Kim, Seong-Sik;Kwak, Kyoung-Ho;Ko, Ching-Chang;Park, Soo-Byung;Son, Woo-Sung;Kim, Yong-Il
대한치과교정학회지
/
제46권6호
/
pp.372-378
/
2016
Objective: The purpose of the present study was to evaluate the postoperative three-dimensional (3D) changes in the proximal segments after mandibular setback sagittal split ramus osteotomy and to compare the changes between the conventional mini-plate fixation and semi-rigid sliding plate fixation. Methods: Cone-beam computed tomography (CBCT) images were used to evaluate the postoperative 3D changes in the proximal segments during the healing process. CBCT images were superimposed using the symphysis and the lower anterior mandible as references. Results: There were no statistically significant differences between the conventional mini-plate and semi-rigid sliding plate groups (p > 0.05). With respect to the distribution of changes greater than 2 mm in the landmarks, the right condylion, right coronoid process, and left condylion showed ratios of 55.6%, 50.0%, and 44.4%, respectively, in the semi-rigid sliding plate group; however, none of the landmarks showed ratios greater than 30% in the conventional mini-plate group. Conclusions: There were no statistically significant differences in postoperative changes in the segments between the conventional mini-plate and semi-rigid sliding plate groups. Nevertheless, while selecting the type of fixation technique, clinicians should consider that landmarks with greater than 2 mm changes were higher in the semi-rigid sliding plate group than in the conventional mini-plate group.
During the operation, fatigue failures and cracks of duct plate due to excessive duct vibration occurred in the fan-duct systems of fossil fueled boilers. We measured static pressure variation(pressure pulsation) in the outlet, and also measured vibration at the outlet duct of a centrifugal fan. It was found that strong pressure Pulsation caused by the inlet vortex occurred in inlet vane of centrifugal fan in the middle range of vane opening. Thus, excessive duct vibration is caused by strong pressure pulsation. In this paper, it is shown that the frequency and amplitude of pressure pulsation depend mainly on vane opening and are compared with duct vibration. Also, effective solution for reducing pressure pulsation and vibration are presented.
This study is on safety improvement measures through analysis of accident cases during plant storage tank construction. Storage tank is a general term for artificial ground facility constructed to store oil, water, gas, and other chemicals. Some companies have clustered storage tanks (tank farm). The construction methods vary according to the component and types of fluids. Because most of the construction procedures include lifting heavy weight materials using heavy construction equipment and are carried out at high places, storage tank construction contains more risk factors than normal aerial construction. Recently, major accidents such as storage tank collapse have occurred often, and cost many lives due to the characteristics of the structure. In this study we would like to analyze the cause of these accidents and propose measures to improve safety.
To mitigate the effects of cavitation and flashing, several types of orifices have been installed in the pipeline of new nuclear power plants. To review the effects of wall thinning caused by flow-accelerated corrosion by the types of orifices, which are cone and plate, and the relation between flow behavior and local wall thinning, experiments and numerical analyses for the downstream pipe of two types of orifices were performed. The experimental results in terms of static pressure obtained for the experimental facilities were compared with those of three-dimensional (3D) numerical analyses using the FLUENT code. As the results of review of flow-accelerated corrosion effects based on the experiment and numerical analysis, it was identified that the orifice of cone-type can be comparatively mitigated the effects of cavitation and flashing, but can not be mitigated the effect of flow-accelerated corrosion.
This paper is investigated about the effect of vibration of the water surface for hydrogen gas generation by non-thermal plasma. The vibration of the water surface is more powerful with increasing applied voltage. In this experimental reactor which is made of multi-needle and plate, the maximum acquired hydrogen production rate is about 6.8[ml/sec]. Although the generation of hydrogen gas is increased with elevating time, it is saturated after specific time due to the volume of reactor and the saturation of taylor cone.
