• 제목/요약/키워드: Al$_2$TiO$_5$

검색결과 523건 처리시간 0.036초

침입형 및 치환형 화합물을 함유한 Ti 정밀주조용 Al2O3 주형의 α-case 계면반응 거동 (α-case Interfacial Reaction Behavior of Al2O3 Mold Containing Interstitial and Substitutional Compounds for Titanium Investment Casting)

  • 최봉재;이슬;김영직
    • 대한금속재료학회지
    • /
    • 제49권7호
    • /
    • pp.577-582
    • /
    • 2011
  • The newly developed ${\alpha}-case$ controlled mold material for Ti investment castings was suggested in this research. The $Al_2O_3$ mold containing interstitial $TiO_2$ and substitutional $Ti_3Al$ was manufactured by the reaction between $Al_2O_3$ and Ti. It is obvious that as the $TiO_2$ and $Ti_3Al$ content in the mold surface were increased, the depth of the interfacial reaction was significantly reduced. In addition, substitutional $Ti_5Si_3$ in the mold surface owing to the reaction between Ti and $SiO_2$ from the binder was effective for ${\alpha}-case$ reduction. Therefore, the ${\alpha}-case$ reduction was accomplished by the diffusion barrier effect of interstitial $TiO_2$, substitutional $Ti_3Al$ and $Ti_5Si_3$.

소결조제와 열처리 분위기가 $(1-x)CaTiO_3-xLaAlO_3$ 계의 소결 및 마이크로파 유전특성에 미치는 영향 (Effect of Sintering Additives and Annealing Atmospheres on the Microwave Dielectric and Sintering Characteristics of $(1-x)CaTiO_3-xLaAlO_3$ System)

  • 이경태;여동훈;문종하
    • 한국세라믹학회지
    • /
    • 제34권6호
    • /
    • pp.629-635
    • /
    • 1997
  • The effects of the annealing atmospheres(O2, N2) and sintering additives that Bi2O3 is a major composition on the microwave dielectric and sintering propertie of (1-x)CaTiO3-xLaAlO3 system were investigated. The annealing atmospheres and the increase of annealing time after sintering did not affect the relative dielectric constant($\varepsilon$r) and temperature coefficient of resonant frequency($\tau$f) of (1-x)CaTiO3-xLaAlO3 system. However, the Q.f0 values of (1-x)CaTiO3-xLaAlO3 were very sensitive to annealing atmospheres. As the annealing time increased under O2 atmosphere the Q.f0 values of (1-x)CaTiO3-xLaAlO3 enhanced untill 10 hrs in 0.3$\leq$x$\leq$0.6 region, but degraded over that time. The increasing rate of Q.f0 value increased wth increasing x. On the other hand, as the annealing time increased under N2 atmosphere the Q.f0 values were constant in x$\leq$0.6 region, increased gradually in x$\geq$0.7 region. When 0.97Bi2O3-0.03Al2O3 and 0.76Bi2O3-0.24NiO of 3wt% as sintering additives were added to (Ca0.5La0.5) (Ti0.5Al0.5)O3 (x=0.5) the sintering temperature of 1$600^{\circ}C$ was lowered to 140$0^{\circ}C$, and the relative dielectric constant($\varepsilon$r) and temperature coefficient of resonant frequency($\tau$f) were not nearly changed. The addition of 0.97Bi2O3-0.03Al2O3 and 0.76Bi2O3-0.24NiO of 3wt% to (Ca0.5La0.5)(Ti0.5Al0.5)O3 made the Q.f0 values to be lower about 15% and 34%, respectively.

  • PDF

알루미늄 폐드로스를 활용한 SCR 탈질촉매 제조 및 특성평가 (Characteristic Evaluation of SCR catalyst using Aluminum dross)

