• 제목/요약/키워드: Cu nanopowder

검색결과 20건 처리시간 0.028초

초음파 밀링한 WO3-CuO 나노혼합분말의 수소환원 거동 (The Hydrogen Reduction Behavior of Ultrasonic Ball-milled WO3-CuO Nanopowder)

  • 정성수;윤의식;이재성
    • 대한금속재료학회지
    • /
    • 제47권9호
    • /
    • pp.597-603
    • /
    • 2009
  • The hydrogen reduction behavior of ultrasonic ball-milled $WO_3-CuO$ nanopowder, which is highly related with micro-pore structure, was investigated by thermogravimetry(TG) and hygrometry system. EDS and TEM results represented that the ultrasonic ball-milled $WO_3-CuO$ nanopowder consisted of the agglomerates which was confirmed as a homogeneous mixture of $WO_3$ and CuO particles. It was found that the reduction reaction of CuO was retarded by initial micro-pores which are smaller than 40 nm in the ultrasonic ball-milled $WO_3-CuO$ nanopowder. The earlier agglomeration of Cu particles at comparably low temperature decreased the volume of micro-pores in the $WO_3-CuO$ nanopowder which caused the retardation of $WO_3$ reduction reaction. These results clearly explain that the micro-pore structure significantly affected the reduction reaction of $WO_3$ and CuO in the $WO_3-CuO$ nanopowder.

CIGS nanopowder 제조 및 특성분석 (Preparation and Characteristics of CIGS nanopowder)

  • 함창우;서정대;조정민;송기봉
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 추계학술대회 논문집
    • /
    • pp.371-372
    • /
    • 2009
  • We have prepared and characterized CIGS nanopowder for absorber layer of photovoltaic. CIGS nanopowder were obtained at $260^{\circ}C$ for 6 hours from the reaction of $CuCl_2$, $InCl_3$, $GaCl_3$ and Se powder in solvent. The CIGS nanopowder were identified to have a typical chalcopyrite tetragonal structure by using X-ray diffraction(XRD), Inductively Coupled Plasma Auger Electron Spectroscopy (AES), Scanning Electron Microscopy(SEM).

  • PDF

증류수 중 전기폭발에 의한 Cu 나노분말 제조 및 분석 (Preparation and Analysis of Cu Nanopowder by Wire Explosion in Distilled Water)

  • 조주현;진윤식;강충일;이경자;이창규
    • 전기학회논문지
    • /
    • 제59권7호
    • /
    • pp.1272-1275
    • /
    • 2010
  • The Cu powder was prepared in distilled water. It has a wide range of size distribution. The submicron-sized particles in the Cu powder were removed by using continuous type centrifugal separator. The average particle size after classification was approximately 50nm. The XRD analysis showed that pure Cu phase and oxide phase ($Cu_2O$)weremixedinthepowderpreparedbythismethod.

전기폭발법에서 SMPS를 이용한 Cu 나노분말의 실시간 입자특성평가 (In-situ Particle Characterization of Cu Nanopowder using Scanning Mobility Particle Sizer in Pulsed Wire Evaporation Method)

  • 이창우;맹덕영;박중학;유지훈;이재훈;이창규;김흥회
    • 한국분말재료학회지
    • /
    • 제10권4호
    • /
    • pp.275-280
    • /
    • 2003
  • Synthesis and characteristics of Cu nanopowder were considered by in-situ characterization method using SMPS in pulsed wire evaporation process. With increasing pressure in chamber, particle size and degree of agglomeration increased by increase of collision frequency. Also, it was found from the XRD analyses and BET measurements that crystallite size and particle size decreased with elevating applied voltage. However, SMPS measurements and TEM observation revealed the increase of particle size and degree of agglomeration with increase of applied voltage. These results suggested that particle growth and agglomeration depend on overheating factor in chamber at the early stage and thermal coagulation in filtering system during powder formation until collection.

Structure and Magnetic Properties of a Fe73.5Si13.5B9Nb3Cu1 Alloy Nanopowder Fabricated by a Chemical Etching Method and Milling Procedure

  • Hong, Seong-Min;Kim, Jeong-Gon;Kim, Cheol-Gi
    • Journal of Magnetics
    • /
    • 제14권2호
    • /
    • pp.71-74
    • /
    • 2009
  • The magnetic and structural properties of FINEMET (the Hitachi product name of the Fe-Si-B-Nb-Cu alloy) nanopowder with a composition of $Fe_{73.5}Si_{13.5}B_9Nb_3Cu_1$ atomic percent were investigated after annealing, chemical etching, and mechanical milling. The primary and secondary crystallization temperatures were 523 and $550^{\circ}C$, respectively. The grain size of the particles was adjusted by annealing time. Optimally annealed particles exhibited a homogenous microstructure composed of nanometer-sized crystalline grains. The grain boundary of the annealed particles was etched preferentially by chemical etching. Chemically etched particles were broken at the grain boundary by high-energy ball milling. As a result, a nanometer-sized FINEMET powder with a uniform size of crystalline grains was fabricated.

