Nd:YAG 레이저 맞대기 용접의 비드형상 예측에 관한 유한요소해석 (Finite element analysis for prediction of bead shape of Nd:YAG laser butt welding)

  • 김관우;남기정;이제훈;서정;조해용
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제32권1호
    • /
    • pp.137-146
    • /
    • 2008
  • Nd:YAG pulse laser welding of stainless steel plate was simulated to find welding condition by using commercial finite element code MARC. Due to geometric symmetry, a half model of AISI 304 stainless steel plate was considered and user subroutines were applied to boundary condition for the heat transfer. Material properties such as conductivity, specific heat, mass density and latent heat were given as a function of temperature. As results, Three dimensional heat source model for pulse laser beam conditions of butt welding has been designed by the comparison between the finite element analysis results and experimental data on AISI 304 stainless steel plate. Nd:YAG laser welding for AISI 304 stainless steel was successfully simulated and it should be useful to determine optimal welding condition.

Nd:YAG 레이저 필렛 용접의 비드형상 예측에 관한 유한요소해석 (Finite Element Analysis for Prediction of Bead Shape of Nd:YAG Laser Fillet Welding)

  • 김관우;이제훈;서정;조해용
    • 대한기계학회논문집A
    • /
    • 제31권8호
    • /
    • pp.839-846
    • /
    • 2007
  • Nd:YAG pulse laser fillet welding of stainless steel plate was simulated to find welding condition by using commercial finite element code MARC. Full model of AISI 304 stainless steel plate was considered and user subroutines were applied to boundary condition for the heat transfer. Material properties such as conductivity, specific heat, mass density and latent heat were given as a function of temperature. As results, Three dimensional heat source model for pulse laser beam conditions of fillet welding has been designed by the comparison between the finite element analysis results and experimental data on AISI 304 stainless steel plate. Nd:YAG laser welding for AISI 304 stainless steel was successfully simulated and it should be useful to determine optimal welding condition.

판재의 비드 용접에서 구속경계조건을 적용한 열응력 및 각변형 해석 (An Analysis of Thermal Stress and Angular Distortion in Bead-on-Plate Welding Incorporating Constrained Boundary Conditions)

  • 배강열;최태완
    • Journal of Welding and Joining
    • /
    • 제17권1호
    • /
    • pp.104-115
    • /
    • 1999
  • 판재의 비드 용접과정에서 열응력과 각변형의 발생기구 및 크기를 판재 단면에 대한 2차원 유한 요소해석을 통해 규명하고자 할 때 판재의 3차원 특성을 판재 길이의 크기효과로 간주하여, 구속경계조 건으로 설정함으로써 2차원 해석으로도 더욱 실제에 근접한 현상해석이 가능함을 제안하고자 하였다. 먼저 용접 입열에 의한 판재 내부의 천이 온도분포를 해석하였고, 이를 열응력 해석에 활용하였다. 2차 원 열응력 해석에 있어, 용접도중에 단면 전체가 길이 방향으로 동일한 크기의 변위를 한다고 가정하여 일정 변위를 길이 방향 경계조건으로 설정하고, 판재의 길이에 따라 각변형의 발생이 구속된다고 가정 하여, 판재의 길이에 의한 구속효과를 상당 구속력으로 간주하여 이를 단면 부재의 회전방향에 대한 경 계조건으로 설정함으로써 판재의 3차원 특성을 고려하고자 하였다. 제안된 방법에 의한 응력 분포 형태, 각변형 크기 등의 해석 결과가 기존의 2차원 해석 결과에 비해 실제에 더 근접함을 보여 주었다.

  • PDF

용접각변형에 미치는 용접길이의 영향 (The Effects of Welding Length on the Angular Distortion)

  • 박정웅;이해우
    • Journal of Welding and Joining
    • /
    • 제23권4호
    • /
    • pp.48-52
    • /
    • 2005
  • To estimate welding deformation for large steel structures, either experiment result with small specimen or analysis result of FEM with small numerical model is used. Consequently, it is important to decide the welding length of specimen and numerical model not to have an effect on welding deformation for accurate estimation of whole welding deformation. This study experimentally clarifies the effect of welding length on angular distortion due to welding by varying welding length of specimens, but fixing width and thickness of specimens on V-groove butt welding, fillet welding and bead on plate welding. As a resell the critical welding length on fillet welding and on bead on plate welding is over 500mm and on V-groove butt welding is over 1,000mm.

Ar/He 보호가스분위기에서 Al 5083 합금의 대전류 MIG 용접특성 (High Current MIG Welding of Al 5083 Alloy under Ar/He Mixed Gas Shielding)

  • 최영배;황인성;강문진;김동철
    • Journal of Welding and Joining
    • /
    • 제32권1호
    • /
    • pp.87-92
    • /
    • 2014
  • Recently, use of thick Al 5083 plate has increased in production of LNG storage tank. In general, multi-pass welding has been used to achieve sufficient penetration in thick plate welding. High current welding which enables high deposition and deep penetration is preferred in thick plate welding because the increase of number of pass increases manufacturing cost and formation of weld defect. In this study, welding characteristics according to various Ar/He shielding gas composition was investigated in high current MIG welding. The bead-on-plate welding and V groove welding were conducted on Al 5083 alloy with a thickness of .25 mm. The effect of shielding gas composition on bead shape was evaluated and proper shielding gas composition was proposed. Also arc stability was examined under selected shielding gas composition. One side-one pass welding experiments were conducted for V groove specimen with a thickness of 25 mm. Mechanical properties and hardness profiles were measured for the V groove specimens.

