• Title/Summary/Keyword: Eco-Al

Search Result 124, Processing Time 0.028 seconds

Thermal Stability and Fracture Toughness of Epoxy Resins Modified with Epoxidized Castor Oil and Al2O3 Nanoparticles

  • Zhu, Lin;Jin, Fan-Long;Park, Soo-Jin
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.8
    • /
    • pp.2513-2516
    • /
    • 2012
  • This study examined the effects of the epoxidized castor oil (ECO) and $Al_2O_3$ content on the thermal stability and fracture toughness of the diglycidylether of bisphenol-A (DGEBA)/ECO/$Al_2O_3$ ternary composites using a range of techniques. The thermal stability of the composites was decreased by the addition of ECO and $Al_2O_3$ nanoparticles. The fracture toughness of the composites was improved significantly by the addition of ECO and $Al_2O_3$ nanoparticles. The composite containing 3 wt % $Al_2O_3$ nanoparticles showed the maximum flexural strength. Scanning electron microscopy (SEM) revealed tortuous cracks in the DGEBA/ECO/$Al_2O_3$ composites, which prevented deformation and crack propagation.

Solvothermal Synthesis of α-Al2O3 from Boehmite with Seeding Technique

  • Jo, Hye Youn;Park, Min-Gyeong;Lee, Seung-Ho;Kim, Dae Sung;Lee, Young Kwan;Lim, Hyung Mi
    • Journal of the Korean Ceramic Society
    • /
    • v.52 no.4
    • /
    • pp.273-278
    • /
    • 2015
  • ${\alpha}-Al_2O_3$ was synthesized by solvothermal synthesis using ${\alpha}-Al_2O_3$ seed, precursor of fine boehmite (Al(OOH)) or gibbsite ($Al(OH)_3$), and 1, 4-butanediol solvent. The seed content and precursor type were selected as variables in order to synthesize ${\alpha}-Al_2O_3$. The formation time of ${\alpha}-Al_2O_3$ was reduced and the size of the particles was decreased with addition of the seed. When the seed content was increased, the size of the synthesized ${\alpha}-Al_2O_3$ was reduced. Morphologies of the as-synthesized ${\alpha}-Al_2O_3$ with ${\alpha}-Al_2O_3$ seed were polyhedron-shaped, while the shape was plate-like or polyhedral without the seed, depending on the additives or the average particle size of the boehmite precursor. The aggregation of as-synthesized ${\alpha}-Al_2O_3$ from boehmite was smaller than that from gibbsite. As-synthesized ${\alpha}-Al_2O_3$, with 140 nm size, was obtained by using the seed and boehmite precursor.

Ignition resistance of CaO added Mg-3Al, Mg-6Al and Mg-9Al Eco-Mg alloys (CaO가 첨가된 Mg-3Al, Mg-6Al 및 Mg-9Al Eco-Mg 합금의 발화 저항성 평가)

  • Lee, Jin-Kyu;Kim, Shae-K.
    • Journal of Korea Foundry Society
    • /
    • v.31 no.2
    • /
    • pp.60-65
    • /
    • 2011
  • Molten magnesium alloys and magnesium products are easily oxidized and burned when they are exposed to high temperature for manufacturing process and by accident. In order to solve these problems, CaO addition in magnesium alloys has been developed. The ignition resistance of CaO added Mg-3Al, Mg-6Al, and Mg-9Al Eco-Mg alloys were investigated in comparison with those of magnesium alloys without CaO. The ignition resistance was examined by three methods : DTA, furnace chip ignition test, and torch ignition test. DTA was carried out for obtaining quantitative ignition temperature data with respect to specimen geometry and test environment; the furnace ignition test for burr and chip ignition temperature data; and the torch test for ignition temperature data for manufactured products. The ignition resistance of magnesium alloys under all conditions greatly increased by CaO addition.