  • 배민아;김홍대;이만식
    • 한국산학기술학회논문지
    • /
    • 제14권10호
    • /
    • pp.4672-4678
    • /
    • 2013
  • 알루미늄 금속이 용해될 시 대기와 접촉한 용탕 표면에서 생성되는 알루미늄 드로스는 알루미늄 생산 공정에서 발생되는 필수적인 부산물이다. 그러나 알루미늄 드로스의 대부분은 매립에 의한 처리가 이루어지고 있어 환경오염의 원인이 되고 있다. 본 연구에서는 알루미늄 드로스를 재자원화 하여 SCR(Selective Catalytic Reduction) 촉매의 담체에 일부 대체하는 연구를 진행하였다. 재활용 된 알루미늄 드로스를 촉매 원료 $WO_3$, $V_2O_5$, $TiO_2$와 혼합하여 $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR촉매를 제조하였다. 제조 된 $V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR촉매는 XRD, XRF, BET 분석을 통해 특성평가를 진행 하였으며, 내구성 평가를 통해 $Al_2O_3$ 함량이 증가할수록 V$V_2O_5-WO_3/TiO_2-Al_2O_3$ SCR촉매의 강도가 증가하는 것을 확인 할 수 있었다. MR(Micro-Reactor)을 이용한 촉매 활성평가를 진행하여 촉매의 실사용 온도 $350^{\circ}C{\sim}400^{\circ}C$에서 90%이상의 촉매효율을 나타내었다.

Synthesis of Metallic Gold Colored α-Al2O3 Nanoplate-TiO2 Core-Shell Pigments with Robust and Photo-Stable Smooth TiO2 Shell

  • Lee, Su Jin;You, Myoung Sang;Park, Jin Kyoung;Park, Bum Jun;Im, Sang Hyuk
    • 공업화학
    • /
    • 제31권4호
    • /
    • pp.390-397
    • /
    • 2020
  • To synthesize non-corrosive metallic gold colored α-Al2O3 nanoplate-TiO2 core-shell pigments with controlled roughness, we systematically checked the morphological variation of the TiO2 shell with the mole ratio of TiCl4 and NaOH from 1 : 1 to 1 : 1.5, 1 : 2, 1 : 2.5, 1 : 3, 1 : 3.5, and 1 : 4. The more increased mole ratio of TiCl4 and NaOH resulted in the smoother TiO2 shell due to the promoted formation of anatase TiO2 than that of the rutile one. By the heat-treatment of pigments at 500 ℃, we could improve the adhesiveness between TiO2 shell and α-Al2O3 nanoplates without changing their topology and roughness. In addition, the α-Al2O3 nanoplate with the robust TiO2 by heat-treatment exhibited comparable photo-stability against photo-catalytic degradation by UV exposure compared with the commercially available α-Al2O3/TiO2 lustering pigment.

Effect of Al2O3 Addition and WO3 Modification on Catalytic Activity of NiO/Al2O3-TiO2/WO3 for Ethylene Dimerization

  • Pae, Young-Il;Sohn, Jong-Rack
    • Bulletin of the Korean Chemical Society
    • /
    • 제28권10호
    • /
    • pp.1763-1770
    • /
    • 2007
  • Strong solid acid catalysts, NiO/Al2O3-TiO2/WO3 for ethylene dimerization were prepared by the addition of Al2O3 and the modification with WO3. The acid sites and acid strength were increased by the inductive effect of WO3 species bonded to the surface of catalysts. The larger the dispersed WO3 amount, the higher both the acidity and catalytic activity for ethylene dimerization. The addition of Al2O3 to TiO2 up to 5 mol% enhanced acidity and catalytic activity gradually due to the interaction between Al2O3 and TiO2 and consequent formation of Al-O-Ti bond.

반응결합 강화 알루미나세라믹스의 제조에 관한 연구 (A Study on the Fabrication of Reinforced Reaction Bonded Alumina Ceramics)

  • 김일수;강민수;박정현
    • 한국세라믹학회지
    • /
    • 제35권4호
    • /
    • pp.311-318
    • /
    • 1998
  • The reaction bonded alumina ceramics with reinforced particles which have low shrinkage were pro-duced by blending of SiC or TiC or ZrO2 powders to the mixture of Al metal and Al2O3 powder. The powd-ers were attrition milled isostantically pressed and preheated tio 110$0^{\circ}C$ with a heating rate of $1.5^{\circ}C$/min The specimens were then sintered at the temperature range 1500 to 1$600^{\circ}C$ for 5 hours with a heating rate of 5$^{\circ}C$/min. The specimens showed 5-9% weight gain and 2-9% dimensional expansion through the complete oxidation of Al after preheating up to 11--$^{\circ}C$ the overall dimensional change of the specimens after the reaction sintering at 1500-1$600^{\circ}C$ was 6-12% The maximum densities were 92% theoretical. The fine grain-ed(average grain size :0.4 ${\mu}{\textrm}{m}$) microstructure were observed in the specimen with ZrO2 and SiC. But the microstructure of specimen with TiC was relatively coarse.(average grain size : 2.1 ${\mu}{\textrm}{m}$) The mullite phase was formed by the reaction of Al2O3 and SiO2 in a specimen with SiC. In the TiC contained specimen TiC was oxidized into TiO2 and finally reacted with Al2O3 to form Al2TiO5 during sintering.

