• Title/Summary/Keyword: Clad

Search Result 408, Processing Time 0.029 seconds

Process Conditions for Low Bonding Strength in Pressure Welding of Cu-Al Plates at Cold and Warm Temperatures (Cu-Al 판재의 냉간 및 온간 압접에서 낮은 접합강도를 갖는 공정 조건에 관한 연구)

  • 심경섭;이용신
    • Transactions of Materials Processing
    • /
    • v.13 no.7
    • /
    • pp.623-628
    • /
    • 2004
  • This paper is concerned with pressure welding, which has been known as a main bonding mechanism during the cold and warm forming such as clad extrusion or bundle extrusion/drawing. Bonding characteristics between the Cu and Al plates by pressure welding are investigated focusing on the weak bonding. Experiments are performed at the cold and warm temperatures ranging from the room temperature to $200^{\circ}C$. The important factors examined in this work are the welding pressure, pressure holding time, surface roughness, and temperature. A bonding map, which can identify the bonding criterion with a weak bonding strength of IMPa , is proposed in terms of welding pressure and surface roughness fur the cold and warm temperature ranges.

Three-Dimensional Finite Element Modeling of Laser Cladding Process (레이저 클래딩 공정의 3차원 유한요소 모델링)

  • Zhao Guiping;Si Ho-Mun;Lee Heungshik;Cho Chongdu
    • Journal of Surface Science and Engineering
    • /
    • v.37 no.5
    • /
    • pp.279-288
    • /
    • 2004
  • This paper describes a three-dimensional transient finite element model for a laser cladding process. In the model, an adaptive finite element technique is used for dilution control. Using the proposed finite element model, the effects of process parameters such as scanning speed, laser's power, and preheating on the dilution of clad layer, the shape of melting pool, and the temperature distribution are calculated. It is also shown that the optimal process parameters for the required dilution can be determined from the proposed finite element model. An experiment is performed to validate the proposed model. The numerical results are compared with experimental ones.

Microstrip Line Fed Rectangular Microstrip Patch Antenna and its Array (마이크로스트립 전송선으로 급전되는 사각형 마이크로스트립 패치 안테나 및 배열 안테나에 관한 해석 및 실험)

  • 박동국
    • Proceedings of the Optical Society of Korea Conference
    • /
    • 1989.02a
    • /
    • pp.152-156
    • /
    • 1989
  • Parameters of a microstrip patch antenna such as the resonant frequency, radiation conductance, and the bandwidth are calculated. The rectangular microstrip patch antenna fed by a microstrip transmission line is fabricated and its resonant frequency, radiation pattern, and input voltage standing wave ratio are measured. The measured resonant frequency for 13.0mm$\times$9.7mm copper clad woven PTFE/glass laminate plate is 9.06Ghz, where the calculative is 9.00Ghz. And the measured vswr shows that the bandwidth of the antenna is 225MHz for vswr less then 2.0 which the calculated quality factor of the patch gives the bandwidth OF 280ghZ. The measured radiation pattern for 5 element as well as 4 element patch array shows less then 4dB deviation in the first side lobes from the designed values for both E and H plane pattern. This diviation is believed to be the power division errors of the power divider.

  • PDF

Reactivity feedback effect on loss of flow accident in PWR

  • Foad, Basma;Abdel-Latif, Salwa H.;Takeda, Toshikazu
    • Nuclear Engineering and Technology
    • /
    • v.50 no.8
    • /
    • pp.1277-1288
    • /
    • 2018
  • In this work, the reactor kinetics capability is used to compute the design safety parameters in a PWR due to complete loss of coolant flow during protected and unprotected accidents. A thermal-hydraulic code coupled with a point reactor kinetic model are used for these calculations; where kinetics parameters have been developed from the neutronic SRAC code to provide inputs to RELAP5-3D code to calculate parameters related to safety and guarantee that they meet the regulatory requirements. In RELAP5-3D the reactivity feedback is computed by both separable and tabular models. The results show the importance of the reactivity feedback on calculating the power which is the key parameter that controls the clad and fuel temperatures to maintain them below their melting point and therefore prevent core melt. In addition, extending modeling capability from separable to tabular model has nonremarkable influence on calculated safety parameters.

Research of Diffusion Bonding of Tungsten/Copper and Their Properties under High Heat Flux

