• Title/Summary/Keyword: Coating mixture

Search Result 281, Processing Time 0.037 seconds

Mechanical evaluation of superhard Ti-Si-C-N coatings prepared by a hybrid coating system (하이브리드 코팅 시스템으로 제조된 초고경도 Ti-Si-C-N 코팅막의 기계적 특성 평가)

  • Kang S. H.;Kang M. C.;Kim K. H.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2005.10a
    • /
    • pp.178-181
    • /
    • 2005
  • Quaternary Ti-Si-C-N coatings were deposited on WC-Co substrates by a hybrid coating system of arc ion plating (AIP) and sputtering techniques using Ti and Si targets, in an $Ar/N_2/CH_4$ gaseous mixture. The crystallinity, bending status, and microstructure of the Ti-Si-C-N coatings were measured by X-ray diffractometer (XRD) and X-ray photoelectron spectroscope (XPS), The micro-hardness of Ti(C,N) and Ti-Si-N coatings were about 30 and 40 GPa, respectively. As the Si was incorporated into Ti(C,N) coatings, the Ti-Si-C-N coatings having Si content of $8.9\;at.\%$ showed the maximum hardness value of about 55 GPa. In this work, the microstructure and mechanical properties of Ti-Si-C-N coatings were systematically investigated.

  • PDF

Microenvironmental Optimizaton of Immobilized Invertase for Methyl- $\beta$ -D-Fructofuranoside Synthesis (Methyl- $\beta$ -D-Fructofuranoside 합성을 위한 고정화 전화당 효소의 미소환경 최적화)

  • 허주형;안형환
    • Journal of the Korea Safety Management & Science
    • /
    • v.1 no.1
    • /
    • pp.259-272
    • /
    • 1999
  • In order to enhance the selectivity, productivity and yield of methyl fructoside, which was synthesized by enzymatic glycosylation of sucrose and methanol solution, controlling of surface property of solid support using different immobilization procedures optimized microenvironment of immobilized invertase. Silanization and polyethylene imine coating methods were adopted to give a hydrophobic and hydrophilic environment of immobilized invertase. As a result, polyethyleneimine coating method gave higher loading of enzyme, effective activity, and relative activity than silanization method, because it brought on increasing the functional density of amino group and enhancing the conservation of activity by regulating of hydrophilicity. And then, hydrophilic environment was possible to restraint the assessing of methyl fructoside molecule, which was more hydrophobic than sucrose, fructose, and glucose molecule in the reaction mixture, into .the active site of immobilizedinvertase. Consequently, hydrophilic microenvironment of immobilized invertase by polyethyleneimine coating obtained higher yield and productivity with increasing conversion than silanized and native invertase. Thus, this procedure optimized the microenvironment of immobilized invertase suitable for the enzymatic synthesis of methyl fructoside.

  • PDF

A Study on the Tensile Performance according to Quantities Characteristics of Charcoal in Poly-Urethane Waterproofing Material (폴리우레탄 방수재의 숯 첨가량에 따른 인장성능 변화추이 연구)

  • Park, Jin-Sang;Kim, Dong-Bum;Park, Wan-Goo;Ha, Mi-Young;Kim, Byoung-Il;Oh, Sang-Keun
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.11a
    • /
    • pp.120-121
    • /
    • 2017
  • Polyurethane coating materials are widely used in waterproofing construction because they ensure easy workability and high performance mechanical properties, and such polyurethane coating materials are in various mixture ratios. This study carried out a test to determine the basic physical property changes of polyurethane coating material based on the amount of charcoal additives to. The results showed that he tensile strength was found to be 3.1 N / ㎟ when the charcoal amount was at 2%, displaying the highest performance rate.

  • PDF

Dry Coated Particle for Plasma Spraying

  • Briones-Rodriguez, C.;Mayagoitia-Barragan, V.;Cuenca-Alvarez, R
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.156-157
    • /
    • 2006
  • The preparation of composite powders for plasma spraying by an in-house designed mechanofusion process is investigated. Results show that dry particle coating depends on the chemical and mechanical properties of powders. In metal/oxide and metal/oxide/carbide powder mixtures, fine ceramic particles coat the surface of the metallic coarser particles. A nearly rounded shape of the final composite particles is induced by the mechanical energy input with no formation of new phases. However with the carbide/metal powdered system, only an intimate mixture of components is achieved. It is suggested that the coating mechanism is governed by agglomeration and rolling phenomena.

