Prediction of Propagation Path for the Interface Crack in Bonded Dissimilar Materials (이종접합재의 계면균열에 대한 진전경로의 예측)

  • 정남용;송춘호
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.4 no.3
    • /
    • pp.112-121
    • /
    • 1996
  • Applications of bonded dissimilar materials such as metal/ceramics and resin/metal joints, are very increasing in various industry fields. It is required to find crack propagation direction and path applying to the fracture mechanics on the bonded joint of dissimilar meterials. In this paper, crack propagation direction and path were simulated numerically by using boundary element method. Crack propagation angle is able to easily determine based on the maximum stress concept. Fracture tests of Al/Epoxy dissimilar materials with an interface crack are carried out under various mixed mode conditions by using the specimens of bonded scarf joints. It is found that the experimental results are well coincide with the analysis results of boundary element method.

Effect of Frit Content on Microstructure and Flexural Strength of Porous Frit-Bonded Al2O3 Ceramics (Frit 함량이 다공질 Frit-Bonded 알루미나 세라믹스의 미세조직과 꺾임강도에 미치는 영향)

  • Lim, Kwang-Young;Kim, Young-Wook;Song, In-Hyuck;Kim, Hai-Doo;Bae, Ji-Soo
    • Journal of the Korean Ceramic Society
    • /
    • v.47 no.6
    • /
    • pp.529-533
    • /
    • 2010
  • Porous frit-bonded alumina ceramics were fabricated using alumina and frit as raw materials. The effects of frit content and sintering temperature on microstructure, porosity, and flexural strength were investigated at low temperature of $750{\sim}850^{\circ}C$. Increased addition of frit content or higher sintering temperature resulted in improved flexural strength of porous frit-bonded alumina ceramics. It was possible to produce frit-bonded alumina ceramics with porosities ranging from 35% to 40%. A maximum strength of 52MPa was obtained at a porosity of ~38% when 90 wt% alumina and 10 wt% frit powders were used.

A Study on the Development of Diamond Grinding Wheel with Multi-Porous Structure (다기공 다이아몬드 연삭숫돌의 개발에 관한 연구)

    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.7 no.2
    • /
    • pp.100-107
    • /
    • 1998
  • Diamond wheels with fine grains and multi-porous structures are newely trial developed for smoothing and mirror finishing materials. Grinding wheel must have performed both to remove tool marks efficienitly and to contact elastically with curved surfaces, that are employed for ultra precision and high performance grinding of difficult-to materials such as tungsten carbide alloy using tool and die materials, Diamond grains are bonded by a melamine resin to prevent the decrease of machining efficiency due to grain sinking within the bond materials. Also, highly foamed structures are developed to increase the flexibility of the grinding wheel, and to induce self-sharpening by increasing contact pressure between the grinding wheel and workpiece surfaces. In this paper, melamine-bonded diamond wheels try to manufacture, then the forming method of grinding wheel are suggested, and the grinding characteristics of melamine-bonded diamond grinding wheel are also illustrated.

  • PDF

Analysis of stress and stress intensity factor in bonded dissimilar materials by boundary element method (경계요소법을 이용한 이종재료 접착.접합재의 응력 및 응력세기계수 해석)

  • Yi, W.;Chung, N.Y.;Yu, Y.C.;Jeong, E.S.
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.21 no.9
    • /
    • pp.1357-1363
    • /
    • 1997
  • Currently it is increasing to use th bonded dissimilar materials in the various field of advanced engineering such as the highly rigid and lighter vehicle, plastic molding LSI package and metal/ceramic bonded joint. In spite of such a wide application of the bonded dissimilar materials, the evaluation method of the bonding strength has not been established yet. Therefore in this paper we analyze the interface crack problem by introducing fracture mechanics parameters as the basic research about estimating of the strength of adhesive joints. The variation of stress intensity factor according to the elastic modulus of adherend and thickness of bonded layer are investigated. Numerical results are based on the results of boundary element analysis of four different type butt joints subjected to uniaxial tension loading.

An Experimental Study on Electrical and Mechanical Characteristics of Al6061/Al6061 and Al6061/Sus304 by Using Thermal Bonding Technology (열처리 본딩 기술을 이용한 Al6061/Al6061 및 Al6061/Sus304의 기계적 및 전기적 특성에 관한 실험적 연구)

  • You, Chung-Jun;Jung, Won-Chae
    • Journal of the Korean institute of surface engineering
    • /
    • v.41 no.6
    • /
    • pp.325-330
    • /
    • 2008
  • Al6061 and Sus304 materials are bonded by using thermal bonding technology. Al6061, Sus304 and thermal bonded Al6061/Al6061 and Al6061/Sus304 materials are characterized by using mechanical and electrical measurement. Especially the experimental characteristic data of thermal bonded Al6061/Al6061 and Al6061/Sus304 are not well known until today. We have investigated on Al6061, Sus304 and thermal bonded material. The thermal bonded material Al6061/Al6061 and Al6061/Sus304 can be used for the LCD frame and the other electrical products. For the future, we expect that the more various experiments should be needed to carry out for the data accumulation in the bonded new materials.

