Influence of heat treatment on the microstructure and the physical and mechanical properties of dental highly translucent zirconia

  • Dimitriadis, Konstantinos;Sfikas, Athanasios Konstantinou;Kamnis, Spyros;Tsolka, Pepie;Agathopoulos, Simeon
    • The Journal of Advanced Prosthodontics
    • /
    • v.14 no.2
    • /
    • pp.96-107
    • /
    • 2022
  • PURPOSE. Microstructural and physico-mechanical characterization of highly translucent zirconia, prepared by milling technology (CAD-CAM) and repeated firing cycles, was the main aim of this in vitro study. MATERIALS AND METHODS. Two groups of samples of two commercial highly-translucent yttria-stabilized dental zirconia, VITA YZ-HTWhite (Group A) and Zolid HT + White (Group B), with dimensions according to the ISO 6872 "Dentistry - Ceramic materials", were prepared. The specimens of each group were divided into two subgroups. The specimens of the first subgroups (Group A1 and Group B1) were merely the sintered specimens. The specimens of the second subgroups (Group A2 and Group B2) were subjected to 4 heat treatment cycles. The microstructural features (microstructure, density, grain size, crystalline phases, and crystallite size) and four mechanical properties (flexural strength, modulus of elasticity, Vickers hardness, and fracture toughness) of the subgroups (i.e. before and after heat treatment) were compared. The statistical significance between the subgroups (A1/A2, and B1/B2) was evaluated by the t-test. In all tests, P values smaller than 5% were considered statistically significant. RESULTS. A homogenous microstructure, with no residual porosity and grains sized between 500 and 450 nm for group A and B, respectively, was observed. Crystalline yttria-stabilized tetragonal zirconia was exclusively registered in the X-ray diffractograms. The mechanical properties decreased after the heat treatment procedure, but the differences were not statistically significant. CONCLUSION. The produced zirconia ceramic materials can be safely (i.e., according to the ISO 6872) used in extensive fixed prosthetic restorations, such as substructure ceramics for three-unit prostheses involving the molar restoration and substructure ceramics for prostheses involving four or more units. Consequently, milling technology is an effective manufacturing technology for producing zirconia substructures for dental fixed all-ceramic prosthetic restorations.

Influence of resin-nanoceramic CAD/CAM block shade and thickness on the microhardness of dual-cured resin cement (레진-나노세라믹 CAD/CAM블록의 색조와 두께가 이원중합 레진시멘트의 미세경도에 미치는 영향)

  • Choi, Ga-Young;Park, Jeong-Kil;Jin, Myoung-Uk;Kwon, Yong Hoon;Son, Sung-Ae
    • Korean Journal of Dental Materials
    • /
    • v.44 no.2
    • /
    • pp.151-161
    • /
    • 2017
  • The purpose of this study was to examine the effect of shade and thickness of resin-nanoceramic CAD-CAM block (RNB) on the microhardness of dual-cured resin cement, as well as to measure the number of photons transmitted through RNBs of different thicknesses and colors. One dual-cured resin cement was used to prepare resin cement specimens. Resin cement specimens were light-cured for 40 seconds through 3 shades (A1, A2, A3 in HT (high translucency) and LT (low translucency) respectively) and four thicknesses (1, 2, 3, 4 mm) of RNB specimens. Vickers microhardness measurements of resin cement specimens were performed using a Vickers hardness tester. The light transmission of RNB specimens was measured using a spectrometer (SpectroPro-500, Acton Research, Acton, MA, U.S.A.), and the translucency parameter was calculated using the CIEL*a*b* system. Data were statistically analyzed by ANOVA and Tukey's test. There was a significant decrease of microhardness of resin cement specimen with an overlay of 4 mm of RNB thickness and A3 shade in comparison to A1 and 1 mm, respectively (p<0.05). The translucency parameter values and light transmission of RNBs tested differed significantly, according to the thicknesses of the specimen (p<0.05). Light transmission is decreased with increase in the thicknesses of RNBs. Shade A1 transmitted more light than darker blocks. A decrease in microhardness of resin cement specimens was observed with increasing thickness and shade (A1 to A3) of RNBs.

