• 제목/요약/키워드: Diamond film

검색결과 446건 처리시간 0.02초

Patterning of Diamond Micro-Columns

  • Cho, Hun-Suk;Baik, Young-Joon;Chung, Bo-Keon;Lee, Ju-Yong;Jeon, D.;So, Dae-Hwa
    • The Korean Journal of Ceramics
    • /
    • 제3권1호
    • /
    • pp.34-36
    • /
    • 1997
  • We have fabricated a patterned diamond field emitter on a silicon substrate. Fine diamond particles were planted on a silicon wafer using conventional scratch method. A silicon oxide film was deposited on the substrate seeded with diamond powder. An array of holes was patterned on the silicon oxide film using VLSI processing technology. Diamond grains were grown using a microwave plasma-assisted chemical vapor deposition. Because diamond could not grow on the silicon oxide barrier, diamond grains filled only the patterned holes in the silicon oxide film, resulting in an array of diamond tips.

  • PDF

투과 전자 현미경을 이용한 다이아몬드 박막과 실리콘 기판의 계면 연구 (Investigation of the interface between diamond film and silicon substrate using transmission electron microscopy)

  • 김성훈
    • 한국결정성장학회지
    • /
    • 제10권2호
    • /
    • pp.100-104
    • /
    • 2000
  • 다이아몬드 박막을 마이크로웨이브 플라즈마 방법을 이용하여 실리콘 기판위에 증착하였다. 증착된 다이아몬드 박막과 실리콘 기판의 단면을 이온 밀링 방법으로 식각한후, 경계면을 투과 전자 현미경으로 분석하였다. 다이아몬드 박막은 실리콘 기판위에 직접 성장되거나 또는 중간층이 형성된후 성장됨을 알 수 있었다. 중간층의 구성은 주로 Sic 또는 무정형 탄소로 이루어졌으며 중간층의 두께는 경계면을 따라 다르게 변하였다. 전자 회절 패턴으로부터, 경계면 주위에 잘 발달된 실리콘 기판과 다이아몬드의 결정면들이 서로 적합하게 성장되었고 있음을 알 수 있었다. 이 결과들로부터 실리콘 기판위에 성장되는 다이아몬드 박막의 초기 성장 형태를 추론할 수 있었다.

  • PDF

MWPCVD법에 의한 다이아몬드 박막의 제조 및 결정성장 특성 (Preparation and Crystalline Growth Properties of Diamond Thin Film by Microwave Plasma CVD)

  • 김규식;박수길
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2000년도 하계학술대회 논문집
    • /
    • pp.905-908
    • /
    • 2000
  • The growth properties of diamond grain were examined by Raman spectroscopy and microscope images. Diamond thin films were prepared on single crystal Si wafers by microwave Plasma chemical vapor deposition. Preparation conditions, substrate temperature, boron concentration and deposition time were controlled differently. Prepared diamond thin films have different surface morphology and grain size respectively Diamond grain size was gradually changed by substrate temperature. The biggest diamond grain size was observed in the substrate, which has highest temperature. The diamond grain size by boron concentration was slightly changed but morphology of diamond grain became amorphous according to increasing of boron concentration. Time was also needed to be a big diamond grain. However, time was not a main factor for being a big diamond grain. Raman spectra of diamond film, which was deposited at high substrate temperature, showed sharp peaks at 1334$cm^{-1}$ / and these were characteristics of crystalline diamond. A broad peak centered at 1550$cm^{-1}$ /, corresponding to non-diamond component (sp$^2$carbon), could be observed in the substrate, which has low temperature.

  • PDF

다이아몬드 분말상에 무전해 Ni-B 도금을 위한 계면활성제의 영향 (Effect of Surfactant in Electroless Ni-B Plating for Coating on the Diamond Powder)

  • 양창열;유시영;문환균;이정호;유봉영
    • 한국표면공학회지
    • /
    • 제50권3호
    • /
    • pp.177-182
    • /
    • 2017
  • The properties of electroless Ni-B thin film on diamond powder with different parameters (temperature, pH, surfactant etc.) were studied. The surface morphology, structure and composition distribution of the Ni-B film were observed by field effect scanning electron microscope (FE-SEM), energy-dispersive spectrometer (EDS), X-ray diffraction (XRD) and Auger electron spectroscopy (AES). The growth rate of Ni-B film was increased with increase of bath temperature. The B content in Ni-B film was reduced with increase of bath pH. As a result the structure of Ni-B film was changed from amorphous to crystalline structure. The PVP in solution plays multi-functional roles as a dispersant and a stabilizer. The Ni-B film deposited with adding 0.1 mM-PVP was strongly introduced an amorphous structure with higher B content (25 at.%). Also the crystallite size of Ni-B film was reduced from 12.7 nm to 5.4 nm.

