• 제목/요약/키워드: Dynamic Tensile Test

검색결과 248건 처리시간 0.026초

변형률속도효과를 고려한 일반냉연강판 점용접부의 피로수명평가 (Fatigue Life Evaluation of Spot Weldments of SPC Sheet Including Strain Rate Effect)

  • 송준혁;나석찬;유효선;강희용;양성모
    • 한국자동차공학회논문집
    • /
    • 제14권1호
    • /
    • pp.48-53
    • /
    • 2006
  • A methodology is described for predicting the fatigue life of the resistance spot weldment including strain rate effect. Because it is difficult to perform a physical failure test with high strain rate, an analytical method is necessary to get the mechanical properties of various strain rate, To this end, quasi-static tensile-shear tests at several strain rate were performed on spot weldments of SPC. These test provided the empirical data with the strain rate. With these results, we formulated the function of fatigue life prediction using the lethargy coefficient which is the global material property from tensile test. And, we predicted the fatigue life of spot weldment at dynamic strain rate. To confirm this method for fatigue life prediction, analytical results were compared with the experimental fatigue data.

計裝化 샬피 시험법 에 의한 알루미늄 합금 용접부 의 동적파괴 인성 (The dynamic fracture toughness of aluminum alloy weld zone by instrumented charpy test)

  • 문경철;강락원;이준희
    • Journal of Welding and Joining
    • /
    • 제3권2호
    • /
    • pp.42-51
    • /
    • 1985
  • The dynamic fracture toughness, fracture characteristics, impact tension and tensile properties of Al-Mg-Si T5 alloy and Al-Zn-Mg T6 alloy respectively welded with filler metal of Alcan 4043 were investigated. The dynamic fracture toughness values were obtained rapidly and simply for the specimen of small size by using instrumented Chirpy impact testing machine. the testing temperatures of the specimen were a range of room temperature and-196.deg. C. The results obtained in this experiment are summarized as follows. With decreasing the testing temperatures, dynamic tensile stress and fracture load were increased, on the other hand the deflection and impact value showed decreasing tendency in order of base metal>HAZ>weld. Changes of total absorbed energy were more influenced by the crack propagation energy than the crack initiation energy. At the low temperatures, the unstable rapid fracture representing the crack propagation appeared for the specimens of Charpy press side notched in Al-Zn-Mg alloy, but it was difficult to obtain the unstable rapid fracture in Al-Mg-Si alloy. Because of the development of plastic zone at the notch root, it was difficult to obtain thevalid $K_{1d}$ value in Al-Mg-Si alloy. Therefore the fatigue cracked specimens were effective in both Al-Mg-Si and Al-Zn-Mg alloys. With decreasing the impact testing temperatures, specimens underwent a transition from dimple-type transgranular fracture to lamella surface-type intergranular fracture because of the precipitate at the grain boundaries, impurities and crystal structure of the precipitates.s.

  • PDF

석탄회 기반 채움재를 활용한 아스팔트 콘크리트의 공학적 특성 (Characteristics of Asphalt Concrete Utilizing Coal Ash Based Filler)

  • 김영욱;박근배;우양이;문보경
    • 한국건설순환자원학회논문집
    • /
    • 제5권3호
    • /
    • pp.305-312
    • /
    • 2017
  • 본 연구에서는 국내 화력발전소에서 발생되고 있는 산업부산물을 활용하여 아스팔트 콘크리트용 채움재를 개발 및 혼합물에 적용하여 함량에 따른 특성 및 소성변형 저항성에 미치는 영향을 관찰하였다. 실험결과 석탄회 기반 채움재를 사용할 경우 최적아스팔트함량(OAC)는 기존 채움재 대비 0.1% 낮은 값을 나타내었다. 도출된 최적아스팔트함량에서 채움재 함량에 따른 간접인장강도 및 인장강도비 측정 결과 함량 증가에 따라 높은 성능을 발현하였고, 2.0% 이상의 함량에서 국내 단체표준 품질관리 기준 각 0.8 이상과 0.75 이상을 만족하는 결과를 얻을 수 있었다. 동적안정도는 채움재 2.5%의 함량에서 가장 높은 저항성을 나타내었으며, 함량이 2.5%를 넘어설 때 오히려 성능발현이 저하되는 결과를 나타내었다. 과도한 채움재의 혼입은 상대적으로 아스팔트 함량이 감소되기 때문에 취성파괴를 유발할 수 있으므로 최적의 채움재/아스팔트 의 비율을 찾아 적용하는 방안이 필요할 것으로 판단된다.

