ALD ZnO 버퍼층 증착 온도가 전착 Cu2O 박막 태양전지 소자 특성에 미치는 영향 (The Influence of Deposition Temperature of ALD n-type Buffer ZnO Layer on Device Characteristics of Electrodeposited Cu2O Thin Film Solar Cells)

  • 조재유;트란 휴 만;허재영
    • Current Photovoltaic Research
    • /
    • 제6권1호
    • /
    • pp.21-26
    • /
    • 2018
  • Beside several advantages, the PV power generation as a clean energy source, is still below the supply level due to high power generation cost. Therefore, the interest in fabricating low-cost thin film solar cells is increasing continuously. $Cu_2O$, a low cost photovoltaic material, has a wide direct band gap of ~2.1 eV has along with the high theoretical energy conversion efficiency of about 20%. On the other hand, it has other benefits such as earth-abundance, low cost, non-toxic, high carrier mobility ($100cm^2/Vs$). In spite of these various advantages, the efficiency of $Cu_2O$ based solar cells is still significantly lower than the theoretical limit as reported in several literatures. One of the reasons behind the low efficiency of $Cu_2O$ solar cells can be the formation of CuO layer due to atmospheric surface oxidation of $Cu_2O$ absorber layer. In this work, atomic layer deposition method was used to remove the CuO layer that formed on $Cu_2O$ surface. First, $Cu_2O$ absorber layer was deposited by electrodeposition. On top of it buffer (ZnO) and TCO (AZO) layers were deposited by atomic layer deposition and rf-magnetron sputtering respectively. We fabricated the cells with a change in the deposition temperature of buffer layer ranging between $80^{\circ}C$ to $140^{\circ}C$. Finally, we compared the performance of fabricated solar cells, and studied the influence of buffer layer deposition temperature on $Cu_2O$ based solar cells by J-V and XPS measurements.

유동층 화학기상증착법으로 제조된 TRISO 피복입자의 ZrC 층 미세구조와 경도에 미치는 증착온도의 영향 (Effect of Deposition Temperature on Microstructure and Hardness of ZrC Coating Layers of TRISO-Coated Particles Fabricated by the FBCVD Method)

  • 고명진;김대종;김원주;조문성;윤순길;박지연
    • 한국세라믹학회지
    • /
    • 제50권1호
    • /
    • pp.37-42
    • /
    • 2013
  • Tristructural-isotropic (TRISO)-coated particles were fabricated by a fluidized-bed chemical vapor deposition (FBCVD) method for use in a very high temperature gas-cooled reactor (VHTR). ZrC as a constituent layer of TRISO coating layers was deposited by a chloride process using $ZrCl_4$ and $CH_4$ source gases in a temperature range of $1400^{\circ}C$ and $1550^{\circ}C$. The change in the microstructure of ZrC depending on the deposition temperature and its effect on the hardness were evaluated. As the deposition temperature increased to $1500^{\circ}C$, the grain size of the ZrC increased and the hardness of the ZrC decreased according to the Hall-Petch relationship. However, at $1550^{\circ}C$, the ZrC layer was highly non-stoichiometric and carbon-rich and did not obey the Hall-Petch relationship in spite of the decrease of the grain size. A considerable amount of pyrolytic carbon at the grain boundaries of the ZrC as well as coarse granular pyrolytic carbon were locally distributed in the ZrC layer deposited at $1550^{\circ}C$. Therefore, the hardness decreased largely due to the formation of a large amount of pyrolytic carbon in the ZrC layer.

Layer by Layer 법으로 제작한 박막의 에피택셜 성장 (Epitaxy Growth of the Thin Films Fabricated by Layer by Layer Method)

  • 김태곤;천민우;양승호;박용필;박노봉;이희갑
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.529-530
    • /
    • 2006
  • $Bi_2Sr_2CuO_x$ thin films have been fabricated by atomic layer-by-layer deposition using the ion beam sputtering method. During the deposition, 10 and 90 wt%-ozone/oxygen mixture gas of typical pressure of $1{\sim}9{\times}10^{-5}\;Torr$ are supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal out that a buffer layer with some different compositions is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.

