• Title/Summary/Keyword: Copper electrode

Search Result 377, Processing Time 0.029 seconds

The Lift-off and Fall-down Characteristics due to Particles in Coaxial Electrode (동축원통 전극내 금속이물의 부상 및 하강전압 특성)

  • Lee, Jae-Gul;Lee, Kon;Jin, Sang-Bum;Park, Hyun-Su;Cho, Kook-Hee;Kim, Kyong-Hwa;Kwak, Hee-Ro
    • Proceedings of the KIEE Conference
    • /
    • 1998.07e
    • /
    • pp.1711-1713
    • /
    • 1998
  • This paper describes the insulation characteristics of GIS by the free conducting particles under alternating voltage. The particles of the GIS can cause decrease in breakdown voltages. Various materials and sizes of free conducting particles were used to study the lift-off and fall-down characteristics. The measured lift-off voltage for copper particle agreed with the calculated one.

  • PDF

Functional Inks for Printed Electronics

  • Choi, Young-Min;Jeong, Sun-Ho
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2012.05a
    • /
    • pp.63.1-63.1
    • /
    • 2012
  • In recent years, the functional inks for printed electronics that can be combined with a variety of printing techniques have attracted increasingly significant interest for use in low cost, large area, high performance integrated electronics and microelectronics. In particular, the development of solution-processable conductor, semiconductor and insulator materials is of great importance as such materials have decisive impacts on the electrical performance of various electronic devices, and, therefore, need to meet various requirements including solution processability, high electrical performance, and environmental stability. Semiconductor inks such as IGO, CIGS are synthesized by chemical solution method and microwave reaction method for TFT and solar cell application. Fine circuit pattern with high conductivity, which is valuable for flexible electrode for PCB and TSP devices, can be printed with highly concentrated and stabilized conductor inks such as silver and copper. Solution processed insulator such as polyimide derivatives can be use to all printed TFT device. Our research results of functional inks for printed electronics provide a recent trends and issues on this area.

  • PDF

Effect of temperature and oxygen partial pressure on the growth and development of Cu2O nanorods by radio frequency magnetron sputtering

  • You, Jae-Lok;Jo, Kwang-Min;Kim, Se-Yoon;Lee, Joon-Hyung;Kim, Jeong-Joo;Heo, Young-Woo
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2013.05a
    • /
    • pp.102-103
    • /
    • 2013
  • As an important p-type semiconductor metal oxide with a narrow band gap (1.2 - 2.6eV), copper oxide (Cu2O) has been studied because of its various applications as material for heterogeneous catalysts, gas sensors, optical switch, lithium-ion electrode materials, field emission devices, solar cells. The fundamental properties of oxide-semiconductor can be greatly affected by the surface morphology, size, geometry and spatial orientation.

  • PDF

Electrochemical Behaviors of ABTS2- on the Thiol-modified Gold Electrodes

  • Kim, Hyug-Han
    • Journal of the Korean Electrochemical Society
    • /
    • v.9 no.3
    • /
    • pp.113-117
    • /
    • 2006
  • The electrochemical properties of the redox mediator, 2,2'-azinobis (3-ethylbenzothiazoline-6-sulfonate) ($ABTS^{2-}$) were studied using cyclic voltammetry. The measured potentials (${E^o}'$ vs SCE) of the two redox couples of ABTS are 0.45 V for $ABTS^{2-}/ABTS^{\cdot-}$ and 0.87 V for $ABTS^{\cdot-}/ABTS^0$. The rate constant for heterogeneous electron transfer and the diffusion coefficients for $ABTS^{2-}$ are $5x10^{-3}cm\;s^{-1}$ and $3.1x10^{-6}cm^2\;s^{-1}$, respectively. Our interest in $ABTS^{2-}$ stems from the fact that this molecule functions as a substrate to the copper oxidase, laccase, by providing the reducing equivalents necessary for the biocatalyzed reduction of dioxygen to water. Consequently, when laccase is tethered to an electrode surface or dissolved in solution, $ABTS^{2-}$ can be used to quantify enzyme activity electrochemically.