OHT 차량 벨트 동특성 및 피로 수명에 관한 연구 (A Study on Dynamic Analysis and Fatigue Life of the Belt in the OHT Vehicle)

  • 정일호;김창수;조동협;박중경;박태원
    • 대한기계학회논문집A
    • /
    • 제29권8호
    • /
    • pp.1085-1092
    • /
    • 2005
  • The OHT(Over Head Transportation) Vehicle transports heavy products quickly and repeatedly at the industrial workplace. The belt in the OHT vehicle is used to support the weight of the OHT Cage. The fatigue of the belt is caused by the dynamic load during the operation time. Since the fatigue fracture of the belt affects the safety at the workplace, the correct prediction of the dynamic load is necessary to calculate the fatigue life of the belt on the design step. In this paper a computer aided analysis method is proposed for the belt in the early design stage using dynamic analysis, stress analysis, belt tensile test, belt fatigue test and fatigue lift prediction method. From the dynamic load time histories and the stress of the belt FE model, a dynamic stress time history is produced. Using linear damage law and cycle counting method, fatigue life cycle is calculated. The method developed in this paper is used to reduce the time and cost for designing the OHT belt in different environment and condition.

열처리한 A5082와 A6060합금의 인장특성에 미치는 변형율속도 및 예비변형율의 영향 (Effect of Strain Rate and Pre-strain on Tensile Properties of Heat-treated A5082 and A6060 Aluminium Wrought Alloys)

  • 이충도
    • 열처리공학회지
    • /
    • 제33권4호
    • /
    • pp.161-172
    • /
    • 2020
  • The tensile property of A5082 and A6060 aluminium wrought alloys was investigated, in terms of the strain rate sensitivity on alloy conditions by heat treatment and bake hardenability on pre-strain prior to strain ageing. The tensile test was carried out in a range of strain rate of 4.17 × 10-5 s-1 ~ 4.17 × 10-5 s-1 in room temperature and the nominal range of pre-strain was 3.0 ~ 10.5%. The tensile deformation of A5082 alloys is characterized as typical case of dynamic strain ageing with negative strain rate sensitivity for all conditions, and the tensile strength indicates a similar level regardless of alloy conditions, except only in full annealed condition. The stress-relief annealing on A6060 alloys can induce practical decrease in strength level of over approximately 100 MPa without any ductility loss, compared to as-rolled condition, while a full annealed and aged condition leads remarkable strengthening effect with the decrease of tensile elongation. Additionally, the bake hardenability of A5082 alloy by strain ageing indicates a negative dependence upon the increase of pre-strain, while A6060 alloy exhibits a positive sign even in low level relatively compared with conventional SPCC.

식생뿌리에 의한 비탈면 안정과 보강에 관한 실험적 연구 (An Experimental Study on the Reinforcement and Stabilization of Slope by Vegetation Roots)

  • 조주형;안봉원
    • 한국환경복원기술학회지
    • /
    • 제1권1호
    • /
    • pp.54-62
    • /
    • 1998
  • This study measured the shearing resistance of the roots of the Sasamorpha purpurascens, Miscanthus sinensis, Lespedeza cyrtobotrya by the tensile strength gained through their individual tensile test for the Root Reinforcement Model. The results to have measured this stress by experiment are as follows. 1) The mean root diameter of the Lespedeza cyrtobotrya used for this experiment was 2.19mm and the mean tensile stress was calculated as $929.489kgf/cm^2$. As for the Sasamorpha purpurascens, its mean root diameter was 1.727mm, and the mean tensile stress was $292.069kgf/cm^2$. And as for the Miscanthus sinensis, its mean root diameter was 0.814mm, and the mean tensile stress was $696.947kgf/cm^2$. And so, it was grasped that Lespedeza cyrtobotrya was highest in tensile stress. 2) ${\Delta}Cr(kg/cm^2)$ of the shearing resistance calculated by estimating the areal ratio of roots at $10^{-3}$ is $1.069kg/cm^2$ in Lespedeza cyrtobotrya, $0.336kg/cm^2$ in Sasamorpha purpurascens, and $0.801kg/cm^2$ in Miscanthus sinensis. That is, Lespedeza cyrtobotrya has the highest shearing resistance. However, since a precise analysis of the controlled factors of the slope analyses are demanded for more accurate dynamic analyses, the future demands a study on this.

