• 제목/요약/키워드: Dislocation Structure

검색결과 131건 처리시간 0.03초

Radiation induced grain boundary segregation in ferritic/martensitic steels

  • Xia, L.D.;Ji, Y.Z.;Liu, W.B.;Chen, H.;Yang, Z.G.;Zhang, C.;Chen, L.Q.
    • Nuclear Engineering and Technology
    • /
    • 제52권1호
    • /
    • pp.148-154
    • /
    • 2020
  • The radiation induced segregation of Cr at grain boundaries (GBs) in Ferritic/Martensitic steels was modeled assuming vacancy and interstitialcy diffusion mechanisms. In particular, the dependence of segregation on temperature and grain boundary misorientation angle was analyzed. It is found that Cr enriches at grain boundaries at low temperatures primarily through the interstitialcy mechanism while depletes at high temperatures predominantly through the vacancy mechanism. There is a crossover from Cr enrichment to depletion at an intermediate temperature where the Cr:Fe vacancy and interstitialcy diffusion coefficient ratios intersect. The bell-shape Cr enrichment response is attributed to the decreasing void sinks inside the grains as temperature rises. It is also shown that low angle grain boundaries (LAGBs) and special Σ coincidence-site lattice (CSL) grain boundaries exhibit suppressed radiation induced segregation (RIS) response while high angle grain boundaries (HAGBs) have high RIS segregation. This different behavior is attributed to the variations in dislocation density at different grain boundaries.

Reconstruction of Vacancy Defects in Graphene and Carbon Nanotube

  • Lee, Gun-Do;Yoon, Eui-Joon;Hwang, Nong-Moon;Wang, Cai-Zhuang;Ho, Kai-Ming
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2009년도 제38회 동계학술대회 초록집
    • /
    • pp.340-340
    • /
    • 2010
  • Various structures of vacancy defects in graphene layers and carbon nanotubes have been reported by high resolution transmission electron microscope (HR-TEM) and those arouse an interest of reconstruction processes of vacancy defects. In this talk, we present reconstruction processes of vacancy defects in a graphene and a carbon nanotube by tight-binding molecular dynamics (TBMD) simulations and by first principles total energy calculations. We found that a structure of a dislocation defect with two pentagon-heptagon (5-7) pairs in graphene becomes more stable than other structures when the number of vacancy units is ten and over. The simulation study of scanning tunneling microscopy reveals that the pentagon-heptagon pair defects perturb the wavefunction of electrons near Fermi level to produce the $\sqrt{3}\;{\times}\;\sqrt{3}$ superlattice pattern, which is in excellent agreement with experiment. It is also observed in our tight-binding molecular dynamics simulation that 5-7 pair defects play a very important role in vacancy reconstruction in a graphene layer and carbon nanotubes.

  • PDF

5052 알루미늄 합금 마찰교반접합부 특성에 미치는 접합인자의 영향 (Effect of Welding Parameters on the Friction Stir Weldability of 5052 Al alloy)

  • 이원배;김상원;이창용;연윤모;장웅성;서창제;정승부
    • Journal of Welding and Joining
    • /
    • 제22권3호
    • /
    • pp.69-76
    • /
    • 2004
  • Effects of friction stir welding parameters such as tool rotation speed and welding speed on the joints properties of 5052 Al alloys were studied in this study. A wide range of friction stir welding conditions could be applied to join 5052 AA alloy without defects in the weld zone except for certain welding conditions with a lower heat input. Microstructures near the weld zone showed general weld structures such as stir zone (SZ), thermo-mechanically affected zone (TMAZ) and heat affected zone (HAZ). Each zone showed the dynamically recrystallized grain, transient grain and structure similar to base metal's, respectively. Hardness distribution near the weld zone represented a similar value of the base metal under wide welding conditions. However, in case of 800 rpm of tool rotation speed, hardness of the stir zone had a higher value due to the fine grain with lots of dislocation tangle, a higher angle grain boundary and some of Al3Fe particles. Except joints with weld defects, tensile strength and elongation of the joints had values similar to the base metal values and fracture always occurred in the regions approximately 5mm away from the weld center.