  • PDF

Study on the Tic Coating of Steel by C.V.D. Process (CVD법에 의한 강의 TiC 피복에 관하여)

  • 강국해;최진일;영동영
    • Journal of the Korean institute of surface engineering
    • /
    • v.15 no.4
    • /
    • pp.208-217
    • /
    • 1982
  • To study the effect of TiC coating on weight change, microhardness, wear and heat - resistance of TiC layer, chemical vapour deposition on the various substrates has been carried out with the gaseous mixture of TiCl4, toluene, and H2 in the temperature range of 900 - 1000$^{\circ}C$. The results obtained are as follows ; (1) There is a limited value of carrier and reductant H2 gas flow rate, above which deteriorate effect on the TiC depoition arises (2) Increased thickness of TiC layer was resulted with increasing temperature and time. Better deposition was obtained with stainless steels and the best results were introduced by cobalt coating of substrates. (3) Wear resistance of the TiC coated specimen improved markedly. Heat resistivity of the coated steel showed excellent result, whereas the coated stainless Steels were infer-ior to the substrate.

  • PDF

Effects of Stoichiometry on Properties of NiAl Intermetallics coated on Carbon Steel through Combustion Synthesis (연소합성 코팅된 NiAl 금속간화합물의 화학양론이 미끄럼 마모특성에 미치는 영향)

  • Lee, Han-Young;Lee, Jae-Sung
    • Tribology and Lubricants
    • /
    • v.36 no.3
    • /
    • pp.124-132
    • /
    • 2020
  • The effect of the stoichiometry on the sliding wear properties of NiAl coatings has been investigated. Three different powder mixtures with the compositions of Ni-50at%Al, Ni-54at%Al and Ni-42at%Al were diepressed respectively, and which were subsequently coated on mild steel through combustion synthesis in an induction heating system. Sliding wear behavior of the coatings was examined against an alloyed tool steel using a pin-on-disc type sliding wear test machine. As results, it could be seen that powder mixture(Ni-54at%Al) with displaying Al-rich deviations from the stoichiometry of NiAl(Ni-50at%Al) was promoted the most the synthetic reactivity. The microstructure of the coating layer with the compositions of Ni-54at%Al exhibits the porous NiAl single phase structure. However, the microstructure of the coating layer of the compositions of Ni-42at%Al exhibits the denser multi-phase structure containing several intermediate phases in addition to NiAl. Densification of the coating layer was enhanced by increasing the reacting temperature. On the other hand, the wear properties of the coating layers showed that the wear mode at speeds of around 1 m/s was severe wear, regardless of the stoichiometry and reacting temperature. However, wear properties of coating layer with the compositions of Ni-42at%Al were superior to those of coating layer with the compositions of Ni-54at%Al. This would be attributed by the fact that coating layer with the compositions of Ni-42at%Al develops little void and much intermediate phases with high strength.

Study on the Adhesive Strength by the Manufacturing Process Parameter of the Aluminum Pouch for Secondary Battery (이차전지용 알루미늄 파우치 필름의 제조 공정 변수에 따른 접착력에 대한 연구)

  • Yu, Min Sook;Kim, Do Hyun;Cho, Jung Min;Bae, Sung Woo;Kim, Dong Soo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.33 no.2
    • /
    • pp.149-155
    • /
    • 2016
  • In this study, we investigated the adhesive strength by molecular weight, mixture ratio, coating thickness, lamination temperature and aging condition of adhesive in manufacture process of Nylon-Aluminum for secondary aluminum pouch. It found that as the molecular weight of adhesive gets lower, the adhesive strength increases. In the mixture ratio, as the content of hardener get higher and as the content of solvent get lower, the adhesive strength increases. Also, as the coating thickness of adhesive get thicker, the adhesive strength increase. In addition, the adhesive strength is higher at 90 degrees of lamination temperature. So, it found that 90 degrees of lamination temperature is appropriate. In the aging condition when aged for 5 days, it found that the reaction and curing of adhesive is sufficient by measuring the adhesive strength.

