Electrochemical Evaluation of Si-Incorporated Diamond-Like Carbon (DLC) Coatings Deposited on STS 316L and Ti Alloy for Biomedical Applications

  • Kim, Jung-Gu;Lee, Kwang-Ryeol;Kim, Young-Sik;Hwang, Woon-Suk
    • Corrosion Science and Technology
    • /
    • 제6권1호
    • /
    • pp.18-23
    • /
    • 2007
  • DLC coatings have been deposited onto substrate of STS 316L and Ti alloy using r.f. PACVD (plasma-assisted chemical vapor deposition) with a mixture of $C_{6}H_{6}$ and $SiH_{4}$ as the process gases. Corrosion performance of DLC coatings was investigated by electrochemical techniques (potentiodynamic polarization test and electrochemical impedance spectroscopy) and surface analysis (scanning electron microscopy). The electrolyte used in this test was a 0.89% NaCl solution of pH 7.4 at temperature $37^{\circ}C$. The porosity and protective efficiency of DLC coatings were obtained using potentiodynamic polarization test. Moreover, the delamination area and volume fraction of water uptake of DLC coatings as a function of immersion time were calculated using electrochemical impedance spectroscopy. This study provides the reliable and quantitative data for assessment of the effect of substrate on corrosion performance of Si-DLC coatings. The results showed that Si-DLC coating on Ti alloy could improve corrosion resistance more than that on STS 316L in the simulated body fluid environment. This could be attributed to the formation of a dense and low-porosity coating, which impedes the penetration of water and ions.

Elastic Wave Properties of STS316L with Different Subzero Temperature and Time (서브제로 온도 및 시간이 다른 STS316L의 탄성파 특성)

  • Lee, Gum-Hwa;Gu, Kyoung-Hee;Tak, Young-Joon;Kwon, Yung-Kug;Shin, Ki-Hang;Nam, Ki-Woo
    • Journal of the Korean Society of Industry Convergence
    • /
    • 제25권5호
    • /
    • pp.783-789
    • /
    • 2022
  • In this study, STS316L rolled at five rolling degrees were treated with two types of subzero temperatures for 10, 30, and 60 minutes, respectively, and the dominant frequencies of elastic waves was investigated. The dominant frequency was higher as the subzero temperature was lower and the subzero treatment time was longer at each rolling degree. On the other hand, the dominant frequency was higher as the elongation decreased. In the time-frequency analysis for subzero temperature and time of the specimen with a rolling degree of 33%, the dominant frequency was higher at a subzero temperature of -196℃ than -50℃ regardless of subzero treatment time.

Electrochemical Corrosion Damage Characteristics of Alumium Alloy and Stainless Steel with Sea Water Concentration (알루미늄 합금 및 스테인리스강의 해수 농도 변화에 따른 전기화학적 부식 손상 특성)

  • Park, Il-Cho;Kim, Young-Bok;Kim, Seong-Jong
    • Journal of the Korean institute of surface engineering
    • /
    • 제50권4호
    • /
    • pp.259-265
    • /
    • 2017
  • 5000 series aluminium alloys and austenitic stainless steels have excellent corrosion resistance and sufficient strength, which are widely used as materials for marine equipment and their parts in the marine environment. The corrosion characteristics of materials are important factors for selecting the appropriate material due to fluid component changes in the estuarine and coastal areas where seawater and fresh water are mixed. Therefore, for 5083 Al alloy, STS304 and STS316L widely used in the marine environment, anodic polarization experiments were performed to compare the corrosion damage characteristics of each material by three kinds of solutions of 100 % tap water, 50 % tap water+50 % natural seawater and 100 % natural seawater. As a result of the anodic polarization experiments, aluminum alloy (5083) caused locally corrosion on the surface in the tap water, and corrosion damage occurred all over the surface when the seawater was included. Stainless steels (STS304 and STS316L) presented almost no corrosion damage in tap water, but they grew pitting corrosion damage with increasing seawater concentration. STS316L showed better corrosion resistance than STS304.

