졸 - 겔법에 의한 바륨헥사알루미네이트 합성 (Synthesis of barium hexaaluminate by sol - gel method)

  • 백영순;김형진
    • 한국결정성장학회지
    • /
    • 제5권2호
    • /
    • pp.142-151
    • /
    • 1995
  • 금속 알콕사이드법에 의해 복합 알콕사이드를 합성하고, 이를 sol - gel법으로 가수분해 반응시켜 얻은 전구체를 소성하여 barium hexaaluminate를 제조하였다. 복합 알콕사이드 합성시 알코올의 종류 및 양, 반응시간을 변화시켜 barium hexaaluminate 전구체 물성에 미치는 영향을 관찰하였으며, 가수 분해시 물의 양 및 반응온도, 그리고 숙성시간에 따른 barium hexaaluminate의 비표면적과 입자크기에 미치는 영향을 알아보았다.

  • PDF

Fabrication of Barium Ferrite Films by Sol-Gel Dip Coating and Its Properties.

  • T. B. Byeon;W. D. Cho;Kim, T. O.
    • Journal of Magnetics
    • /
    • 제2권1호
    • /
    • pp.16-21
    • /
    • 1997
  • Those were investigated, the crystallographic, morphological, and magnetic properties of barium ferrite film (SiO2/Si substrate) prepared by sol-gel dip coating. Appropriate sol was prepared by dissolvin barium and iron nitrate in ethylene glycol at 80$^{\circ}C$. To obtain the films, thermally oxidized p-type silicon substrate with (111) of crystallographic orientation were dipped into the sol, dried at 250$^{\circ}C$ to remove organic material, and heated at 800$^{\circ}C$ for 3 hours in air for the crystallization of barium ferrite. It was found that the particles of barium ferrite formed on the substrate exhibited needle-like shape placing parallel to the substrate and its c-axis is long axis direction. There was tendency that the coercive force in horizontal direction to the substrate was higher than that in vertical direction to it. This tendency was profound in large thickness.

  • PDF

EFFECT of PREPARATION METHODS and CONDITIONS of PRECURSORS on the PROPERTIES of $BATIO_3$ ALKOXIDE FILMS

  • N., Korobova;Soh, Dea-Wha
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.714-718
    • /
    • 2003
  • Usually for the commercial preparation of barium titanate films or ceramics the reaction atmosphere must be preferably in air. However, normally air is not used because it contains carbon dioxide, which can easily react with barium to form the undesired product barium carbonate, leading to unwanted second-phase formation in the (mal stages of the process. In the present work a series of perovskite barium titanate films was prepared by the sol-gel method, using a metal alkoxide solutions in the electrophoretic deposition (EPD). The influence of several process parameters, like sintering temperature of sol preparation before EPD and heat-treatment temperature and non-oxidized atmosphere, on the film properties is described.

  • PDF

Synthesis of Monodispersed Barium Titanate Nanopowders by Alkoxide-Hydroxide Sol-Precipitation Method

  • Yoon, Song-Hak;Kim, Min-Gyu;Shin, Nam-Soo;Kim, In-Sung;Baik, Sung-Gi
    • 한국세라믹학회지
    • /
    • 제43권11호
    • /
    • pp.710-714
    • /
    • 2006
  • Barium titanate nanoparticles were synthesized under N$_2$ atmosphere by the hydrolysis and condensation of barium hydroxide octahydrate and titanium (IV) isopropoxide. The synthesized particles were aggregates of nanosized primary particles. The primary particles of about 20-50 nm in diameter became building blocks of larger secondary particles, which are in most cases spherical in shape. The size and morphological evolution of secondary particles are strongly related to the precursor concentration. The observations suggest that formation and control of secondary particles is an essential step in the alkoxidehydroxide sol-precipitation process to obtain monodispersed barium titanate nanopowders.

졸겔법을 이용한 바륨페라이트 박막 제조 (Preparation of Barium Ferrite Thin Film by Sol-Gel Method)

  • 변태봉;조원덕;김태옥
    • 한국세라믹학회지
    • /
    • 제34권1호
    • /
    • pp.37-44
    • /
    • 1997
  • 졸겔법중 딥코팅법을 이용하여 조성비 2Fe/Ba=5.25 졸로부터 바륨페라이트 박막을 제조하였다. 졸의 겔화과정은 4단계로 구분할 수 있으며, 8$0^{\circ}C$에서 90분간 반응시켜 제조한 졸이 코팅용 졸로서 가장 적합한 특성을 나타내었다. 박막층에 형성된 침상 형태의 입자들은 기판에 수평 하게 위치하고 있었으며, 박막 두께가 증가함에 따라 그 경향은 증가하였다. 침상형 입자의 자화용이축 방향은 장축 방향이었다.

  • PDF

Effect of La3+ and Ti4+ Ions on the Magnetic Properties of Barium Hexaferrite Powders Synthesized Using Sol-Gel Method

  • Ertus, Emre Burak;Yildirim, Serdar;Celik, Erdal
    • Journal of Magnetics
    • /
    • 제21권4호
    • /
    • pp.496-502
    • /
    • 2016
  • Doped and undoped barium hexaferrite powders ($BaFe_{12}O_{19}$, $Ba_{0.7}Ti_{0.3}Fe_{12}O_{19}$ and $Ba_{0.7}La_{0.3}Fe_{12}O_{19}$) were produced by the sol-gel method. The effects of substituting elements were studied in terms of the magnetic properties of barium hexaferrite powders. The magnetic properties were remarkably changed by the substitution of $La^{3+}$ and $Ti^{4+}$ ions for the $Ba^{2+}$ ion and were accompanied by oxygen deficiency in the $BaFe_{12}O_{19}$. Coercivities ($H_C$) from 4200 to 5100 Oe, remanences ($M_R$) from 22 to 49 emu/g and saturation magnetizations ($M_S$) from 41 to 73 emu/g were obtained for different samples. The obtained results were discussed in detail.

