• 제목/요약/키워드: Al-Si-Fe system

검색결과 109건 처리시간 0.026초

Proximity Effect in Nb/Gd Layers

  • Jung, Dong-Ho;Char, K.
    • Progress in Superconductivity
    • /
    • 제12권2호
    • /
    • pp.110-113
    • /
    • 2011
  • We have grown a Nb/Gd bilayer on a$SiO_2$/Si substrate by using a DC magnetron sputtering system, which was fabricated in situ with silicon stencil masks. In order to investigate proximity effect of the Nb/Gd bilayer, we used a planar tunnel junction with an AlOx tunnel barrier by oxidizing the Al ground electrode at the bottom. A $Co_{60}Fe_{40}$ backing of Al was deposited so as to reduce the superconductivity of the Al, ensuring a normal counterelectrode. With a 50-nm-thick Nb layer, we have measured dI/dV (dynamic conductance) by varying the thickness of Gd, which can reveal the density of states (DOS) of the Nb/Gd bilayer as a function of the Gd thickness resulting from the proximity effect of a superconductor/ferromagnet bilayer (S/F). The SF proximity effect in Nb/Gd will be discussed in comparison to our previous results of the CoFe/Nb, Ni/Nb and CuNi/Nb proximity effect; Gd is expected to show different effects since Gd has f-electrons, while CoFe, Ni, and CuNi have only d-electrons. Our studies will focus on the triplet correlation in a superconducting pair.

A review on thermohydraulic and mechanical-physical properties of SiC, FeCrAl and Ti3SiC2 for ATF cladding

  • Qiu, Bowen;Wang, Jun;Deng, Yangbin;Wang, Mingjun;Wu, Yingwei;Qiu, S.Z.
    • Nuclear Engineering and Technology
    • /
    • 제52권1호
    • /
    • pp.1-13
    • /
    • 2020
  • At present, the Department of Energy (DOE) in Unite State are directing the efforts of developing accident tolerant fuel (ATF) technology. As the first barrier of nuclear fuel system, the material selection of fuel rod cladding for ATFs is a basic but very significant issue for the development of this concept. The advanced cladding is attractive for providing much stronger oxidation resistance and better in-pile behavior under sever accident conditions (such as SBO, LOCA) for giving more coping time and, of course, at least an equivalent performance under normal condition. In recent years, many researches on in-plie or out-pile physical properties of some suggested cladding materials have been conducted to solve this material selection problem. Base on published literatures, this paper introduced relevant research backgrounds, objectives, research institutions and their progresses on several main potential claddings include triplex SiC, FeCrAl and MAX phase material Ti3SiC2. The physical properties of these claddings for their application in ATF area are also reviewed in thermohydraulic and mechanical view for better understanding and simulating the behaviors of these new claddings. While most of important data are available from publications, there are still many relevant properties are lacking for the evaluations.

석류석-사방휘석 지질온도계와 지질학적 응용 (Garnet-Orthopyroxene Geothermometer and Geological Applications)

  • 이한영
    • 자원환경지질
    • /
    • 제21권1호
    • /
    • pp.29-44
    • /
    • 1988
  • 석류석과 사방휘석의 평형관계를 20-45kb, $975-1400^{\circ}C$, FMAS시스템에서 상호역반응 실험을 통해서 연구하였으며 반응 촉매제로써 사용한 PbO와 0.55 $PbF_2$의 혼합물은 매우 효과적이었다. Fe-Mg의 교환반응은 이 실험온도, 압력범위 내에서는 조성성분의 영향을 받지 않는다. 실험결과와 석류석의 혼합 모델을 사용한 석류석-사방휘석의 지질온도계는 다음과 같다. $$T^{\circ}C=(1971+11.91P(Kb)+1510(X_{Ca}+X_{Mn})^{Gt}/(lnK_D+0.96)-273$$.