Full mouth rehabilitation of patient with severe dental caries with implant fixed prosthesis fabricated with milling and 3D printing method: A case report (밀링 및 3D 프린팅 방법으로 제작된 임플란트 보철물을 이용한 심한 우식 환자의 완전 구강 회복 증례)

  • Kim, Taeyoon;Lee, Jun-Suk;Hong, Seoung-Jin;Kim, Hyeong-Seob;Kwon, Kung-Rock
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.3
    • /
    • pp.288-295
    • /
    • 2019
  • Passive fit of prosthesis is an essential property of implant supported prosthesis for long term success and minimization of complications. And the property is determined mostly by fabrication procedure. There were limitations of extensive implant prosthesis because conventional casting method generate contraction error of long span prosthesis. However, Computer-aided design/Computer-aided manufacturing (CAD/CAM) technology of 3D printing and milling metal framework can overcome those limitations. This case is a full mouth rehabilitation using extensive implant fixed prosthesis. Removable interim prosthesis was made for esthetic, functional evaluation and a guide for implant insertion. After the insertion, implant fixed interim prosthesis was delivered. After additional evaluation and adjustment, final prosthesis was designed with CAD, the fabricated with CAM. Milling technique was used for anterior screw type implant superstructure and 3D printing technique was used for the anterior and posterior implant copings. Fit of the final restoration was favorable. The practitioner and patient were both esthetically and functionally satisfied with the final result.

Comparison on marginal fitness and mechanical properties of copings with zirconia block and CAM type (지르코니아 블록과 CAM 종류에 따른 코핑의 변연적합도와 기계적 특성 비교)

  • Chung, In-Sung;Jeon, Byung-Wook;Kim, Won-Young;Kang, Jae-Min
    • Journal of Technologic Dentistry
    • /
    • v.39 no.2
    • /
    • pp.75-82
    • /
    • 2017
  • Purpose: This study provided the basic data for selection the zirconia block and CAM by means of marginal fitness observations, flexural strength test and hardness test. Methods: Three dental zirconia blocks(ABCera, NaturaZ, ST98) and two dental milling machines(CAD/CAM MS, DWX-50) were used in this study. Metal abutment(diameter 10 mm, height 5 mm, inclined angle $3^{\circ}$ taper, 1 mm chamfer margin) was fabricated by Ti customized abutment, and then zirconia copings were fabricated for each ten specimens. Silicone replica technique was used to observe the marginal fitness of cross-sections with a stereomicroscope at ${\times}50$ magnification. The dental zirconia blocks was cut into 10 pieces each having a size of $25mm{\times}5mm{\times}1mm$, and fabricated according to the manufacturer's instructions, and flexural strength was measured using a universal testing machine. For hardness test, a micro Vickers hardness tester was used as it was in the flexural strength test. Statistical analysis was performed by one way ANOVA and post-test was performed by Scheffe test. Results: For marginal fitness of bucco-lingual axial, ZU group($59.7{\pm}10.3{\mu}m$) was the lowest, followed by RA, ZA, ZD, RD, RU. For marginal fitness of mesio-distal axial, ZU group($59.3{\pm}10.2{\mu}m$) was the lowest, followed by RA, ZA, RD, ZD, RU. One-way ANOVA showed statistically significant difference between groups(p<0.05). For flexural strength, ABCera block($718.0{\pm}57.2MPa$) was the highest, followed by NaturaZ, ST98. For hardness, ABCera block($1550.3{\pm}19.8Hv$) was the highest, followed by ST98, NaturaZ. There was no significant difference in flexural strength and hardness between blocks(p>0.05). Conclusion: Based on the results of this study, the type of dental zirconia block did influence the marginal fitness, and all dental zirconia blocks are expected to be suitable for clinical application. The highest flexural strength and hardness were ABCera block, and no statistically significant difference was observed.