  • PDF

삼광 금-은 광상에서 산출되는 함 티타늄 광물들의 산상 및 화학조성 (Occurrence and Chemical Composition of Ti-bearing Minerals from Samgwang Au-ag Deposit, Republic of Korea)

  • 유봉철
    • 광물과 암석
    • /
    • 제33권3호
    • /
    • pp.195-214
    • /
    • 2020
  • 삼광 금-은 광상은 과거 한국에서 가장 큰 금-은 광상들 중의 하나였다. 이 광상은 선캠브리아기의 변성퇴적암류내에 발달된 열극대를 충진한 8개조의 석영맥으로 구성된 조산형 금-은 광상이다. 이 광상에서 함 티타늄 광물로는 설석, 티탄철석 및 금홍석이며 설석과 티탄철석은 모암에서만 산출되나 금홍석은 모암과 엽리상 석영맥에서 산출된다. 이들 광물들은 모암에선 흑운모, 백운모, 녹니석, 백색운모, 모나자이트, 저어콘 및 인회석과 엽리상 석영맥에선 백색운모, 녹니석 및 유비철석 등과 함께 산출된다. 설석은 최대 3.94 wt.% (Al2O3), 0.49 wt.% (FeO), 0.52 wt.% (Nb2O5), 0.46 wt.% (Y2O3) 및 0.43 wt.% (V2O5) 값을 갖는다. 이 설석은 0.06~0.14 (Fe/Al 비) 값으로 변성기원의 설석이고 XAl (=Al/Al+Fe3++Ti) 값이 0.06~0.15 값으로 저 함량 알루미늄 설석에 해당된다. 티탄철석은 최대 0.07 wt.% (ZrO2), 0.12 wt.% (HfO2), 0.26 wt.% (Nb2O5), 0.04 wt.% (Sb2O5), 0.13 wt.% (Ta2O5), 2.62 wt.% (As2O5), 0.29 wt.% (V2O5), 0.12 wt.% (Al2O3), 1.59 wt.% (ZnO)로써 As2O5 함량이 높게 산출된다. 금홍석의 화학조성은 모암과 엽리상 석영맥에서 각각 최대 0.35 wt.%, 0.65 wt.% (HfO2), 2.52 wt.%, 0.19 wt.% (WO3), 1.28 wt.%, 1.71 wt.% (Nb2O3), 0.03 wt.%, 0.07 wt.% (Sb2O3), 0.28 wt.%, 0.21 wt.% (As2O5), 0.68 wt.%, 0.70 wt.% (V2O3), 0.48 wt.%, 0.59 wt.% (Cr2O3), 0.70 wt.%, 1.90 wt.% (Al2O3), 4.76 wt.%, 3.17 wt.% (FeO)로써 엽리상 석영맥의 금홍석에서 HfO2, Nb2O3, As2O5, Cr2O3, Al2O3 및 FeO 원소들의 함량이 모암의 금홍석보다 높지만 WO3 원소의 함량은 낮다. 이 미량원소들은 모암의 금홍석[(Fe3+, Al3+, Cr3+) + Hf4++(W5+, As5+, Nb5+) ⟵⟶; 2Ti4++ V4+, 2Fe2++(Al3+, Cr3+) + Hf4++(W5+, As5+, Nb5+) ⟵⟶ 2Ti4++2V4+], 엽리상 석영맥의 금홍석 [(Fe3+, Al3+) + As5+ ⟵⟶ Ti4++ V4+, (Fe3+, Al3+) + As5+ ⟵⟶ Ti4++Hf4+, 4(Fe3+, Al3+) ⟵⟶ Ti4++(W5+, Nb5+) + Cr3+]로써 치환관계가 있었다. 이들 자료를 근거로, 모암내 산출되는 설석, 티탄철석 및 금홍석은 광역변성작용 동안 모암광물들의 변질 시 광물내 존재했던 W5+, Nb5+, As5+, Hf4+, V4+, Cr3+, Al3+, Fe3+, Fe2+ 등과 같은 양이온들의 재 용해 및 농집에 의해 형성되었다. 그후 계속된 연성전단 시 엽리상 석영맥내 금홍석은 열수 용액의 유입에 따른 백색운모와 녹니석의 모암변질작용에 의한 양이온들의 재 용해 및 재 농집과 더불어 초기에 형성된 설석, 티탄철석 및 금홍석과의 반응에 의해 기존에 이들 광물내에 존재하였던 Nb5+, As5+, Hf4+, Cr3+, Al3+, Fe3+, Fe2+과 같은 양이온들의 재농집에 의해 형성된 것으로 생각된다.

