• 제목/요약/키워드: DLC Film

검색결과 239건 처리시간 0.026초

DLC 박막을 이용한 액정 배향 효과 (Liquid Crystal Alignment Effects using a DLC Thin Film)

  • 조용민;황정연;서대식;노순준;이대규;백흥구
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 추계학술대회 논문집
    • /
    • pp.346-349
    • /
    • 2001
  • We studied the nematic liquid crystal (NLC) aligning capabilities using the new alignment material of diamond like carbon (DLC) thin film. A high pretilt angle of about 4$^{\circ}$ was measured by ion beam(IB) exposure on the DLC thin film surface. A good LC alignment was observed by the IB alignment method on the DLC thin film surface at annealing temperature of 200$^{\circ}C$, and the alignment defect of the NLC was observed above annealing temperature of 220$^{\circ}C$ . Consequently, the high NLC pretilt angle and the good thermal stability of LC alignment can be achieved by the IB alignment method on the DLC thin film surface.

  • PDF

Si 함유량에 따른 Si-DLC/DLC 코팅의 건조마찰 특성 (Tribological Behavior of Si-DLC/DLC Coatings with Various Si Contents)

  • 안효석
    • 한국공작기계학회논문집
    • /
    • 제16권6호
    • /
    • pp.212-216
    • /
    • 2007
  • Although DLC coatings have good tribological properties, these are dependent on the deposition method, property of contact surface, and test condition. Si-DLC/DLC coatings with various Si content were deposited on Si substrates and tested using a reciprocating friction tester against steel balls. The results revealed that the tribological behavior of Si-DLC/DLC coatings was dependent on the Si content. The formation of transfer film and wear particles on the contact surface was greatly influenced by the Si content in DLC coatings. In particular, silicon oxide transfer film formed by tribochemical reaction contributed to reduce wear and friction.

DLC 박막의 전기전도성, 투과율 및 가스베리어 특성에 관한 연구 (Study on Electrical Conductivity, Transmittance and Gas Barrier Properties of DLC Thin Films)

  • 박새봄;김치환;김태규
    • 열처리공학회지
    • /
    • 제31권4호
    • /
    • pp.187-193
    • /
    • 2018
  • In this study, the electrical conductivity, transmittance and gas barrier properties of diamond-like carbon (DLC) thin films were studied. DLC is an insulator, and has transmittance and oxygen gas barrier properties varying depending on the thickness of the thin film. Recently, many researchers have been trying to apply DLC properties to specific industrial conditions. The DLC thin films were deposited by PECVD (Plasma Enhanced Chemical Vapor Deposition) process. The doping gas was used for the DLC film to have electrical conductivity, and the optimum conditions of transmittance and gas barrier properties were established by adjusting the gas ratio and DLC thickness. In order to improve the electrical conductivity of the DLC thin film, $N_2$ doping gas was used for $CH_4$ or $C_2H_2$ gas. Then, a heat treatment process was performed for 30 minutes in a box furnace set at $200^{\circ}C$. The lowest sheet resistance value of the DLC film was found to be $18.11k{\Omega}/cm^2$. On the other hand, the maximum transmittance of the DLC film deposited on the PET substrate was 98.8%, and the minimum oxygen transmission rate (OTR) of the DLC film of $C_2H_2$ gas was 0.83.

비구면 유리렌즈 성형용 SiC 코어의 DLC 코팅에 관한 연구 (A Research on DLC Thin Film Coating of a SiC Core for Aspheric Glass Lens Molding)

  • 박순섭;원종호
    • 한국정밀공학회지
    • /
    • 제27권12호
    • /
    • pp.28-32
    • /
    • 2010
  • Technical demands for aspheric glass lens formed in market increases its application from simple camera lens module to fiber optics connection module in optical engineering. WC is often used as a metal core of the aspheric glass lens, but the long life time is issued because it fabricated in high temperature and high pressure environment. High hard thin film coating of lens core increases the core life time critically. Diamond Like Carbon(DLC) thin film coating shows very high hardness and low surface roughness, i.e. low friction between a glass lens and a metal core, and thus draw interests from an optical manufacturing industry. In addition, DLC thin film coating can removed by etching process and deposit the film again, which makes the core renewable. In this study, DLC films were deposited on the SiC ceramic core. The process variable in FVA(Filtered Vacuum Arc) method was the substrate bias-voltage. Deposited thin film was evaluated by raman spectroscopy, AFM and nano indenter and measured its crystal structure, surface roughness, and hardness. After applying optimum thin film condition, the life time and crystal structure transition of DLC thin film was monitored.

Metal Nano Particle modified Nitrogen Doped Amorphous Hydrogenated Diamond-Like Carbon Film for Glucose Sensing

  • Zeng, Aiping;Jin, Chunyan;Cho, Sang-Jin;Seo, Hyun-Ook;Lim, Dong-Chan;Kim, Doo-Hwan;Hong, Byung-You;Boo, Jin-Hyo
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.434-434
    • /
    • 2011
  • Electrochemical method have been employed in this work to modify the chemical vapour deposited nitrogen doped hydrogen amorphous diamond-like carbon (N-DLC) film to fabricate nickel and copper nano particle modified N-DLC electrodes. The electrochemical behaviour of the metal nano particle modified N-DLC electrodes have been characterized at the presence of glucose in electrolyte. Meanwhile, the N-DLC film structure and the morphology of metal nano particles on the N-DLC surface have been investigated using micro-Raman spectroscopy, X-ray photoelectron spectroscopy and atomic force microscopy. The nickel nano particle modified N-DLC electrode exhibits a high catalytic activity and low background current, while the advantage of copper modified N-DLC electrode is drawn back by copper oxidizations at anodic potentials. The results show that metal nano particle modification of N-DLC surface could be a promising method for controlling the electrochemical properties of N-DLC electrodes.

