• 제목/요약/키워드: Coiling Temperature

검색결과 30건 처리시간 0.028초

Strip Tail부 재질 편차 감소를 위한 권취 온도 미단 제어 정도 향상 (Coiling Temperature Control of Strip Tail for Minimizing the Deviation of Mechanical Properties in Mini-Mill Process)

  • 안종준;성영훈;백계주
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1999년도 제3회 압연심포지엄 논문집 압연기술의 미래개척 (Exploitation of Future Rolling Technologies)
    • /
    • pp.57-65
    • /
    • 1999
  • This document illustrates the way to control of coiling temperature(CTC) of stip tail part in minimill process. The coiling temperature (CT) is very important fact in hot rolling process because the mechnical properties of strip depend on it. In mini-mill pocess, the speed pattern of rolling is different from that of conventional hot rolling. We have a lot of difficulties in controlling the coiling temperature at strip tail part, because after the strip tail is passed out the final stand, it's impossible to control the coiling temperature by using coiling speed. So we have CT deveiation in this gauge, about 160$^{\circ}C$ below in comparison with target CT. It's clear that deviation of mechanical properties(tensile strength, vield ratio etc) of strip to direction of length is so large, so we could not produce middle carbon steel, like this temperature condition. New coiling temperature control of strip especially in strip tail was developed. An innovative method for calculate the deceleration speed of strip tail has been implemented in CTC program, so called

  • PDF

Effect of Coiling Temperature on the Annealed Texture in Cu/Nb Added Ultra Low Carbon Steels

  • Jiang, Yinghua;Park, Young-Koo;Lee, Oh-Yeon
    • 한국재료학회지
    • /
    • 제18권2호
    • /
    • pp.65-68
    • /
    • 2008
  • The present work was performed to investigate the effect of coiling temperature on the annealed texture in Cu/Nb-added ultra-low-carbon steels. The ultra-low-carbon steels were coiled at 650 and $720^{\circ}C$, respectively. The result showed that the Cu-added ultra-low-carbon steel at a low coiling temperature produced a desirable annealed texture related to good formability. On the other hand, Nb-added ultra-low-carbon steel at a high coiling temperature also produced a desirable texture. This is attributed to the effect of Nb, which retards recrystallization during the coiling process.

냉연 판재의 권취공정에 있어서 장력/열/변형 해석 (Tension/Heat/Thermal Deformation Analysis of a Cold Coiled Strip in Coiling Process)

  • 정영진;이규택;강충길
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.39-43
    • /
    • 2002
  • A new model for heat transfer and thermal deformation analysis according to strip mm in coiling process has been proposed. Finite difference analyses for heat transfer of cold rolled coil have been carried out under various coiling tensions and strip crown using the equivalent thermal conductivity for the radial direction of cold rolled coil which is a function of strip thickness, surface characteristics and compressive pressure. The compressive pressure is calculated from a equation expressed as a function of hoop stress and coil tension considering strip mm obtained by experiment. Finite element method for thermal deformation of cold rolled coil has been performed to investigate the effects of the strip crown, the coil tension and temperature. From these analyses, it is found that the axial inhomogeneity of thermal deformation is increased as the strip crown, compressive pressure, and temperature drop in cold coiled strip increase.

  • PDF

Ti-Nb-P 첨가 극저탄소 고강도 강판의 기계적 성질과 연성-취 천이거동 (Mechanical Property and Ductile-Brittle Transition Behavior of Ti-Nb-P Added Extra Low Carbon High Strength Steel Sheets)