Ti-34wt%Al-1.5wt%Mn 합금의 고온산화에 미치는 $Y_2O_3$ 분산입자 첨가효과 (The Effect of $Y_2O_3$ Dispersoids on the High Temperature Oxidation of Ti-34wt%Al-1.5wt%Mn Alloys)

  • 이동복
    • 한국표면공학회지
    • /
    • 제39권6호
    • /
    • pp.288-294
    • /
    • 2006
  • Alloys of TiAl-Mn-(0, 5, 10)wt.% $Y_2O_3$ were prepared by a powder metallurgical route, and their oxidation behavior was studied at 800, 900 and $1000^{\circ}C$ in 1 atm of air. The scale formed on the alloys consisted of $TiO_2$ and $Al_2O_3$ oxides. During oxidation, Mn tended to diffuse outward, whereas oxygen diffused inward. The dispersoids of $T_2O_3$, which segregated at the matrix grain boundaries, acted as a diffusion channel for cations and oxygen ions, nucleation sites for oxides, and vacancy annihilation sites. $T_2O_3$ increased the scale thickness, but improved the scale adherence.

BaTiO$_3$ 세라믹스의 전기저항에 미치는 첨가제와 냉각속도의 영향(I) - TiO$_2$, SiO$_2$ 및 Al2O$_3$ 단미첨가 - (Effect of Additives and Cooling Rates on the Electrical Resistivity of BaTiO3 Ceramics (I))

  • 염희남;하명수;이재춘;정윤중
    • 한국세라믹학회지
    • /
    • 제28권9호
    • /
    • pp.661-666
    • /
    • 1991
  • Microstructure, room temperature resistivity and temperature coefficient of resistance of BaTiO3 ceramics were studied by varying cooling rates and additives such as TiO2, SiO2 and Al2O3. The basic composition of the BaTiO3 ceramics was formed by adding 0.25 mol% Dy2O3 and 0.07 mol% MnO2 to the BaTiO3 composition. Unlike the additives of SiO2 and Al2O3, an addition of 2 mol% TiO2 to the basic composition was effective to control the grain size of the fired specimens. The room temperature resistivity and the temperature coefficient of resistance for the specimen of this particular compostion were measured as about 102 ohm.cm and 16.5%/$^{\circ}C$, respectively. The observed grain boundary phase of the sample with Al2O3 additive was BaTi3O7, while that of the samples with SiO2 additive was confirmed as BaTiSiO5.

  • PDF

Fabrication and Machinability of Mullite-ZrO2-Al2TiO5 Ceramics

  • Shin, Young Been;Lee, Won Jae;Kim, Il Soo
    • 한국세라믹학회지
    • /
    • 제52권6호
    • /
    • pp.423-428
    • /
    • 2015
  • The machinability of materials is an important factor in engineering applications. Many ceramic components that have complex shapes require machining, typically using diamond tools, which leads to high production cost. Machinable ceramics containing h-BN have recently been developed, but these materials are very expensive because of high cost of raw materials and machining. Therefore the development of low-cost machinable ceramics is desirable. In this study, mullite-$ZrO_2$ ceramics were prepared additions of $Al_2TiO_5$. $ZrSiO_4$, $Al_2O_3$, and $Al_2TiO_5$ powders mixed at various molar ratios with sintering at 1400, 1500, and $1600^{\circ}C$ for 1 hr. Phase formation and microstructure of the sintered ceramics were observed by XRD and SEM, respectively. The machinability of each specimen was tested using the micro-hole machining method. The machinability results show that the ceramics sintered at temperatures over $1500^{\circ}C$ can be used as good low-cost machinable mullite-$ZrO_2-Al_2TiO_5$ ceramics.