PURPOSES : In this study, analyze the characteristics of IOC indicator 'threshold' which is needed when evaluating the traffic signal operation status with ESPRESSO in various grade road traffic environment of Seoul metropolitan city and derive suggested value to use in field practice. METHODS : Using the computerized database program (Postgresql), we extracted data with regional characteristics (Arterial, Collector road) and temporal characteristics (peak hour, non-peak hour). Analysis of variance and Duncan's validation were performed using statistical analysis program (SPSS) to confirm whether the extracted data contains statistical significance. RESULTS : The analysis period of the main and secondary arterial roads was confirmed to be suitable from 14 days to 60 days. For the arterial, it is suggested to use 20 km/h as the critical speed for PM peak hour and weekly non peak hour. It is suggested to use 25 km/h as the critical speed for AM peak hour and night non peak hour. As for the collector road, it is suggested to use 20 km/h as the critical speed for PM peak hour and weekly non peak hour. It is suggested to use 30 km/h as the critical speed for AM peak hour and night non peak hour. CONCLUSIONS : It is meaningful from a methodological point of view that it is possible to make a reasonable comparative analysis on the signal intersection pre-post analysis when the signal operation DB is renewed by breaking the existing traffic signal operation evaluation method.
본 연구는 아스팔트 혼합물의 주요 파손 형태인 피로균열과 러팅 저항성을 증가시키기 위한 섬유보강아스팔트 혼합물을 개발하기 위한 연구로서, 보강섬유를 고려한 골재 혼합물의 배합설계법에 대한 연구 결과를 나타내고 있다. 실험을 통하여 다졌을 때와 다지지 않았을 때의 단위중량 및 단위중량 비를 산정하였으며, 굵은 골재와 중간골재의 단위 중량비는 1.100, 1.119, 잔골재의 단위 중량비는 1.137로 굵은 골재나 중간 골재에 비하여 다소 큰 것으로 확인되었다. 부피 개념을 이용하여 특정 골재(4.75mm, #4)를 아령형 보강 섬유로 치환하는 방법을 베일리 방법을 사용하여 확인하였는데 1950g의 혼합물에 0.3%의 보강 섬유를 첨가하였을 때 섬유와 교체되어야 할 PCS골재의 무게는 11.88g으로 계산되었다. 따라서 본 연구에서는 골재와 보강섬유의 특성을 최대한 설계에 반영할 수 있는 골재의 배합설계 방법 개발을 통하여 기존의 수퍼페이브 배합설계법이 가지는 단점을 극복하고 자원 활용을 극대화 하고자 한다.
PURPOSES : The objective of this study is to evaluate the tack-coating material's properties using the bitumen bond strength(BBS) test and damping test as function of changed curing times. In this study, bonding strength tests were performed according to the curing time of tack coating materials. METHODS : In order to investigate bonding characteristic of tack coating materials, the Pneumatic Adhesion tensile Testing Instrument(PATTI) device is used to measure the bond strength between the tack coating materials and aggregate substrate based on the AASHTO TP-91. Also, damping test as in situ test was used to determine an appropriate traffic openting time for construction vehicle. Four different tack-coating materials were used in this study. The BBS tests were performed a one hour curing and testing temperatures of $5^{\circ}C$, $15^{\circ}C$, and $25^{\circ}C$. Damping test was conducted at 30min, 60min, 90min, and 120 min of curing times with temperatures of $20^{\circ}C$ and $30^{\circ}C$. RESULTS and CONCLUSIONS : The BBS test results show various bond strength as function of tack coat materials. At the same testing condition, A tack coat material shows almost two times higher than D tack coat materials although both materials are satisfied the criteria of material's physical properties. Also, Dampting test results shows similar trend with BBS test result. The damping test result was significantly changed as function of tack coat materials. Based on this study, the tack coating material's curing time is very important. Therefore, both curing time and the bond strength's characteristic has to be considered in standard specification.