Development of Dental Scanning System and Reproduction of Adjustable Upper Dental Impression Tray (치과용 스캐닝 시스템의 개발과 가변형 상악용 트레이의 재현성)

  • Cha, Young-Youp;Eom, Sang-Ho
    • Journal of Institute of Control, Robotics and Systems
    • /
    • v.16 no.3
    • /
    • pp.300-304
    • /
    • 2010
  • This study was performed to development a dental three-dimensional laser scanning system and measure the accuracy of new adjustable upper dental impression tray. The metal stock, individual, and new adjustable stock trays were used for 30 stone casts(10 casts each) duplicated a resin master model of maxilla. The dental stone was poured in a vinyl polysiloxane impressions and allowed to set for on hour. The master model and the duplicated casts were digitized using an dental scanning system. The distance between the reference points were measured and analyzed on the graphic image of 3D graphic software of CATIA. The statistical significance of the differences between the groups was determined by a two-way ANOVA. There were no significant differences between the accuracies of the adjustable stock tray and the master model except only anterior arch width on the upper arch. The adjustable upper stock tray showed clinically acceptable accuracies of the study cast produced by them.

디지털 가이드 시스템과 사전 제작된 임플란트 상부보철물을 이용한 전치부의 임플란트 수복 : 증례보고

  • Choi, Yongkwan
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.30 no.1
    • /
    • pp.24-32
    • /
    • 2021
  • Dental implant have been in use for a long time to restore at missing tooth. But, To place dental implant at good position very is difficult. Improperly positioned dental implants make some problems to have a good function of dental implant. so, To place dental implant at accurate position is the most important step throughout the whole process. Digital guided system of dental implant is very useful to have a accurate position of dental implant and it makes upper restoration more esthetic and funcional.

Esthetic Restoration of Complicated Crown-Root Fractures Utilizing Orthodontic Extrusion (복합 치관-치근 파절의 교정적 정출술을 이용한 심미적 수복)

  • Kim, Minji;Kim, Jinyoung;Kim, Suhyun;Lim, Sumin
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.43 no.1
    • /
    • pp.60-69
    • /
    • 2016
  • Complicated crown-root fracture of permanent incisors cause esthetic, functional, and psychological problems to patients. Therefore, treatment is important and multidisciplinary treatment is required. This case report describes the clinical procedures involved in the treatment of trauma-induced complicated crown-root fractures in the maxillary incisor of two young patients. Conventional root canal treatment and apexification were performed in each patient. To expose the fracture margins to the supragingival level and to reestablish the biologic width, orthodontic extrusions with fixed appliances were performed followed by a retention period. During the retention period, fiber-optic posts and cores were built up and provisional crowns were placed. Finally, ceramic crowns manufactured using a computer-aided design/computer-aided manufacturing (CAD/CAM) system were placed. In both patients, the teeth presented satisfactory functional and esthetic outcomes without relapse. The periodontal tissues were healthy.

Comparative Study of the Surface Roughness of Working Models Fabricated by Dental CAD/CAM Scannable Stone and Type IV Gypsum Products (치과용 캐드캠 스캔전용 석고와 Type IV 석고로 제작된 작업모형의 표면조도 비교 연구)

  • Kim, Sa-Hak;Kim, Jae-Hong
    • Journal of dental hygiene science
    • /
    • v.14 no.4
    • /
    • pp.455-460
    • /
    • 2014
  • This study compared the surface roughness and surface characteristics between a type IV stone and scannable stone. Materials used were a type IV stone, two different kind of scannable stone. Ten specimens per experimental group were prepared according to manufacturer's direction. Surface roughness of specimen was measured using profilometer. The measurement was based on the standard of Japanese Industrial Standards 1994. The mean and standard deviations of each reference point were analyzed using one-way ANOVA and Scheff$\acute{e}$ post hoc test. The program used to handle statistical analysis was SPSS 20.0 and the significance level was set at 0.05. The difference of surface roughness was statistically significant in order of Scannable Stone $10.07{\pm}0.02{\mu}m$, Scannable Stone $20.08{\pm}0.03{\mu}m$, Type IV $0.10{\pm}0.04{\mu}m$. These results will have to be confirmed in further clinical application researches.

