• Title/Summary/Keyword: Coating tool

Search Result 198, Processing Time 0.023 seconds

Atomic Layer Deposition for Powder Coating (분말 코팅을 위한 원자층 증착법)

  • Choi, Seok;Han, Jeong Hwan;Choi, Byung Joon
    • Journal of Powder Materials
    • /
    • v.26 no.3
    • /
    • pp.243-250
    • /
    • 2019
  • Atomic layer deposition (ALD) is widely used as a tool for the formation of near-atomically flat and uniform thin films in the semiconductor and display industries because of its excellent uniformity. Nowadays, ALD is being extensively used in diverse fields, such as energy and biology. By controlling the reactivity of the surface, either homogeneous or inhomogeneous coating on the shell of nanostructured powder can be accomplished by the ALD process. However, the ALD process on the powder largely depends on the displacement of powder in the reactor. Therefore, the technology for the fluidization of the powder is very important to redistribute its position during the ALD process. Herein, an overview of the three types of ALD reactors to agitate or fluidize the powder to improve the conformality of coating is presented. The principle of fluidization its advantages, examples, and limitations are addressed.

Development and Analysis of Graphene Oxide Thin Film Coating (산화그래핀 박막 코팅기술 개발 및 특성평가)

  • Cheon, Yeong Ah;Nam, Jin-Su;Son, Kyung Soo;Im, Young Tae;Ahn, Won Kee;Chung, Bong Geun
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.39 no.5
    • /
    • pp.463-469
    • /
    • 2015
  • In this study, we synthesized graphene oxide and developed novel spin-spray coating technology. The graphene oxide thin film was uniformly coated on amine-functionalized glass surfaces using spin-spray coating technology. We also stacked up to four layers of graphene oxide on glass substrates in a uniform manner. From the results, we infer that this spin-spray coating of graphene oxide thin film could be a powerful tool for various electronic display coating applications.

The study on the influence of surface cleanness and water soluble salt on corrosion protection of epoxy resin coated carbon steel

  • Shon, MinYoung
    • Corrosion Science and Technology
    • /
    • v.13 no.5
    • /
    • pp.163-169
    • /
    • 2014
  • The corrosion resistance of epoxy-coated carbon steel was evaluated. The carbon steel surface was subjected to different treatment methods such as steel grit blasting and power tool treatment as well as contamination of water soluble salt. To study the effect of the surface treatments and contamination, the topology of the treated surface was observed by confocal microscopy and a pull-off adhesion test was conducted. The corrosion resistance of the epoxy-coated carbon steel was further examined by electrochemical impedance spectroscopy (EIS) combined with immersion test of 3.5 wt% of NaCl solution. Consequently, the surface contamination by sodium chloride with $16mg/m^2$, $48mg/m^2$ and $96mg/m^2$ didn't affect the adhesion strength for current epoxy coated carbon steel and blister and rust were not observed on the surface of epoxy coating contaminated by various concentration of sodium chloride after 20 weeks of immersion in 3.5 wt% NaCl aqueous solutions. In addition, the results of EIS test showed that the epoxy-coated carbon steel treated with steel grit blasting and power tool showed similar corrosion protection performance and surface cleanness such as Sa 3 and Sa 2.5 didn't affect the corrosion protectiveness of epoxy coated carbon steel.

Characterization of Product Surface according to Tool Surface Conditions when Forming TRIP1180 Steel Sheets with PVD CrN-coated Tools (PVD CrN 코팅 금형의 TRIP1180 판재 성형 시 금형의 표면상태에 따른 제품 표면특성 평가)

  • J. H. Bang;G. H. Bae;M. Kim;M. G. Lee;H. G. Kim;J. H. Song
    • Transactions of Materials Processing
    • /
    • v.32 no.5
    • /
    • pp.247-254
    • /
    • 2023
  • This study conducted the wear tests on bending punches coated with PVD CrN and examined the surface quality of the product formed by each punch in the forming of uncoated TRIP1180 sheets. The study quantitatively estimated the surface quality of the product by measuring the roughness and imaging the product surface. The correlation between the punch wear depth and the product surface roughness was quantitatively analyzed. The results showed that before failure occurs, the product roughness was comparable with that of the as-received, and the product surface was smooth without scratches and defects. However, after failure, the punch wear is caused by fretting wear mechanism, and a punch whose coating is not completely peeled plows the product surface, resulting in severe scratches with grooves and ridges on the product surface. Severe wear on the punch surface caused by fretting wear can rapidly degrade the product surface quality as it is directly affected by the punch surface condition, and the product surface quality accurately reflects the punch wear condition.

Statistical analysis and modelization of tool life and vibration in dry face milling of AISI 52100 STEEL in annealed and hardened conditions

  • Benghersallah, Mohieddine;Medjber, Ali;Zahaf, Mohamed Zakaria;Tibakh, Idriss;Amirat, Abdelaziz
    • Advances in materials Research
    • /
    • v.9 no.3
    • /
    • pp.189-202
    • /
    • 2020
  • The objective of the present work is to investigate the effect of cutting parameters (Vc, fz and ap) on tool life and the level of vibrations velocity in the machined part during face milling operation of hardened AISI 52100 steel. Dry-face milling has been achieved in the annealed (28 HRc) and quenched (55 HRc) conditions using multi-layer coating micro-grain carbide inserts. Statistical analysis based on the Response surface methodology (RSM) and ANOVA analysis have been conducted through a plan of experiments methodology using a reduced Taguchi table (L9) in order to obtain engineering models for tool life and vibration velocity in the workpiece for both heat treatment conditions. The results show that the cutting speed has a dominant influence on tool life for both soft and hard part. Cutting speed and feed per tooth is the most significant parameters for vibration levels. Comparing the experimental values with those predicted by the developed engineering models of tool life and levels of vibrations velocity, a good correlation has been obtained (between 97% and 99%) in annealed and hard conditions.