  • PDF

개질 유황결합재를 사용한 중온아스팔트 혼합물의 특성 (Characteristics of the Warm-Mix Asphalt Mixtures Using the Modified Sulfur Binder)

  • 김세원;박흥석;김종규;정용욱
    • 한국건설순환자원학회논문집
    • /
    • 제4권4호
    • /
    • pp.489-495
    • /
    • 2016
  • 본 연구는 원유정제과정에서 발생되는 산업부산물인 유황에 폴리머 성분의 첨가제를 혼입한 개질유황결합재를 사용하여 중온아스팔트 혼합물을 제조하고, 개질유황결합재를 사용한 중온아스팔트 혼합물의 간접인장강도, 수침전후 및 동결융해 전후 인장강도비와 휠트랙킹 시험에 의한 동적안정도 등의 역학 및 내구 특성을 평가하였다. 실험결과, 개질유황 결합재를 사용한 중온아스팔트 혼합물의 수침전후 인장강도비는 0.88로 중온 폼드 개질 아스팔트의 약 1.13배이며, 동결융해 전후의 인장강도비 또한 0.82로 인장강도비 KS 품질기준 값 0.75 이상을 모두 만족하였다. 간접인장강도는 1.60MPa로 KS 품질기준 값 0.80MPa의 2배, 일반가열아스팔트의 1.29MPa과 비교하여 약 1.24배 높은 간접인장강도를 나타내었다. 또한, 휠트랙킹 시험에 의한 동적안정도는 14,075회/mm로 일반가열아스팔트의 약 15배, 중온 폼드 개질 아스팔트의 약 3배로 피로균열 등 소성변형에 대한 저항성이 매우 우수하게 나타났다.

익스펜디드 금속을 내부 구조체로 가지는 ISB 판넬의 정적.동적 특성 분석 (Investigation into static and dynamic characteristics of ISB panels with the expanded metal as an internally structured material)

  • 안동규;이상훈;김민수;한길영;정창균;양동열
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.832-835
    • /
    • 2005
  • The objective of this research work is to investigate into static and dynamic characteristics of ISB panels with the expanded metal as an internally structured material. In order to investigate static and dynamic characteristics of ISB panels, several experiments, the tensile test, three-point bending test and impact test, are carried out. From the results of the experiments, the mechanical properties, bending stiffness and impact absorption energy of the ISB panel have been obtained. In addition, it has been shown that the static and dynamic characteristics of ISB panel are highly dependent on the crimping angle of the pyramidal structure for the expanded metal.

  • PDF

변형률속도 변화에 따른 INCONEL 718 초내열합금의 동적 물성특성 (Dynamic Material Characteristics of Superalloy INCONEL 718 with the Variation of Strain Rates)

  • 송정한;허훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 춘계학술대회 논문집
    • /
    • pp.275-278
    • /
    • 2005
  • INCONEL 718, nickel based superalloy, has good formability, high strength, excellent corrosion resistance and mechanical properties at high temperature. Owing to theses attractive properties, it finds use in applications such as combustion system, turbine engines and nuclear reactors. In such applications, components are typically required to be tolerant of high stress impact loading. This may cause material degradation and lead to catastrophic failure during service operation. In order to design optimal structural parts made of INCONEL 718, accurate understanding of material's mechanical properties, dynamic behavior and fracture characteristic as a function of strain rates are required. This paper concerned with the dynamic material properties of the INCONEL 718 for the various strain rates. The dynamic response of the INCONEL 718 at intermediate strain rate is obtained from the high speed tensile test machine test and at the high strain rate is from the split Hopkinson pressure bar test. Based on the experimental results, the effects of strain rate on dynamic flow stress, work hardening characteristics, strain rate sensitivity and elongation to the failure are evaluated. Experimental results from both quasi-static and high strain rate up to the 5000/sec are interpolated in order to construct the Johnson-Cook model as the constitutive relation that should be applied to simulate and design the structural parts made of INCONEL 718.

  • PDF

고속충격하의 노치형상에 따른 동적거동연구 (A study of dynamic behavior with effect of notch shape on high impact)

  • 장영환;박성도;윤희석
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1997년도 추계학술대회 논문집
    • /
    • pp.795-798
    • /
    • 1997
  • This study is about the dynamic behavior of steel(SM45C). Dynamic tests were performed using SHPB(Split Hopkinson Pressure Bar) which is designed and modified to be used in both tensile and compressive modes. Quasi-static compression tests were also carried out for the comparison to the dynamic results. Not only the dynamic mechanical properties but also the effect of the notch of the specimen on stress-strain curve were investigated. The dynamic test results reveal that strain and stress are sensitively affected by the notch. The depth and the number of notch increase the stress and decrease the strain.

  • PDF