  • PDF

순차 스퍼터법에 의한 Bi-초전도 박막의 제작 (Fabrication of Bi-superconducting Thin Films by Layer-by-layer Sputtering Method)

  • 심상흥;양승호;박용필
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2001년도 하계학술대회 논문집
    • /
    • pp.613-616
    • /
    • 2001
  • Bi$_2$Sr$_2$CuO$_{x}$ thin films have been fabricated by atomic layer-by-layer deposition using ion beam sputtering(IBS) method. During the deposition, 10 and 90 wt%-ozone/oxygen mixture gas of typical pressure of 1~9$\times$10$^{-5}$ Torr are supplied with ultraviolet light irradiation for oxidation. XRD and RHEED investigations reveal out that a buffer layer with some different compositions is formed at the early deposition stage of less than 10 units cell and then Bi-2201 oriented along the c-axis is grown.n.

  • PDF

고분자 전해질 연료전지용 촉매 소재 개발을 위한 원자층증착법 연구 동향 (Recent Research Progress on the Atomic Layer Deposition of Noble Metal Catalysts for Polymer Electrolyte Membrane Fuel Cell)

  • 한정환
    • 한국분말재료학회지
    • /
    • 제27권1호
    • /
    • pp.63-71
    • /
    • 2020
  • It is necessary to fabricate uniformly dispersed nanoscale catalyst materials with high activity and long-term stability for polymer electrolyte membrane fuel cells with excellent electrochemical characteristics of the oxygen reduction reaction and hydrogen oxidation reaction. Platinum is known as the best noble metal catalyst for polymer electrolyte membrane fuel cells because of its excellent catalytic activity. However, given that Pt is expensive, considerable efforts have been made to reduce the amount of Pt loading for both anode and cathode catalysts. Meanwhile, the atomic layer deposition (ALD) method shows excellent uniformity and precise particle size controllability over the three-dimensional structure. The research progress on noble metal ALD, such as Pt, Ru, Pd, and various metal alloys, is presented in this review. ALD technology enables the development of polymer electrolyte membrane fuel cells with excellent reactivity and durability.

Conformal $Al_2$O$_3$ Nanocoating of Semiconductor Nanowires by Atomic Layer Deposition

  • Hwang, Joo-Won;Min, Byung-Don;Kim, Sang-Sig
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • 제3C권2호
    • /
    • pp.66-69
    • /
    • 2003
  • Various semiconductor nanowires such as GaN, GaP, InP, Si$_3$N$_4$, SiO$_2$/Si, and SiC were coated conformally with aluminum oxide (Al$_2$O$_3$) layers by atomic layer deposition (ALD) using trimethylaluminum (TMA) and distilled water ($H_2O$) at a temperature of 20$0^{\circ}C$. Transmission electron microscopy (TEM) revealed that A1203 cylindrical shells conformally coat the semiconductor nanowires. This study suggests that the ALD of $Al_2$O$_3$ on nanowires is a promising method for preparing cylindrical dielectric shells for coaxially gated nanowire field-effect transistors.

표면 반응 제어를 통한 영역 선택적 원자층 증착법 연구 동향 (Area selective atomic layer deposition via surface reaction engineering: a review)

  • 고은총;안지상;한정환
    • 한국표면공학회지
    • /
    • 제55권6호
    • /
    • pp.328-341
    • /
    • 2022
  • Area selective atomic layer deposition (AS-ALD) is a bottom-up nanopattern fabrication method that can grow the ALD films only on the desired substrate areas without using photolithography and etching processes. Particularly, AS-ALD has attracted great attention in the semiconductor manufacturing process due to its advantage in reducing edge placement error by fabricating self-aligned patterns. In this paper, the basic principles and characteristics of AS-ALD are described. In addition, various approaches for achieving AS-ALD with excellent selectivity were comprehensively reviewed. Finally, the technology development to overcome the selectivity limit of AS-ALD was introduced along with future prospects.

Investigation of TaNx diffusion barrier properties using Plasma-Enhanced ALD for copper interconnection

