• Title/Summary/Keyword: Ceramic-glass

Search Result 1,315, Processing Time 0.028 seconds

Research on the Oxidation-Protective Coatings for Carbon/Carbon Composites

  • Li, He-Jun;Fu, Qian-Gang;Huang, Jian-Feng;Zeng, Xie-Rong;Li, Ke-Zhi
    • Carbon letters
    • /
    • v.6 no.2
    • /
    • pp.71-78
    • /
    • 2005
  • Anti-oxidation coatings are the key technique for carbon/carbon (C/C) composites used as the thermal structural materials. The microstructure and oxidation behavior of several kinds of high-performance ceramic coatings for C/C composites prepared in Northwestern Polytechnical University were introduced in this paper. It showed that the ceramic coatings such as SiC, Si-$MoSi_2$, SiC-$MoSi_2$, $Al_2O_3$-mullite-SiC and SiC/yttrium silicate/glass coatings possessed excellent oxidation resistance at high temperatures, and some of these coatings were characterized with excellent thermal shock resistance. The SiC-$MoSi_2$ coating system has the best oxidation protective property, which can effectively protect C/C composites from oxidation up to 1973 K. In addition, the protection and failure reasons of some coatings at high temperature were also provided.

  • PDF

Hydrophilic/Hydrophobic Conversion of $TiO_2$ Films by Reactive Magnetron Sputtering (Reactive Magnetron Sputtering법으로 제조된 $TiO_2$의 친수성/소수성 변환 특성)

  • 이영철;박용환;안재환;고경현
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.11
    • /
    • pp.1211-1216
    • /
    • 1999
  • TiO2 thin films were prepared by reactive magnetron sputtering on glass substrate and subjected into investigation about their hydrophilic properties. Varing Ar/O2 ration and post annealing at 50$0^{\circ}C$ for 12h anatase and rutile phases of TiO2 films were obtained. Hydrophilic properties were evaluated by determination of contact angle of water droplet on TiO2 surface. On as-annealed TiO2 films water droplet spreaded widely with ~0$^{\circ}$contact angle. Sonication(60 Hz, 28kHz 40kHz) and following dark room treatments turned these hydrophilic TiO2 films into hydrophobic state. All of hydrophobic films were converted recersibly into their original state after UV illumination. Hydrophobic states of anatase films were saturated after sonication and remain same during dark room treatment. But it was found that the conversion into hydrophobic state of rutile films progressed. further after sonication. Therefore it was concluded that Ti3+/Ti+4 ratio is the key to determine hydrophilicity of TiO2 surface so that different surface structure of polymorphs could lead to unique characteristics.

  • PDF

Phase Separation in $Nd_2$$O_3$-${Al_2}{O_3}-{SiO_2}-{TiO_2}$Glass ($Nd_2$$O_3$-${Al_2}{O_3}-{SiO_2}-{TiO_2}$유리계의 상분리현상)

  • 최우형;김형순
    • Journal of the Korean Ceramic Society
    • /
    • v.37 no.12
    • /
    • pp.1221-1228
    • /
    • 2000
  • TiO$_2$를 포함한 희토류 알루미노 규산염계 (NAS: Nd$_2$O$_3$-Al$_2$O$_3$-SiO$_2$) 유리의 상분리 현상에 대하여 연구되었다. 0~10wt%의 TiO$_2$포함한 NAS 조성은 유리전이온도(T$_{g}$) 부근에서 열처리하여 HF로 부식 후 주사전자현미경, 라만 및 IR 분석기로 상분리가 조사되었다. 그 결과로 상분리한 내부결정화는 8wt% 이상의 TiO$_2$를 포함한 NAS 조성에서 나타났다. 어닐링후 T$_{g}$ 부근에서 열처리의 결과는 투명 연핑크색의 유리를 불투명의 연푸른 우유빛 색으로 변하게 하였으며, Si와 Nd-Ti가 각각 풍부한 10$mu extrm{m}$ 이상과 0.1$\mu\textrm{m}$ 이하의 크기인 구형상의 영역으로 균일한 다상분리를 일으켰다. Nd$_2$O$_3$-Al$_2$O$_3$-SiO$_2$-TiO$_2$계에서 상분리는 내부 결정화와 관련하여 매우 중요한 인자로 확인되었다.

