• 제목/요약/키워드: Different Blank Force

검색결과 23건 처리시간 0.026초

사각용기 드로잉시의 플랜지 주름에 관한 실험 (Experiments on the flange wrinkling for a deep-drawn rectangular container)

  • 이계섭;이기환;박천희;한영호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 1996년도 추계학술대회 논문집
    • /
    • pp.123-127
    • /
    • 1996
  • The tendency of wrinkling formation on the flange of a deep-drawn rectangular container was investigated experimentally under different process conditions. Such process variables as blank size, sheet thickness, blank-holding force, and depth of drawing are chosen to examine their effects on the flange wrinkles of the products. Number and amplitudes of the wrinkles are measured along the periphery of the flange and compared between each case of process condition.

  • PDF

박판 금속의 회전 전단가공에 관한 연구 (A Study on the Rotary Shearing Operation of Sheet Metal)

  • 서윤수;박재우;김영호
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2000년도 춘계학술대회 논문집
    • /
    • pp.747-752
    • /
    • 2000
  • Rotary shearing using of rotating and locally shear force has been studied. It is possible to be obtained in any case for requested blank diameters. In this paper, different local forming zones, that are clearances between upper roller and vertically taped low roller, were investigated. Required shearing force is calculated by undecided coefficient method for clearances and strokes of upper roller. Rotary shearing is completed undergoing some processes composed of pressing steps and standing steps. The reason for using these processes is to avoid jamming or tearing of blank by means of upper roller during shearing.

  • PDF

Formability Study on Weld Line Location and Movement of Laser-Tailor Welded Blanks

  • Hong, Joo-Pyo;Kim, Heon-Young;Oh, Soo-Ik
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1997년도 춘계학술대회논문집
    • /
    • pp.19-24
    • /
    • 1997
  • The weld line location and the weld line movement in stamping with laser-tailor welded blanks(TWB) were investigated through square cup deep drawing tests. The step blank holder was introduced to form TWB of different thicknesses without wrinkling, and the non-uniform blank holding force(BHF) was enforced to control weld line movement. Test results of the blanks with shifted weld lines showed that the large portion of the thinner area could result in a large weld line movement. Careful selection of the weld line location and the BHF control should be adapted in TWB design to avoid failures and to ensure its formability.

  • PDF

AZ31B 마그네슘합금 판재의 고온 스프링백 특성 (Springback Characteristics of AZ31B Magnesium Alloy Sheet at Elevated Temperature)

  • 최선철;이한수;김형종;이경택;김헌영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.60-63
    • /
    • 2007
  • The effect of process parameters on springback of AZ31B magnesium alloy sheet was investigated by performing 2D draw bending test at the elevated temperatures. And also the springback characteristics were studied different blank holding forces between 30 to 250 kgf. Springback was considerably reduced at higher temperatures than $200^{\circ}C$. The blank holding force in the range used, however, had little influence on springback in isothermal tests. For a given temperature, springback decreased with increasing blank holding force in non-isothermal tests.

  • PDF

딥드로잉공정에서의 재료 수율 향상에 관한 연구 (A Study on Improving The Coefficient of Utilization of Material in Deep Drawing Process)

  • 하종호;강형선;백호현
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제33권4호
    • /
    • pp.509-516
    • /
    • 2009
  • This paper is the study on improving the coefficient of utilization of material in deep drawing process. Cylindrical cup drawing process is widely used in sheet metal forming process. The blank shape is one of the important things in sheet metal forming process. It is produced for the bridge of blank in a blanking process. The coefficient of utilization of material is much effected by this bridge of blank. This study offered a new process method to reduce the loss of material. The new blank shape offered and manufactured by new process method is investigated by a finite element method and the experiment. Then the wrinkling, the punch load, the thickness distribution is observed. This result is different from the result of circular blank process. And it is got that the Max strain, the wrinkle and the height of the wrinkle are effected by the holding force and the punch load. As a result, if the processing optimum condition is found, the loss of material will be reduced. It is necessary to research systematically about determining the optimum value of process variables.

