A Comparative Analysis of Thermal Properties of COB LED based on Thermoelectric Device Structure (열전소자 구조에 따른 COB LED의 방열 성능 비교 분석)

  • Kim, Hyo-Jun;Kang, Eun-Yeong;Im, Seong-Bin;Hoang, Geun-Chang;Kim, Yong-Kab
    • The Journal of the Institute of Internet, Broadcasting and Communication
    • /
    • v.15 no.2
    • /
    • pp.189-194
    • /
    • 2015
  • In this study, the heat radiation performance of COB LED according to the structure of thermoelectric device were compared. Thermoelectric device of the sheet copper structure and ceramic structure were used for bonding with the heating part of the COB LED. The temperature distribution in the bonding part of the thermoelectric device of COB LED was measured with a contact-type thermometer. The temperature variation of the thermoelectric device was measured by inputting the currents of 0.1A, 0.3A, 0.5A, and 0.7A. When 0.7A was applied, the temperature of the bonding part where there was a heat aggregation phenomenon of the COB LED was $59^{\circ}C$ for thermoelectric device of the sheet copper structure and $67^{\circ}C$ for the thermoelectric device of the ceramic structure. Therefore, the sheet copper thermoelectric device whose temperature was lower by $9^{\circ}C$ showed better heat radiation performance than those of the ceramic structure.

AN EXPERIMENTAL STUDY ON THE BONDING FORCE OF GLASS IONOMER CEMENT (Glass Ionomer Cement의 접착력(接着力)에 관(關)한 실험적(實驗的) 연구(硏究))

  • Lee, Myung-Jong
    • Restorative Dentistry and Endodontics
    • /
    • v.7 no.1
    • /
    • pp.77-83
    • /
    • 1981
  • The purpose of this study was to observe the bonding strength between tooth surface (enamel and dentin) and restorative filling materials which are two composite resins (Clearfil and Concise) and Glass ionomer cement, after etching with 50% phoshoric acid and 37% citric acid. To measure the bonding strength in enamel, the labial surface of upper anterior tooth was cut flatly with using carborundum disk and polished with sand paper disk, and to measure in dentin, the dentin surface was prepared by grinding upper part of posterior tooth horizontally. After washing the tooth surface with water and drying with air blast, the prepared tooth surface was etched. In glass ionomer cement, 50% phosphoric acid and 37% citric acid were used, in Clearfil 40% phosphoric acid was used and in Concise, 50% phosphoric acid and 37% citric acid were used as etchant for 1 minute. After the copper band which is 5 mm in diameter and 5 mm in height was fixed on the prepared surface and each filling material was inserted into the copper band, the hooking loop was inserted into filled material in the copper band before setting to make it easily that the load is applied on the specimen. After all specimens were immersed in water at $37^{\circ}C$ for 1 week, this specimen was placed on the load cell of tensile test apparatus, and specimen was pulled at the cross-head speed of 0.8 mm per minute. The following results were obtained 1) In glass ionomer cement, the bond strength obtained by 37% citric acid was higher than one obtained by 50% phosphoric acid in enamel and dentin surfaces. The bond strength obtained in non-etched surface was much less than one by etchants in enamel and dentin surface. 2) In Clearfil, the bond strength obtained by 40% phosphoric acid was 4 times more than one obtained by non etch ant. 3) In Concise, the bond strength obtained by 50% phosphoric acid was almost same as one obtained by 37% citric acid, and the bond strength obtained by non etch ant was much less than one obtained by etchants.

  • PDF

The Effect of the Composition of Metallizing Paste on the Bonding Strength in the Joining of Al2O3/Cu to Cu (Al2O3/Cu 접합에서 Metallizing paste의 조성이 접합강도에 미치는 영향)

  • Yoon, Jong-Hyuk;Park, Hyun Gyoon
    • Journal of Welding and Joining
    • /
    • v.31 no.6
    • /
    • pp.65-70
    • /
    • 2013
  • In joining Alumina to copper plate by Mo-Mn metallizing process, the effects of the composition of metallizing paste on the bonding strength were investigated. The bonding strength increased with increasing Mn amount in the paste up to 20% but followed by the decrease with addition of Mn. The maximum bonding strength reached 50MPa at 20%Mn when heated to $1550^{\circ}C$ for 60minute. The addition of Si to the metallizing powder increased the bonding strength of the joint by enhancing the mechanical bonding between the Alumina and the metallizing layer due to the decrease of layer viscosity with the addition of $SiO_2$. It is thought that MnO reacted with $Al_2O_3$ to yield $MnAl_2O_4$ spinel, forming a joint.

