the results from marginal accuracy according to measuring point proved to be not statistically significant by two-way ANOVA test (p>0.05). 2. The difference in the results from marginal accuracy according to three cement types Proved that The Variolink $II^{(R)}$ cement group had the least gap, $35.43{\pm}5.03{\mu}m$, and showed superior marginal accuracy while there existed statistic significance in Protec $cem^{(R)}$ cement group, $39.06{\pm}4.41{\mu}m$ or Panavia $21^{(R)}$ cement group, $39.16{\pm}4.39{\mu}m$ by two-way ANOVA test & multiple range test (p<0.05). 3. The difference in the results from fractures strength testing according to three cement type groups proved to be statistically significant (p<0.05). The Variolink $II^{(R)}$ cement group shows highest fracture strength of $1257.33{\pm}226.77N$, Panavia $21^{(R)}$ cement group has $1098.08{\pm}138.45N$, and Protec $cem^{(R)}$ cement group represents the lowest fracture strength of $926.75{\pm}115.75N$. 4. Three different cement groups of different components showed acceptable marginal fidelity and fracture strength. It is concluded that IPS Empress $2^{(R)}$ crowns luted using Variolink $II^{(R)}$ cement group had stronger fracture strength and smaller marginal gap than the other cement groups. Although Variolink $II^{(R)}$ resin cement seemed acceptable to clinical applications in IPS Empress $2^{(R)}$ system, the IPS Empress $2^{(R)}$ system still requires long-term research due to the lack of data in clinical applications.

IPS Empress $2^(R)$를 이용한 전부도재관의 변연적합성과 파절강도에 관한 연구 (A STUDY ON THE MARGINAL FIDELITIES AND FRACTURE STRENGTH OF IPS EMPRESS $2^(R)$ CERAMIC CROWNS)

  • 유지형;김용철;강동완
    • 대한치과보철학회지
    • /
    • 제38권5호
    • /
    • pp.606-617
    • /
    • 2000
  • The purpose of this study was to measure the marginal fidelities and the fracture strength of IPS Empress $2^{(R)}\;and\;In-Ceram^{(R)}$ ceramic crowns. After constructed of 12 experimental dies for each group, ceramic crowns were fabricated on the metal master dies prepared on the maxillary right premolar Marginal gaps were measured on the specimen between the margin of each crown and finish-ing line of the metal master die by using stereo-microscope($SZ-ST^{(R)}$ Olympus, Japan) and all specimens were cemented on the metal master die with Bistite $II^{(R)}$ (Tokuyama soda Co, LTD., Japan) resin cement. Finally marginal gaps were measured again. To measure of the fracture strength, buccal incline on the functional cusp of specimens were loaded until the catastrophic failure occurred by using the AGS-1000 $D^{(R)}$(Shimadzu, Japan). The result of marginal fidelities and fracture strength were statistically analyzed with the SPSS version 8.0 programs. The results of this study were as follows : 1. No significant difference was found in the mean marginal fidelities and fracture strength between the IPS Empress $2^{(R)}\;and\;In-Ceram^{(R)}$. 2. In comparison of marginal fidelities between before and after cementation, there was significant difference(P<0.05). The IPS Empress 2 system was shown in this study that had good marginal fidelities and fracture strength compared to In-Ceram ceramics. Although this system was acceptable to clinical applications, the system still has to be considered long-term researches about marginal fidelities and fracture strength due to the lack of data about the clinical researches.

  • PDF

다양한 IPS Empress Esthetic$^{(R)}$ ingot으로 제작한 laminate veneer의 최종 색조에 대한 영향 (Influencing factors on the final color of laminate veneer restorations with various IPS Empress Esthetic$^{(R)}$ ingots)

  • 양미선;김석규
    • 대한치과보철학회지
    • /
    • 제49권4호
    • /
    • pp.308-315
    • /
    • 2011
  • 연구 목적: IPS Empress Esthetic$^{(R)}$ system의 ingot은 다양한 반투명도를 가지고 있지만, 실제 다양한 색조의 자연치를 배경으로 각각의 ingot을 laminate veneer로 제작했을 때 어느 정도의 차폐능력을 나타내는지 알 수 없다. 본 연구의 목적은 반투명도가 서로 다른 ingot으로 제작한 IPS Empress Esthetic$^{(R)}$ laminate veneer 수복 시 다른 색상의 지대치상에서 최종 색조의 차이(color difference, ${\Delta}E$)를측정, 분석해서 그 차폐효과를 평가하고, 최종 색조에 미치는 영향을 알아보고자 하였다. 연구 재료 및 방법: Laminate veneer 수복을 위해 삭제된 6가지 다른 색조(A1, A3, A4, B2, B3, C3)의 자연치아 위에 반투명도가 서로 다른 6가지 IPS Empress Esthetic$^{(R)}$ ingot (E 01, E 03, E OC1, E TC1, E TC2, E TC3)으로 제작된 총 두께 0.6 mm의 도재 시편들을 translucent shade의 시적용 합착제로 시적한 뒤 각 시편 조합의 색조를 색채계(colorimeter)를 이용하여 측정하였다. 서로 다른 색조의 지대치아 위에서 측정된 도재시편들의 색차를 비교, 분석하였다. 결과: 지대치 색조 및 coping의 반투명도에 따라서 laminate veneer 수복물의 최종 색조가 다르게 나타났다(P<.05). 모든 도재 시편에서 A3, B3, 그리고 C3 shade를 가진 지대치들 사이의 평균 색차값(${\Delta}E$)이 2.7 이하로 나타났고, 지대치들 간의 색조가 A3 와 A4, B3 와 A4, 그리고 C3 와 A4 인 경우 평균 색차값은 몇 가지 도재 시편에서 2.7 이하를 나타내어 laminate veneer 수복물에 의한 지대치 색조의 차폐효과를 보여 주었다. 반면, A1 과 B2 shade의 지대치는 다른 지대치들과 비교하여 높은 색조 차이를 보였으며, 특히A4와 B2, A3 와 B2, 그리고 A1 과 A4 색조의 지대치들 사이에는 그 색조 차이가 컸다. 결론: IPS Empress Esthetic$^{(R)}$ coping으로 제작된 laminate veneer의 최종 색조는 지대치 색조 및 coping의 반투명도에 의해 영향을 받았다. 서로 다른 $a^*$$b^*$ 값을 나타내는 지대치들의 색상 차이는 어느 정도 차폐 되는 효과를 보여주고 있으나, 명도($L^*$)의 차이가 많이 나타나는 지대치 색조들을 차폐하는 것은 한계가 있었다.