Cu-16 at % Ag 미세복합재료의 미세구조와 전도도 (Microstructure and Electrical Conductivity of Cu-16 at % Ag Microcomposite)

  • 임문수;안장호;홍순익
    • 한국재료학회지
    • /
    • 제9권6호
    • /
    • pp.569-576
    • /
    • 1999
  • In this study, the effect of the microstructural evolution on the electrical of Cu-Ag microcomposite was investigated. The nature of interfaces between silver filaments and Cu matrix may have pronounced effects on the physical properties of Cu-Ag filamentary microcomposites, little is known about these interfaces. In heavily drawn Cu-Ag filamentary microcomposities, the microstructure is too fine and the interfacial area is too large to maintsin a stable internal dislocation structure because of closely spaced filaments. Rather, most dislocations are thought to be gradually absorbed at the interfaces as the draw ratio increases. The mechanical and electrical properties of Cu-Ag filamentary microcomposites wires were also examined and correlated with the microstructural change caused by thermomechanical treatments. The study on the electrical conductivity combined to resistivity in Cu-Ag filamentary microcomposites and the rapid increase of the electrical conductivity at high annealing temperatures is mainly caused by the dissolution and coarsening of silver filaments. The relatively low ratio of the resistivities is mainly caused by the dissolution and coarsening of silver filaments. The relatively low ratio of the resistivities at 295K($\rho$\ulcorner/$\rho$\ulcorner) in as-drawn Cu-Ag microcomposites can also be explained by the contribution of the interface scattering.

  • PDF

수지 골절-탈구 치료의 최신 지견 (The Current Concepts in Treatment of Fracture-Dislocations of the Finger)

  • 강호정;김지섭
    • 대한정형외과학회지
    • /
    • 제55권6호
    • /
    • pp.457-471
    • /
    • 2020
  • 수지는 복잡한 구조와 필수적인 기능을 가진 신체 부위로, 외상에 노출되기 가장 쉬운 부위이다. 수지 골절의 치료 원칙은 적절한 고정으로 골절부의 안정성을 획득하는 것과 안정성을 담보로 한 조기 관절 운동 간의 균형을 신중하게 결정하는 것이다. 치료에도 불구하고 합병증으로 강직이나 변형 등으로 인해 기능적, 미용적 문제가 되는 경우가 많다. 본 종설은 수지 골절 치료의 최신 지견을 소개하고, 치료가 어렵고 결과가 좋지 않은 것으로 알려진 관절면의 손상을 포함한 지절 관절 주위의 골절 및 탈구 위주로 정리하였으며, 치료 증례 소개와 합병증에 대한 접근 및 치료 순서로 기술하였다.

스크랩 불순물이 Zr 합금의 미세조직 및 기계적 특성에 미치는 영향 (Effect of Scrap Impurities on Microstructure and Mechanical Properties of Zr Alloys)

  • 정구범;김인원;송재숙;신평우;홍순익
    • 한국주조공학회지
    • /
    • 제36권3호
    • /
    • pp.81-87
    • /
    • 2016
  • In this study, the effect of scrap ratio on the mechanical properties of Zr alloys was studied. Oxygen content in the ingot cake increased rapidly with increasing fraction of scrap, which can be attributed to the surface oxide of scrap including small pieces of turning, chips, etc. Iron content did not increase much with the increasing addition of scrap, suggesting scrap materials was well reserved in the iron-free container. As-cast structure of Zr alloy with the scrap:sponge ratio displayed plate/or needle ${\alpha}$ phase and no appreciable change of the cast structure was observed with change of scrap fraction. The strength increases with increasing fraction of scrap, which can be attributed to the increase of oxygen content. The ductility decreased slightly with increase of scrap fraction. Dislocation-oxygen interaction is known to increase the strength at the expense of ductility. Ingot cake with intentionally added $Fe_2O_3$ exhibited the drastic decrease of the formability, even exhibited the brittle fracture behavior during rolling. The oxidation resistance, however, increased with the increase of scrap fraction because of high oxygen content, which may prevent more penetration and diffusion of oxygen into matrix.

분무주조 고속도공구강의 고온변형 거동에 관한 연구 (A Study on High Temperature Deformation Behavior of Spray-Formed High Speed Steels)