A Study on the Improvement of Performance of High Speed Cutting Tool using Magnetic Fluid Grinding Technique(A Performance Estimation of High Speed Cutting Tool) (자기연마기술을 이용한 고속절삭공구의 성능향상에 관한 연구 (고속절삭공구의 성능평가를 중심으로))

  • Cho J.R.;Yang S.C.;Jung Y.G.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.10a
    • /
    • pp.354-361
    • /
    • 2005
  • In high speed cutting process, due to the friction between the tool and workpiece, a temperature rise of contacting part is serious. It need to develop cutting tool for overcoming such a poor condition. So now, some studies, the optimization of tool shapes, the fine grains of tool material, multi-layer coating of tools are processing. If mirror finishing on the tool is processed, there is advantage of relation between chip and tool, because of less friction, and also tool's lift would be increased. As a result mirror like finishing is expected efficient enhancement of tool. Generally, it is too difficult to process by a general way for tools of complex shapes, it is required a new method to process such complex shape tools. The magnetic fluid polishing technique can polish the workpiece of complex shape, because the polishing method which polishes as compress the workpiece by the magnetism abrasives to arrange to the linear according to the line of magnetic force. In this paper, We polished the surface of the high speed cutting tool using the magnetic fluid polishing technique, to enhance the performance of the high speed cutting tool.

  • PDF

Effect of Retained Pre-construction Primer on the Corrosion Protection Properties of Epoxy Coatings

  • Lee, Chul-Hwan;Shin, Chil-Seok;Lee, Ho-Il;Chung, Mong-Kyu;Baek, Kwang-Ki
    • Corrosion Science and Technology
    • /
    • v.6 no.5
    • /
    • pp.219-226
    • /
    • 2007
  • Pre-construction primer (PCP), or shopprimer, have been applied to steel plates to control temporary corrosion during ship fabrication. For surface preparation at ship block stage, in common shipyard practices, welding beads, burnt and rusted areas shall be blasted or power tool cleaned and the contamination such as zinc salt shall be removed with blasting or power tool. Whereas, the sound film of PCP needs not to be removed or roughened as the paint having good compatibility with PCP is used for the first coat. In many cases, however, full blasting or sweep blasting on the sound PCP treated block assemblies was requested. There still has been argument about the legitimacy of this practice, thus, it is critical to evaluate the quality of the coating system applied on the sound PCP retained condition, comparing with the one applied on the full blasted or sweep blasted condition. In this study, two different epoxy systems for water ballast tank were applied on the surfaces with sound PCP condition, full blasted condition, and sweep blasted condition. Coating performances such as durability, anti-corrosion, cathodic disbondment resistance were evaluated. The test results clearly indicated that the sound film of PCP needed not to be removed or roughened as the paint having good compatibility with PCP based on inorganic zinc silicate.

Experimental investigation of friction in guide zone of tube hydroforming with material and lubricant (튜브 액압성형 공정의 가이드영역에서 소재 및 윤활에 따른 마찰 특성의 실험적 연구)

  • Yi, H.K.;Yim, H.S.;Lee, G.Y.;Lee, S.M.;Chung, C.S.;Moon, Y.H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2008.10a
    • /
    • pp.83-86
    • /
    • 2008
  • In this study, friction test was proposed to obtain coefficient of friction between tube and die in guide zone of tube hydroforming and friction coefficients were evaluated at different materials, viscosity of lubricants and internal pressures. For this study, STKM11A and SUS tubes were prepared. The tube was expanded by an internal pressure against the tool wall. By pushing the tube through the tool, a friction force at the contact surface between the tube and the tool occurs From the recorded axial feeding forces, the friction coefficients between tube and die at the guide zone in tubular hydroforming can be estimated. The effects of the various internal pressures, viscosity of lubricants, tube materials, tube size and die coating on the friction forces and friction coefficients are discussed.

  • PDF

A Study on the Coated Characteristics of Ceramic Tools (세라믹공구 재료의 피복특성에 관한 연구)

  • Lee, Myeong-Je;Im, Hong-Seop;Yu, Bong-Hwan
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.4 s.175
    • /
    • pp.900-906
    • /
    • 2000
  • Ceramic, PCD and CBN tools are available for the difficult-to-cut-materials such as hardened carbon tool steel, stainless steel, Inconel 718 and etc. Ceramic tools are likely to be chipped and abruptly broken before the appearance of normal wear in turning. Ceramic tools are suitable for continuous in turning, not for intermittent in milling. In this study, TiN/TiCN multi-layer coated ceramic tools were found to restrain the chipping, breaking and early fracture and to increase the critical cutting speed owing to TiN/TiCN multi-layer coating in Arc Ion Plating of PVD method.