Eddy Current and Ultrasonic IRIS Signal Characteristics of Reboiler Tube by Using STS 316L Calibration Specimen (STS 316L 교정시험편을 이용한 재가열기 튜브의 와전류신호와 초음파 IRIS 신호 특성)

  • Tak, Kyeong-Joo;Kim, Byung-Il;Gook, Jin-Seon
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • 제32권1호
    • /
    • pp.56-63
    • /
    • 2012
  • In this study, a field applicability of reboiler tube was evaluated by comparing ECT signal with IRIS signal about wall loss rate and remaining wall thickness using worked austenite STS 316L ASME standard calibration tube. In the case of wall-loss rate, as a result, tolerance about $20%{\times}4$ flat bottom hole and 10% O D groove(ECT), 80% defect and 10% O D groove(IRIS) occurred up to ${\pm}15%$. In the case of remaining wall thickness, ECT was satisfied with the both tolerance, but tolerance about 80% defect occurred up to ${\pm}15%$ in IRIS. Therefore, if the IRIS is performed for interpretation of non-relevant indication and measurement of wall-loss rate after ECT, reliability is supposed to be improved.

The Oxidation Behavior of Sintered STS 316L at High-Temperature in the Air (STS 316L 소결체의 대기중 고온산화 거동)

  • Kim, Hye Seong;Lee, Jong Pil;Park, Dong Kyu;Ahn, In Shup
    • Journal of Powder Materials
    • /
    • 제20권6호
    • /
    • pp.432-438
    • /
    • 2013
  • In this study, analysis on the oxidation behavior was conducted by a series of high-temperature oxidation tests at both $800^{\circ}C$, $900^{\circ}C$ and 1000 in the air with sintered STS 316L. The weight gain of each oxidized specimen was measured, the oxidized surface morphologies and composition of oxidation layer were analyzed with Scanning Electron Microscope-Energy Dispersive x-ray Spectroscopy (SEM-EDS), finally, the phase change and composition of the oxidized specimen were shown by X-Ray Diffraction (XRD). As a result, the weight gain increased sharply at $1000^{\circ}C$ when oxidation test was conducted for 210 hours. Also, a plentiful of pores were observed in the surface oxidation layers at $900^{\circ}C$ for 210 hours. In addition, the following conclusions on oxidation behavior of sintered STS 316L can be obtained: $Cr_2O_3$ can be formed on pores by influxing oxygen through open-pores, $(Fe_{0.6}Cr_{0.4})_2O_3$ can be generated on the inner oxidation layer, and $Fe_2O_3$ was on the outer oxidation layer. Also, $NiFe_2O_4$ could be precipitated if the oxidation time was kept longer.

Study on Microstructures and Hardness of STS316L Fabricated by Selective Laser Melting (선택적 레이저 용융공정을 이용한 316L 스테인리스강 분말 3차원 조형체의 미세조직 및 경도 연구)

  • Shin, Gi Hun;Choi, Joon Phil;Kim, Kyung Tae;Kim, Byoung Kee;Yu, Ji Hun
    • Journal of Powder Materials
    • /
    • 제24권3호
    • /
    • pp.210-215
    • /
    • 2017
  • In this study, STS316L powders prepared by gas atomization are used to manufacture bulk structures with dimensions of $10{\times}10{\times}10mm^3$ using selective laser melting (SLM). The microstructures and hardness of the fabricated 316L stainless steel has been investigated with the laser beam overlap varied from 10% to 70%. The microstructures of the fabricated STS316L samples show a decrease in the balling and satellite of powders introducing defect in the bulk samples and the porosity caused by the gap between the molten metal pools disappearing as the overlap ratio increases, whereas a low overlap ratio results in significant balling and a large amount of isolated powders due to the increased gap between the melt pools. Furthermore, the highest value in Vickers hardness is obtained for the sample fabricated by 30% overlapped laser beams. These results show that the overlap ratio of laser beams in the SLM process should be considered as an important process parameter.