Deposition of Diamond Film by Hydrogen-oxyacetylen Combustion Flame

  • Ko, Chan-Kyoo;Park, Dong-Wha
    • The Korean Journal of Ceramics
    • /
    • 제4권1호
    • /
    • pp.1-4
    • /
    • 1998
  • Diamond film was deposited on Mo substrate at atmospheric pressure using combustion flame apparatus with the addition of H2. At a temperature above 100$0^{\circ}C$, parts of the film were converted into graphites and these were etched by hydrogen atoms. With increasing $C_2H_2/O_2$ ratio, the nucleation density of the film increased. But the greater part of the film was formed with cauliflower-shaped amorphous carbon. These amorphous carbn were crystallized etching amorphous carbon.

  • PDF

The Effects of Impurities in Silicon Nitride Substrate on Tribological Behavior between Diamond Film and Silicon Nitride Ball

  • Lim, Dae-Soon;Kim, Jong-Hoon
    • Tribology and Lubricants
    • /
    • 제11권5호
    • /
    • pp.20-25
    • /
    • 1995
  • Diamond films were prepared by a hot filament vapor deposition onto polycrystal silicon nitride substrates. Different kinds of silicon nitride containing CaO and $Fe_{2}O_{3}$ were manufactured to investigate the impurity effect of substrate on the morphology of diamond films and their wear behaviors. Nucleation rates and morphologies of diamond films deposited on various kinds of silicon nitride were compared. The highest nucleation rate was observed in a substrate containing 1% of CaO. Wear tests were performed with a silicon nitride ball on the disk geometry to investigate the tribological behavior of diamond film against silicon nitride. This study demonstrated that different morphologies of diamond film due to substrate impurities produced different wear behavior against silicon nitride.

Bonding and Etchback Silicon-on-Diamond Technology

  • Jin, Zengsun;Gu, Changzhi;Meng, Qiang;Lu, Xiangyi;Zou, Guangtian;Lu, Jianxial;Yao, Da;Su, Xiudi;Xu, Zhongde
    • The Korean Journal of Ceramics
    • /
    • 제3권1호
    • /
    • pp.18-20
    • /
    • 1997
  • The fabrication process of silicon-diamond(SOD) structure wafer were studied. Microwave plasma chemical vapor deposition (MWPCVD) and annealing technology were used to synthesize diamond film with high resistivity and thermal conductivity. Bonding and etchback silicon-on-diamond (BESOD) were utilized to form supporting substrate and single silicon thin layer of SOD wafer. At last, a SOD structure wafer with 0.3~1$\mu\textrm{m}$ silicon film and 2$\mu\textrm{m}$ diamond film was prepared. The characteristics of radiation for a CMOS integrated circuit (IC) fabricated by SOD wafer were studied.

  • PDF

NITROGEN DOPED DIAMOND LIKE CARBON FILM SYNTHESIZED BY MICROWAVE PLASMA CVD

  • Urao, Ryoichi;Hayatsu, Osamu;Satoh, Toshihiro;Yokota, Hitoshi
    • 한국표면공학회지
    • /
    • 제29권5호
    • /
    • pp.549-555
    • /
    • 1996
  • Diamond Like Carbon film is amorphous film which is considered to consist of three coordinate graphite structure and tetrahedron coordinate diamond structure. Its hardness, thermal conductivity and chemical stability are nearly to one of diamond. It is well known to become semi-conductor by doping of inpurity. In this study Diamond Like Carbon film was synthesized by Microwave Plasma CVD in the gas mixture of hydrogen-methan-nitrogen and doped of nitrogen on the single-crystal silicon or silica glass. The temperature of substrate and nitrogen concentration in the gas mixture had an effect on the bonding state, structural properties and conduction mechanism. The surface morphology was observed by Scanning Electron Microscope. The strucure was analyzed by laser Raman spectrometry. The bonding state was evaluated by electron spectroscopy. Diamond Like Carbon film synthesized was amorphous carbon containing the $sp^2$ and $sp^3$ carbon cluster. The number of $sp^2$ bonding increased as nitrogen concentration increased from 0 to 40 vol% in the feed gas at 1233K substrate temperature and at $7.4\times10^3$ Pa. Increase of nitrogen concentration made Diamond Like Carbon to be amorphous and the doze of nitragen could be controlled by nitrogen concentration of feed gas.

