• Title/Summary/Keyword: Ag Powder

Search Result 319, Processing Time 0.033 seconds

Structural Properties of PZT BT Mulitilayered Films (PZT BT 이종 박막의 구조적 특성)

  • Lee, Sang-Heon;Lim, Sung-Soo;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 2005.07c
    • /
    • pp.1960-1961
    • /
    • 2005
  • Ploycrystalline $Pb(Zr_{0.5},Ti_{0.5})O_3$ and $BaTiO_3$ powder were prepared by sol-gel process. The alumina substrate were sintered at $1400^{\circ}C$ with bottom electrode of Pt for 2 hours. The Pb(Zr0.5, Ti0.5)O3/BaTiO3 multilayered thick films with laminating times were fabricated on alumina substrate by screening printing method. The obtained thick films were sintered at $800^{\circ}C$ with upper electrode of Ag paste for 1 hour, Structural properties of Pb(Zr0.5,Ti0.5)O3/BaTiO3 multilayered thick films were investigated. As a result of the Differential Thermal Analysis(DTA) of Pb(Zr0.5,Ti0.5)O3, exothermic peak was observed at around $650^{\circ}C$. The X-ray diffraction (XRD) patterns indicated that BaTiO3 and Pb(Zr0.5,Ti0.5)O3 phases and porosities were formed in the interface of Pb(Zr0.5,Ti0.5)O3 / EaTiO3 multilayered thick films.

  • PDF

Ac Loss Characteristics under Critical Current Degradation of HTS Tapes (고온 초전도체의 임계전류 저하에 따른 교류 손실 특성)

  • Kim, Hae-Joon;Kim, Jae-Ho;Sim, Ki-Deok;Cho, Jeon-Wook;Kwag, Dong-Soon;Kim, Hae-Jong;Seong, Ki-Chul
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.286-287
    • /
    • 2005
  • Critical current(Ic) degradation of HTS tapes and AC loss under mechanical load is one of the hottest issues in HTS development and application. Mechanical load reduces the critical current of superconducting wire, and the Ie degradation affects the AC loss of the wire. We measured the Ie degradation and AC loss under tension and bending of Bi-2223 tapes processed by "Powder-in-Tube" technique at 17K with self-field. And we have studied the frequency dependence of self-field AC loss in multi-filamentary Bi-2223/Ag tape at 77K. The measurement results and discussions on the relationship between Ic degradation and AC loss are presented.

  • PDF

Electrochromic Performance of NiOx Thin Film on Flexible PET/ITO Prepared by Nanocrystallite-Dispersion Sol

  • Kwak, Jun Young;Jung, Young Hee;Park, Juyun;Kang, Yong-Chul;Kim, Yeong Il
    • Journal of the Korean Chemical Society
    • /
    • v.65 no.2
    • /
    • pp.125-132
    • /
    • 2021
  • An electrochromic nickel oxide thin film was fabricated on a flexible PET/ITO substrate using a nanocrystallite- dispersed coating sol and bar coater. Nanocrystalline NiOx of 3-4 nm crystallite size was first synthesized by base precipitation and thermal conversion. This NiOx nanocrystallite powder was mechanically dispersed in an alcoholic solvent mixed with a silane binder to prepare a coating sol for thin film. This sol method is different from the normal sol-gel method in that it does not require the conversion of precursor by heat treatment. Therefore, this method provides a very facile method to prepare NiOx thin films on any kind of substrate and it can be easily applied to mass production. The electrochromic performance of this NiOx thin film on PET/ITO electrode with a thickness of about 400 nm was investigated in a nonaqueous LiClO4 electrolyte solution by cyclic voltammetric and repeated chronoamperometric measurements in conjunction with spectrophotometry. The visible light modulation of 44% and the colorization efficiency of 41 ㎠/C at 550 nm were obtained at the step potentials of -0.8/+1.2 V vs Ag and a duration of 30 s.