CREEP-FATIGUE CRACK GROWTH AND CREEP RUPTURE BEHAVIOR IN TYPE 316 STAINLESS STEELS- EFFECT OF HOLD TIME AND AGING TREATMENT

  • Mi, J.W.;Won, S.J.;Kim, M.J.;Lim, B.S.
    • International Journal of Automotive Technology
    • /
    • 제1권2호
    • /
    • pp.71-77
    • /
    • 2000
  • High temperature materials in service are subjected to mechanical damage due to operating load and metallurgical damage due to operating temperature. Therefore, when designing or assessing life of high temperature components, both factors must be considered. In this paper, the effect of tensile hold time on high temperature fatigue crack growth and long term prior thermal aging heat treatment on creep rupture behavior were investigated using STS 316L and STS 316 austenitic stainless steels, which are widely used for high temperature components like in automotive exhaust and piping systems. In high temperature fatigue crack growth tests using STS 316L, as tensile hold time increased, crack growth rate decreased in relatively short tensile hold time region. In long term aged specimens, cavity type microcracks have been observed at the interface of grain boundary and coarsened carbide.

  • PDF

Applications of Micro-Droplet Cell to Study of Localized Corrosion Resistance of Stainless Steels (스테인리스강의 국부부식 저항성 연구에 미세방울셀의 응용)

  • Kim Sung-Yu;Kim Hee-San
    • Journal of the Korean Electrochemical Society
    • /
    • 제9권2호
    • /
    • pp.70-76
    • /
    • 2006
  • Micro-droplet cell with free droplet as a micro-electrochemical technique has been limited to apply to electrochemical systems with high wetting properties such as an acidic solution and low grade stainless steels(Type 316L). By loading negative pressure to a droplet, control of droplet size, and use of hydrophobic gasket, the cell is modified to be allowed to use for electrochemical systems with high wetting properties. For giving the reliability of new cell, studies on local corrosion were conducted for three different systems-an acidic chloride solution and high chromium ferritic stainless steel, the other acidic chloride solution and type 316, and a neutral chloride solution and type 316. stainless steel. Firstly, the modified micro-droplet cell allows the anodic polarization curves in an acidic chloride solution to show the fact that the local corrosion of high chromium stainless steel near the $\alpha/\sigma$ interface is due to the Cr depleted zone. Secondly, the local anodic polarization test of type 316 L in the other acidic chloride solution can be successfully conducted in the cell. Furthermore, the local polarization curves help elucidating the corrosion of type 316 with $\delta-ferrite$ phase. Finally, the polarization curves of type 316 L in a neutral chloride solution indicates that the factor affecting the pitting corrosion resistance was inclusions rather than $\delta-ferrite$.

Creep Life Prediction of Friction Welded Joints (Cu-Alloy/STS316L) for Nuclear Power Plant (원자력 발전소용 마찰용접재 (Cu합금/STS316L)의 크리프 수명예측)

  • 유인종;공유식;오세규;김선진
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 한국해양공학회 2001년도 추계학술대회 논문집
    • /
    • pp.258-263
    • /
    • 2001
  • In this paper, the real-time prediction of high temperature creep life was carried out for the friction welded joints of dissimilar heat resistintg steels (CulCr0.5Zr-STS316L). Various life prediction methods such as LMP (Larson-Miller Parameter) and ISM (initial strain method) were applied. The creep behaviors of those steels and the welds under static load were examined by ISM combined with LMP at 300, 400 and 50$0^{\circ}C$, and the relationship between these two methods was investigated. A real-time creep life (tsub/r/, hr) prediction equation by initial strain ($\varepsilon_0$, %) under any creep stress ($\sigma$, MP$\alpha$) at any high temperature (T, K) was developed

  • PDF

Corrosion Resistance Characteristics of Cr-free Coating Solution for Degraded STS316L (열화한 STS316L에 대한 Cr-free 코팅액의 내식특성)

  • Lee, So-Young;Kim, Young-Soo;Jeong, Hee-Rock;Ahn, Seok-hwan;Nam, Ki-Woo
    • Journal of Ocean Engineering and Technology
    • /
    • 제29권6호
    • /
    • pp.475-480
    • /
    • 2015
  • In this study, we developed a Cr-free organic/inorganic hybrid solution and investigated its coating properties on degraded STS316L. Both the OIBD-1 solution and OIBD-2 solution had excellent corrosion resistance and adhesion ability. However, the solution had some problems in a boiling water environment. In addition, the flexibility was excellent, and the scratch resistance was relatively good.