Eco-friendly Fabrication Process of Al-Ti-C Grain Refiner

  • Cho, Hoon;Kim, Bong-Hwan
    • Journal of Korea Foundry Society
    • /
    • v.30 no.4
    • /
    • pp.147-150
    • /
    • 2010
  • An eco-friendly production technique of Al-8.6Ti-0.025C refiner was developed by melting a Al-Ti master alloy in a graphite crucible, in which the potential nucleation site, TiC effectively formed by the spontaneous in-situ reaction between excessive Ti and carbon from graphite crucible. The A3003 alloy refined by the Al-8.6Ti-0.025C showed effectively refined macrostructure and enhanced mechanical properties comparable to the commercial Al-Ti-B refiner. The effective refinement was achieved in a shorter compare to the melt-treating time commercial Al-Ti-B refiner.

Microstructure and Mechanical Properties at Room and Elevated Temperatures in AM50-0.3 wt%CaO Alloy (AM50-0.3 wt%CaO 합금의 미세조직과 상·고온 기계적 특성)

  • Cho, Eun-Ho;Jun, Joong-Hwan;Kim, Young-Jik
    • Korean Journal of Materials Research
    • /
    • v.22 no.10
    • /
    • pp.499-503
    • /
    • 2012
  • The present study is intended to comparatively investigate the changes in microstructure and tensile properties at room and elevated temperatures in commercial AM50(Mg-5%Al-0.3%Mn) and 0.3 wt%CaO added ECO-AM50 alloys produced by permanent mould casting. The typical microstructure of AM50 alloy was distinctively characterized using two intermetallic compounds, ${\beta}(Mg_{17}Al_{12})$ and $Al_8Mn_5$, along with ${\alpha}$-(Mg) matrix in an as-cast state. The addition of a small amount of CaO played a role in reducing dendrite cell size and quantity of the ${\beta}$ phase in the AM50 alloy. It is interesting to note that the added CaO introduced a small amount of $Al_2Ca$ adjacent to the ${\beta}$ compounds, and that inhomogeneous enrichment of elemental Ca was observed within the ${\beta}$ phase. The ECO-AM50 alloy showed higher hardness and better YS and UTS at room temperature than did the AM50 alloy, which characteristics can be mainly ascribed to the finer-grained microstructure that originated from the CaO addition. At $175^{\circ}C$, higher levels of YS and UTS and higher elongation were obtained for the ECO-AM50 alloy, demonstrating that even 0.3 wt%CaO addition can be beneficial in promoting the heat resistance of the AM50 alloy. The combinational contributions of enhanced thermal stability of the Ca-containing ${\beta}$ phase and the introduction of a stable $Al_2Ca$ phase with high melting point are thought to be responsible for the improvement of the high temperature tensile properties in the ECO-AM50 alloy.

ECO(Electro-Coagulation & Oxidation) 공법에서 전극 및 전류밀도에 따른 축산폐수 처리특성 변화

  • Kim, Hak-Seok;Kim, Hong-Tae;Kim, Jeong-Bae;Lee, Du-Hui
    • Proceedings of the Korean Environmental Sciences Society Conference
    • /
    • 2008.11a
    • /
    • pp.510-514
    • /
    • 2008
  • 본 연구에서는 전극의 특성에 따른 돈사유래 축산폐수의 ECO 공법에 의한 처리특성을 평가하기 위해 ECO 시스템 모듈내 Fe-Fe 및 Al-Al 계열의 용해성 전극과 Al-SUS, Ir-SUS 등 불용성 전극을 대상으로 5$\sim$20mA/cm$^2$의 전류밀도하에서 축산폐수내 유기물 및 영양염류의 제거특성을 평가하여 다음과 같은 결론을 얻을 수 있었다. 1. 전기응집산화에 의한 축산폐수의 처리시 수중 유기물질 및 영양염류의 제거효율은 전류밀도의 증가에 비례하여 증가한다. 2. 불용성 전극조합 및 불용성-용해성 전극조합은 전류밀도가 높을수록 수중 유기물 및 오염물질 제거효율이 안정되고, 용해성 전극은 15mA/cm$^2$ 이하의 저 전류밀도의 조건하에서 전류밀도의 증가에 따라 안정된 제거효율 향상을 기대할 수 있다. 3. 불용성전극 조합인 Ir-SUS 전극조합을 사용하여 축산폐수를 처리할 경우 COD$_{Mn}$ 제거효율을 약 10% 향상시킬 수 있으며, TN 20mA/cm$^2$에서 Al-Al 전극조합과 TP 15mA/cm$^2$ 이하에서 Fe-Fe 전극조합은 제거효율이 저하되는 경향이 나타난다.