레이저 용접 테일러드 블랭크의 기본 성형특성 III : 신장성형 특성 (Forming Characteristics of Laser Welded Tailored Blanks III : Stretch Forming Characteristics)

  • 박기철;한수식;진조관;권오준
    • 소성∙가공
    • /
    • 제7권4호
    • /
    • pp.354-363
    • /
    • 1998
  • In order to analyze the stretch forming characteristics of tailored blanks, laser welded blanks of different thickness and strength combinations were prepared and stretching tests were done. The stretching formability of laser welded blanks was reduced as increasing the deformation restraining force ($strength{\times}thickness$) ratio between two welded sheets. Weld line movement was attributed to strain concentration at weaker sheets and resulted in fracture at weaker sid, so that fracture could be predicted by the forming limit of the weak sheet. In the case of a welded blank with the similar deformation restraining force rations between two welded sheets, crack occurred at weld and its forming limit was about 15% less than the base sheet. The effects of lubrication and weld line position on stretch-ing formability were also investigated by experiments. Lower friction did not always give better formability for tailored blanks. Stretching formability was observed to be improved as increasing the area of weak sheet.

  • PDF

툴 표면처리 및 온도가 AZ31 마그네슘 판재의 드로잉성에 미치는 영향 (The Effect of Tool Surface Treatment and Temperature on Deep Drawability of AZ31 Magnesium Alloy Sheet)

  • 추동균;이준희;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2005년도 추계학술대회 논문집
    • /
    • pp.118-121
    • /
    • 2005
  • The square cup drawing of magnesium alloy AZ31 $(aluminum\;3\%,\;Zinc\;1\%)$ sheets was studied by experimental approach in various temperatures (200, 250, 300, 350, $400^{\circ}C$) when blank holding force (BHF) was controlled in real-time. And so on, the drawability was measured with the different die and punch coating. The square cup drawing test was performed by three different coated punches (CrN, TiCN, Non-coated). BHF was set about 2.0 KN, forming speed was 50 mm/min, blank thickness were 0.5, 1.0mm and the cup size was 40 mm by 60 mm after forming. The experimental data of square cup drawing test show that the tools coating and temperature were effect on the drawbility.

  • PDF

AZ31B 마그네슘 합금판재의 온간 성형한계도 및 스프링백 특성 시험 (Experiments for Forming Limit Diagram and Springback Characteristics of AZ31B Magnesium Alloy Sheet at Elevated Temperature)

  • 최선철;이한수;김형종;이경택;김헌영
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.289-293
    • /
    • 2007
  • The effect of temperature on the forming limit diagram was investigated for AZ31B magnesium alloy sheet through the limit dome height test in the range from room temperature to $300^{\circ}C$. The formability of AZ31B sheet was improved significantly according to the increasing temperature. Also we studied the springback characteristics through the 2D draw bending test with different blank holding forces at elevated temperatures. Springback quantity was considerably reduced as temperature went up. The blank holding force in the range used, however, had little influence on springback. Experimental results obtained in this study may provide a material database for AZ31B sheet.

  • PDF

AZ31B 마그네슘 합금판재의 온간 성형한계도 및 스프링백 특성 시험 (Experiments for Forming Limit Diagram and Springback Characteristics of AZ31B Magnesium Alloy Sheet at Elevated Temperature)

  • 김헌영;최선철;이한수;김형종;이경택
    • 소성∙가공
    • /
    • 제16권5호통권95호
    • /
    • pp.364-369
    • /
    • 2007
  • The effect of temperature on the forming limit diagram was investigated for AZ31B magnesium alloy sheet through the limit dome height test in the range from room temperature to $300^{\circ}C$. The formability of AZ31B sheet was improved significantly according to the increasing temperature. Also we studied the springback characteristics through the 2D draw bending test with different blank holding forces at elevated temperatures. Springback quantity was considerably reduced as temperature went up. The blank holding force in the range used, however, had little influence on springback. Experimental results obtained in this study may provide a material database for AZ31B sheet.

원형컵 디프 드로잉의 성형해석에 의한 공정설계 (New Design of Cylindrical Cup Deep Drawing by Forming Analysis)

  • 정완진;김종호;류제구
    • 소성∙가공
    • /
    • 제12권7호
    • /
    • pp.647-653
    • /
    • 2003
  • A systematic approach for the process design in deep drawing is necessary to improve the quality of drawn cups. This study concentrates mainly on the influence of process design strategy on the product quality. Different types of process design were chosen from initial blank of 100mm in diameter to make final cup of 50mm in diameter. In order to make this cup, we used 2-stage deep drawing. Forming analyses are carried out to find out better design in terms of drawing force. It is proposed that the process design, in which maximum drawing forces during successive operations are equal, is a more desirable one. Through experiment, it is found that the proposed case shows equivalent values in terms of maximum drawing force during successive operations in real process and can achieve the best product quality in terms of dimensional accuracy. Thus, it is shown that proposed design is very effective in the improvement of quality in drawn cups and may be extended to deep drawing with more stages.