The Properties of Sintered Body by Using the Slip Casting Process with Remained Dental Zirconia Block after Machining (치과용 지르코니아 코어 가공후의 잔여물을 활용하여 주입성형법으로 제조한 소결체의 특성)

  • Kim, Sang-Su;Lee, Dong-Yoon;Seo, Jeong-Il;Bae, Won-Tae
    • Journal of Technologic Dentistry
    • /
    • v.34 no.2
    • /
    • pp.75-81
    • /
    • 2012
  • Purpose: All ceramic crown, made from zirconia instead of metal for core material, is recognized the best esthetical prosthesis. Recently, high-priced zirconia blocks and expensive CAD/CAM machines come into use for making zirconia core. In this study, slip casting process is adapted to evaluate the possibility of the recycling the remained parts of zirconia block after machining. Methods: Remained zirconia blocks were reduced to powders with zirconia mortar, and screened with 180 mesh sieve. Passed powders were ball milled under various conditions to obtain the optimum zirconia slip for casting. Solid casting method was used for casting the specimens with plaster mold. Formed specimens were dried and biscuit fired at $1,000^{\circ}C$ for 1 hour. Biscuit fired specimens were finished with exact shape of square pillar. Finished specimens were fired from $1,200^{\circ}C$ to $1,550^{\circ}C$ at $50^{\circ}C$ intervals for 1 hour. Linear shrinkage, apparent porosity, water absorption, bulk density, and flexural strength were tested. Microstructures were observed by SEM. Results: Above examinations indicated that the optimum firing temperture was $1,500^{\circ}C$, and when fired at this temperature for 1 hour, apparent porosity was 0% and flexural strength was 680MPa. SEM photomicrographs showed uniform 200~300nm grain size, which is equal with microcture of sintered commercial zirconia block. when compare 24% linear shrinkage of cast specimen with 20% linear shrinkage of CAD/CAM machined block, it was estimated that the size controlling of cast core was not so difficult. Conclusion: According to the all of this experimental results, the cast zirconia core produced from the remained parts of zirconia block was possible to use for all ceramic denture.

A Study on the Fracture Strength of the Cement Gap (Cement Gap에 따른 Zirconia Crown의 파절강도 비교)

  • Kim, Nam-Joong;Lee, Chung-Jae;Kwak, Woon-Seon
    • Journal of Technologic Dentistry
    • /
    • v.38 no.4
    • /
    • pp.299-304
    • /
    • 2016
  • Purpose: This research is conducted for better clinical test of Zirconia as we find out the fracture strength difference of Zirconia on cement gaps of full Crown that made use of Zirconia which is somewhat being used in recent dental technology. Methods: We produced each nine of Zirconia Crown of Zirconia fracture cement gaps A group(0.03 mm), B group(0.05 mm), C group(0.08 mm) on cement gaps by use of CAD/CAM, and compared the results. We could end up getting conclusions as following. Results: There was fracture strength difference per cement gaps but no impact(P<0.05). There was difference between $1.962{\pm}0.259$ from group A and $2.005{\pm}0.367$ from group B, but no impact(P<0.05). There was difference between $1.962{\pm}0.259$ from group A and $2.478{\pm}0.331$ from group C, but it's hard to be considered as an impact(P<0.05). Conclusion: Because of the hight pressure 0.08 mm is fractured and Margin has a lot of empty space due to gap for 0.08 mm. To identify the difference between 0.08 mm and 0.05 mm, 0.08 mm is selected as a gap. Therefore when it comes to using 0.05 mm authentically 0.05 mm is quite practical to use as a gap.