  • Li, Jun;Yang, Jianfeng
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2011.05a
    • /
    • pp.14-14
    • /
    • 2011
  • W (tungsten)-alloys will be the most promising plasma facing armor materials in highly loaded plasma interactive components of the next step fusion reactors due to its high melting point, high sputtering resistance and low deuterium/tritium retention. The bonding technology of tungsten to Cu alloy was one of the key issues. In this paper, W/CuCrZr diffusion bonding has been performed successfully by inserting pure metal interlay. The joint microstructure, interfacial elements migration and phase composition were analyzed by SEM, EDS, XRD, and the joint shear strength and micro-hardness were investigated. The mock-ups were fabricated successfully with diffusion bonding and the cladding technology respectively, and the high heat flux test and thermal fatigue test were carried out under actively cooling condition. When Ni foil was used for the bonding of tungsten to CuCrZr, two reaction layers, Ni4W and Ni(W) layer, appeared between the tungsten and Ni interlayer with the optimized condition. Even though Ni4W is hard and brittle, and the strength of the joint was oppositely increased (217 MPa) due primarily to extremely small thicknesses (2~3 ${\mu}m$). When Ti foil was selected as the interlayer, the Ti foil diffused quickly with Cu and was transformed into liquid phase at $1,000^{\circ}C$. Almost all of the liquid was extruded out of the interface zone under bonding pressure, and an extremely thin residual layer (1~2 ${\mu}m$) of the liquid phase was retained between the tungsten and CuCrZr, which shear strength exceeded 160 MPa. When Ni/Ti/Ni multiple interlayers were used for bonding of tungsten to CuCrZr, a large number of intermetallic compound ($Ni_4W/NiTi_2/NiTi/Ni_3T$) were formed for the interdiffusion among W, Ni and Ti. Therefore, the shear strength of the joint was low and just about 85 MPa. The residual stresses in the clad samples with flat, arc, rectangle and trapezoid interface were estimated by Finite Element Analysis. The simulation results show that the flat clad sample was subjected maximum residual stress at the edge of the interface, which could be cracked at the edge and propagated along the interface. As for the rectangle and trapezoid interface, the residual stresses of the interface were lower than that of the flat interface, and the interface of the arc clad sample have lowest residual stress and all of the residual stress with arc interface were divided into different grooved zones, so the probabilities of cracking and propagation were lower than other interfaces. The residual stresses of the mock-ups under high heat flux of 10 $MW/m^2$ were estimated by Finite Element Analysis. The tungsten of the flat interfaces was subjected to tensile stresses (positive $S_x$), and the CuCrZr was subjected to compressive stresses (negative $S_x$). If the interface have a little microcrack, the tungsten of joint was more liable to propagate than the CuCrZr due to the brittle of the tungsten. However, when the flat interface was substituted by arc interfaces, the periodical residual stresses in the joining region were either released or formed a stress field prohibiting the growth or nucleation of the interfacial cracks. Thermal fatigue tests were performed on the mock-ups of flat and arc interface under the heat flux of 10 $MW/m^2$ with the cooling water velocity of 10 m/s. After thermal cycle experiments, a large number of microcracks appeared at the tungsten substrate due to large radial tensile stress on the flat mock-up. The defects would largely affect the heat transfer capability and the structure reliability of the mock-up. As for the arc mock-up, even though some microcracks were found at the interface of the regions, all microcracks with arc interface were divided into different arc-grooved zones, so the propagation of microcracks is difficult.

  • PDF

Fabrication and Evaluation of a VHF Focusing Ultrasonic Transducer Made of PVDF Piezoelectric Film (PVDF 압전막을 이용한 초고주파 집속 초음파 트랜스듀서의 제작 및 특성 평가)

  • Yoon, Ju-Ho;Oh, Jung-Hwan;Kim, Jung-Soon;Kim, Moo-Joon;Ha, Kang-Lyeol
    • The Journal of the Acoustical Society of Korea
    • /
    • v.30 no.4
    • /
    • pp.215-222
    • /
    • 2011
  • In order to obtain high resolution images, a focusing ultrasonic transducer operated in very high frequency (VHF) range was fabricated and its characteristics were evaluated. A 9-${\mu}m$ thick PVDF film with only one metalized surface for electric ground was adhered to a CCP (Copper-clad polyimide) film by using epoxy. It was pressed by a metal ball to form a concave surface and its rear side was filled with the epoxy. The radius of curvature and the f-number of the fabricated transducer are 7.5 mm and 1.7, respectively. The pulse-echo measurement results from a target located at the focal point showed that the frequency bandwidth was 35.0 MHz and the insertion loss near the peak frequency of approximately 40 MHz was about 60 dB. Those values agreed well with the simulation results by the KLM equivalent circuit analysis including the effect of the epoxy bonding layer. When the image of thin copper lines by the 35 MHz transducer of the UBM (Ultrasonic Backscattering Microscope) system was compared with the image by the transducer fabricated in this study, the fabricated transducer was observed that the axial resolution was improved although the lateral resolution was degraded.

Effect of Diamine Composition on Thermo-Mechanical Properties and Moisture Absorption of Polyimide Films (디아민 변화에 따른 폴리이미드 필름의 물리적 특성과 흡습률 분석)