IPS Empress 도재관의 파절강도 : 하악 제2소구치에서 교합면 두께와 축면 경사도에 따른 영향 (FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER SECOND PREMOLAR)

  • 김희진;이해형;남영성;동진근
    • 대한치과보철학회지
    • /
    • 제40권5호
    • /
    • pp.441-450
    • /
    • 2002
  • The purpose of this study was compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower second premolar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement. The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1284 N). Crowns of 1.5mm depth and $8^{\circ}$ inclination had the lowest strength (951 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth.

IPS Empress 도재관의 파절강도: 하악 제1대구치에서 교합면 두께와 축면경사도에 따른 영향 (FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECT OF OCCLUSAL DEPTH AND AXIAL INCLINATION ON LOWER FIRST MOLAR)

  • 김성훈;이진한;김유리;동진근
    • 대한치과보철학회지
    • /
    • 제41권1호
    • /
    • pp.48-60
    • /
    • 2003
  • The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the occlusal depth (1.5mm, 2.0mm, 2.5mm) and axial inclination ($4^{\circ},\;8^{\circ},\;12^{\circ}$) of the lower First Molar. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and cemented with resin cement(Bistite resin cement, Tokuyama Soda Co. LTD., Japan). The cemented crowns were mounted on the testing jig with inclination of 30 degrees and the universal testing machine(Zwick Z020, Zwick, Germany)was used to measure the fracture strength. The results of this study were as follows : 1. The fracture strength of the ceramic crown with 2.5mm depth and $12^{\circ}$ inclination was the highest (1789 N). Crowns of 1.5mm depth and $4^{\circ}$ inclination had the lowest strength (1091 N). 2. There were no significant differences in the fracture strength by axial inclination of the same occlusal depth group. 3. Most fracture lines began at the loading area and extended through proximal surface perpendicular to the margin, irrespective of occlusal depth. Size of fragment was affected by the amount of occlusal reduction.

IPS Empress 도재관의 파절강도 : 상악 견치에서 절단연 삭제량과 축면 경사도에 따른 영향 (FRACTURE STRENGTH OF THE IPS EMPRESS CROWN : THE EFFECTS OF INCISAL REDUCTION AND AXIAL INCLINATION ON UPPER CANINE)

  • 신동국;강한중;박용석;박광수;동진근
    • 대한치과보철학회지
    • /
    • 제43권1호
    • /
    • pp.30-40
    • /
    • 2005
  • Purpose. The purpose of this study was to compare the fracture strength of the IPS Empress ceramic crown according to the incisal reduction (2.0mm, 2.5mm, 3.0mm) and axial inclination ($4^{\circ}$, $8^{\circ}$, $12^{\circ}$) of the upper canine. Material and methods. After 10 metal dies were made for each group, the IPS Empress ceramic crowns were fabricated and each crown was cemented on each metal die with resin cement. The cemented crowns mounted on the testing jig were inclined 30 degrees and the universal testing machine was used to measure the fracture strength. Results. 1. The fracture strength of the ceramic crown with 3.0mm depth and $12^{\circ}$ inclination was the highest (839N) Crowns of 2.0mm depth and $12^{\circ}$ inclination had the lowest strength (559N). 2. There was no significant difference in the fracture strength by axial inclination in the same incisal reduction group. 3. The fracture mode of the crowns was similar. Most of fracture lines began at the loading area and extended through proximal surface perpendicular to the margin irrespective of incisal reduction.

재 사용된 IPS-empress ingot의 pressing accuracy에 관한 연구 (A STUDY ON THE PRESSING ACCURACY OF THE REUSED IPS-EMPERESS INGOT)

  • 송병권;박현배;오상천;진태호
    • 대한치과보철학회지
    • /
    • 제35권2호
    • /
    • pp.357-364
    • /
    • 1997
  • IPS-empress system is one of widely used all ceramic system. The purpose of this study was to determine the pressing accuracy of reused IPS%Empress ingot. 10 specimens were made using new ingot first, and using the rests of the specimen the another group of specimens were made next. finally, the third group of specimens were made with same procedure mentioned above. The results obtained in this study were as follows ; 1. The pressing accuracy of the first group of specimen was 96.1%, that of the second group was 95.4%, and that of the third group was 95.4%. There was no statistical significance among them, that is, the reuse of the IPS-Empress ingot did not influence on the pressing accuracy. 2. the common site of the defect in pressed ingot was central area at the margin opposite of sprue hole.

  • PDF