  • PDF

플라이애쉬-점토-광미계의 소결특성 (The sintering characteristics of fly ash-clay system with mine tailing)

  • 김경남;우동명;박현
    • 한국결정성장학회지
    • /
    • 제21권6호
    • /
    • pp.259-265
    • /
    • 2011
  • 본 연구는 석탄회(Fly Ash)와 점토를 이용하여 광미(tailing)의 중금속 안정화를 연구하였다. 플라이애쉬-점토-광미계의 특성은 여러 분석기기(SEM, XRD, XRF, TG-DTA, Dilatometer, UTM)를 이용하여 광미의 첨가량에 따른 물리 화학적 특성을 조사하였다. 플라이애쉬의 화학조성은 $SiO_2$가 33.01 wt%, $Al_2O_3$는 28.54 wt%, CaO가 9.97 wt%이고 이외에 $Fe_2O_3$와 알카리 성분 등을 함유하고 있으며, 강열감량은 플라이애쉬가 20.26 wt%로 나타났다. 플라이애쉬의 $SiO_2$$Al_2O_3$ 조성양은 점토성분이 61 wt% 이상이다. 그리고 광미의 화학조성은 $SiO_2$가 26.91 wt%, CaO가 24.25 wt%, $Fe_2O_3$는 22.97 wt%이다. 그러므로 플라이애쉬-점토-광미계에서 플라이애쉬가 점토의 원료로 대체가 가능하다. 시편의 수축은 $850^{\circ}C$ 부근에서 서서히 수축이 시작되어 $1100^{\circ}C$ 부근에서 급격하게 수축하는 것을 볼 수 있었으며 플라이애쉬의 탄화 분해 과정에 의해 영향을 받는다. 시편의 미세구조는 광미를 첨가한 시편이 치밀하였다. 열처리 온도에 따른 물리적 특성 조사를 위하여 흡수율과 압축강도를 측정하였으며 광미를 첨가한 시편의 압축강도가 높으며 약 200~420 kgf/$cm^2$로 KS L 4201의 점토 블록 기준 내에 있다. 그리고 광미의 중금속의 안정화는 소결한 후에 한국폐기물 규격내에서 안정화한 것을 알 수 있다.

고전도성 부품용 Al-Fe-Zn-Cu합금의 물성 및 주조성 (Properties and Casting Capabilities of Al-Fe-Zn-Cu Alloys for High Conductivity Parts)

  • 윤호섭;김정민;박준식;김기태;고세현
    • 한국주조공학회지
    • /
    • 제33권6호
    • /
    • pp.242-247
    • /
    • 2013
  • The most widely utilized commercial, aluminum-casting alloys are based on an aluminum-silicon system due to its excellent casting, and good mechanical, properties. Unfortunately, these Al-Si based alloys are inherently poor energy conductors; compared to pure aluminum, because of their high silicon content. This means that they are not suitable for applications demanding high eletrical or thermal conductivity. Therefore, efforts are currently being made to develop new, highly-conductive aluminum-casting alloys containing no silicon. In this research, a number of properties; including potential for castability, were investigated for a number of Al-Fe-Zn-Cu alloys with varying Cu content. As the copper content was increased, the tensile strength of Al-Fe-Zn-Cu alloy tended to increase gradually, while the electrical conductivity was slightly reduced. Fluidity was found to be lower in high-Cu alloys, and susceptibility to hot-cracking was generally high in all the alloys investigated.

