압입축에 발생하는 프레팅 피로균열 발생 및 진전 특성 실험 (Experimental Study on Fatigue Crack Initiation and Propagation due to Fretting Damage in Press-fitted Shaft)

  • 이동형;권석진;최재붕;김영진
    • 대한기계학회논문집A
    • /
    • 제31권6호
    • /
    • pp.701-709
    • /
    • 2007
  • To clarify the characteristics of surface damage due to fretting in press-fitted shaft, experimental methods were applied to small scale specimen with different bending load condition. Fatigue tests and interrupted fatigue tests of press-fitted specimen were carried out by rotate bending fatigue test. Macroscopic and microscopic characteristics were examined using scanning electron microscope (SEM), optical microscope or profilometer. It is found that small fatigue cracks are nucleated early in life regardless of bending stress, and thus the most portion of fatigue life on press fits can be considered to be crack propagation process. Most of surface cracks are initiated near the contact edge, and multiple cracks are nucleated and interconnected. Furthermore, the fretting wear rates at the contact edge are increased rapidly at the initial stage of total fatigue life. It is thus suggested that the fatigue crack nucleation and propagation process is strongly related to the evolution of surface profile by fretting wear in press fits.

Creep-permeability behavior of sandstone considering thermal-damage

  • Hu, Bo;Yang, Sheng-Qi;Tian, Wen-Ling
    • Geomechanics and Engineering
    • /
    • 제18권1호
    • /
    • pp.71-83
    • /
    • 2019
  • This investigation presented conventional triaxial and creep-permeability tests on sandstones considering thermally-induced damage (TID). The TID had no visible effects on rock surface color, effective porosity and permeability below $300^{\circ}C$ TID level. The permeability enlarged approximately two orders of magnitude as TID increased to $1000^{\circ}C$ level. TID of $700^{\circ}C$ level was a threshold where the influence of TID on the normalized mass and volume of the specimen can be divided into two linear phases. Moreover, no prominent variations in the deformation moduli and peak strength and strain appeared as TID< $500^{\circ}C$ level. It is interesting that the peak strength increased by 24.3% at $700^{\circ}C$ level but decreased by 11.5% at $1000^{\circ}C$ level. The time-related deformation and steady-state creep rate had positive correlations with creep loading and the TID level, whereas the instantaneous modulus showed the opposite. The strain rates under creep failure stresses raised 1-4 orders of magnitude than those at low-stress levels. The permeability was not only dependent on the TID level but also dependent on creep deformation. The TID resulted in large deformation and complexity of failure pattern for the sandstone.

경질양극산화된 5083-H321 알루미늄 합금의 해수 내 액적충격침식부식 손상 연구 (Investigation of Liquid Droplet Impingement Erosion Corrosion based on the Flow Rate of Anodized 5083-H321 Al Alloy in Seawater)

  • 신동호;김성종
    • Corrosion Science and Technology
    • /
    • 제19권6호
    • /
    • pp.310-317
    • /
    • 2020
  • This study investigated the damage to the specimen due to liquid droplet impingement erosion corrosion, which improved the corrosion resistance and durability via hard anodization of 5083-H321 aluminum alloy, which is widely used for small ships and marine structures. The experiment combined liquid droplet impingement erosion and electrochemical equipment with the flow rates in natural seawater solution. Subsequently, Tafel extrapolation of polarization curves was performed to evaluate damage due to the liquid droplet impingement erosion corrosion. The damaged surface was observed using a 3D microscope and a scanning electron microscope. The degree of pitting damage was measured using the Image J program, and the surface hardness was measured using the micro-Vickers hardness tester. The corrosion current density, area, depth, and ratio of the damaged areas increased with the increase in flow rate. The grain size of the damaged area at a flow rate of 20 m s-1 showed fewer and minor differences in height, and a smooth curved shape. The hardness of the damaged surface tended to decrease with increase in flow rate.

항방사선 인삼분획의 butanol 추출물과 수용성 성분이 세포 생존율에 미치는 영향 (Effects of Butanol Extract and Water-Soluble Constituent of Radioprotective Ginseng Fractioil on Cell Survival)

  • 김춘미;최향옥
    • Journal of Ginseng Research
    • /
    • 제15권3호
    • /
    • pp.167-170
    • /
    • 1991
  • Radiation protective fraction was Isolated and partially purified from Korean white ginseng. The effect of the fraction was studied on the cell survival of W-damaged CHO-Kl cells. As a result, it was found that the fraction increased the survival rate of damaged cells significantly within the dose range of which cytotoxicity did not appear This fraction was separated into two parts by adding butanol, namely the precipitated protein component and the butanol extract. Damaged cells were treated with each of these components and their survival rates were measured. The protein component demonstrated significant increase in the survival rates, while the butanol extract showed no such increment. These results suggest that the radiation protective effect of the ginseng fraction is originated from the butanol-precipitated protein component, not from the butanol-soluble compounds.

  • PDF

전시 최단수송경로 선정 (Determination of the Shortest Transportation Path in Wartime)

  • 윤종옥;하석태
    • 한국국방경영분석학회지
    • /
    • 제17권2호
    • /
    • pp.72-89
    • /
    • 1991
  • In transportation network problems, it is often desirable to select multiple number of the shortect paths. On problems of finding these paths, algorithms have been developed to choose single shortest path, k-shortest paths and k-shortest paths via p-specified nodes in a network. These problems consider the time as the main factor. In wartime, we must consider availability as well as time to determine the shortest transportation path, since we must take into account enemy's threat. Therefore, this paper addresses the problem of finding the shortest transportation path considering both time and availability. To accomplish the objective of this study, values of k-shortest paths are computed using the algorithm for finding the k-shortest paths. Then availabilties of those paths are computed through simulation considering factors such as rates of suffering attack, damage and repair rates of the paths. An optimal path is selected using any one of the four decision rules that combine the value and availability of a path.