  • Park, Yun-Jun;Yu, Duk-Man;Choi, Jong-Ho;Ahn, Jeong-Ho;Hong, Young-Taik
    • Polymer(Korea)
    • /
    • v.36 no.3
    • /
    • pp.275-280
    • /
    • 2012
  • Poly(amic acid)s were successfully synthesized from 1,4-bis(4-aminophenoxy)benzene (1,4-APB) or 2,2-bis[4-(4-aminophenoxy)phenyl]hexafluoropropane (HFBAPP) with pyromellitic dianhydride (PMDA), 3,3'-4,4'-benzopenonetetracarboxylic dianhydride (BPDA) and $p$-phenylenediamine ($p$-PDA) and then they were effectively converted into polyimide films by thermal imidization. The chemical structure and thermo-mechanical properties of polyimide films were examined using Fourier transform infrared spectroscopy (FTIR), thermo-gravimetric analyzer (TGA), thermo-mechanical analyzer, dynamic mechanical analyzer (DMA) and universal tensile machine (UTM). The moisture absorption, thermal and mechanical properties of polyimide films decreased with increasing the amount of 1,4-APB and HFBAPP. The polyimide films using HFBAPP showed lower properties than that of 1,4-APB at the same ratio, but it displayed better thermal properties and lower moisture absorption at the similar coefficient of thermal expansion (CTE) with a copper. On the basis of our finding, it is concluded that 4-component polyimide films could be utilized for base films for flexible copper clad laminates (FCCL) of flexible printed circuit boards.

Flexible Durability of Ultra-Thin FPCB (초박형 FPCB의 유연 내구성 연구)

  • Jung, Hoon-Sun;Eun, Kyoungtae;Lee, Eun-Kyung;Jung, Ki-Young;Choi, Sung-Hoon;Choa, Sung-Hoon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.21 no.4
    • /
    • pp.69-76
    • /
    • 2014
  • In this study, we developed an ultra-thin flexible printed circuit board(FPCB) using the sputtered flexible copper clad laminate. In order to enhance the adhesion between copper and polyimide substrate, a NiMoNb addition layer was applied. The mechanical durability and flexibility of the ultra-thin FPCB were characterized by stretching, twisting, bending fatigue test, and peel test. The stretching test reveals that the ultra-thin FPCB can be stretched up to 7% without failure. The twisting test shows that the ultra-thin FPCB can withstand an angle of up to $120^{\circ}$. In addition, the bending fatigue test shows that the FPCB can withstand 10,000 bending cycles. Numerical analysis of the stress and strain during stretching indicates the strain and the maximum von Mises stress of the ultra-thin FPCB are comparable to those of the conventional FPCB. Even though the ultra-thin FPCB shows slightly lower durability than the conventional FPCB, the ultra-thin FPCB has enough durability and robustness to apply in industry.

The Effects of Levelers on Electroplating of Thin Copper Foil for FCCL (전기도금법을 이용한 FCCL용 구리박막 제조시 레벨러의 영향 연구)

  • Kang, In-Seok;Koo, Yeon-Soo;Lee, Jae-Ho
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.19 no.2
    • /
    • pp.67-72
    • /
    • 2012
  • In recent days, the wire width of IC is narrowed and the degree of integration of IC is increased to obtain the higher capacity of the devices in electronic industry. And then the surface quality of FCCL(Flexible Copper Clad Laminate) became increasingly important. Surface defects on FCCL are bump, scratch, dent and so on. In particular, bumps cause low reliability of the products. Even though there are bumps on the surface, if leveling characteristic of plating solution is good, it does not develop significant bump. In this study, the leveling characteristics of additives are investigated. The objective of study is to improve the leveling characteristic and reduce the surface step through additives and plating conditions. The additives in the electrodeposition bath are critical to obtain flat surface and free of defects. In order to form flat copper surface, accelerator, suppressor and leveler are added to the stock solution. The reason for the addition of leveler is planarization surface and inhibition of the formation of micro-bump. Levelers (SO(Safranin O), MV(Methylene Violet), AB(Alcian Blue), JGB(Janus Green B), DB(Diazine Black) and PVP(Polyvinyl Pyrrolidone) are used in copper plating solution to enhance the morphology of electroplated copper. In this study, the nucleation and growth behavior of copper with variation of additives are studied. The leveling characteristics are analyzed on artificially fabricated Ni bumps.

Synthesis and Characterization of 4-Component Polyimide Films with Various Diamine and Dianhydride Compositions (다양한 조성 변화에 따른 4성분계 폴리이미드 필름 제조와 물성분석)

  • Park, Yun Jun;Yu, Duk Man;Choi, Jong Ho;Ahn, Jeong-Ho;Hong, Young Taik
    • Applied Chemistry for Engineering
    • /
    • v.22 no.6
    • /
    • pp.623-626
    • /
    • 2011
  • Various poly(amic acid)s were synthesized from PMDA/BPDA/p-PDA/ODA with different mole ratios and effectively converted into 4-component polyimide films by thermal imidization. The chemical structures and thermo-mechanical properties of polyimide films were examined using Fourier transform infrared spectroscopy (FT-IR), thermo-gravimetric analyzer (TGA), thermo-mechanical analyzer (TMA), dynamic mechanical analyzer (DMA) and universal tensile machine (UTM). The tensile strength, modulus, and thermal properties of polyimides films increased with the amount of rigid PMDA and p-PDA, while the elongation and moisture absorption of polyimide films increased with the amount of flexible BPDA and ODA. One of 4-component polyimide films exhibited a similar coefficient of thermal expansion (CTE) value to that of copper when it was composed of PMDA : BPDA : p-PDA : ODA with the ratio of 5 : 5 : 4 : 6. Thus, this polyimide film could be useful for a base film for flexible copper clad laminates (FCCL) of flexible printed circuit boards.