  • PDF

Sputtering Growth of ZnO Thin-Film Transistor Using Zn Target (Zn 타겟을 이용한 ZnO 박막트랜지스터의 스퍼터링 성장)

  • Yu, Meng;Jo, Jungyol
    • Journal of the Semiconductor & Display Technology
    • /
    • v.13 no.3
    • /
    • pp.35-38
    • /
    • 2014
  • Flat panel displays fabricated on glass substrate use amorphous Si for data processing circuit. Recent progress in display technology requires a new material to replace the amorphous Si, and ZnO is a good candidate. ZnO is a wide bandgap (3.3 eV) semiconductor with high mobility and good optical transparency. ZnO is usually grown by sputtering using ZnO ceramic target. However, ceramic target is more expensive than metal target, and making large area target is very difficult. In this work we studied characteristics of ZnO thin-film transistor grown by rf sputtering using Zn metal target and $CO_2$. ZnO film was grown at $450^{\circ}C$ substrate temperature, with -70 V substrate bias voltage applied. By using these methods, our ZnO TFT showed $5.2cm^2/Vsec$ mobility, $3{\times}10^6$ on-off ratio, and -7 V threshold voltage.

Nondestructive Test of Optical Connector by Resonant Ultrasound Spectroscopy Method (공명초음파분광법에 의한 광컨넥터용 결합소자의 비파괴검사)

  • Kim, Sung-Hoon;Lee, Kil-Sung;Kim, Dong-Sik;Kim, Young-Nam;Jeong, Sang-Hwa;Yang, In-Young
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.12 no.6
    • /
    • pp.143-150
    • /
    • 2004
  • In this paper, resonant ultrasound spectroscopy(RUS) was used to determine the natural frequency of a ceramic ferrule and a ball lens. The ceramic ferrules are cylinderical shape with $\phi$ 2.56mm diameter and l0mm in length. Crack lengths of these ferrules are 10.40$\mu$m, 21.18$\mu$m and 32.35$\mu$m. The spherical ball lens was made of BK-7 glass, one's diameter in 2mm and 5mm. RUS system is consisted of spectrum analyzer, power amplifier, PZT sensor and support frame. The principle of RUS is that the mechanical resonant frequency of the materials depends on density and the coefficient of elasticity. Rus system is based on that given resonant frequency of the materials can be represented by the function of density and the coefficient of elasticity, and it is applied to excite specimen and to inspect the difference of natural frequency pattern between acceptable specimen and defective ones. Defect evaluation by RUS are performed to investigate the natural frequency measure of ferrule and ball lens.

Influence on the Chemical Durability of $B_2O_3-SiO_2$ and $Al_2O_3-SiO_2$ Thin Films at the Addition of $P_2O_5$ ($P_2O_5$의 첨가가 $B_2O_3-SiO_2$$Al_2O_3-SiO_2$ 박막의 화학적내구성에 미치는 영향)

  • 황규석;김병훈;최석진
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.8
    • /
    • pp.615-622
    • /
    • 1993
  • In order to increase chemical durability of thin films in binary system B2O3-SiO2 and Al2O3-SiO2 on the slide glass by the dip-coating technique from TEOS(Tetraethyl Orthosilicate) and boric acid or aluminum nitrate, phosphoric acid(5~20mol%) was added, respectively. Corrosion of acid and alkali of samples treated with 1N, HCl, NaOH and distilled water at 10$0^{\circ}C$ for 15 minute, were measured IR transmittance and variance of transmittance at visible range. Surface structure of thin film was investigated with SEM and formation of crystal phase according to additiion of phosphoric acid was measrued with XRD. In Al2O3-SiO2 system, change of remarkable characteristic was not obtained at the addition of P2O5 but transmittance of thin film was decreased with addition of P2O5 in B2O3-SiO2 system.

  • PDF

Elevated Temperature Static Fatigue in Silicon Nitride (질화규소의 고온정피로거동)

  • Choi, Guen;Choi, Bae-Ho;Kim, Ki-Yong
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.1
    • /
    • pp.15-20
    • /
    • 1999
  • Elevated temperature static fatigue behavior of silicon has been investigated by stress intensity/life test method. Static fatigue crack growth rate increase with the increase of temperature. Such tendency is found to be mainly related to the decrease of fracture toughness with the increase of temperature. That is, when static fatigue crack growth rate, da/dt is expressed by da/dt=AK1m, a constant A is a function of fracture toughness Kc and the exponent m is a constant which is independent of temperature or Kc. However, in the case of high temperature that glass phase is softened, the crack growth rate is found to be deviated from the above relation. This reason is, thus, discussed.