MAGNETORESISTANCE OF NiFeCo/Cu/NiFeCo/FeMn MULTILAYERED THIN FILMS WITH LOW SATURATION FIELD

  • Bae, S.T.;Min, K.I.;Shin, K.H.;Kim, J.Y.
    • 한국자기학회지
    • /
    • 제5권5호
    • /
    • pp.570-574
    • /
    • 1995
  • Magnetoresistance of NiFeCo/Cu/NiFeCo/FeMn uncoupled exchange biased sandwiches has been studied. The magnetoresistance change ratio, ${\Delta}R/R_{s}$ showed 4.1 % at a saturation field as low as 11 Oe in $Si/Ti(50\;{\AA})/NiFeCo(70\;{\AA})/Cu(23\;{\AA})/NiFeCo(70\;{\AA})/FeMn(150\;{\AA})/Cu(50\;{\AA})$ spin valve structure. In this system, the magnetoresistance was affected by interlayer material and thickness. When Ti and Cu were used as the interlayer material in this structure, maximum magnetoresistance change ratio were 0.32 % and 4.1 %, respectively. 6.1 % MR ratio was obtained in $Si/Ti(50\;{\AA})/NiFeCo(70\;{\AA})/Cu(15\;{\AA})/NiFeCo(70\;{\AA})/FeMn(150\;{\AA})/Cu(50\;{\AA})$ spin valve structure. The magnetoresistance change ratio decreased monotonically as the interlayer thickness increased. It was found that the exchange bias field exerted by FeMn layer to the adjacent NiFeCo layer was ~25 Oe, far smaller than that reported in NiFe/Cu/NiFe/FeMn spin valve structure(Dieny et. al., ~400 Oe). The relationship between the film texture and exchange anisotropy ha been examined for spin valve structures with Ti, Cu, or non-buffer layer.

  • PDF

둔전금광산 북광상에서 산출되는 다상포유물내의 고상 (Solid Phases in Polyphase Inclusions from North Ore Deposits, Dunjeon Gold Mine)

  • 박희인;이찬희
    • 자원환경지질
    • /
    • 제24권1호
    • /
    • pp.1-8
    • /
    • 1991
  • North ore deposits of the Dunjeon gold mine is disseminated-stockworks deposits emplaced in Ordovician Dongjeom quartzite. Six types of fluid inclusions are recongnized in the stage I quartz. Among them polyphase inclusions(type-IV-A, B) are predominent in the lower part of stage I quartz crystals whereas liquid and gas inclusions(type I, II) are abundant in the upper part of the same quartz crystals. Liquid $CO_2$-bearing inclusions(type III-A, B)occur as pseudosecondary inclusions. Solid phases in polyphase inclusions are identified by using scanning electron microscopy combined with energy dispersive x-ray spectroscopy. The solid phases are as follows; halite, sylvite, hydrophyllite, quartz, muscovite, calcite, ankerite, K-Mg-Fe-Al-Si mineral, Ca-Fe-Si mineral, Mg-Al-Si mineral, two kinds of Fe-mineral and Cu-Fe mineral. Results of freezing and heating experiments of fluid inclusions and identification of daughter minerals in polyphase inclusions in the stage I quartz reveal that ore fluids were high saline system NaCl-KCl-$CaCl_2$-$H_2O$ in the earier stage and then evolved to rather simple system NaCl-$H_2O$ in the later stage, and temporally fluid mixing occured with system $CO_2$-$H_2O$. Homogenization temperatures and salinity of fluid inclusions in the stage I range from 290 to $454^{\circ}C$ and from 0.2 to 54.2 wt. % equivalent to NaCl.

  • PDF

Clay-EAF Dust계 소지의 소결온도 범위에 미치는 Al2O3의 영향 (The Effect of Al2O3 upon Firing Range of Clay-EAF Dust System Body)