Transient Liquid Phase Diffusion Bonding Technology for Power Semiconductor Packaging (전력반도체 접합용 천이액상확산접합 기술)

  • Lee, Jeong-Hyun;Jung, Do-hyun;Jung, Jae-Pil
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.25 no.4
    • /
    • pp.9-15
    • /
    • 2018
  • This paper shows the principles and characteristics of the transient liquid phase (TLP) bonding technology for power modules packaging. The power module is semiconductor parts that change and manage power entering electronic devices, and demand is increasing due to the advent of the fourth industrial revolution. Higher operation temperatures and increasing current density are important for the performance of power modules. Conventional power modules using Si chip have reached the limit of theoretical performance development. In addition, their efficiency is reduced at high temperature because of the low properties of Si. Therefore, Si is changed to silicon carbide (SiC) and gallium nitride (GaN). Various methods of bonding have been studied, like Ag sintering and Sn-Au solder, to keep up with the development of chips, one of which is TLP bonding. TLP bonding has the advantages in price and junction temperature over other technologies. In this paper, TLP bonding using various materials and methods is introduced. In addition, new TLP technologies that are combined with other technologies such as metal powder mixing and ultrasonic technology are also reviewed.

Preparation of BaTiO3 Powder in $BaO2-TiO2-Reduction Agent-PSCA (Particle Size Control Agent) System by SHS and Its Dielectric Properties (B3O2-TiO2-환원제-입자제어제계에서 자전연소합성법에 의한 BaTiO3분말의 제조 및 유전특성)

  • Yun, Ki-Seok;Lim, Sung-Jae;Nersisyan, Hayk;Won, Chang-Whan
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.11
    • /
    • pp.842-850
    • /
    • 2004
  • We have investigated on the preparation of BaTiO$_3$ powder at the system of BaO$_2$-TiO$_2$-Reduction ag.-PSCA by SHS. C and Mg were used as reduction agent, and NaCl was used as PSCA (Particle Size Control Agent). The effects of the various reduction agent and its concentration, particle size control agent, reaction mixture mass on the product in the preparation of BaTiO$_3$ powder at the optimum system by SHS were investigated. The optimum conditions for reaction system and composition were BaO$_2$+TiO$_2$+0.11 Mg +0.2C+0.75NaCl in the As atmosphere. NaCl as PSCA showed the effect of controlling the particle size of product as well as the combustion temperature. The particle size of BaTiO$_3$ synthesized at the optimum condition was about 0.5 ${\mu}{\textrm}{m}$. And as the mixture mass for the reaction was increased, the more stable combustion wave appeared. We have conducted the sintering experiment at the temperature of 130$0^{\circ}C$, the time of 2 h and the atmosphere of air to measure the dielectric properties of BaTiO$_3$ synthesised in this work, and the sample sintered in this condition showed 2,290 of dielectric constant at 10$0^{\circ}C$ and 13,890 at curie point (129$^{\circ}C$).

Application in Conductive Filler by Low-Temperature Densification and Synthesis of Core-Shell Structure Powder for Prevention from Copper Oxidation (구리 산화 방지를 위한 Core-Shell 구조 입자 합성과 저온 치밀화를 통한 도전성 필러 응용)

  • Shim, Young Ho;Park, Seong-Dae;Kim, Hee Taik
    • Applied Chemistry for Engineering
    • /
    • v.23 no.6
    • /
    • pp.554-560
    • /
    • 2012
  • Recently, it has been increasing trend to use conductive materials as electronics and communication technology in electronics industry are developing. The noble metal such as Ag, Pt, Pd etc. are mostly used as conductive materials, To reduce production cost, alternative materials with similar characteristics of noble metals are needed. Copper has advantages, i.e its electronic properties are similar to noble metals and low cost than noble metal, but its use has been restricted because of oxidation in air. In this study, the tin film was coated on copper by electroless plating to protect copper from oxidation and to confirm the effects of temperature, pH, amount of $SnCl_2$, and feeding speed in plating conditions. Additionally, we apply $Cu_{core}Sn_{shell}$ powder as conductive filler with low-temperature densification and analysis by SEM, XRD, FIB and 4-Point Probe techniques. As result of the study, tin film was coated well on copper and was protected from oxidation. After low-temperature densification treatment, the meted tin made chemical interconnections with copper. Accordingly, conductivity was increased than before condition. We hope $Cu_{core}Sn_{shell}$ powder to replace noble metals and use in the electronic field.