PURPOSES : It is necessary to clarify the rheological properties of cement paste as a basic research in the development of mechanistic concrete mix design. The rheological properties of cement paste with different binder types, mix propositions, and with/without high range water reducers have been analyzed. METHODS : In this study, ordinary Portland cement, fly-ash, blast furnace slag, silica fume, and limestone powder were used as binders. The range of water-binder ratio was 0.3-0.5, and a total of 30 different mixes have been tested. The slump flow test, V-funnel test, and Dynamic Shear Rheometer (DSR) test were performed to analyze the rheological properties of cement paste. RESULTS : As a result of the slump flow test, it was found that the composition ratio of the binder contents greatly affected the paste flow when the high range water reducers were added. The results of V-funnel test showed that when the water-binder ratio was decreased without high range water reducers, the binder composition ratio had a large effect on the passing time of the V-funnel tester, but with high range water reducers the impact of the binder composition ratio was decreased. The slump flow and V-funnel have a certain relationship with the rheological factors (yield stress and plastic viscosity), but the correlation was not significant. Finally, we proposed the M-value considering the density and specific surface area of the binder. The correlation between rheological factors and M-value were better demonstrated than experimental values, but there is still a limit to predict the rheological factor in general mix design. CONCLUSIONS :In this study, the rheological properties of cement paste were analyzed. The binder type, composition ratio of binder, and with/without high range water reducers have combined to provide the complex effects on the rheological properties of cement paste. The correlation between the proposed M-value and rheological factor was found to be better than experimental results, but needs to be improved in the future.
PURPOSES : To ensure appropriate RCC properties with sufficient strength development and workability, it is necessary to secure a proper level of consistency. It is also necessary to secure maximum dry density, which is an important factor for increasing the interaction of aggregate interlocking, leading to an augmentation of RCC strength. On the other hand, the dry density of RCC can be changed owing to the compaction conditions, water content, and particle size distribution. A Proctor test and a modified Proctor test were used for determining the optimum water content needed to achieve maximum dry density with different amounts of compaction energy. A Vebe test, on the other hand, was used for checking the level of consistency, which is important for producing a workable mixture. METHODS : To confirm the degree of compaction at various particle sizes, RCC mixtures with different sand/aggregate ratios were evaluated. The Proctor test and modified Proctor test were applied to these mixtures to check the effect of the aggregate gradation and compaction energy on the maximum dry density and optimum water content. During each test, three specimens were produced for all types of water content under each aggregate gradation. A compaction curve and the optimum water content and maximum dry density for each aggregate gradation were then obtained for both tests. The range of water content for the appropriate consistency of each aggregate gradation was determined through a Vebe test. The optimum water content was then evaluated based on this range. RESULTS : The compaction test results show that the modified Proctor test provides a higher maximum dry density and lower optimum water content compared with the standard Proctor test. For the modified Proctor test, two cases of aggregate gradation (s/a = 30% and 70%) had the optimum water contents outside of the appropriate water content range. For the standard Proctor test, on the other hand, none of aggregate gradations provided the optimum water content within the desired range. CONCLUSIONS : The modified Proctor test should be used for an RCC mixture design because it can provide adequacy between maximum dry density and consistency. Moreover, the compaction roller has become highly developed for higher compaction energy.
PURPOSES : The impact performance of flexible barrier system such as structural response, vehicular motion and occupant safety vary depending on the impact point. Thus, to properly evaluate the performance of a flexible barrier system, impact should be made to a point which will lead to the worst possible results. This point is called the Critical Impact Point (CIP). This paper presents the way to determine the CIP for a SB2 class flexible barrier system which is consisted of Thrie-Beam rail and circular hollow tube post of 2m span. METHODS: Barrier VII simulations were made for impact points; Case 1 at a post, Case 2 at 1/3 span downstream from a post, Case 3 at middle of the span, Case 4 at 2/3 span downstream from a post. For the structural performance (deflections), impact simulation of 8000kg-65km/h-15degree was used, and for vehicle motion and occupant safety, simulation of 1300kg-80km/h-20degree impact was made and analysed. RESULTS: Case 1 gave the largest dynamic deflection of 75.72cm and also gave the largest snag value of 44.3cm. Occupant safety and exit angle of the vehicle after the impact were not sensitive to the impact point and were all below the allowable limit. CONCLUSIONS : For the SB2 class flexible barrier system's CIP can be regarded as a post which is sufficiently away from the end of Length of Need in order to avoid the end-effect of the barrier system. It can be more economic in the long run because the normal concrete pavement material is likely to cost more due to higher probability of maintenance and repair and higher social cost due to traffic accident, etc.
일반적으로 주차장은 아스팔트나 콘크리트 등 불투수층으로 조성되기 때문에 강우시 각종 오염물질이 수계로 배출됨에 따라 비점오염원 배출 부하량을 증가시키는 중요한 요인이 된다. 불투수층으로 인한 물순환장애 및 비점오염원 관리를 효과적으로 제어하고 관리할 수 있는 저영향개발(Low Impact Development)의 적용 및 필요성이 대두되고 있으며, 환경부는 개발사업에 대해 저영향개발 기법의 적용을 의무화하는 방안을 추진 중에 있다. 본 연구에서는 효율적인 빗물 및 비점오염원 관리를 위한 저영향개발 기법의 하나인 투수성 주차장에서 발생하는 강우 유출수의 오염물질 농도, 비점오염부하량, 초기세척현상 및 강우유출지연효과를 불투수성 주차장과 비교 분석하여 향후 투수성 주차장 설계시 기초자료로 활용할 수 있도록 하였다.