Synthesis of the New 1,2-Dithiolene Metal Complexes[M$(BDDT)_2^-$] (M=Ni, Cu) and Their Electrode Structures

  • 전기원;Robert D. Bereman
    • Bulletin of the Korean Chemical Society
    • /
    • v.17 no.7
    • /
    • pp.612-616
    • /
    • 1996
  • The new 1,2-dithiolene, 1,4-butanediyldithioethylene-1,2-dithiolate (BDDT2-), has been isolated. In addition, new monoanionic bis-complexes with nickel and copper have been prepared and characterized. In order to investigate the detailed electronic structure of the metal complexes of the new ligand, BDDT2-, in terms of the oxidation state of the central metal ions, we have carried out molecular orbital (MO) calculations of Ni(BDDT)2-and Cu(BDDT)2- utilizing an Extended Huckel method. Cyclic voltammetry data for both complexes were obtained with a potentiostat. We have also compared these results to the previously synthesized Ni(PDDT)2-, Ni(DDDT)2-,Cu(PDDT)2-, and Cu(DDDT)2-.

A STUDY ON CORROSION BEHAVIOR OF DENTAL AMALGAMS AS A FUNCTION OF TIME (시간경과에 따른 아말감의 부식거동에 관한 연구)

  • Lee, Myung-Jong;Kim, Yung-Hai;Lee, C.S.;Yoon, Soo-Han;Lim, Sung-Sam;Kwon, Hyuk-Choon;Um, Chung-Moon
    • Restorative Dentistry and Endodontics
    • /
    • v.16 no.1
    • /
    • pp.6-15
    • /
    • 1991
  • The purpose of this study was to observe in vitro chloride corrosion behavior from 5 kinds of amalgam (Caulk spheracal, Amalcap, Dispersalloy, Tytin, Sybralloy) as a function of time after tritruration by using potentiostat. After each amalgam alloy and Hg was triturated as the direction of the manufacturer by the mechanical amalgamator, the triturated mass was inserted the cyrindrical matal mold ($12{\times}10mm$) and was condensed by using routine manner. The specimen was removed from the mold and was stored at room temperature for 1 week, 1 month and 3 months, and standard surface preparation was routine carried out. The 0.9% saline solution was used as electrolyte in pH 6.8~7.0 at $30{\pm}0.5.^{\circ}C$. The open circuit potential was determined after 30 minutes' immersion of 1 week, 1 month and 3 month old specimens. The scan rate was 1 mV/sec and the surface area of amalgam exposed to the solution was $0.65\;Cm^2$ for each specimen. All potentials reported are with respect to a silver / silver chloride electrode (SSE). The following result was obtained. 1. All amalgam specimens became more noble corrosion potentials which represent the improved corrosion resistance as the time elapsed. 2. Three kinds of high copper amalgam always exhibited more noble potential than low copper amalgam at 1 week, 1 month and 3 months. 3. Two kinds of low copper amalgam had the similar polarization curve pattern with 3 current peaks at each time period and current densities associated with these peaks were decreased as aging especially in caulk spherical amalgam. 4. All kinds of high copper amalgam had the similar polarization curve pattern with absence of prominent current peak at each time period, but the polarization curve of D amalgam had one apparent current peak at 1 week.

  • PDF

ELECTROCHEMICAL STUDY ON THE CORROSION BEHAVIOUR OF DENTAL AMALGAM IN ARTIFICIAL SALIVA (인공타액에서 아말감의 부식거동에 관한 전기화학적 연구)