Effects of Solder Particle Size on Rheology and Printing Properties of Solder Paste (미세피치 접합용 솔더 페이스트의 솔더 분말 크기에 따른 레올로지 및 인쇄 특성 평가)

  • Jun, So-Yeon;Lee, Tae-Young;Park, So-Jeong;Lee, Jonghun;Yoo, Sehoon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.29 no.2
    • /
    • pp.91-97
    • /
    • 2022
  • The wettability and rheological properties of solder paste with the size of the solder powder were evaluated. To formulate the solder paste, three types of solder powder were used: T4 (20~28 ㎛), T5 (15~25 ㎛), and T6 (5~15 ㎛). The viscosities of the T4, T5, and T6 solder pastes at 10 RPM were 155, 263, and 418 Pa·s, respectively. After 7 days, the viscosity of the T4 solder paste slightly increased by 2.6% and that of T5 was increased by 20.6%. The viscosity of the T6 solder paste after 7 days could not be measured due to high viscosity. The viscosity variation with solder particle size also affected on the printability of the solder. In the case of the T4 solder paste, printability, slump, bridging, and soldering properties were excellent. On the other hand, T5 showed slight dewetting and solder ball defects. Especially, T6, which the smallest powder size, showed poor printability and dewetting at the edge of solder.

Studies on the Cellulase produced by Myriococcum of albomyces (Myriococcum albomyces가 생산하는 Cellulase에 관한 연구)

  • Chung, Dong-Hyo
    • Applied Biological Chemistry
    • /
    • v.14 no.1
    • /
    • pp.59-97
    • /
    • 1971
  • As a study on the cellulase of Myriococcum albomyces the culture media for enzyme formation and properties of its crude preparation were investigated and the crude enzyme preparation was further fractionated. The results are summarized as follows: 1. Wheat bran solid culture produced stronger activities of cellulase than rice bran or defatted soy bean meal solid culture. 2. Shaking culture with wheat bran, rice bran or defatted soy bean meal produced higher cellulase activities than solid culture with the corresponding media. 3. The enzyme formation was higher at $45^{\circ}C$ than at $37^{\circ}C$ or $50^{\circ}C$ regardless of the kind of culture medium. 4. The formation of CMCase activity was more promoted by organic nitrogen source than inorganic nitrogen source. 5. The formation of cellulase activities were increased 1.5 to 3.0-fold by adding CMC, Avicel or cellulose powder as an inducer into 5% wheat bran basal medium. 6. Cellulase production using a tank culture procedure with addition of CMC or Avicel as an inducer was the highest at fifth day and thereafter decreased slightly. 7. The crude enzyme preparation showed pH optimum in 4.0 to 4.5, and pH stability in the range of 3.5 to 8.0. Optimum temperature for the activity was $65^{\circ}C$ which was higher than among other cellulases and it was stable at $60^{\circ}C$ for 120 minutes. 8. Dialyzed crude enzyme was activated by $Ca^{++}$ and $Mg^{++}$, but inhibited by $Hg^{++}$, $Cu^{++}$ and $Ag^{+}$. 9. Four different types of cellulase, i. e., fraction I, fraction II-a, fraction II-b, and fraction III were purified from the culture filtrate of Myriococcum albomyces through a sequence of ammonium sulfate fractionation, and elution chromatography on DEAE-Sephadex A-25, Amberlite CG-25 type 2 and hydroxyapatite columns. 10. These four cellulase fractions were showed to be homogenous by electrophoresis and ultracentrifugation and also gave a typical ultraviolet absorption spectrum of protein. 11. Four purified fraction showed different specificity toward substrates, fraction I has a stronger activity toward Avicel, cellulose powder, and gauze than that of other cellulase fractions. Fraction II-a had a powerful activity toward cellobiose but it was almost inactive agaisnt fibrous cellulose contrary to fraction I. On the contrary, the main component fraction II-b had a fairly higher activity on CMC and Avicel. Activity of fraction II-b toward cellobiose was about one-third of that of fraction II-a and activity on Avicel was lower than that of fraction I. Fraction III had a more powerful activity in decreasing viscosity of CMC. 12. Final hydrolysis products of fibrous cellulose by each fraction were cellobiose and glucose. Whereas oligosaccharides were predominant in the early stage of hydrolysis, prolonged reaction produced more glucose than cellobiose. Fraction I and fraction II-a acted synergically on Avicel. 13. Optimum pH for the activities of cellulase fraction I, fraction II-a, fraction II-b and fraction III were found to be 5.5, 5.0, 4.0 and $4.0{\sim}4.5$, respectively. These fractions were found to be stable in the range of pH $3.0{\sim}7.5$. 14. Optimum temperature for the activities of fraction I, fraction II-a, fraction II-b, and fraction III were $50^{\circ}C$, $55^{\circ}C$, $60^{\circ}C$ and $55^{\circ}C$, respectively. No less of activity was found by heating 120 minutes at $55^{\circ}C$ and fraction II-a was more stable than the others at $60^{\circ}C$. 15. Fraction I and fraction II-b were activated by $Ca^{++}$ and $Mg^{++}$ but inhibited by $Hg^{++}$ and $Ag^{+}$.