  • 박종재;이오연;박영구;한상호;진광근
    • 한국재료학회지
    • /
    • 제14권12호
    • /
    • pp.863-869
    • /
    • 2004
  • The purpose of this research is to investigate the mechanical property and ductile-brittle transition temperature of Ti-Nb-P added extra low carbon interstitial free steel having a tensile strength of 440 MPa. The mechanical property and transition temperature of hot rolled steel sheets were more influenced by the coiling temperature rather than by the small amount of alloying element. Further, at the same composition, the property of the specimen coiled at low temperature was superior to that obtained at higher coiling temperature. The fracture surface of 0.005C-0.2Si-1.43Mn steel coiled at $630^{\circ}C$ showed a ductile fracture mode at $-100^{\circ}C$, but coiling at $670^{\circ}C$ showed a transgranular brittle fracture mode at $-90^{\circ}C$. The galvannealed 0.006C-0.07Si-1.33Mn steel sheet annealed at $810^{\circ}C$ has tensile strength and elongation of 442.8 MPa and $36.6\%$, respectively. The transition temperature of galvannealed 0.006C-0.07Si-1.33Mn steel sheet was increased with a drawing ratio, and the transition temperature of the galvannealed 0.006C-0.07Si-1.33Mn steel was $-60^{\circ}C$ at a drawing ratio of 1.8

극저탄소강의 고용 탄소 함량에 미치는 시멘타이트 석출 속도 모델링 (Modeling of Cementite Precipitation Kinetics on Solute Carbon Content in Extra and Ultra Low Carbon Steels)

  • 최종민;박봉준;김성일;이경섭;이경종
    • 대한금속재료학회지
    • /
    • 제48권3호
    • /
    • pp.187-193
    • /
    • 2010
  • The solute carbon content in ferrite is one of the important factors to obtain good formability in low carbon steels. Although most of the carbons are consumed by the formation of grain boundary cementite during coiling after hot-rolling, the carbon content after coiling is normally observed much more than that of equilibrium. In this study, a classical nucleation and growth model is used to simulate the precipitation kinetics of the grain boundary cementite from coiling temperature (CT) to room temperature (RT). The predicted precipitation behaviors depending on the initial carbon content and the cooling rate are compared with the reported. As a result, the lateral growth of thickening of cementite is a major factor for the sluggish reaction of grain boundary cementite. The reduction of solute carbon content after coiling is divided into three regions: a) increase due to no cementite precipitation, b) decrease due to the fast length-wise growth of cementite, c) increase due to the slow thickness-wise growth of cementite.

980 MPa급 열연강의 권취온도와 탄화물 거동에 따른 신장플랜지성 (Effects of Coiling Temperature and Carbides Behavior on Stretch-flangeability for 980MPa Hot-rolled Steels)

  • 천은준;이주승;도형협;김성주;최윤석;박용호;강남현
    • 대한금속재료학회지
    • /
    • 제50권7호
    • /
    • pp.487-493
    • /
    • 2012
  • To analyze the factors on stretch-flangeability for 980 MPa-grade hot-rolled steels, two types of steels (Fe-Cr and Fe-Mo) were manufactured by hot-rolling. Manufactured steels at the low coiling temperature, such as 400 and $500^{\circ}C$, had poor stretch-flangeability due to un-uniformly distributed carbides and a large deviation of interphase hardness. However, when the coiling temperature was set at $650^{\circ}C$ with Fe-Cr steel, 998 MPa of ultimate tensile strength, 19% of total elongation and 65% of the hole expanding ratio were achieved by microstructural constituents of polygonal ferrite (PF) and granular ferrite (GF) dispersed with fine carbides (<50 nm). Therefore, the material to attain 980 MPa with superior formability was the Fe-Cr steel that was precipitation-hardened in polygonal ferrite and granular ferrite at the coiling temperature $650^{\circ}C$.

열연 권취중 냉각이력 해석을 통한 재질예측 및 제어기술 개발 (The Prediction and Control of Plate Mechanical Properties By the Analysis of Temperature History on ROT in Hot Strip Mill)

  • 이중형;김홍준;김재부
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.111-113
    • /
    • 2007
  • The Mechanical properties of steel in hot strip mill were associated with the alloy composition, plastic deformation, cooling history and so on. In the case of the same alloy composition and deformation conditions, cooling history on ROT (run out table) is the main factor in affecting mechanical properties of steel, especially, in carbon steel. On ROT, the steel undergoes under various kinds of cooling conditions such as radiation, convection by air, water and wetting zone. The coiling temperature (CT) of the steel is also important factor in affecting mechanical properties. But with the same CT, the mechanical properties of steel can be different because the temperature history of cooling is more important factor than CT itself. In this study, we have studied the relations between temperature history and mechanical properties of steel and then the predicted mechanical properties have compared with the measured values.

