하이브리드 코팅 시스템으로 제조된 초고경도 Cr-Si-C-N 나노복합 코팅막의 미세구조 및 기계적 특성 (Microstructure and Mechanical Properties of Superhard Cr-Si-C-N Coatings Prepared by a Hybrid Coating System)

  • 장철식;허수정;송풍근;김광호
    • 한국표면공학회지
    • /
    • 제38권3호
    • /
    • pp.100-105
    • /
    • 2005
  • Cr-Si-C-N coatings were deposited on steel substrate (SKD 11) by a hybrid system of arc ion plating (AIP) and sputtering techniques. From XRD, XPS, and HRTEM analyses, it was found that Cr-Si-C-N had a fine composite microstructure comprising nano-sized crystallites of Cr(C, N) well distributed in the amorphous phase of $Si_3N_4/SiC$ mixture. Microhardness of Cr(C, N) coatings and Cr-Si-N coatings were reported about $\~22 GPa$ and $\~35 GPa$, respectively. As the Si was incorporated into Cr(C, N) coatings, The Cr-Si-C-N coatings having a Si content of $9.2 at.\%$ showed the maximum hardness value. As increased beyond Si content of $9.2 at.\%$, the interaction between nanocrystallites and amorphous phase was gone, the hardness was reduced as dependent on amorphous phase of $Si_3N_4/SiC$. In addition, the average coefficient of Cr-Si-C-N coatings largely decreased compared with Cr(C, N) coatings.

탄화규소로 코팅된 탄소-탄소 복합재료의 단열 특성 (Characterizations on the Thermal Insulation of SiC Coated Carbon-Carbon Composites)

  • 서형일;임병주;신인철;배수빈;이형익;최균;이기성
    • Composites Research
    • /
    • 제33권3호
    • /
    • pp.101-107
    • /
    • 2020
  • 본 논문에서는 탄화규소로 코팅된 탄소-탄소복합재료의 단열 특성을 고찰하였다. 탄소-탄소 복합재료 상에 탄화규소를 화학증착법(CVD)법으로 코팅하였다. 먼저 탄화규소로 코팅한 복합재와 코팅되지 않은 복합재에 대해, 공기 중에서 1350℃의 온도를 급작스럽게 부가하였을 때의 단열특성을 서로 비교하는 연구를 수행하였다. 또한 본 연구에서는 최대 1700℃ 및 2000℃의 온도에 복합재의 표면을 노출시키는 고온 버너실험을 수행하였다. 버너실험 전, 후의 무게를 측정하여 무게변화를 고찰하였다. 고온 버너실험 후 탄소-탄소 복합재 및 탄화규소로 코팅된 복합재의 손상여부를 비교, 고찰하였다. 그 결과 2000℃의 온도에 노출 시 탄화규소 코팅재에서 박리, 균열, 공동 등의 결함손상들이 발견되었으나, 고온으로부터 탄소-탄소 복합재를 보호하는데 효과적이었다.

산화크롬/몰리브덴 복합 플라즈마 용사 코팅의 마찰, 마모 특성 연구 (A study on friction and wear properties of plasma-sprayed $Cr_2O_3/Mo$ composite coatings)

  • 여인웅;안효석
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제28회 추계학술대회
    • /
    • pp.17-24
    • /
    • 1998
  • Plasma-sprayed coatings were obtained by spray-dried $Cr_2O_3$ powder with and without Mo addition. A reciprocal type tribo-tester was employed to examine friction and wear behavior of the specimens at room temperature. The composition and the worn surface of coated specimens were observed by XRD and SEM. The results showed that friction Coefficient of the Mo added specimens were lower than one of $Cr_2O_3$ specimen. But $Cr_2O_3$ specimen had a lower wear loss. Protecting layer were observed at the worn surface of coated specimens with Mo addition.