  • PDF

육묘용 로봇 이식기의 개발(I) - 기계시각 시스템 - (Development of a Robotic Transplanter for Bedding Plants(I) - Machine Vision System -)

  • 류관희;김기영;이희환;황호준
    • Journal of Biosystems Engineering
    • /
    • 제22권3호
    • /
    • pp.317-324
    • /
    • 1997
  • This study was conducted to develope a machine vision system for a robotic transplanter for bedding plants. Specific objectives of this study were 1) to get coordinates of the healthy seedlings in high-density plug tray, and 2) to get the angle of the leaves of the healthy seedlings to avoid the damage to seedlings by gripper. Results of this study were summarized as follows. (1) The machine vision system of a robotic transplanter was developed. (2) Success rates of detecting empty cell and bad seedlings for 72-cell and 128-cell plug-trays were 98.8% and 94, 9% respectively. (3) Success rates of calculating the angle of leaves fer 72-cell and 128-cell plug-trays were 93.5% and 91.0% respectively.

  • PDF

육묘용 로봇 이식기의 개발(I)-로봇 이식기의 기계시각 시스템의 개발- (Development of a Robotic Transplanter for Bedding Plants (I)-Development of the Machine Vision System of a Robotic Transplanter-)

  • 류관희;이희환;김기영;황호준
    • 한국농업기계학회:학술대회논문집
    • /
    • 한국농업기계학회 1997년도 동계 학술대회 논문집
    • /
    • pp.392-400
    • /
    • 1997
  • This study was conducted to develope the machine vision system of a robotic transplanter for bedding plants. Specific objectives of this study were 1) to get coordinates of the healthy seedlings except empty cells and bad seedlings in high-density plug tray, and 2) to get the angle of the leaves of the healthy seedlings to avoid damage to the seedlings by gripper. The results of this study are summarized as follows. (1) The machine vision system of a robotic transplanter was developed. (2) The success rates of detecting empty cell and bad seedlings in 72-cell and 128-cell plug trays were 98.8% and 94.9% respectively. (3) The success rates of calculating the angle of leaves in 72-cell and 128-cell plug trays were 93.5% and 91.0% respectively.

  • PDF

용접 계면균열의 크리프 균열성장 거동에 관한 연구 (A Study on Creep Crack Growth Behavior of Weld Interface Crack)

  • 윤기봉;김광웅;정용근
    • Journal of Welding and Joining
    • /
    • 제16권4호
    • /
    • pp.83-91
    • /
    • 1998
  • Cracking problems which high temperature plant components suffer during long-term service, occur very often at welded locations. The crack occurs due to accumulated creep damage near fusion line or at heat affected zone (HAZ). However, most of the studies on creep crack growth behavior have been performed with matrix metal not wit welded metal due to the difficulty of interpreting the test results. In this study, creep crack growth rates were measured with C(T) specimens whose cracks were formed along the fusion line or HAZ. The measured crack growth rates were characterized by {TEX}$C_{t}${/TEX}-parameter derived for elastic-primary-secondary creeping material. Since contribution of primary creep was significant for the tested 1Cr-0.5Mo steel, its effect was carefully studied. Effects of crack tip plasticity and material aging were also discussed.

  • PDF

Correlative Changes between Photosynthetic Activities and Chlorophyll Fluorescence in Wheat Chloroplasts Exposed to High Temperature

  • Young-Nam Hong
    • Journal of Plant Biology
    • /
    • 제37권1호
    • /
    • pp.37-42
    • /
    • 1994
  • Correlative changes between photosynthetic O2 exchange rates and room temperature Chl fluorescence were investigated in wheat (Triticum aestivum L.) chloroplasts treated with high temperature for 5 min. With increasing treatment temperature, photosynthetic O2 evolution rate mediated by PSII was decreased, showing 50% inhibition at 38$^{\circ}C$ (I50). But PSI activity measured by O2 uptake rates was stimulated as a function of increasing temperature. Dark level fluorescence (Fo)-temperature (T) analysis showed that fluorescence rising temperature (Tr), critical temperature (Tc), and peak temperature (Tp) was 38, 43, and 52$^{\circ}C$, respectively. Quenching analysis of Chl fluorescence showed that both the oxidized fraction of plastoquinone (qQ) and degree of thylakoid membrane energization (qNP) increased up to 4$0^{\circ}C$ and then declined dramatically. These results suggest that Tr is correlated with temperature showing a 50% of inhibition of photosynthesis and under mild high temperature stress, qNP is worth regarding as indicator for heat-induced damage of photosynthesis.

  • PDF

코로나바이러스감염증-19와 수면 (COVID-19 and Sleep)

  • 신재공
    • 수면정신생리
    • /
    • 제29권2호
    • /
    • pp.29-34
    • /
    • 2022
  • Coronavirus disease 2019 (COVID-19), which was a global pandemic caused by severe acute respiratory syndrome corona virus 2 (SARS-CoV-2), is still a serious public health problem. COVID-19 causes various symptoms not only in the respiratory system but also in various parts of the body and has a significant effect on sleep. Insomnia and poor sleep quality were observed at high rates in patients with COVID-19 as well as in the uninfected general population. Obstructive sleep apnea is also considered a risk factor in patients with severe COVID-19. Virus-induced central nervous system damage is likely to be the cause of many sleep disorders in COVID-19, but psychosocial influences also seem to have played a significant role. Sleep problems persisted at high rates for a considerable period after the infection phase was over. More attention and research on the effect of COVID-19 on sleep is needed in the future.