Effects of welding parameters on ultrasonic bonding strength of solar collector (태양열집열판의 초음파 심용접 시 접합부 강도에 미치는 공정변수의 영향)

  • Lee Jeong-Han;Kim Suk-Hwan;Cheon Chang-Geun;Kim Seong-Uk;Kim Jong-Do
    • Proceedings of the KWS Conference
    • /
    • 2006.05a
    • /
    • pp.233-235
    • /
    • 2006
  • This study was performed to find the best bonding conditions by comparing mechanical properties in solar collector. The solar collector that consists of copper plate and tube was successfully bonding by ultrasonic seam welding. In this experiment, we varied the values of welding pressure and welding amplitude and fixed the values of speed and frequency. Consequently, it was find that the welding pressure had higher effort on bonding strength than the welding amplitude.

  • PDF

Method of Solving Oxidation Problem in Copper Pillar Bump Packaging Technology of High Density IC (고집적 소자용 구리기둥범프 패키징에서 산화문제를 해결하기 위한 방법에 대한 연구)

  • Jung, One-Chul;Hong, Sang-Jeen;Soh, Dae-Wha;Hwang, Jae-Ryong;Cho, Il-Hwan
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.12
    • /
    • pp.919-923
    • /
    • 2010
  • Copper pillar tin bump (CPTB) was developed for high density chip interconnect technology. Copper pillar tin bumps that have $100{\mu}m$ pitch were introduced with fabrication process using a KM -1250 dry film photoresist (DFR), copper electroplating method and Sn electro-less plating method. Mechanical shear strength measurements were introduced to characterize the bonding process as a function of thermo-compression. Shear strength has maximum value with $330^{\circ}C$ and 500 N thenno-compression process. Through the simulation work, it was proved that when the copper pillar tin bump decreased in its size, it was largely affected by the copper oxidation.

Synthesis of Cu Sintering Paste Using Growth of Nanofiber on Cu Microparticles Mixed with Formic Acid (포름산 혼합 나노섬유 성장 구리마이크로입자를 이용한 구리 소결 페이스트 합성)

  • Young Un Jeon;Ji Woong Chang
    • Applied Chemistry for Engineering
    • /
    • v.35 no.2
    • /
    • pp.96-99
    • /
    • 2024
  • A sintering paste for bonding copper plates was synthesized using Cu formate nanofibers on Cu microparticles, mixed with formic acid. Copper oxide nanofibers of 10 ㎛ grown at 400 ℃ on Cu microparticles on the surface were transformed into copper formate nanofibers through the mixing of formic acid. Compared to Cu bulk particles or nanoparticles, Cu formate on Cu microparticles decomposed into metallic Cu at a lower temperature of 210 ℃, facilitating the sintering of copper paste. The growth of nanofiber on Cu microparticles allowed for an increase in the reaction rate of formation to copper formate, aggregating surface area, and decomposition rate of copper formate, resulting in fast sintering.

Energy Calibration of ESCA Spectrum for the Copper in the Interface of Copper and Cordierite (구리와 코디에라이트와의 접촉점에서 구리에 대한 ESCA 스펙트럼의 에너지 교정)

  • Han, Byoung-Sung
    • Journal of the Korean Institute of Telematics and Electronics
    • /
    • v.25 no.1
    • /
    • pp.27-32
    • /
    • 1988
  • Electron Spectroscopy for Chemical Analysis(ESCA) allowes the determination of the elemental composition and the bonding state of the surface atomes in the interface between two materials. In the binding energies of ESCA spectrum, there are zero error, voltage scaling error and random error. Accurate analysis of the intensity energy response functions and accurate calibration of the energy scale are essential to use X-ray photoelectron spectron meter. At the results of the calibration of the ESCA spectra in the copper and cordierite (Mg2Al4Si5kO18) interfaces, the errors relative to the copper are -3.03 eV for the zero error -z,-197 ppm for the voltage scaling error -V and 6.9 meV for the random error -R. The method of the calibration is able to apply for the binding energy calibration of the another ESCA spectra.