목적 : 강내에 발생된 종양치료용 원통형 전자선 조사기구(Electron cone)는 기하학적으로 강내벽에 위치한 종양치료에 부적당하므로 후방 또는 측면방향으로 산란되는 전자선을 이용하여 체강 내벽점막 등에 발생된 종양을 효과적으로 치료할 수 있는 산란전자선 치료방법을 개발하고자 한다. 강내조사기구내에 전자선 입사방향에 수직 또는 일정한 각도의 산란판을 배치하여 측면방향으로 산란전자선을 방출시키는 강내 측면조사기구를 제작하고 산란판의 제원과 전자선 에너지에 따라 산란방출된 산란선의 특성과 조직내 선량분포를 측정 평가하였다. 새상 미 방법 : 외부조사용 전자선조사기구(Electron cone) 대신에 강내 삽입용 전자산란선 조사통(Intracavitary backscatter electron cone)과 이를 콜리메이터와 연결시킬 수 있는 차폐연결기구(Shielded electron device)를 고안하였다. 산란전자선 조사기구는 직경이 $2\~3\;cm$이고 길이가 25 cm인 금속(내식강)원통을 이용하였으며 입구에서 20 cm위치에 산란판을 부착시키고 원통 측면에 직경 $1\~2\;cm$의 산란선 방출구를 제작하였다. 산란판은 $2\~10\;mm$의 연판을 사용하였으며, 오제전자와 특성 엑스선을 제거하기 위하여 주석, 구리, 알루미늄판 등을 부착시켰으며 종양위치를 관찰할 수 있도록 표면을 처리하였다. 고에너지 방사선치료용 선형가속기(Clinac 2100C/D)에서 발생된 $6\~12\;MeV$ 에너지의 전자선을 이용하였으며 선량측정은 평행평판형 전리상(Markus chamber, PTW 23343)을 조직등가 팬텀(Polystyrene)에 삽입하여 측정하였다. 전자산란선의 에너지분포는 Monte Carlo (EGS4) 계산으로 예측하였으며 조직내 선량분포는 필름 흑화도(X-Omat V, Wellhofer 700i)에 의하여 측정하였다. 결과 : 전자선 입사에너지가 6 MeV일 때 전자산란선의 평균 에너지는 약 1.5 MeV 이었으며 산란각이 클수록 에너지는 줄어들었다. 입사 전자선 에너지 6 MeV 에서 산란판의 각도 $30^{\circ},\;45^{\circ}$ 에 따른 최대선량지점은 산란선 방출구의 중심에서 각각 5 mm 및 -10 mm지점의 표면에서 발생되며 입사전자선에 대한 전자산란선의 선량비는 약 $8.5\%$ 내외로 측정되었다. 입사전자선에너지 6 MeV에서 산란판각도 $45^{\circ},\;60^{\circ}$에 의한 $50\%$의 심부선량분포는 각각 6 mm와 7 mm 깊이에 도달하였으며 입사에너지 증가에 비례하였다. 결론 : 전자선 후방산란의 특성을 연구하고 이를 인체 강내 측방 점막부위에 발생한 종양을 효과적으로 치료할 수 있는 강내 전자산란선 조사통을 고안 제작 하였다. 시험용으로 제작한 전자산란선 조사기구를 이용하여 전자선 에너지와 산란판의 각도에 따른 산란선의 선량비율과 심부율을 측정하였다. 구강, 자궁, 직장 등 강내측벽 점막 등에 발생된 악성종양의 모양과 깊이에 가장 적당한 입사 에너지, 산란판의 각도, 산란창구 및 조사각도를 선택함으로서 방사선치료방법을 향상시킬 수 있을 것이라고 기대된다.
Wall interactions of direct injection spray were investigated using laser-sheet imaging, shadowgraphy, wetted footprint and phase Doppler interferometry techniques. A narrow-cone high-pressure swirl injector is used to inject iso-octane fuel onto a plate, which has three different impact angles inside a pressurized chamber. Heated air and plate conditions were compared with unheated cases. Injection interval was also varied in the heated case to compare dry- and wet- wall impingement behaviors. High-speed macroscopic Mie-scattering images showed that presence of wall and air temperature has only minor effect on the bulk spray structure and penetration speed for the narrow-cone injector tested. The overall bulk motions of the spray plume and its spatial position at a given time are basically unaffected until a few millimeters before impacting the wall. The surface properties of the impact surface, such as the temperature, the presence of a preexisting liquid film also have a small effect on the amount of wetting or the wetted footprint; however, they have strong influence on what occurs just after impact or after a film is formed. The shadowgraph in particular shows that the plate temperature has a significant effect on vapor phase propagation. Generally, 10-20% faster horizontal vapor phase propagation is observed along the wall at elevated temperature condition. For impingement onto a preexisting film, more splash and evaporation were also observed. Contrary to some preconceptions, there is no significant splashing and droplet rebounding from surfaces that are interposed in the path of the DI gasoline spray, especially for the oblique impact angle cases. There also appears to be a dense spray front consists of large sac spray droplets in the oblique impact angle cases. The bulk of the spray is not impacted on the surface, but rather is deflected by it The microscopic details as depicted by phase Doppler measurements show that the outcome of the droplet impaction events can be significantly influenced. Only droplets at the spray front have high enough Weber numbers for wall impact to wet, splash or rebound. Using the sign of vertical velocity, the time-resolved downward droplets and upward droplets are compared. The Weber number of upward moving droplets, which seldom exceeds unity, also decreases as the impact angle decreases, as the droplets tend to impact less and move along the wall in the deflected spray plume.