Evaluation of Fracture Toughness on Interface Cracks in Bonded Components of Dissimilar Materials (이종 접합부재의 계면균열 파괴인성의 평가)

  • Chung, Nam-Yong;Lee, Myung-Dae;Park, Chul-Hee
    • Proceedings of the KSME Conference
    • /
    • 2003.04a
    • /
    • pp.346-351
    • /
    • 2003
  • In this paper, an evaluation method of fracture toughness on interface cracks has been investigated under various mixed-mode conditions of the bonded scarf joints. Two types of the bonded scarf joints with an interface crack were prepared to analyze the stress intensity factors using boundary element method(BEM) and to perform the fracture toughness test. From the results of fracture toughness experiments and BEM analysis, an evaluation method of fracture toughness on interface cracks in the bonded components of dissimilar materials has been proposed and discussed.

  • PDF

A study on the Fracture Mechanical Strength Evaluation in Joint Interface of Ceramics and Metal (세라믹스/금속 접합계면에서의 파괴력학적 강도평가에 관한 연구)

  • 최병기
    • Journal of the Korean Society of Safety
    • /
    • v.11 no.3
    • /
    • pp.20-24
    • /
    • 1996
  • Indentation fracture method and 4-point bending test are carried out to measure the residual stresses and the bending strength, and to investigate the mechanism of fracture mechanics in the bonded interface of ceramic and metal. The results obtained are as follows ; 1) The fracture patterns of bonded materials shows that the delamlnatlon fracture of Interfaces is stablely developed from the interfaces of ceramic/active metallic bonded materials at the specimen center, and the fracture is unstablely generated through a refraction on the middle ceramic. 2) Distribution of residual stresses is quantitatively investigated on the ceramic side of bonded materials. 3) It Is found that the residual stresses of interface vertical direction are concentrated on the bonded interface at the ceramic side.

  • PDF

An Evaluation Method of fracture Toughness on Interface Cracks in Bonded Dissimilar Materials (이종 접합체의 계면균열에 대한 파괴인성의 평가방법)

  • 정남용
    • Transactions of the Korean Society of Automotive Engineers
    • /
    • v.11 no.4
    • /
    • pp.110-116
    • /
    • 2003
  • In this paper, an evaluation method of fracture toughness on interface cracks has been investigated under various mixed-mode conditions of the bonded scarf joints. Two types of the bonded scarf joints with an interface crack were prepared to analyze the stress intensity factors using boundary element method(BEM) and to perform the fracture toughness test. From the results of fracture toughness experiments and BEM analysis, an evaluation method of fracture toughness on interface cracks in the bonded dissimilar materials has been proposed and discussed.

Effect of Si:C Ratio on Porosity and Flexural Strength of Porous Self-Bonded Silicon Carbide Ceramics (Si:C Ratio가 다공질 Self-Bonded SiC 세라믹스의 기공율과 곡강도에 미치는 영향)

  • Lim, Kwang-Young;Kim, Young-Wook;Woo, Sang-Kuk;Han, In-Sub
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.5
    • /
    • pp.285-289
    • /
    • 2008
  • Porous self-bonded silicon carbide (SiC) ceramics were fabricated at temperatures ranging from 1750 to $1850^{\circ}C$ using SiC, silicon (Si), and carbon (C) powders as starting materials. The effect of the Si:C ratio on porosity and strength was investigated as a function of sintering temperature. It was possible to produce self-bonded SiC ceramics with porosities ranging from 36% to 43%. The porous ceramics showed a maximal porosity when the Si:C ratio was 2:1 regardless of the sintering temperature. In contrast, the maximum strength was obtained when the ratio was 5:1.

Study on the Formation and the Magnetic Properties of $Sm_2Fe_{17}N_x$-type Interstitial Material

  • Kwon, H.W.
    • Journal of Magnetics
    • /
    • v.1 no.1
    • /
    • pp.19-23
    • /
    • 1996
  • In the present study, the $Sm_2Fe_{17}N_x$-type interstitial materials have been prepared by reaction between Nb-free or Nb-containing $Sm_2Fe_{17}$-type alloy and $N_2$ gas. Nitrogenation behaviour of the $Sm_2Fe_{17}N_x$-type material and disproportionation characteristics of the nitrogenated materials have been studied by means of differential thermal analysis (DTA) and thermopiezic analysis (TPA). Magnetic properties of the produced $Sm_2Fe_{17}N_x$-type interstitial materials were characterised in vibrating sample magnetometer (VSM) or thermomagnetic analyser (TMA). Epoxy-bonded or Zn-bonded $Sm_2Fe_{17}N_x$-type magnets were prepared, and their magnetic properties were investigated. It has been found that nitrogenation kinetics of the Sm2Fe17Nx-type alloy is improved significantly by the Nb-substitution for Fe in the alloy. The Nb-substitution is also found to enhance thermal stability of the $Sm_2Fe_{17}N_x$-type interstitial material. Hard magnetic properties of the interstitial materials produced from Nb-free orNb-containing alloy is high enough (intrinsic coercivity : over 7 kOe) for application as bonded permanent magnets. The good hard magnetic properties of the interstitial material are maintained in the epoxy-bonded magnet. Intrinsic coercivity of the Zn-bonded magnets is improved significantly as post-bonding annealing time increases.