  • 김광수;강승구;이기강;김유택;김영진;김정환
    • 한국세라믹학회지
    • /
    • 제40권5호
    • /
    • pp.494-500
    • /
    • 2003
  • 금속 제련공정에서 배출되는 특정폐기물인 EAF(Electrical Arc furnace) dust를 점토와 혼합하여 건축용 벽돌을 제조함에 있어 A1203의 첨가가 소결범위에 미치는 영향을 연구하였다. $Al_2$O$_3$ 첨가되지 않은 시편은 1200-125$0^{\circ}C$에서 과량의 액상에 의해 기포가 형성되고 개기공(open pores)이 감소함으로 겉보기 밀도가 크게 감소하였으며 125$0^{\circ}C$ 이상에서는 기포가 시편 외부로 소멸되어 흡수율이 증가되었다. 그러나 $Al_2$O$_3$가 첨가된 Clay-Dust 계 소결체는 1200-125$0^{\circ}C$ 구간에서 소결온도에 따른 밀도 변화율이 크게 감소되었고, 125$0^{\circ}C$ 이상에서는 흡수율(%)의 증가율이 둔화되었다. $Al_2$O$_3$가 첨가되지 않은 시편은 1275$^{\circ}C$에서 소결된 경우 cristobalite상이 주된 상인 반면, mullite(3Al$_2$O$_3$ 2SiO$_2$)상은 소량 합성되었고, 원료성분인 hematite(FeAl$_2$O$_4$)는 소멸되지 않아 액상이 과량 생성되는 조성임을 확인하였다. 반면 $Al_2$O$_3$가 l5 wt% 첨가된 시편의 경우, 1275$^{\circ}C$에서 cristobalite는 완전 소멸되고 mullite상이 합성되어 주상이 되며, hematite 상이 일부 AI$_2$O$_3$와 반응하여 hercynite(FeAl$_2$O$_4$)상을 형성하여 액상 생성량이 많지 않을 것으로 분석되었다. 이상의 결과로부터 Clay-Dust계에 $Al_2$O$_3$를 첨가하면 액상의 발생량과 특성 및 결정상 종류를 변화시켜줌으로써 시편물성의 변화율을 감소시켜 소결온도 범위를 넓히는 효과가 있는 것으로 분석되었다.

Formation of $Al_O_3$Barrier in Magnetic Junctions on Different Substrates by $O_2$Plasma Etching

  • Wang, Zhen-Jun;Jeong, Won-Cheol;Yoon, Yeo-Geon;Jeong66, Chang-Wook;Joo, Seung-Ki
    • Journal of Magnetics
    • /
    • 제6권3호
    • /
    • pp.90-93
    • /
    • 2001
  • Co/$Al_O_3$/NiFe and CO/$Al_O_3$/Co tunnel junctions were fabricated by a radio frequency magnetron sputtering at room temperature with hard mask on glass and $4^{\circ}$ tilt cut Si (111) substrates. The barrier layer was formed through two steps. After the Al layer was deposited, it was oxidized in the chamber of a reactive ion etching system (RIE) with $O_2$plasma at various conditions. The dependence of the TMR value and junction resistance on the thickness of Al layer (before oxidation) and oxidation parameters were investigated. Magnetoresistance value of 7% at room temperature was obtained by optimizing the Al layer thickness and oxidation conditions. Circular shape junctions on $4^{\circ}$tilt cut Si (111) substrate showed 4% magnetoresistance. Photovoltaic energy conversion effect was observed with the cross-strip geometry junctions on Si substrate.

  • PDF

Characterization of Solidification and Microstructure of an Al-Zn-Mg-Si Alloy

  • He Tian;Dongdong Qu;Zherui Tong;Nega Setargew;Daniel J. Parker;David StJohn;Kazuhiro Nogita
    • Corrosion Science and Technology
    • /
    • 제23권2호
    • /
    • pp.104-112
    • /
    • 2024
  • Al-Zn-Mg-Si alloy coatings have been developed to inhibit corrosion of cold rolled steel sheets, and an understanding of the alloy system helps prevent coating defects. We used a Bridgman furnace to characterise the nature and formation mechanisms of the phases present in the quaternary system with 0.4 wt% Fe. In the directional solidification experiments we imposed steep temperature gradients and varied the pull rate. After the samples were quenched in the furnace, detailed characterization of the samples was carried out by electron microscopy (SEM/EDS). From the dT/dt vs T plots of the cooling curves of the alloys, the solidification path was determined to be $Liquid{\longrightarrow[80]^{544-558}}{\alpha}-Al{\longrightarrow[80]^{453-459}}Al/Mg_2Si{\longrightarrow[80]^{371-374}}Al/Zn{\longrightarrow[80]^{331-333}}Zn/mgZn_2$. The formation mechanisms of the Mg and Zn containing phases and their morphology was discussed together with the effects of the cooling rate. Key findings include the lengthening of the mushy zone in directionally solidified samples remelted against a positive temperature gradient, as well as an enrichening of the α-Al phase by Zn through remelting. Mg2Si and other Si based phases were observed to adopt a much finer faceted microstructure in favour of a script-like microstructure when exposed to the higher cooling rate of coolant quenching.