용접부 강도특성 미치는 후처리 영향 (Effects of post treatment on the fatigue strength of weldment)

  • 김현수;박윤기;윤중근
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 추계학술발표대회 개요집
    • /
    • pp.246-248
    • /
    • 2004
  • Effects of the post treatment on the fatigue strength of a bead-on-plate weldment were investigated in order to improve fatigue strength of the weldment. The post treatment applied were the grinding of weld toe and hammer peening at the weld toe. The fatigue strength of the weldment after post treatment increases. It is attributed to the decrease of the residual stress and the maximum stress at the weld toe by the post treatments. Based on the result, the principal factor controlling the fatigue strength of the weldment was identified as the toe shape of the bead-on-plate weldment.

  • PDF

레이저 용접의 비드 형상에 대한 실험치와 이론 결과의 비교 (Comparison of Theoretical model with Experiment in Bead Shape of Laser Welding)

  • Kim, J.D.;Kim, J.D.
    • 한국정밀공학회지
    • /
    • 제11권1호
    • /
    • pp.201-210
    • /
    • 1994
  • A theoretical heat-flow model incorporating with a constant moving CO$_{2}$ laser beam has been analyzed to predict depth and the shape of bead section during last beam welding. The laser beam is exponentially attenuated with an abosrption coefficient in the material. The solution can be expressed in terms of normalized variables. The experimental data were generated by usint CW 2 CO$_{2}$ laser with multi beam mode and CW 3 kW CO$_{2}$laser with Gaussian mode. The specimens were made as bead-on-plate welds for SM 10C, STS 304, STS 316, STS 420 and pure Nickel. The maximum possible penetration depth and the shape of beas section for given sources of laser power, travel speed and beam spot size can be prdicted with this model in a given material.

  • PDF

알루미늄 熔接構造物의 變形橋正을 위한 Autogeneous GTAW의 適用 可能性 硏究 (A Feasibility Study on the Use of Autogeneous GTAW for Correction of Distortions in Welded Aluminum Alloy Structures)

  • 하용훈;강춘식;유순영
    • Journal of Welding and Joining
    • /
    • 제10권1호
    • /
    • pp.20-34
    • /
    • 1992
  • Characteristics of two correcting methods, a new Autogeneous GTAW heating (TIG) method and the conventional GMAW bead-on plate welding(MIG) method, for distorted aluminum fabrication structures were studied. As a result of microscopic study of Autogeneous GTAW heating and GMAW bead-on plate welding areas, porosities in weld metal and surface cracks in local heating zone were found. Through the mechanical tests, it was verified that porosities decrease tensile strength and surface of distortion, angular displacement and transeverse shrinkage were measures and compared. In order to investigate changes of material properties in heating area and cause of defects such thermal stresses were calculated by ADINA. Through the computations of transient thermal stresses and microscopic observation of fracture surface, thermal stress was found to be the cause of crack during Autogeneous GTAW heating.

  • PDF

굴삭기 버킷 용접부의 피로수명에 관한 연구 (A Study on Fatigue Life of Weld Method for Excavator Bucket)

  • 박경동;정재욱
    • 동력기계공학회지
    • /
    • 제9권4호
    • /
    • pp.102-109
    • /
    • 2005
  • An attachment part of the construction equipment frequently claimed from the crack occurrence that takes especially at the bucket. therefore we execute the fatigue examination and changes the welding method at the same materials. we executed a fatigue crack propagation experiment and got the conclusions at the normal temperature and Frequency 10Hz. We carried out butt welding for structure steel of SM490A and make three kinds of specimen of different weld method each. The fatigue limit of CASE 1 was determined to the low than CASE 2, CASE 3. the CASE 2 putting the interval of the 2mm creates back plate and make fatigue limit to high. Bead shapes and weld surfaces shape influence on fatigue life of materials. Specially, the crack growth becomes starting point that gap of back-plate and boundary surface of bead. It is confirmed by fracture showing on this study.

  • PDF

CO2 레이저용접시 용접조건에 따른 플라즈마 방사신호의 특성연구 (A Study on Characteristics of Plasma Emission Signals with Welding Conditions in CO2 Laser)

  • 김종도;이창제
    • 대한기계학회논문집A
    • /
    • 제33권11호
    • /
    • pp.1256-1261
    • /
    • 2009
  • Today, implementation of the defect detection in laser welding has been researched for a long time, but most studies have been made around thin plate within $1{\sim}3mm^t$. Therefore, this study was measured and analyzed light emission signals of the induced plasma in $CO_2$ laser lap welding of $6mm^t$ Zn primer-coated steel, and based on this analysis, research made an investigation into possibility of monitoring in thick plate welding. It was been analyzing the measured signals by RMS and FFT processing, as a results, we were able to confirm definite difference of two signals between humping bead and sound bead. Thus, possibility of real time monitoring in $CO_2$ laser lap welding verified experimentally.