본 연구는 노상토의 다짐특성 평가를 위해 특성이 다른 세 가지 강성측정 시험법으로 측정한 탄성계수의 상관관계 및 연관성에 대해 논의하였다. 미소변형률(${\approx}0.001%$) 범위의 흙강성측정기(SSG), 중변형률(${\approx}0.01{\sim}0.1%$) 범위의 정적 평판재하시험(PLT), 관입저항을 이용하는 동적콘관입시험기(DCP)가 탄성계수 측정에 이용되었다. 변형률 범위가 다른 시험방법에 의해 측정한 탄성계수를 실무에 적용하기 위해서는, 각각의 측정치에 대한 상관관계 및 연관성에 대해 사전에 파악되어야 한다. 국내 외 여러 조건의 노상토에 대해서 세 가지 방법을 이용하여 측정한 탄성계수($E_{SSG}$, $E_{PLT}$, $E_{DCP}$)를 비교 분석한 결과에 따르면, 흙의 종류 및 응력 조건에 따라 각 방법에 의해 측정된 탄성계수가 상이한 결과를 나타내었다. 전체 수집된 데이터 중 시멘트 처리토를 제외한 일반적인 노상토를 대상으로 한 상관성 분석결과, 정적 탄성계수($E_{PLT}$)는 동적 탄성계수($E_{SSG}$) 대비 60~80%의 크기를 나타나는 것으로 평가되었다. 시멘트 처리토와 같은 특이 토질은 정적 탄성계수($E_{PLT}$) 측정 시 구속압의 영향을 크게 받기 때문에, 다른 일반 토질과 상관관계 비교시 응력보정을 수행하여야 한다. 또한, 동적콘관입시험 결과를 이용하여 탄성계수($E_{DCP}$) 예측 시, 200MPa 이내의 범위에서 탄성계수 데이터가 좀더 신뢰도 높은 상관관계를 나타내었다.
본 연구에서는 헬리컬 파일의 관입시간과 극한하중에 관한 연구를 진행하고자 1/6 축소모형 실험을 진행하였다. 균질한 상대밀도의 사질토 지반을 형성하기 위하여 강사법을 사용하였다. 실험 조건으로 헬리컬 파일의 나선형 원판(heilx plate) 간격을 50mm와 150mm 두 Type으로 제작하였고, 헬리컬 파일의 회전관입 시 회전속도를 15rpm과 30rpm으로 진행하였다. 관입 완료된 헬리컬 파일에 콘 장비를 항타하여 관입하였다. 콘 장비 관입으로 헬리컬 파일의 극한하중 증가와 폐색의 정도를 확인 할 수 있었다. 위의 실험 결과를 토대로 헬리컬 파일의 관입시간은 "회전속도 30rpm-나선형 원판 간격 50mm"에서 단축 되었고, 극한하중은 "회전속도 30rpm-나선형 원판 간격 150mm-콘 장비 유"인 조건에서 높은 극한하중을 보였다.
이 논문은 콘크리트 콘 파괴에 의해 지배될 때의 인장력의 예측과 Headed bar의 인발 파괴 양상을 보여준다. 1개의 다른 플레이트 형상과 세가지의 서로 다른 용접 방법에 따라 시험이 이루어졌다. 시험의 변수는 Headed plate에 연결된 철근의 직경(16mm, 19mm, 22mm), 형상(원형, 직사각형, 정사각형)과 head plate의 차원(면적, 두께), 철근과 head plate와의 연결을 위한 용접 방법(일반용접, 마찰용접)이다. Headed bar는 ASTM 970-98에 기초한 모양과 두께를 가진 다른 단면적으로 제조되었으며 콘크리트의 부착 길이는 CSA 23.3-94에 의거하여 산정되었다. 정적 인장하중이 적용되었으며 시험 인발 성능은 ACI-349와 CCD 방법과 같은 현재의 설계방법에 의해 산출된 값과 비교하였다. 실험결과와 기존식을 비교하면 Headed bar가 앵커와 달리 넓은 플레이트 면적과 이형철근으로 인해 기준식에 비해 높은 강도와 큰 파괴 반경을 나타내었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.