Ba-Sol을 도포한 $\delta$-FeOOH로부터 Ba-Ferrite 단결정 미리자의 제조와 그 자기적 특성 (The Preparation and Magnetic Properties of Single-Crystallite of Ba-Ferrite from Ba-Sol Coated $\delta$-FeOOH)

  • 박영도;이훈하;이재형;오영우;김태옥
    • 한국세라믹학회지
    • /
    • 제32권12호
    • /
    • pp.1383-1391
    • /
    • 1995
  • Hexagonal $\delta$-FeOOH was coated with Ba-Sol, which was produced by hydrolizing Ba(OC2H5)2, Ba-Sol coated $\delta$-FeOOH spread on a stainless plate, dried at 8$0^{\circ}C$ and then heat-treated. In this way, Ba-ferrite fine particles were produced. although there was a difference in a degree of hydrolysis of Ba(OC2H5)2, crystalline phase of Ba-ferrite appeared around 617$^{\circ}C$, and Ba-ferrite single phase was obtained after heat treatment at 80$0^{\circ}C$ for 2 hr. When Ba-ferrite was made from Ba-Sol coated $\delta$-FeOOH, $\delta$-FeOOH was thermally decomposed to $\alpha$-Fe2O3 at $700^{\circ}C$, producing a porous structure which was observed by TEM photographs. But the porous structure was not observed at 80$0^{\circ}C$. Ba-ferrite, heat-treated at 80$0^{\circ}C$ for 2 hr, had mean particle size of 1000$\AA$, lattice parameter of a0=5.889243 $\AA$ and c0=23.214502 $\AA$, a saturation magnetization ($\sigma$8) of 45.3 emu/g and a coercive force (Hc) of 5200Oe.

  • PDF

Cobalt가 치환된 Barium Ferrite 분말 제조 시 자기적 특성변화 (Changes in Magnetic Properties When Manufacturing Cobalt-substituted Barium Ferrite Powder)

  • 엄명헌;연제욱;이차진;하범용
    • 한국산학기술학회논문지
    • /
    • 제21권10호
    • /
    • pp.30-39
    • /
    • 2020
  • 본 연구에서는 Sol-Gel 방법을 이용하여 단일상의 Barium ferrite 분말을 제조하였으며, 이때 Ba에 대한 Fe(Fe/Ba)의 몰비와 열처리 온도를 달리하여 단일상의 Barium ferrite를 제조하기 위한 최적의 실험조건을 찾고자 하였다. 또한 고밀도 자기기록매체에 사용되기 위한 2.5 ~ 5.5 kOe 크기의 보자력을 가지는 ferrite 미립자 제조를 위해 보자력 제어에 뛰어난 효과를 지닌 cobalt를 첨가제로 하여 cobalt가 치환된 Barium ferrite 미립자를 제조하고 이들에 대한 자기적 특성 변화를 조사하였다. 제조된 Barium ferrite의 결정구조 및 단일상의 합성여부를 확인하기 위해 X-Ray Diffractometer(XRD), Thermogravimetric-Differential Thermal Analysis(TG-DTA), Field Emission Scanning Electron Microscope(FE-SEM)을 이용하여 분석하였으며, 화학적 구조와 조성의 분석을 위해 Fourier Transform Infrared Spectroscopy(FT-IR), Energy Dispersive X-Ray Spectrometer(EDS)를 사용하였다. 또한 Vibrating Sample Magnetometer(VSM)을 통해 cobalt가 치환된 Barium ferrite 분말의 보자력을 측정하였다. 그 결과 단일상의 Barium ferrite는 Fe/Ba의 몰비가 10, 900 ℃의 열처리 온도에서 가장 잘 합성되었다. Co의 첨가량이 증가할수록 보자력은 감소하였으며 Fe에 대한 Co(Co/Fe)의 몰비가 0.16 이내 일 때, 고밀도 자기기록매체에 사용할 수 있는 보자력 값인 2.5 ~ 5.5 kOe를 가지는 Barium ferrite가 합성되었다.

Highly Donor-doped LaxBa1-xTiO3 Ceramics

  • Korobova Nataly;Soh Dea-Wha
    • Transactions on Electrical and Electronic Materials
    • /
    • 제4권4호
    • /
    • pp.18-21
    • /
    • 2003
  • Sol-gel processing of $BaTiO_3$ ceramics doped with La(0.01-1.00 at. $\%$) were prepared from metal barium, titanium n-butoxide and lanthanum iso-propoxide. Characterization of the sol-gel-derived powder using XRD, SEM is also reported. The obtained results showed that insulator to semiconductor transition for highly donor-doped barium titanate was closely related to the incorporation of donor into the grains and to the resultant grain size, which were significantly affected by the sinterability of $BaTiO_3$ powders and sintering conditions used.