• Title/Summary/Keyword: Average grain size

Search Result 610, Processing Time 0.023 seconds

Grain Size and Thickness Effects of Electrical Breakdown Behavior of $BaTiO_3$ Ceramics ($BaTiO_3$ 세라믹스의 절연파괴거동에 미치는 결정립 크기와 시편두께의 영향)

  • 조경호;남효덕;박철우;이희영
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.11
    • /
    • pp.1217-1222
    • /
    • 1996
  • Undoped barium titanate ceramic samples with high density were produced by using both high purity hydro-thermally synthesized and oxalate-derived powders. Sintering temperature was varied in the temperature range 128$0^{\circ}C$-140$0^{\circ}C$ to control the average grain sizes of the samples. Electrical breakdown test was performed at two different temperature with 3$0^{\circ}C$(below Tc) and 15$0^{\circ}C$ (above Tc) for samples immersed in silicon oil bath using 60kV dc power supply. From the experimental results at below and above Curie temperature the grain size and thickness dependence of electrical breakdown strength for BaTiO3 ceramics was presented and breakdown behavior was also studied.

  • PDF

Inheritance of Grain Weight and Size of a High Yielding Japonica cultivar, Sobibyeo (자포니카 다수성 품종 소비벼의 입중과 입형의 유전)

  • Tae Hwan Noh
    • KOREAN JOURNAL OF CROP SCIENCE
    • /
    • v.48 no.3
    • /
    • pp.142-146
    • /
    • 2003
  • To obtain information on the inheritance of grain weight and grain size of japonica cultivar, Sobibyeo which has high yielding potential and large grain in rice, the genetic variation, heritability and phenotypic correlation of 1,000 grain weight, grain length, width and thickness were investigated in two crosses, Iksan 429/Sobibyeo and Iksan 430/Sobibyeo. The gram characteristics of $\textrm{F}_1$ hybrids exceeded mid-parental values, while grain length: width ratio was intermediate between the parents. In $\textrm{F}_2$ populations, the average grain length, width and thickness were intermediate as mid-parental values, but grain weight exceeded the mid-parental values. In $\textrm{F}_2$ populations of Iksan 429/Sobibyeo and Iksan 430/Sobibyeo, mean 1,000 grain weights were 24.86g and 25.04 g on the average, and ranged 18.4g-32.2g and 19.5g-33.4g, respectively. The segregation mode for grain weight was regarded as a nearly normal distribution in two crosses of $\textrm{F}_2$ populations. Estimates of broad sense heritabilities for grain weight in Iksan 429/Sobibyeo and Iksan 430/Sobibyeo were high as 89.00% and 89.06%, and grain length showed the highest heritability among grain characteristics as 97.45% and 97.35%, respectively. Grain weight was highly correlated with grain length, width and thickness, and grain length was highly correlated with grain width and thickness. These grain characteristics were apparently controlled by polygenes. Accordingly, these traits will be readily improved through selection in the early segregating generations.

Evaluation Method for Graphene Grain Boundary by UV/ozone-oxidation Chemical-etching Process (UV/ozone 산화처리 및 화학적 식각공정을 적용한 그래핀 Grain Boundary 평가 방법)

  • Kang, Jaewoon;Park, Hongsik
    • Journal of Sensor Science and Technology
    • /
    • v.25 no.4
    • /
    • pp.275-279
    • /
    • 2016
  • Chemical vapor deposited (CVD) polycrystalline graphene is widely used for various sensor application because of its extremely large surface-to-volume ratio. The electrical properties of CVD-graphene is significantly affected by the grain size and boundaries (GGBs), but evaluation of GGB of continuous monolayer graphene is difficult. Although several evaluation methods such as tunneling electron microscopy, confocal Raman, UV/ozone-oxidation are typically used, they still have issues in evaluation efficiency and accuracy. In this paper, we suggest an improved evaluation method for precise and simple GGB evaluation which is based on UV/ozone-oxidation and chemical etching process. Using this method, we could observe clear GGBs of CVD-graphene layers grown by different process conditions and statistically evaluate average grain sizes varying from $1.69{\sim}4.43{\mu}m$. This evaluation method can be used for analyzing the correlation between the electrical properties and grain size of CVD-graphene, which is essential for the development of graphene-based sensor devices.