  • PDF

Influence of the Thin-Film Ag Electrode Deposition Thickness on the Current Characteristics of a CVD Diamond Radiation Detector

  • Ban, Chae-Min;Lee, Chul-Yong;Jun, Byung-Hyuk
    • Journal of Radiation Protection and Research
    • /
    • 제43권4호
    • /
    • pp.131-136
    • /
    • 2018
  • Background: We investigated the current characteristics of a thin-film Ag electrode on a chemical vapor deposition (CVD) diamond. The CVD diamond is widely recognized as a radiation detection material because of its high tolerance against high radiation, stable response to various dose rates, and good sensitivity. Additionally, thin-film Ag has been widely used as an electrode with high electrical conductivity. Materials and Methods: Considering these properties, the thin-film Ag electrode was deposited onto CVD diamonds with varied deposition thicknesses (${\fallingdotseq}50/98/152/257nm$); subsequently, the surface thickness, surface roughness, leakage current, and photo-current were characterized. Results and Discussion: The leakage current was found to be very low, and the photo-current output signal was observed as stable for a deposited film thickness of 98 nm; at this thickness, a uniform and constant surface roughness of the deposited thin-film Ag electrode were obtained. Conclusion: We found that a CVD diamond radiation detector with a thin-film Ag electrode deposition thickness close to 100 nm exhibited minimal leakage current and yielded a highly stable output signal.

박막증착시 티타늄 표면의 마손저항도와 세포독성에 관한 연구 (A STUDY ON THE RESISTANCE OF WEAR AND CYTOTOXICITY OF THE TITANIUM SURFACE AFTER FILM DEPOSITIONS)

  • 김형우;김창회;김영수
    • 대한치과보철학회지
    • /
    • 제39권1호
    • /
    • pp.84-95
    • /
    • 2001
  • Titanium is widely used in dentistry for its low density, high strength, fatigue resistance, corrosion resistance, and biocompatibility. But it has a tendency of surface damage under circumstance of friction and impact for its low hardness of the surface. Coating is one of methods fir increasing surface hardness. Its effect is to improve surface physical characteristics without change of titanium. Diamond-like carbon and titanium nitride are known for its high hardness of the surface. So that this study was aimed at the wear test and the cytotoxicity test of the commercially pure titanium and Ti-6Al-4V alloy which were deposited by diamond-like carbon film or titanium nitride film to acertain improvement of the surface hardness and the biocompatibility. A disk (25mm diameter, 2mm thickness) was made of commercially pure titanium and Ti-6Al-4V alloy and these substrates were deposited by diamond-like carbon film or titanium nitride film. Diamond-like carbon film was deposited by the method of radiofrequency plasma assisted chemical vapor deposition and titanium nitride film was deposited by the method of reactive arc ion plating. Then these substrates were tested about wear characteristics by the pin-on-disk type wear tester in which ruby ball was used as a wear causer under the load of 32N, The fracture cycles were measured by rotating the substrates until their films were fractured. The wear volume was measured after 150 cycles and 3,000 cycles using surface profiler. The cytotoxicity test was peformed by the method of the MTT assay. The results were as follows : 1. In the results of the wear volume test, commercially pure titanium and titanium alloy which were coated by diamond-like carbon film or titanium nitride aim had higher resistance against wear than the substrates which were not coated by any films (P<0.05). 2. In the results of the fracture cycle test and the wear volume test, diamond-like carbon film had higher resistance against wear than titanium nitride film (P<0.05). 3. In both coatings of diamond-like carbon aim and titanium nitride film, Ti-6Al-4V alloy had higher resistance against wear than commercially pure titanium (P<0.05) 4. In the results of the cytotoxicity test, diamond-like carbon film and titanium nitride film had little cytotoxicity as like commercially pure titanium or Ti-6Al-4V alloy (P>0.05).

  • PDF