  • 하태권;정재영
    • 소성∙가공
    • /
    • 제27권2호
    • /
    • pp.123-129
    • /
    • 2018
  • In the present study, the mechanical behavior of the spray-formed high speed steel was investigated employing the internal variable theory of inelastic deformation. Special attention was focused on the effect of the microstructure evolution during the hot working process, such as the distribution of carbides to provide a basic database for the production condition of high speed steels with excellent properties. The billets of high speed steel ASP30TM were fabricated by a spray forming, and the subsequently hot-rolled and heat-treated process to obtain uniformly distributed carbide structure. As noted the spray-formed high speed steel showed relatively coarser carbides than hot-rolled and heat-treated one with fine and uniformly distributed carbide structure. The step strain rate tests and high temperature tensile tests were carried out on both the spray-formed and the hot-rolled specimens, to elucidate their high temperature deformation behavior. The spray-formed high speed steel showed much higher flow stress and lower elongation than the hot-rolled and heat-treated steel. During the tensile test at $900^{\circ}C$, the interruption of the deformation for 100 seconds was conducted to reveal that the recovery was a main dynamic deformation mechanism of spray formed high speed steel. The internal variable theory of the inelastic deformation was used to analyze data from the step strain rate tests, revealing that the activation energies for hot deformation of as-spray-formed and hot-worked steels, which were 157.1 and 278.9 kJ/mol, and which were corresponding to the dislocation core and lattice diffusions of ${\gamma}-Fe$, respectively.

A Chemically-driven Top-down Approach for the Formation of High Quality GaN Nanostructure with a Sharp Tip

  • 김제형;오충석;고영호;고석민;조용훈
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.48-48
    • /
    • 2011
  • We have developed a chemically-driven top-down approach using vapor phase HCl to form various GaN nanostructures and successfully demonstrated dislocation-free and strain-relaxed GaN nanostructures without etching damage formed by a selective dissociation method. Our approach overcomes many limitations encountered in previous approaches. There is no need to make a pattern, complicated process, and expensive equipment, but it produces a high-quality nanostructure over a large area at low cost. As far as we know, this is the first time that various types of high-quality GaN nanostructures, such as dot, cone, and rod, could be formed by a chemical method without the use of a mask or pattern, especially on the Ga-polar GaN. It is well known that the Ga-polar GaN is difficult to etch by the common chemical wet etching method because of the chemical stability of GaN. Our chemically driven GaN nanostructures show excellent structure and optical properties. The formed nanostructure had various facets depending on the etching conditions and showed a high crystal quality due to the removal of defects, such as dislocations. These structure properties derived excellent optical performance of the GaN nanostructure. The GaN nanostructure had increased internal and external quantum efficiency due to increased light extraction, reduced strain, and improved crystal quality. The chemically driven GaN nanostructure shows promise in applications such as efficient light-emitting diodes, field emitters, and sensors.

  • PDF

베타 티타늄합금의 준 안정상 TEM 회절도형 분석 (TEM Diffraction Analysis of Metastable Phases in Beta Ti Alloys)

  • 최병학;심종헌;김승언;현용택;박찬희;강주희;이용태;김영욱
    • 한국재료학회지
    • /
    • 제25권8호
    • /
    • pp.403-409
    • /
    • 2015
  • Metastable phase characteristics of beta Ti alloys were investigated to consider the relationship of the microstructure and diffraction pattern in TEM. TEM analysis showed that the microstructure was mottled as a modulated structure, and the diffraction pattern was composed of spot streaks between the main spots of a stable beta phase with a specific lattice relationship. The modulated structure may be induced by short distance slip or atom movement during a very short interval of solution treated and quenched (STQ) materials. The athermal ${\omega}$ phase, which could be precipitated at low temperature aging, is also analysed by the metastable phase. The metastable phases including athermal ${\omega}$ phase had a common characteristic of hardened and brittle behavior because the dislocation slip was restricted by a super lattice effect due to short distance atom movement at the metastable state.

초음파 나노표면개질 공정기술에 의한 AISI304 스테인리스강의 표면나노구조화 및 압축잔류응력 형성 (Formation of Nano-structure and Compressive Residual Stress on AISI304 Stainless Steel by Ultrasonic Nanocrystalline Surface Modification)

  • 조인식;동계령;유대황;서정화;아마노프;신기삼;이창순;편영식;박인규
    • 대한금속재료학회지
    • /
    • 제48권9호
    • /
    • pp.807-812
    • /
    • 2010
  • In this paper, the Ultrasonic Nanocrystalline Surface Modification (UNSM) surface treatment process was used to induce compressive residual stress and nanocrystalline structure by severe plastic deformation on the UNSM-treated surface. The test results for AISI304 stainless steel demonstrated that the grain size was found to be 23 nm, the dislocation density was increased by $0.2085{\times}10^{18}\;m^{-2}$, and the volume fraction of martensite is defined as 27.6% from austenite so that the surface hardness of the surface is increased from 200 Hv up to 515 Hv. The initial tensile residual stress is changed from 300 MPa to a compressive residual stress of 500 MPa after UNSM treatment. In addition, UNSM was applied under five various conditions, and the results of those conditions were defined as a function of depth quantitative.