Grain Size Dependence of Soft Magnetic Properties in $Fe_{68.5}Co_5M_3Cu_1Si_{13.5}B_9(M=Nb, Mo, Mn, Cr)$ Nanocrystalline Alloys ($Fe_{68.5}Co_5M_3Cu_1Si_{13.5}B_9(M=Nb, Mo, Mn, Cr)$계 초미세결정립합금의 결정립 크기에 따른 자기적 특성의 변화)

  • 조용수;김택기
    • Journal of the Korean Magnetics Society
    • /
    • v.1 no.2
    • /
    • pp.37-41
    • /
    • 1991
  • Amorphous $Fe_{68.5}Co_5M_3Cu_1Si_{13.5}B_9(M=Nb, Mo, Mn, Cr)$ alloys were prepared by using rapidly quenching techinque and were annealed above their crystallization temperatures. Coercive force, initial permeability and AC power loss of the annealed $Fe_{68.5}Co_5M_3Cu_1Si_{13.5}B_9(M=Nb, Mo, Mn, Cr)$ alloys have been studied systematically. Nanocrystallines are formed in the annealed alloys which include Mo and Nb. Remarkably improved soft magnetic properties are obtained in the alloys whose average grain size is around 10 nm. However, soft magnetic properties of the alloys are degraded when grain size is less than IOnm or larger than 15nm. It is considered that the degradation of soft magnetic properties in the alloys whose average grain size is less than 10 nm is due to the Fe-rich amorphous phase retained at grain boundary during the initial crystallization process.

  • PDF

Grain Size Analysis by Hot-Cooling Cycle Thermal Stress at Y-TZP Ceramics using Full Width at Half Maximum(FWHM) of X-ray Diffraction (X-ray 회절의 반치전폭(FWHM)을 이용한 Y-TZP세라믹스에서 반복 열응력에 의한 입계크기 분석)

  • Choi, Jinsam;Park, Kyu Yeol;Kong, Young-Min
    • Korean Journal of Materials Research
    • /
    • v.29 no.4
    • /
    • pp.264-270
    • /
    • 2019
  • As a case study on aspect ratio behavior, Kaolin, zeolite, $TiO_2$, pozzolan and diatomaceous earth minerals are investigated using wet milling with 0.3 pai media. The grinding process using small media of 0.3 pai is suitable for current work processing applications. Primary particles with average particle size distribution D50, ${\sim}6{\mu}m$ are shifted to submicron size, D50 ${\sim}0.6{\mu}m$, after grinding. Grinding of particles is characterized by various size parameters such as sphericity as geometric shape, equivalent diameter, and average particle size distribution. Herein, we systematically provide an overview of factors affecting the primary particle size reduction. Energy consumption for grinding is determined using classical grinding laws, including Rittinger's and Kick's laws. Submicron size is obtained at maximum frictional shear stress. Alterations in properties of wettability, heat resistance, thermal conductivity, and adhesion increase with increasing particle surface area. In the comparison of the aspect ratio of the submicron powder, the air heat conductivity and the total heat release amount increase 68 % and 2 times, respectively.

The Technology for Reducing Abnomal Grain Growth in 3- Roll Type Wire Rod Rolling (3-Roll 선재압연에서의 결정립조대화 방지기술)

  • 임규환;김병홍;김기환;권정석
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1999.08a
    • /
    • pp.163-171
    • /
    • 1999
  • The abnormal grain coarsening in wire rolling induces detrimental defects, such as jagged size tolorance, severe bending after heat treatments and drawing troubles, in the following secondary processes. Neishi et al observed that there is a band type region where grain coarsenting occurs in the plastic strain vs. deformation temperature plot. Based on the finding, we have investigate whether grain sizes and ferrite volume fractions are correlation to deformation strain with three kinds of wire rod diameters as for the different average deformation conditions. The samples were chosen from the No.2 Wire Rod Mill of POSCO where 3-roll type of finishing mill stand are used. It was found in the present work that the grain size and ferrite volume fraction of the rolled and cooled microstructure were changed with rolling reduction and rolling temperature. Abnormally grown grains at various observed points were also found. To have homogeneously fine grains of microstructure from the No. 2 Wire Rod Mill, it will be easier to control finish rolling temperature at around 750$^{\circ}C$ rather than to find another rolling schedule.