  • PDF

Effects of Hardeners and Catalysts on the Reliability of Copper to Copper Adhesive Joint (Cu-Cu 접착부의 고온고습 내구성에 미치는 경화제 및 촉매제의 영향)

  • Min, Kyung-Eun;Kim, Hae-Yeon;Bang, Jung-Hwan;Kim, Jong-Hoon;Kim, Jun-Ki
    • Korean Journal of Materials Research
    • /
    • v.21 no.5
    • /
    • pp.283-287
    • /
    • 2011
  • As the performance of microelectronic devices is improved, the use of copper as a heat dissipation member is increasing due to its good thermal conductivity. The high thermal conductivity of copper, however, leads to difficulties in the joining process. Satisfactory bonding with copper is known to be difficult, especially if high shear and peel strengths are desired. The primary reason is that a copper oxide layer develops rapidly and is weakly attached to the base metal under typical conditions. Thus, when a clean copper substrate is bonded, the initial strength of the joint is high, but upon environmental exposure, an oxide layer may develop, which will reduce the durability of the joint. In this study, an epoxy adhesive formulation was investigated to improve the strength and reliability of a copper to copper joint. Epoxy hardeners such as anhydride, dihydrazide, and dicyandiamide and catalysts such as triphenylphosphine and imidazole were added to an epoxy resin mixture of DGEBA and DGEBF. Differential scanning calorimetry (DSC) analyses revealed that the curing temperatures were dependent on the type of hardener rather than on the catalyst, and higher heat of curing resulted in a higher Tg. The reliability of the copper joint against a high temperature and high humidity environment was found to be the lowest in the case of dihydrazide addition. This is attributed to its high water permeability, which led to the formation of a weak boundary layer of copper oxide. It was also found that dicyandiamide provided the highest initial joint strength and reliability while anhydride yielded intermediate performance between dicyandiamide and dihydrazide.

Synthesis, Structure and Biological Properties of a Novel Copper (II) Supramolecular Compound Based on 1,2,4-Triazoles Derivatives

  • Qiu, Guang-Mei;Wang, Cui-Juan;Zhang, Ya-Jun;Huang, Shuai;Liu, Xiao-Lei;Zhang, Bing-Jun;Zhou, Xian-Li
    • Bulletin of the Korean Chemical Society
    • /
    • v.33 no.8
    • /
    • pp.2603-2608
    • /
    • 2012
  • A novel mononuclear supramolecule of copper(II) has been synthesized with Ippyt ligand (Ippyt=3-(4'-imidazole phenyl)-5-(pyrid-2''-yl)-1,2,4-triazole) (1). Compound 1, namely [$Cu(Ippyt)_2(H_2O)_2$], has been characterized by single-crystal X-ray diffraction, IR spectrum, elemental analysis and thermogravimetric analysis. Structure determination reveals that the elongated-octahedral geometry is formed in the vicinity of the copper (II) atom being coordinated by four nitrogen atoms from two Ippyt ligands occupying the equatorial position and two oxygen atoms from two coordinated water molecules in the axial position, which together form the $N_4O_2$ donor set. Hydrogen bonding interactions between nitrogen and oxygen atoms result in the set up of a supramolecular network architecture. Biological properties including antibacterial activity and superoxide dismutase (SOD) mimetic activity of compound 1 have been investigated by agar diffusion method and the modified Marklund method, respectively. The results indicate that compound 1 exhibits a stronger antibacterial efficiency than the parent ligand and it also has a certain radical-scavenging activity.

Characteristics of electrically conductive adhesives filled with silver-coated copper

  • Nishikawa, Hiroshi;Terad, Nobuto;Miyake, Koich;Aoki, Akira;Takemoto, Tadashi
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.217-220
    • /
    • 2009
  • Conductive adhesives have been investigated for use in microelectronics packaging as a lead-free solder substitute due to their advantages, such as low bonding temperature. However, high resistivity and poor mechanical behavior may be the limiting factors for the development of conductive adhesives. The metal fillers and the polymer resins provide electrical and mechanical interconnections between surface mount device components and a substrate. As metal fillers used in conductive adhesives, silver is the most commonly used due to its high conductivity and the stability. However the cost of conductive adhesives with silver fillers is much higher than usual lead-free solders and silver has poor electro-migration performance. So, copper can be a promising candidate for conductive filler metal due to its low resistivity and low cost, but oxidation causes this metal to lose its conductivity. In this study, electrically conductive adhesives (ECAs) using surface modified copper fillers were developed. Especially, in order to overcome the problem associated with the oxidation of copper, copper particles were coated with silver, and the silver-coated copper was tested as a filler metal. Especially the effect of silver coating on the electrical resistance just after curing and after aging was investigated. As a result, it was found that the electrical resistance of ECA with silver-coated copper filler was clearly lower and more stable than that of ECA with pure copper filler after curing process. And, during high temperature storage test, the degradation rate of electrical resistance for ECA with silver coated copper filler was quite slower than that for ECA with pure copper filler.

  • PDF