  • Kim, Yeoung-Nam;Um, Chung-Moon
    • Restorative Dentistry and Endodontics
    • /
    • v.13 no.2
    • /
    • pp.221-235
    • /
    • 1988
  • The purpose of this study was to observe characteristic properties through the polarization curves and EMPA images from 4 different types of amalgam obtained by using the potentiostats (EG & G PARC) & EPMA (Jeol JSM-35), to investigate the degree of corrosion of each phase of amalgam on the oxidation peak, and to identify corrosion products from the corroded amalgam by use of X-ray diffractometer(Rigaku). After each amlgam alloy and Hg were triturated as the direction of the manufacturer by means of the mechanical amalgamator(Shofu), the triturated mass was inserted into the cylindrical metal mold which was 12mm in diameter and 10mm in height and was condensed by means of routine manner. The specimen was removed from the mold and stored at room temperature for about 7 days. The standard surface preparation was routinely carried out. Anodic polarization measurement was employed to compare the corrosion behaviours of the amalgams in 0.9% saline solution(pH6.8~7.0) and artificial saliva (pH6.8~7.0) at $37^{\circ}C$. The open circuit potential was determined after 30 minutes' immersion of specimen in electrolyte and the potential scan was begun at the potential of 100mV cathodic from the corrosion potential. The scan rate was 1mV/sec and the surface area of amalgam exposed to the solution was 0.64$cm^2$ for each specimen. All the potentials reported are with respect to a saturated calomel electrode (SCE). EPMA images on the determined oxidation peaks of each amalgam in artificial saliva were observed. X-ray diffraction patterns of each sample were recorded before and after polarization in artificial saliva (Aristaloy, Caulk Spherical, Dispersalloy and Tytin: at +770mV, +585mV, +8.10m V and +680m V respectively) by use of a recording diffractometer. Nickel filtered Cu $K_{{\alpha}_1}$ radiation was used and sample was scanned at $4^{\circ}(2{\theta})/min.$ from $25^{\circ}$ to $80^{\circ}$. The following results were obtained. 1. Oxidation peak potential in artificial saliva shifted to more anodic direction than that in saline solution. 2. The corrosion potential of high copper amalgam was more anodic than the potential of low copper amalgam. 3. The current density was lower in artificial saliva than in saline solution. 4. One of the corrosion products, AgCl was identified by X-ray diffraction analysis. 5. ${\gamma}_2$ phase was the most susceptible to corrosion and e phase was stable in low copper amalgam and ${\eta}$' phase and Ag-Cu eutectic were susceptible to corrosion in high copper amalgam.

  • PDF

Trajectory Simulation of ASR Particles in Induction Electrostatic Separation (유도형 정전선별에서 ASR 입자의 궤적모사)

  • Kim, Beom-uk;Park, Chul-hyun
    • Resources Recycling
    • /
    • v.28 no.6
    • /
    • pp.96-105
    • /
    • 2019
  • Automobile shredder residue (ASR) is the final waste produced when end-of-life vehicles (ELVs) are shredded. ASR can be separated using mineral-processing operations such as comminution, air classification, magnetic separation, and/or electrostatic separation. In this work, trajectory analyses of conductors (copper) and non-conductors (glass) in the ASR have been carried out using induction electrostatic separator for predicting or improving the ASR-separation efficiency. From results of trajectory analysis for conductors, the trajectories of copper wire by observation versus simulation for coarse particles of 0.5 and 0.25 mm showed consistent congruity. The observed 0.06 mm fine-particles trajectory was deflected toward the (-) attractive electrode owing to the charge-density effects due to the particle characteristics and relative humidity. In the case of non-conductors, the actual trajectory of dielectric glass deflected toward the (-) electrode, showing characteristics similar to those of conductive particles. The analyses of stereoscopic microscope and SEM & EDS found heterologous materials (fine ferrous particles and conductive organics) on the glass surface. This demonstrates the glass decreasing separation efficiency for non-ferrous metals during electrostatic separation for the recycling of ASR. Future work will require a pretreatment process for eliminating impurities from the glass and advanced trajectory-simulation processes.

Electricity Generation and De-contamination Effect for Characteristic Electrode Material in a Microbial Fuel Cell System Using Bay Sediment (MFC의 금속 및 탄소전극에 의한 전기생산 특성과 오염저감 효과)