  • PDF

A Study on the Mechanical Properties of $ZrO_2$ Based Composite ($ZrO_2$를 이차상으로한 복합체의 기계적 특성)

  • 신동우;김종희
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.5
    • /
    • pp.76-84
    • /
    • 1985
  • Mechanical property enhancing mechanisms of $Al_2O_3-ZrO_2$ two phase ceramic composites were studied for several compositions of different $ZrO_2$/$Al_2O_3$ ratio. Microstructural analysis of $Al_2O_3-ZrO_3$(pure) composites indicated that pre-existing microcrack due to larger $ZrO_2$ particle at grain boundary extended along alumina grain boundaries within process zone. Microcracks also nucleated when very small $ZrO_2$ particles at the grain boundaries transformed to monoclinic phase at near of main crack tip. These types of microcracks could contribute to the toughening achieved by creating additional crack surface area during crack propagation. Microstructural analyses also showed that the average grain size and abnormal grain size of $Al_2O_3$ were decreased with increasing $ZrO_2$ vol% in $Al_2O_3$ matrix. As a result it could be concluded as follows In TEX>$Al_2O_3-ZrO_3$(pure) system 1. Microcrack nucleation (stress-induced microcracking) and extension was effective mechanism for absorpiton of fracture energy 2, More narrow distribution and smaller grain size of $Al_2O_3$ due to $ZrO_2$particles mainly contributed to main-tatin the strength and hardness.

  • PDF

Dielectric Breakdown and Electric Stress Distribution in Ferroelectrics (강유전체에서의 전계분포 및 절연파괴)

  • 신병철;김호기
    • Journal of the Korean Ceramic Society
    • /
    • v.24 no.4
    • /
    • pp.392-396
    • /
    • 1987
  • Pure barium titanate was sintered at $1340^{\circ}C$ for 2, 4, 8, 16 hr to control their grain size. The measurements of breakdown strength and partial discharge characteristics were performed under rising AC voltage(60Hz). With increase of sintering time, the average grain size was increased and breakdown strength was slightly decreased. Partial discharge in pores was observed under high voltage, and a model of dielectric break down in barium titanate ceramics is proposed.

  • PDF

Study on the emulsion and its physical properties (전자현미경(電子顯微鏡) 건판(乾板)의 제작(製作) 및 그 특성(特性) 조사(調査) 연구(硏究))

  • Kim, Hyun-Chang;Pak, Kyoo-Eun
    • Applied Microscopy
    • /
    • v.1 no.1
    • /
    • pp.3-10
    • /
    • 1969
  • By the use of electron microscope, the study has beek made on the grain size in photo graphic emulsions, which are made at different temperature. It is found that ,the optimum temperature is $60^{\circ}C$, at which the average grain size obtained is the biggest. Also electron micrographs show NaCl-type crystal structure of AgBr and AgCl, as we expected.

  • PDF

A Study on Grain Size Dependency of Selected Heavy Metals in the Surface Sediment of Lake Paldang (팔당호 표층 퇴적물에 함유된 중금속의 입도 의존성에 관한 연구)

  • Shin, Kyung-Yong;Jun, Sang-Ho
    • Journal of Environmental Health Sciences
    • /
    • v.38 no.5
    • /
    • pp.424-430
    • /
    • 2012
  • Objective: The purpose of this study was to present the standard deviation of the elemental normalization of concentration of selected heavy metals in the surface sediment of Lake Paldang. Methods: Grain size dependency of selected heavy metal concentrations in the surface sediments of Lake Paldang was analyzed by the extrapolation method. The heavy metal concentrations were the sum of all fractions. Results: Cd and Cu showed an increase of the coefficient of determination($r^2$) in the fractional content of particle size, from <256 ${\mu}m$ to <20 ${\mu}m$, and a decrease from <20 ${\mu}m$ to <1 ${\mu}m$. The normalized concentration of Cd and Cu by extrapolation at 50% <20 ${\mu}m$ were 0.8 mg/kg, 37.0 mg/kg, 57.6 mg/kg and 201.7 mg/kg respectively. Conclusions: The normalized concentrations in the sediment of Lake Paldang are 1.5-2.0 times higher than mean average concentration. We concluded that in interpretation of heavy metal concentration in the sediment of Lake Paldang, normalization of grain size dependency should be considered.