  • PDF

Development of An Eco-friendly Surface Treatment Process for the Design of the Al Lead Tab in Lithium-ion Batteries

  • Cheon, Jeongsuk;Kim, Jongwon
    • Journal of the Korean Chemical Society
    • /
    • v.64 no.3
    • /
    • pp.153-158
    • /
    • 2020
  • With the recent popularity of mobile devices, the demand for lithium-ion batteries is increasing. In this study, the surface treatment process for the development of the Al (aluminum) lead tab for positive electrode, a key component of the pouch-type lithium-ion battery, was investigated. Anodizing and sealing processes were tested as surface treatment techniques. It was found that only a sealing process is needed to obtain sufficient adhesive strength. In the present study, an adhesive strength of 17 N/12 mm was achieved by degreasing and etching pretreatment, followed by a sealing process of 10 min duration. This adhesive strength was greater than that achievable using Cr (chromium) surface treatment. Using various surface analysis techniques, the shape and composition of the surface before and after being subjected to the surface treatment were compared and analyzed. The results of this study are expected to contribute to the development of an eco-friendly lead tab.

Molecular Cloning and Expression of Alkaline Amylase Gene of Alkalophilic Bacillus sp. in Bacillus subtilis and Escherichia coli (알카리성 Bacillus sp.의 호알카리성 amylase 유전자의 Bacillus subtilis와 Escherichia coli로의 cloning과 발현)

  • Bae, Moo;Park, Shin-Hae
    • Microbiology and Biotechnology Letters
    • /
    • v.17 no.2
    • /
    • pp.160-164
    • /
    • 1989
  • A 5.7Kb EcoRI fragment containing alkaline amylase gene of Bacillus sp. AL-8 obtained in the previons experiment (10) was transformed in B. subtilis via plasmid pUB110. The enzymatic proper-ties of the amylase produced by the transformants were Identical to those of the donor strain. Thus, the alkaline amylase activity from the transformant was maximum at pH 10 and 5$0^{\circ}C$. And the enzyme was very stable over the ranges of alkaline pH. In order to determine the location of the alkaline amylase gene within the 5.7Kb DNA fragment, the fragment was subcloned in E. coli. It was found that the alkaline amylase gene was located k EcoRI fragment of 3.7Kb.

  • PDF

Dispersion Property of Al2O3 Nanosol Prepared by Various Dispersion Factors and Silane Modification under Non-Aqueous Solvent (비수계 용매하에서 다양한 분산인자 및 실란 표면개질에 의해 제조된 Al2O3 나노졸의 분산 특성)

  • Na, Ho Seong;Park, Min-Gyeong;Lim, Hyung Mi;Kim, Dae Sung
    • Korean Journal of Materials Research
    • /
    • v.26 no.12
    • /
    • pp.733-740
    • /
    • 2016
  • $Al_2O_3$ nanosol dispersed under ethanol or N-Methyl-2-pyrrolidone(NMP) was studied and optimized with various dispersion factors and by utilizing the silane modification method. The two kinds of $Al_2O_3$ powders used were prepared by thermal decomposition method from aluminum ammonium sulfate$(AlNH_4(SO_4)_2)$ while controlling the calcination temperature. $Al_2O_3$ sol was prepared under ethanol solvent by using a batch-type bead mill. The dispersion properties of the $Al_2O_3$ sol have a close relationship to the dispersion factors such as the pH, the amount of acid additive(nitric acid, acetic acid), the milling time, and the size and combination of zirconia beads. Especially, $Al_2O_3$ sol added 4 wt% acetic acid was found to maintain the dispersion stability while its solid concentration increased to 15 wt%, this stability maintenance was the result of the electrostatic and steric repulsion of acetic acid molecules adsorbed on the surface of the $Al_2O_3$ particles. In order to observe the dispersion property of $Al_2O_3$ sol under NMP solvent, $Al_2O_3$ sol dispersed under ethanol solvent was modified and solvent-exchanged with N-Phenyl-(3-aminopropyl)trimethoxy silane(APTMS) through a binary solvent system. Characterization of the $Al_2O_3$ powder and the nanosol was observed by XRD, SEM, ICP, FT-IR, TGA, Particles size analysis, etc.