  • Kwon, Sung-Hyun;Song, Hyung-Jin;Lee, Eun-Mi;Cho, Dae-Chul;Rhee, In-Hyoung
    • Journal of Environmental Science International
    • /
    • v.19 no.8
    • /
    • pp.951-960
    • /
    • 2010
  • Sediment works as a resource for electric cells. This paper was designed in order to verify how sediment cells work with anodic material such as metal and carbon fiber. As known quite well, sediment under sea, rivers or streams provides a furbished environment for generating electrons via some electron transfer mechanism within specific microbial population or corrosive oxidation on the metal surfaces in the presence of oxygen or water molecules. We experimented with one type of sediment cell using different anodic material so as to attain prolonged, maximum electric power. Iron, Zinc, aluminum, copper, zinc/copper, and graphite felt were tested for anodes. Also, combined type of anodes-metal embedded in the graphite fiber matrix-was experimented for better performances. The results show that the combined type of anodes exhibited sustainable electricity production for ca. 600 h with max. $0.57\;W/m^2$ Al/Graphite. Meanwhile, graphite-only electrodes produced max. $0.11\;W/m^2$ along with quite stationary electric output, and for a zinc electrode, in which the electricity generated was not stable with time, therefore resulting in relatively sharp drop in that after 100 h or so, the maximum power density was $0.64\;W/m^2$. It was observed that the corrosive reaction rates in the metal electrodes might be varied, so that strength and stability in the electric performances(voltage and current density) could be affected by them. In addition to that, COD(chemical oxygen demand) of the sediment of the cell system was reduced by 17.5~36.7% in 600 h, which implied that the organic matter in the sediment would be partially converted into non-COD substances, that is, would suggest a way for decontamination of the aged, anaerobic sediment as well. The pH reduction for all electrodes could be a sign of organic acid production due to complicated chemical changes in the sediment.

AN ELECTROCHEMICAL STUDY ON THE CORROSION BEHAVIOUR OF AMALGAMS IN THE SALINE SOLUTIONS WITH FLUORIDE COMPOUNDS (불소화합물을 첨가한 생리식염수에서 아말감의 부식거동에 관한 전기화학적 연구)

  • Yun, Chong-Hun;Kwon, Hyuk-Choon;Um, Chung-Moon
    • Restorative Dentistry and Endodontics
    • /
    • v.22 no.1
    • /
    • pp.396-412
    • /
    • 1997
  • The purpose of this study is to observe the corrosion characteristics of five dental amalgams(CAULK FINE CUT, OPTALLOY II, DISPERSALLOY, TYTIN, and VALIANT) in the solutions with fluoride compound through the anodic polarization curve obtained by using a potentiostat. After each amalgam alloy and Hg being triturated, the triturated mass was inserted into the cylindrical metal mold, and condensed by hydraulic pressure(160 kg/$cm^2$). Each specimen was removed from the metal mold. Specimens were polished with the silicone carbide grinding paper 24 hours after condensation and stored at room temperature for 1 week. The anodic polarization curves were employed to compare the corrosion behaviours of the amalgams in 0.9 % saline solution and in the saline solutions with 2.2 ppm, 0.05 %, 2 % NaF, and 8 % $SnF_2$ at $37^{\circ}C$ with 3-electrode potentiostat. After the immersion of specimen in electrolyte for 30 minutes, the potential scan was begun. The potential scan range was -1500m V to + 800m V(vs. S.C.E.) in the working electrode and the scan rate was 50 mV/sec. The results were as follows, 1. The corrosion potential, the potential of anodic current peak, and transpassive potential in the saline solutions with NaF shifted to lower direction than those in normal saline solution, and the current density in the saline solutions with NaF was higher than that in normal saline solution. The differences were increased as the concentrations of NaF became higher. 2. The corrosion potential and transpassive potential in the saline solution with $SnF_2$ shifted to higher direction than those in normal saline solution, and the current density in the saline solution with $SnF_2$ was higher than that in normal saline solution after the corrosion potential. The anodic polarization curves in the saline solution with $SnF_2$ had no outstanding anodic current peak. 3. The corrosion potentials for high-copper amalgams were much higher than those for CAULK FINE CUT and OPTALLOY II in normal saline solution, but, as the concentrations of fluoride compound became higher, the differences in corrosion potentials between them were decreased. The corrosion potentials had the similarity in the saline solution with 2% NaF or 8% $SnF_2$. 4. The current density for TYTIN was the lowest among the others in normal saline solution and in the saline solution with 2.2 ppm or 0.05 % NaF. 5. There was no significant difference in current density between Pd-enriched VALIANT and other high-copper amalgams.