Journal of the Korea institute for structural maintenance and inspection
/
v.11
no.2
/
pp.117-124
/
2007
An experimental research has been performed to evaluate the load transfer capacity for the planar joints between existing and new slab in an apartment remodelling constructions expecially for enlarging the interior space. Post-installed dowel bars were used as a joint connector. The existing slabs were obtained from the existing apartment housing which will be demolished, and were retrofitted with carbon fiber plate. Test results showed that the planar joints with post-installed dowel bars behaved in full composite modes until ultimate capacity of test specimens, so sufficient ultimate and serviceability performance are confirmed.
Steel Plate for Rebar Connection was recently developed to splice rebars in delayed slab-wall joints in high-rise building, slurry wall-slab joints, temporary openings, etc. It consists of several couplers and a thin steel plate with shear key. Cyclic loading tests on slab-wall joints were conducted to verify structural behavior of the joints having Steel Plate for Rebar Connection. For comparison, joints with Rebend Connection and without splices were also tested. The joints with Steel Plate for Rebar Connection showed typical flexural behavior in the sequence of tension re-bar yielding, sufficient flexural deformation, crushing of compression concrete, and compression rebar buckling. However, the joints with Rebend Connection had more bond cracks in slabs faces and spalling in side cover-concrete, even though elastic behavior of the joints was similar to that of the joints with Steel Plate for Re-bar Connection. Consequently, the joints with Rebend Connection had less strengths and deformation capacities than the joints with Steel Plate for Re-bar Connection. In addition, stiffness of the joints with Rebend Connection degraded more rapidly than the other joints as cyclic loads were applied. This may be caused by low elastic modulus of re-straightened rebars and restraightening of kinked bar. For two types of diameters (13mm and 16mm) and two types of grades (SD300 and SD400) of rebars, the joints with Steel Plate for Rebar Connection had higher strength than nominal strength calculated from actual material properties. On the contrary, strengths of the joints with Rebend Connection decreased as bar diameter increased and as grade becames higher. Therefore, Rebend Connection should be used with caution in design and construction.
Journal of the Korea institute for structural maintenance and inspection
/
v.14
no.6
/
pp.179-187
/
2010
Corrosion of rebar embedded reinforced concrete is the main cause of collapse and degradation of reinforced concrete structure. Degradation occurs in reinforced concrete structures from corrosion caused by the Chloride that the damage other than the severe degradation of the structure in terms of maintenance and construction when the huge expense required and deciding terms is hard. Therefore, early detection of rebar corrosion is important for efficient maintenance and repairing and planning. Meanwhile, how to evaluate the corrosion of the non-destructive measurements have been used a lot. In particular CM-II (corrosion meter) is used to measurement the natural potential, polarization resistance and the resistivity of the concrete, but has some disadvantages. Embedded mini-sensor has been developed in order to overcome these disadvantages. So Measurement corrosion for using the mini-sensor compares with the measured results CM-II (corrosion meter), the developed mini-sensor verify the validity.
Kim, Woo-Hyoun;Lee, Hyoung-Seok;Kim, Young-Sik;Park, Sung-Moo
Journal of Korean Association for Spatial Structures
/
v.5
no.2
s.16
/
pp.65-71
/
2005
The reinforced concrete becomes deteriorated. In strengthening of reinforced concrete structure, it is recently useing FRP. In research, flexural strengthening of reinforced concrete beam can be Efficient design. But shear srengthening og reinforced concrte beam can't be Efficient design by variable cause. The purpose of this study is to investigate the shear resisting effect of filling-up CFRP in reinforced concrete beams with web reinforced. Ten specimens were manufactured and tested. In the test result, it was analysis. The main variables in the test were a space of web reinforcement and a direction of CFRP.
This study was evaluated in the performance of the connection according to the details of the concrete casing segment in the prestressed composite girder by fabricating and testing specimens with different segments. A total of four comparative specimens were fabricated by using the variables of general composite girders, reinforcement or non-reinforcement, and details of reinforcing bars in the segments so as to evaluate the structural behavior of steel girders. In addition, the possibility of non-cracking grade design of segmented composite girders as well as the effects of stiffness and strength according to the loop connection types after cracking were analyzed, and the appropriateness of the crack width control both the embedded steel plate and the concrete surface were evaluated.