Microwave-Assisted Synthesis of Flower-like and Plate-like CuO Nanopowder and Their Photocatalytic Activity for Polluted Lake Water

  • Xu, Ling;Xu, Hai-Yan;Wang, Feng;Zhang, Feng-Jun;Meng, Ze-Da;Zhao, Wei;Oh, Won-Chun
    • 한국세라믹학회지
    • /
    • 제49권2호
    • /
    • pp.151-154
    • /
    • 2012
  • Flower-like and plate-like CuO nanopowder has been successfully synthesized using a facile microwave-assisted synthetic route. The morphology and size of the final products strongly depended on microwave power. The phase, structures and morphologies of the as-prepared products were investigated in detail by BET surface area analysis, X-ray diffraction (XRD) analysis, and scanning electron microscopy (SEM). In addition, the chemical oxygen demand of polluted lake water was employed for characterization of these new photocatalysts. The results showed correlations between the morphology of CuO micro-crystals and their catalytic properties.

Microstructural Feature of Full-densified W-Cu Nanocomposites Containing Low Cu Content

  • Lee, Jai-Sung;Jung, Sung-Soo;Choi, Joon-Phil;Lee, Geon-Yong
    • 한국분말재료학회지
    • /
    • 제20권2호
    • /
    • pp.138-141
    • /
    • 2013
  • The microstructure evolution during sintering of the W-5 wt.%Cu nanocomposite powders was investigated for the purpose of developing a high density W-Cu alloy. The W-5 wt.%Cu nanopowder compact, fully-densified during sintering at 1623 K, revealed a homogeneous microstructure that consists of high contiguity structures of W-W grains and an interconnected Cu phase located along the edges of the W grains. The Vickers hardness of the sintered W-5 wt.%Cu specimen was $427{\pm}22$ Hv much higher than that ($276{\pm}19$ Hv) of the conventional heavy alloy. This result is mostly due to the higher contiguity microstructure of the W grains compared to the conventional W heavy alloy.

플렉시블 CIGS 태양전지 제조를 위한 저온 나노입자공정 (Low Temperature Nanopowder Processing for Flexible CIGS Solar Cells)

  • 박진호;;;박준영
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2010년도 춘계학술대회 초록집
    • /
    • pp.61.1-61.1
    • /
    • 2010
  • $CuIn_{1-x}-GaxSe_2$ based materials with direct bandgap and high absorption coefficient are promising materials for high efficiency hetero-junction solar cells. CIGS champion cell efficiency(19.9%, AM1.5G) is very close to polycrystalline silicon(20.3%, AM1.5G). A reduction in the price of CIGS module is required for competing with well matured silicon technology. Price reduction can be achieved by decreasing the manufacturing cost and by increasing module efficiency. Manufacturing cost is mostly dominated by capital cost. Device properties of CIGS are strongly dependent on doping, defect chemistry and structure which in turn are dependent on growth conditions. The complex chemistry of CIGS is not fully understood to optimize and scale processes. Control of the absorber grain size, structural quality, texture, composition profile in the growth direction is important to achieving reliable device performance. In the present work, CIS nanoparticles were prepared by a simple wet chemical synthesis method and their structural and optical properties were investigated. XRD patterns of as-grown nanopowders indicate CIS(Cubic), $CuSe_2$(orthorhombic) and excess selenium. Further, as-grown and annealed nanopowders were characterized by HRTEM and ICP-OES. Grain growth of the nanopowders was followed as a function of temperature using HT-XRD with overpressure of selenium. It was found that significant grain growth occurred between $300-400^{\circ}C$ accompanied by formation of ${\beta}-Cu_{2-x}Se$ at high temperature($500^{\circ}C$) consistent with Cu-Se phase diagram. The result suggests that grain growth follows VLS mechanism which would be very useful for low temperature, high quality and economic processing of CIGS based solar cells.

  • PDF

펄스전류활성 가열에 의한 나노구조의 TiCu 급속소결과 기계적 성질 (Rapid Sintering of TiCu by Pulsed Current Activated Heating and its Mechanical Properties)

  • 두송이;김나리;김원백;조성욱;손인진
    • 대한금속재료학회지
    • /
    • 제48권10호
    • /
    • pp.922-928
    • /
    • 2010
  • Nanopowder of TiCu was synthesized by high-energy ball milling. A dense nanostructured TiCu was consolidated using a pulsed-current activated sintering method within 1 minute from mechanically synthesized powders of TiCu and horizontally milled powders of Ti+Cu. The grain size and hardness of the TiCu sintered from horizontally milled Ti+Cu powders and high-energy ball-milled TiCu powder were 68 nm, 27 nm and $490kg/mm^2$, $600kg/mm^2$, respectively.