  • PDF

열연 강판의 잔류 응력 해석 (Residual Stress Analysis of Hot Rolled Strip)

  • 구진모;김홍준;이재권;황상무
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2003년도 춘계학술대회논문집
    • /
    • pp.172-175
    • /
    • 2003
  • Run-Out-Table is the region between EDT and CT. Hot killed strip is cooled by air and water in ROT. In this procedure, phase transformation and shape deformation occur due to temperature drop. Because of un-ideal cooling condition, deformation of strip and non-uniform phase distribution come into existence. This phenomenon affects the strip property and lead th the existence of residual stress. And it exerts effects on the Coiling process, Coil Cooling process, and Un-coiling process. Through these process, the residual stresses of strip are more larger and unbalance of these stresses become more severe. Finite element (FE) based models for the analysises of non-steady state heat transfer and elastoplastic deformation are described in this investigation. The analysises of thermodynamics and phase transformation kinetics are suggested also. Using the ROT simulation result coiling process and coil cooling process simulations are carried out.

  • PDF

권취 공정 중 열연 강판의 잔류 응력 해석 (Residual Stress Analysis of Rot Rolled Strip in Coiling Process)

  • 구진모;김홍준;이재곤;황상무
    • 소성∙가공
    • /
    • 제12권4호
    • /
    • pp.302-307
    • /
    • 2003
  • Hot rolled strip is cooled by air and water in Run-Out-Table. In this process, phase transformation and shape deformation occurs due to temperature drop. Because of un-ideal cooling condition of ROT, irregular shape deformation and phase transformation arise in the strip. which affect the strip property and lead to the residual stress of strip. And these exert effects on the following processes, coiling process, coil cooling process, and re-coiling process. Through these processes, the residual stress becomes higher and severe. For the prediction of residual stress distribution and shape deformation of final product, Finite element(FE) based model was used. It consists of non-steady state heat transfer analysis, elasto-plastic analysis. thermodynamic analysis and phase transformation kinetics. Successive FEM simulation were applied from ROT process to coil cooling process. In each process simulation, previous process simulation results were used for the next process simulation. The simulation results were matched well with the experimental results.

Effects of reversing the coiling direction on the force-deflection characteristics of nickel-titanium closed-coil springs

  • Park, Hwan-Hyung;Jung, Suk-Hwan;Yoon, Juil;Jee, Kwang Koo;Han, Jun Hyun;Baek, Seung-Hak
    • 대한치과교정학회지
    • /
    • 제49권4호
    • /
    • pp.214-221
    • /
    • 2019
  • Objective: To investigate the effects of reversing the coiling direction of nickel-titanium closed-coil springs (NiTi-CCSs) on the force-deflection characteristics. Methods: The samples consisted of two commercially available conventional NiTi-CCS groups and two reverse-wound NiTi-CCS groups (Ormco-Conventional vs. Ormco-Reverse; GAC-Conventional vs. GAC-Reverse; n = 20 per group). The reverse-wound NiTi-CCSs were directly made from the corresponding conventional NiTi-CCSs by reversing the coiling direction. Tensile tests were performed for each group in a temperature-controlled acrylic chamber ($37{\pm}1^{\circ}C$). After measuring the force level, the range of the deactivation force plateau (DFP) and the amount of mechanical hysteresis (MH), statistical analyses were performed. Results: The Ormco-Reverse group exhibited a significant shift of the DFP end point toward the origin point (2.3 to 0.6 mm), an increase in the force level (1.2 to 1.3 N) and amount of MH (1.0 to 1.5 N) compared to the Ormco-Conventional group (all p < 0.001), which indicated that force could be constantly maintained until the end of the deactivation curve. In contrast, the GAC-Reverse group exhibited a significant shift of the DFP-end point away from the origin point (0.2 to 3.3 mm), a decrease in the force level (1.1 to 0.9 N) and amount of MH (0.6 to 0.4 N) compared to the GAC-Conventional group (all p < 0.001), which may hinder the maintenance of force until the end of the deactivation curve. Conclusions: The two commercially available NiTi-CCS groups exhibited different patterns of change in the force-deflection characteristics when the coiling direction was reversed.