  • PDF

Development of Diamond-like Carbon Film as Passivation Layers for Power Transistors

  • Chang, Hoon;Lee, Hae-Wang;Chung, Suk-Koo;Shin, Jong-Han;Lim, Dae-Soon;Park, Jung-Ho
    • The Korean Journal of Ceramics
    • /
    • 제3권2호
    • /
    • pp.92-95
    • /
    • 1997
  • Because of the novel characteristics such as chemical stability, hardness, electrical resistivity and thermal conductivity, diamond-like carbon (DLC) film is a suitable material for the passivation layers. For this purpose, using the PECVD, DLC films were synthesized at room temperature. The adhesion and the hardness of the DLC films deposited on Si an SiO2 substrate were measured. The resistivity of 5.3$\times$$10^8$$\Omega$.cm was measured by automatic spreading resistance probe analysis method. The thermal conductivities of different DLC films were measured and compared with that of phospho silicate glass (PSG) film which is commonly used as passivation layers. The thermal conductivity of DLC film was improved by increasing hydrogen flow rate up to 90 sccm and was better than that of PSG film. The patterning techniques of the DLC film developed using the RIE and the lift-off method to form 5$\mu\textrm{m}$ line. Finally, the thermal characteristics of the power transistor with the DLC film as passiviation layer was analyzed.

  • PDF

Tribological properties of DLC films on polymers

  • Hashizume, T.;Miyake, S.;Watanabe, S.;Sato, M.
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 2002년도 proceedings of the second asia international conference on tribology
    • /
    • pp.175-176
    • /
    • 2002
  • Our study is to search for tribological properties of diamond-like carbon (DLC) films as known as anti- wear hard thin film on various polymers. This report deals with the deposition of DLC films on various polymer substrates in vacuum by magnetron radio frequency (RF) sputtering method with using argon plasma and graphite, titanium target. The properties of friction and wear are measured using a ball-on-disk wear -testing machine. The properties of friction and wear have been remarkably improved by DLC coating. Moreover the composition of DLC films has been analyzed by using auger electron spectroscopy(AES). The wear rate of titanium-containing DLC film is lower than that of no-metal-containing DLC film.

  • PDF

FCVA 방법으로 증착된 다이아몬드상 탄소 박막의 XPS 및 XRR 특성 연구 (A Study on XPS and XRR Characteristics of DLC films Deposited by FCVA Method)

  • 박창균;장석모;엄현석;서수형;박진석
    • 대한전기학회논문지:전기물성ㆍ응용부문C
    • /
    • 제52권3호
    • /
    • pp.109-115
    • /
    • 2003
  • Diamond-like carbon (DLC) films are deposited at room temperature using a filtered cathodic vacuum arc (FCVA) technique. The influence of negative bias voltage (applied to the substrate from 0 to -250V) on the $sp^3$ hybridized carbon fraction is examined by Raman spectroscopy and x-ray photoelectron spectroscopy (XPS) for C 1s core peak. For the first time, depth profile of C 1s, Si 2p, and O 1s XPS peaks for the deposited DLC film are obtained. DLC film is modeled as a multilayered structure. composing of surface, bulk, and interface. In addition, the x-ray reflectivity (XRR) is proposed as a method for estimating the density, surface roughness, and thickness of each layer constituting the DLC film. The estimated thickness of DLC film is in good agreement with the result obtained from the transmission electron microscope (TEM) measurement.

Plasma Enhanced CVD 법으로 증착한 BON박막과 Si-DLC 박막의 산화 (Oxidation of BON and Si-DLC Thin Films deposited by Plasma Enhanced CVD method)

  • 김찬우;홍리석;이동복
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2007년도 춘계학술발표회 초록집
    • /
    • pp.73-73
    • /
    • 2007
  • Amorphous BON and Si-DLC thin films were synthesized by the RF plasma enhanced CVD method, and their oxidation behavior was studied up to $500^{\circ}C$ in air. The oxidation of both films was accompanied by evaporation of volatile species. The oxidation of BON film was preceded by nitrogen escape from the film, and oxygen penetration into the film. The oxidation of Si-DLC film was preceded by carbon escape probably as CO or $CO_2$from the film, and oxygen penetration into the film. The inwardly transported oxygen simply stayed in the oxidized BON and Si-DLC thin films.

  • PDF

DLC 박막 코팅에 의한 IR window의 적외선 투과율 향상에 관한 연구 (The improved transmittance of an IR window by coating a DLC film)

  • 엄현석;박진석;박성래;김규현
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1998년도 하계학술대회 논문집 D
    • /
    • pp.1340-1342
    • /
    • 1998
  • The diamond-like carbon(DLC) film, as an antireflection layer, is coated on a commerically used Ge window. DLC films are deposited by using an rf(13.56 MHz) plasma CVD. The optimal value of thickness and refractive index of DLC layer has been determined from the computer simulation. IR-transmittances of DLC-coated Ge windows are estimated by measuring FTIR spectra in the wavelength range of$ 2.5{\sim}25{\mu}m$. By coating the DLC film on one side of the Ge window, the transmittance measured at a wavelength of $10{\mu}m$ is about 60 %, while that of the bare Ge is lower than 50 %. Also, a higher transmittance up to about 90 % is obtained by coating the DLC film on both sides of the window. It may be suggested that the further improvement of the IR-transmittance can be achieved by more precisely controlling the thickness and the refractive index of DLC layer and also by adopting various muliti-layer antireflection structures.

  • PDF