  • PDF

알루미나 첨가가 플라즈마 용사된 세리아계 전해질체 코팅츠의 미세구조 및 기계적 특성에 미치는 영향 (The Effect of Alumina Addition on Microstructure and Mechanical Properties of Plasma-Sparayed Ceria Based Electrolyte Coatings)

  • 김장엽;유석원;임대순
    • 한국세라믹학회지
    • /
    • 제35권6호
    • /
    • pp.610-618
    • /
    • 1998
  • Alumina were added to ceria based ceramic powders upto 9.7 vol% and composite powders were sprayed by plasma spraying process in order to improve the mechanical properties such as hardness fracture tough-ness and thermal shock resistance. The ceria based coating sprayed without alumina has the typical colum-nar and lamellar structure. Alumina addition has lowered the amount of columnar and lamellar sturcture Added alumina was segreagated in the grain boundary and grain of ceria based crystal accompanied with pore. The maximum value of density and the minimum value of porosity were observed at the sprayed coating with 4.8 vol% alumina. The hardness fracture toughness and thermal shock resistance were increased with alumina addition. The improvement of mechanical properties of plasma sparyed ceria based coatings result-ed from the disapperance of the columnar and lamellar sturcture by addition of alumina.

  • PDF

A Study on the Factors for Improvement of Chemical and Physical Properties in Fluoric Rubber Coating for Use of the Extremely Acidic Environments

  • Chang, Hyun Young;Jin, Tae Eun;So, Il Soo;Lee, Byung Seung;Kang, Min Soo
    • Corrosion Science and Technology
    • /
    • 제7권5호
    • /
    • pp.269-273
    • /
    • 2008
  • It is known that the fluoric resin has the most outstanding properties in the extremely acidic environment of high temperature. However, this resin is the thermal hardening type that needs long time heat treatments above $250^{\circ}C$. It's impossible to use in situ in the extremely acidic environment such as a huge FGD ductworks or industrial chemical tanks. Furthermore, even the natural hardening type fluoric coatings which can be hardened less than $120^{\circ}C$ can not be applied to the highly acidic environmental plants because of its chemical resistance. In this study, new fluoric coatings that has excellent thermal resistance, chemical resistance and corrosion resistance has been developed in order to solve above problems and to be applied to the large plant structures in the field. These newly developed coatings are organic and inorganic composite type that have fluoric rubber(100 wt%), fluoric resin(5~50 wt%), oxalates(5~30 wt%), inorganic fillers mixed with plate-type and bulk-type solids(20~150 wt%), hardeners(0.5~5 wt%), and hardening hasteners(0.1~3 wt%). The best chemical and physical properties of these coatings are acquired by variation of adhesive reinforcement agents, dispersants, leveling agents. Mixing ratios of plate-type and bulk-type inorganic fillers influence the thermal properties, abrasive resistance and chemical infiltration properties of coatings. The mixing control is also very important to have homogeneous surface and removing inner voids of coatings.

슬림 AU 합성보의 내화해석 (Fire Performance Analysis of SLIM AU Composite Beam)

  • 김명한;오명호;민정기
    • 한국공간구조학회논문집
    • /
    • 제16권4호
    • /
    • pp.133-140
    • /
    • 2016
  • SLIM AU(A plus U-shaped) composite beam had been developed for not only reducing the story height in residential and commercial building, but also saving the cost of floor construction. The structural performance and economic feasibility was sufficiently approved by means of structural experiments and analytical studies. Even though fire resistance of the SLIM AU composite beam was evaluated throughout furnace fire test, the fire performance of the composite beam using finite element analysis is not analysed yet. Therefore the predictions of fire resistance simulations with loading as well as temperature distribution of the composite beam are summarized in this paper.

니켈 코팅된 다이아몬드/금속 복합재의 저온분사 코팅특성 (Characteristics of Ni-coated diamond/Metal Composite Coatings by Cold Spray Deposition)

  • 정동진;김형준;이기안
    • 대한금속재료학회지
    • /
    • 제47권9호
    • /
    • pp.550-557
    • /
    • 2009
  • In this study, bronze or SUS304 powders blended with 10 wt.% diamond particles were used to prepare metal/diamond composite materials deposited by cold spraying. The effects of matrix metal, diamond partical size, and the thickness of the Ni coating on the diamond were studied on Al 6061 substrate. The results showed that the hardness of the metal/diamond composite coating layers was higher than that of the same composite materials when using the sintering method. The fraction of diamond content in the coated layer increased when the metal matrix was soft. When the size of the diamond particles was reduced, the fraction of the diamond particles increased. In addition, in the case of diamond with a thicker Ni-coated layer, the fracturing of diamonds was mitigated in the composite coating layers.