Research of Optimum Reflow Process Condition for 0402 Electric Parts (0402칩의 무연솔더링 최적공정 연구)

  • Bang, Jung-Hwan;Lee, Se-Hyung;Shin, Yue-Seon;Kim, Jeong-Han;Lee, Chang-Woo
    • Journal of Welding and Joining
    • /
    • v.27 no.1
    • /
    • pp.85-89
    • /
    • 2009
  • Reflow process conditions were investigated for 0402 electric parts with Sn-3.0Ag-0.5Cu solders. Circle hole shape metal mask with 100 m thickness showed excellent printability. Self alignment abilities were 71% for 1005 chips, 52% for 0603 chips, and 3% for 0402 chips. Average joining strengos were 1990 gf for 1005 chips, 867 gf for 0603 chips, and 525 gf for 0402 chips. As mis-mounting angle increased, joining strength decreased. Considering self-alignment ability, mounting angle had to be under $5^{\circ}$ and contact area of the chips had to be over 40% for Pb-free soldering process for 0402 chips.

Evaluation of Solder Printing Efficiency with the Variation of Stencil Aperture Size (스텐실 개구홀 크기 변화에 따른 솔더프린팅 인쇄효율 평가)

  • Kwon, Sang-Hyun;Kim, Jeong-Han;Lee, Chang-Woo;Yoo, Se-Hoon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.18 no.4
    • /
    • pp.71-77
    • /
    • 2011
  • Main parameters of the screen printing were determined and the printing parameters were optimized for 0402, 0603, and 1005 chips in this study. The solder pastes used in this study were Sn-3.0Ag-0.5Cu and Sn-0.7Cu. The process parameters were stencil thickness, squeegee angle, printing speed, stencil separating speed and gap between stencil and PCB. The printing pressure was fixed at 2 $kgf/cm^2$. From ANOVA results, the stencil thickness and the squeegee angle were determined to be main parameters for the printing efficiency. The printing efficiency was optimized with varying two main parameters, the stencil thickness and the squeegee angle. The printing efficiency increased as the squeegee angle was lowered under 45o for all chips. For the 0402 and the 0603 chips, the printing efficiency increased as the stencil thickness decreased. On the other hand, for the 1005 chip, the printing efficiency increased as the stencil thickness increased.