Characteristics of Diamond Films Deposited on Cemented Tungsten Carbide Substrate (초경합금기판 위에 성장되는 다이아몬드 막의 특성)

  • 김봉준;박상현;박재윤
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.53 no.7
    • /
    • pp.387-394
    • /
    • 2004
  • Diamond films were deposited on the cemented tungsten carbide WC-Co cutting insert substrates by using both microwave plasma chemical vapor deposition(MWPCVD) and radio frequency plasma chemical vapor deposition (RFPCVD) from $CH_4$$-H_2$$-O_2$ gas mixture. Scanning electron microscopy and X-ray diffraction techniques were used to investigate the microstructure and phase analysis of the materials and Raman spectrometry was used to characterize the quality of the diamond coating. Diamond films deposited using MWPCVD from $CH_4$$-H_2$$-O_2$ gas mixture show a dense, uniform, well faceted and polycrystalline morphology. The compressive stress in the diamond film was estimated to be (1.0∼3.6)$\pm$0.9 GPa. Diamond films which were deposited on the WC-Co cutting insert substrates by RFPCVD from $CH_4$$-H_2$$-O_2$ gas mixture show relatively good adhesion, very uniform, dense and polycrystalline morphology.

Preparation of Hard Coating Solutions by Sol-Gel Reaction of Glycidoxypropyl Trimethoxysilane and Methacryloxypropyl Trimethoxysilane (Glycidoxypropyl Trimethoxysilane과 Methacryloxypropyl Trimethoxysilane의 Sol-Gel 반응을 이용한 하드코팅 용액의 제조)

  • Oh, Seung Kyun;Chung, Jae Shik;Lee, Bum Suk;Song, Ki Chang
    • Korean Chemical Engineering Research
    • /
    • v.46 no.2
    • /
    • pp.274-278
    • /
    • 2008
  • Hard coating solutions were prepared from glycidoxypropyl trimethoxysilane (GPTMS) and methacryloxypropyl trimethoxysilane (MPTMS) precursors with different molar ratios of 10:0, 9:1, 7:3, 5:5, 3:7, and 0:10, respectively, by the sol-gel method. The polycarbonate (PC) sheets were spin-coated, and cured at $130^{\circ}C$ for 3 h. The effect of the GPTMS:MPTMS molar ratios of the mixture was investigated on the properties of coating films. The highest pencil hardness and adhesion to PC sheets of coating films were found for solution with GPTMS:MPTMS molar ratio of 5:5. Also, the pencil hardness of coating films was increased with increasing the $H_2O$ content in the coating solutions.

Preparation of Conductive Coating Solutions by Blending Waterborne Acrylic Polyurethane Dispersion with Carbon Nanotube (수분산 아크릴 폴리우레탄과 탄소나노튜브의 혼합에 의한 전도성 코팅용액 제조)

  • Huh, Woo Young;Yun, Dong Gu;Song, Ki Chang
    • Korean Chemical Engineering Research
    • /
    • v.51 no.1
    • /
    • pp.73-79
    • /
    • 2013
  • Waterborne polyurethane dispersion (WPUD) was synthesized from polycarbonate diol (PCD), isophorone diisocyanate (IPDI) and dimethylol propionic acid (DMPA) as starting materials. Then, waterborne acrylic polyurethane dispersion (AUD) was synthesized by reacting the WPUD with an acrylate monomer, methyl methacrylate (MMA). Subsequently, the AUD was mixed with multi-walled carbon nanotube (MWCNT) to yield a conductive coating solution, and the mixture was coated on the polycarbonate substrate. With increasing the amount of MMA in the AUD, the pencil hardness, abrasion resistance and chemical resistance of the coating films were improved, but the electrical conductivity of the coating films was decreased. On the other hand, the pencil hardness, abrasion resistance and chemical resistance of coating films were decreased, but the electrical conductivity was enhanced with increasing the amount of MWCNT in the conductive coating solutions.