  • PDF

Geochemical Enrichment and Migration of Environmental Toxic Elements in Stream Sediments and Soils from the Samkwang Au-Ag Mine Area, Korea (삼광 금-은광산 일대의 하상퇴적물과 토양내 함유된 독성원소의 지구화학적 부화와 이동)

  • Lee, Chan Hee;Lee, Byun Koo;Yoo, Bong-Cheal;Cho, Aeran
    • Economic and Environmental Geology
    • /
    • v.31 no.2
    • /
    • pp.111-125
    • /
    • 1998
  • Dispersion, migration and enrichment of environmental toxic elements from the Samkwang Au-Ag mine area were investigated based upon major, minor and rare earth element geochemistry. The Samkwang mine area composed mainly of Precambrian granitic gneiss. The mine had been mined for gold and silver, but closed in 1996. According to the X-ray powder diffraction, mineral composition of stream sediments and soils were partly variable mineralogy, which are composed of quartz, orthoclase, plagioclase, amphibole, muscovite, biotite and chlorite, respectively. Major element variations of the host granitic gneiss, stream sediments and soils of mining and non-mining drainage, indicate that those compositions are decrese $Al_2O_3$, $Fe_2O_3$, MgO, $TiO_2$, $P_2O_5$ and LOI with increasing $SiO_2$ respectively. Average compositional ranges (ppm) of minor and/or environmental toxic elements within those samples are revealed as As=<2-4500, Cd=<1-24, Cu=6-117, Sb=1-29, Pb=17-1377 and Zn=32-938, which are extremely high concentrations of sediments from the mining drainage (As=2006, Cd=l1, Cu=71, Pb=587 and Zn=481 ppm, respectively) than concentrations of the other samples and host granitic gneiss. Major elements (average enrichment index=6.53) in all samples are mostly enriched, excepting $SiO_2$, $Na_2O$ and $K_2O$, normalized by composition of host granitic gneiss. Rare earth element (average enrichment index=2.34) are enriched with the sediments from the mining drainage. Minor and/or environmental toxic elements within all samples on the basis of host rock were strongly enriched of all elements (especially As, Br, Cu, Pb and Zn), excepting Ba, Cr, Rb and Sr. Average enrichment index of trace elements in all samples is 15.55 (sediments of mining drainage=37.33). Potentially toxic elements (As, Cd, Cr, Cu, Ni, Pb, and Zn) of the samples revealed that average enrichment index is 46.10 (sediments of mining drainage=80.20, sediments of nonmining drainage=5.35, sediments of confluent drainage=20.22, subsurface soils of mining drainage=7.97 and subsurface soils of non-mining drainage=4.15). Sediments and soils of highly concentrated toxic elements are contained some pyrite, arsenopyrite, sphalerite, galena and goethite.

  • PDF

A Study to Recover Si from End-of-Life Solar Cells using Ultrasonic Cleaning Method (초음파 세척법을 이용한 사용 후 태양광 셀로부터 Si 회수 연구)

  • Lee, Dong-Hun;Go, Min-Seok;Wang, Jei-Pil
    • Resources Recycling
    • /
    • v.30 no.5
    • /
    • pp.38-48
    • /
    • 2021
  • In this study, we determine the optimal process conditions for selectively recovering Si from a solar cell surface by removal of impurities (Al, Zn, Ag, etc.). To selectively recover Si from solar cells, leaching is performed using HCl solution and an ultrasonic cleaner. After leaching, the solar cells are washed using distilled water and dried in an oven. Decompression filtration is performed on the HCl solution, and ICP-OES (Inductively Coupled Plasma Optical Emission spectroscopy) full scan analysis is performed on the filtered solution. Furthermore, XRD (X-ray powder diffraction), XRF (X-ray fluorescence), and ICP-OES are performed on the dried solar cells after crushing, and the purity and recovery rate of Si are obtained. In this experiment, the concentration of acid solution, reaction temperature, reaction time, and ultrasonic intensity are considered as variables. The results show that the optimal process conditions for the selective recovery of Si from the solar cells are as follows: the concentration of acid solution = 3 M HCl, reaction temperature = 60℃, reaction time = 120 min, and ultrasonic intensity = 150 W. Further, the Si purity and recovery rate are 99.85 and 99.24%, respectively.