  • 한동석;문대용;권태석;김웅선;황창묵;박종완
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2010년도 제39회 하계학술대회 초록집
    • /
    • pp.178-178
    • /
    • 2010
  • With the scaling down of ULSI(Ultra Large Scale Integration) circuit of CMOS(Complementary Metal Oxide Semiconductor)based electronic devices, the electronic devices become more faster and smaller size that are promising field of semiconductor market. However, very narrow line width has some disadvantages. For example, because of narrow line width, deposition of conformal and thin barrier is difficult. Besides, proportion of barrier width is large, thus resistance is high. Conventional PVD(Physical Vapor Deposition) thin films are not able to gain a good quality and conformal layer. Hence, in order to get over these side effects, deposition of thin layer used of ALD(Atomic Layer Deposition) is important factor. Furthermore, it is essential that copper atomic diffusion into dielectric layer such as silicon oxide and hafnium oxide. If copper line is not surrounded by diffusion barrier, it cause the leakage current and devices degradation. There are some possible methods for improving the these secondary effects. In this study, TaNx, is used of Tertiarybutylimido tris (ethylamethlamino) tantalum (TBITEMAT), was deposited on the 24nm sized trench silicon oxide/silicon bi-layer substrate with good step coverage and high quality film using plasma enhanced atomic layer deposition (PEALD). And then copper was deposited on TaNx barrier using same deposition method. The thickness of TaNx was 4~5 nm. TaNx film was deposited the condition of under $300^{\circ}C$ and copper deposition temperature was under $120^{\circ}C$, and feeding time of TaNx and copper were 5 seconds and 5 seconds, relatively. Purge time of TaNx and copper films were 10 seconds and 6 seconds, relatively. XRD, TEM, AFM, I-V measurement(for testing leakage current and stability) were used to analyze this work. With this work, thin barrier layer(4~5nm) with deposited PEALD has good step coverage and good thermal stability. So the barrier properties of PEALD TaNx film are desirable for copper interconnection.

  • PDF

MOCVD 법에 의해 제조된 $CeO_2$ 버퍼층 증착 거동의 기판 의존성 (Substrate dependence of the deposition behavior of $CeO_2$ buffer layer prepared by MOCVD method)

  • 전병혁;최준규;정우영;이희균;홍계원;김찬중
    • Progress in Superconductivity
    • /
    • 제7권2호
    • /
    • pp.130-134
    • /
    • 2006
  • Buffer layers such as $CeO_2\;and\;Yb_2O_3$ films for YBCO coated conductors were deposited on (100) $SrTiO_3$ single crystals and (100) textured Ni substrates by a metal organic chemical vapor deposition (MOCVD) system of the hot-wall type. The substrates were moved with the velocity of 40 cm/hr. Source flow rate, $Ar/O_2$ flow rate and deposition temperature were main processing variables. The degree of film epitaxy and surface morphology were investigated using XRD and SEM, respectively. On a STO substrate, the $CeO_2$ film was well grown epitaxially above the deposition temperature of $450^{\circ}C$. However, on a Ni substrate, the XRD showed NiO (111) and (200) peaks due to Ni oxidation as well as (111) and (200) film growth. For the films deposited with $O_2$ gas as oxygen source, it was found that the NiO film was formed at the interface between the buffer layer and the Ni substrate. The NiO layer interrupts the epitaxial growth of the buffer layer. It seems that the epitaxial growth of the buffer layer on Ni metal substrates using $O_2$ gas is difficult. We are considering a new method avoiding Ni oxidation with $H_2O$ vapor instead of $O_2$ gas.

  • PDF

Atomic layer deposition of In-Sb-Te Thin Films for PRAM Application

  • Lee, Eui-Bok;Ju, Byeong-Kwon;Kim, Yong-Tae
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.132-132
    • /
    • 2011
  • For the programming volume of PRAM, Ge2Sb2Te5(GST) thin films have been dominantly used and prepared by physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD). Among these methods, ALD is particularly considered as the most promising technique for the integration of PRAM because the ALD offers a superior conformality to PVD and CVD methods and a digital thickness control precisely to the atomic level since the film is deposited one atomic layer at a time. Meanwhile, although the IST has been already known as an optical data storage material, recently, it is known that the IST benefits multistate switching behavior, meaning that the IST-PRAM can be used for mutli-level coding, which is quite different and unique performance compared with the GST-PRAM. Therefore, it is necessary to investigate a possibility of the IST materials for the application of PRAM. So far there are many attempts to deposit the IST with MOCVD and PVD. However, it has not been reported that the IST can be deposited with the ALD method since the ALD reaction mechanism of metal organic precursors and the deposition parameters related with the ALD window are rarely known. Therefore, the main aim of this work is to demonstrate the ALD process for IST films with various precursors and the conformal filling of a nano size programming volume structure with the ALD?IST film for the integration. InSbTe (IST) thin films were deposited by ALD method with different precursors and deposition parameters and demonstrated conformal filling of the nano size programmable volume of cell structure for the integration of phase change random access memory (PRAM). The deposition rate and incubation time are 1.98 A/cycle and 25 cycle, respectively. The complete filling of nano size volume will be useful to fabricate the bottom contact type PRAM.