본 연구는 대입경 혼합물의 배합설계와 소성변형 및 균열특성에 관련된 역학적 특성에 관한 연구결과이다. 대입경 혼합물은 1989년 미국 아스팔트기술쎈타의 Kandhal에 의해서 연구되었으며, 일본 및 아랍의 여러 국가에서 포장건설에 사용하고 있다. 이들의 경험과 연구결과에 의하면 대입경 혼합물을 구성하고 있는 골재의 구성은 결합력이 견고하고 바인더가 고온에서 영향을 받지 않아 소성변형에 큰 저항성을 보이는 것으로 알려져 있으나, 실제로 증명할 수 있는 역학적인 시험을 수행한 자료는 없는 실정이다. 본 연구에서는 크리프시험, 회복탄성계수시험, 휠 트래킹시험 및 라벨링 시험을 실시하여 대입경 혼합물의 특성을 분석하였으며 시험 결과를 일반 혼합물 및 개질아스팔트 혼합물과 비교한 결과 대입경 혼합물의 소성변형에 대한 저항성은 매우 우수한 것으로 나타났다.
소입경 골재노출콘크리트포장은 콘크리트 포장 시공 시 포장표면에 적정 응결지연제를 분사한 후 표면 모르타르를 제거하여 굵은 골재를 노출시킴으로서 표면조직을 형성하는 공법으로써 기존 콘크리트 포장의 소음문제를 해결할 수 있는 저소음 공법이다. 소입경 골재노출 콘크리트 포장은 강도를 크게 개선할 뿐만 아니라 소음저감 효과 및 우수한 미끄럼 저항성을 확보하여 도로이용자의 안정성을 확보할 수 있는 공법이다. 현재 국외 도로 선진국의 경우 골재노출 포장의 상용화가 이루어진 상태이지만 국내의 경우는 실용화 초기단계이기 때문에 현장적용을 위해서는 국내 여건에 맞는 합리적인 관리 기준이 필요하다. 이를 위하여 소입경 골재노출 콘크리트 포장의 최적배합 및 노출기법 연구, 굵은 골재의 선정 및 입도 설계, 환경하중 저항성 평가 등 실내시험을 수행하였으며, 소입경 골재노출 콘크리트 포장의 시공을 위한 시공 장비를 제작하였다. 따라서 본 연구에서는 시험시공을 통해 도출된 결과와 기존 실내시험에서 도출된 결과를 비교 분석하였으며, 시험시공 분석을 통하여 골재 탈리 방지, 강도 및 내구성 확보를 위한 표준배합을 제시하였다. 환경 및 시공조건이 상이한 3차례 시험시공 구간을 선정하여 시공현장여건에 유동성으로 대처할 수 있는 시공 기술 및 시공 기준을 제시하였다. 또한 장 단기 공용성 평가를 통하여 도로 포장의 기능성 측면에서 우수한 소음저감 및 미끄럼 저항성을 확보할 수 있는 노면조직의 품질관리 기준을 제시하였다.
본 연구에서는 제철소에서 발생되는 전기로 산화슬래그로써 제철 슬래그 골재를 사용한 SMA 혼합물에 대한 역학적 특성을 평가하였다. 실험 변수는 일반골재와 제철 슬래그 골재 10mm 및 13mm이다. 슬래그 골재의 기본 물성과 품질(비중, 흡수율등)은 KS기준을 만족하였다. 아스팔트콘크리트 혼합물의 역학적 실험을 수행한 결과, 슬래그 골재 혼합물은 최적아스팔트 함량이 일반 골재 혼합물 대비 낮게 도출되었으나 다른 품질 기준은 모두 만족하였다. 제철 슬래그 골재 혼합물이 일반 골재 혼합물 대비 다소 높은 값으로 측정되었고, 모든 시편에서 동적안정도 시험은 2,000pass/mm 기준을 만족하였다. 또한, 제철 슬래그 골재 혼합물의 회복탄성계수는 일반 골재를 사용한 혼합물에 비해 개선된 값을 나타내었다. 이에, 하중 재하 이후 회복하는 속도가 향상되어 차량의 반복적 통행하중에 따른 공용성능 개선 효과가 있을 것으로 판단된다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.