  • PDF

Synthesis and Characterization of Zeolite Composite Membranes (I):Synthesis of ZSM-5 Type Zeolites (제올라이트 복합 분리막의 합성 및 특성화(I): ZSM-5계 제올라이트의 합성)

  • 현상훈;김준학;송재권
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.9
    • /
    • pp.1064-1072
    • /
    • 1996
  • The synthetic conditions and characteristics of ZSM-5 type zeolites (ZSM-5/silicalite) for the preparation of the zeolite composite membranes for gas separation were investigated. ZSM-5 zeolites could be synthesized by the hydrothermal treatment of the mixture of colloidal silica sol aluminum nitrate sodium hydroxide and TPABr at a temperature range of 150-17$0^{\circ}C$ in the autoclave. Silicalties were done from the solution of water glass water and TPABr. Their crystalline structures transformed from orthorhombic to monoclinic from and their pore structures of three-dimensional channels were opened as TPABr filling channels was burned off at the calcination temperature of 50$0^{\circ}C$. The specific surface area of the calcined zeolite was about 360 m3/g and its surface property was hydrophobic. Crystal sizes of ZSM-5 and silicalite were 0.5-1.0${\mu}{\textrm}{m}$ and 8-10${\mu}{\textrm}{m}$ respectively having no change due to the calcination. In particular the shape and the size of the ZSM-5 type zeolite were sensitively varied with silica sources and concentrations of reaction solutions/sols.

  • PDF

Effects of Heat-treatment Condition on the Characteristics of Sintering and Electrical Behaviors of Two NASICON Compounds (열처리조건이 두 NASICON 조성의 소결 및 전기적특성에 미치는 영향)

  • 강희복;조남희;김윤호
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.7
    • /
    • pp.685-692
    • /
    • 1997
  • Effects of sintering temperature and time on the phase formation, the characteristics of sintering and electrical behaviors of NASICON compounds with Na3Zr2Si2PO12 and Na3.2Zr1.3Si2.2P0.8O10.5 compositions synthesized by solid state reaction were investigated. Maximum relative densities of 96% and 91% were obtained for Na3Zr2Si2PO12 and Na3.2Zr1.3Si2.2P0.8O10.5 compounds, respectively. Complex impedance analysis in a frequency range below 4 MHz was performed to measure the ionic conductivity and migration barrier height of the compounds at RT-30$0^{\circ}C$. The maximum ionic conductivity and the minimum migration barrier height were 0.45 ohm-1cm-1 and 0.07 eV, respectively. The migration barrier height of the high temperature form (space group : R3c) is about 30-40% of that of the low temperature form (space group : C2/c) in two NASICON compounds. Ionic conductivity increases with increasing sinterability, and the presence of glass phase in Na3.2Zr1.3Si2.2P0.8O10.5 compounds lowers significantly ionic conductivity at temperatures above 14$0^{\circ}C$.

  • PDF

Oil Spot Generative Formation of Oil Spot Denmoku (유적 천목의 유적 발생 구조)

  • Jung, Jong-Heuk;Lee, Byung-Ha
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.10 s.293
    • /
    • pp.619-625
    • /
    • 2006
  • The study was intended to investigate production tools and conditions of oil spot following calculating optimal composition of oil spot tenmoku glaze which can be produced at 1250$\sim$l260$^{\circ}C$. Since oil spot is influenced by the viscosity of glaze, viscosity of various glazes fit for oil spot production was determined by an SciGlass 6.0-based calculating method. Applied amount and calcinating conditions of the resulting substance of oil spot, $Fe_2O_3$, were analyzed. As a result, the viscosity of the glaze durable at 1260$^{\circ}C$ was found to range from 4.2 to 4.4, natural cooling was used after oxidizing calcinations at 1260$^{\circ}C$ for an hour, and the best oil spot tenmoku was produced by the natural cooling process after 1 h calcinations at 1150$^{\circ}C$ in the middle of natural cooling. Also, the study showed that thickness of glaze was found to have an effect on the production of oil spot and resulting oil spot was filled mostly with $Fe_2O_3$.