Park, Jae-Sung;Yoon, Yong-Sik;Park, Ki-Tae;Kwon, Sung-Jun
Journal of the Korean Recycled Construction Resources Institute
/
v.5
no.1
/
pp.53-58
/
2017
FRP Hybrid Bar, composed of an embedded steel and the coated composites with epoxy and glass fiber, is an effective construction material with tension-hardening performance and lightweight. The epoxy exposed to UV(Ultra Violet Rays) and FT(Freezing and Thawing) action easily shows a surface deterioration, which can cause degradation of bonding strength between inside-steel and outside-concrete. In the present work, surface inspection for 3 different samples of normal steel, FRP Hybrid Bar before UV, and FRP Hybrid Bar after UV test was performed, then concrete samples with 3 reinforcement types were prepared for accelerated FT test. Through visual inspection on 3 typed reinforcement, no significant deterioration like chalking was evaluated. The results from FT test to 120 and 180 cycles showed FRP Hybrid Bar exposed to UV test has higher bonding strength than normal steel by 106.3% due to enlarged bond area by silica coating. The 3 cases showed a similar bond strength tendency with increasing FT cycles, however a relatively big deviations of bond strength were evaluated in FRP Hybrid Bar after UV test due to loss of silica coating.
As it is important to measure the degree of the deterioration and predict service life caused by chloride in concrete structure the methods of measuring chloride in the concrete is raised important problems. This study is to set a new standard for using of the colorimetric method through grasping the character of the colorimetric distinction method, and measuring the chloride content at the place discolored. Also, to predict chloride content around embeded bar and time reaching limit chloride concentration through measuring the chloride content of concrete surface by colorimetric distinction method and this study presents the new concept of concrete degradation and diagnosis of the durability by salt damage. According the results, it is possible to use colorimetric distinction method as simplified measurement to measure the fixed quantity of the chloride concentration. What is more, it would make calculation of concrete surface chloride had a wide fluctuation at the general environment extended. Also, it would be make estimating durability of reinforced concrete structures applied to the basic data.
Journal of the Korea institute for structural maintenance and inspection
/
v.25
no.6
/
pp.60-67
/
2021
In lately, it's been developed and used a system of using deck plates as formwork in order to solve various problems caused by conventional formwork system. This system is more economical and has higher constructability than the conventional system by permanently embedding most of deck plates into the members. However, for this kind of embedded deck plates formwork system, it's been reported that it is difficult to verify filling of concrete in members like beams with narrow width and complicated rebar arrangement. In addtion, there are several problems such as corrosion of deck plates in terms of constructability and maintenance. Therefore, in this study, it is attempted to develop a removal-deck plate formwork system for beams by removing deck plates after concrete curing. The system consists of a deck plate module that acts as form, a frame preventing deformation by concrete lateral pressure, stirrup frame, and connector that combines these. As a result of this research, it is verified that it has higher constructability, efficiently prevents deformation caused by concrete lateral pressure and could be easily removed in the developed formwork system.
Journal of the Korea institute for structural maintenance and inspection
/
v.25
no.4
/
pp.28-36
/
2021
It is known that buried rebars inside concrete structures are protected from corrosion due to passive layer. It is very important to delay the timing of corrosion or evaluate a detection of corrosion initiation for the purpose of cost-beneficiary service life of a structure. In this study, corrosion monitoring was performed on concrete specimens considering 3 levels of cover depth(60 mm, 45 mm, and 30 mm), W/C(water to cement) ratio(40.0%, 50.0%, and 60.0%) and chloride concentration(0.0%, 3.5%, and 7.0%). OCP(Open Circuit Potential) was measured using agar-based socket type sensors. The OCP measurement showed the consistent behavior where the potential was reduced in wet conditions and it was partially recovered in dry conditions. In the case of 30 mm of cover depth for most W/C ratio cases, the lowest OCP value was measured and rapid OCP recovery was evaluated in increasing cover depth from 30 mm to 45 mm, since cover depth was an effective protection against chloride ion ingress. As the chloride concentration increased, the effect on the cover depth tended to be more dominant than the that of W/C ratio. After additional monitoring and physical evaluation of chloride concentration after specimen dismantling, the proposed system can be improved with increasing reliability of the corrosion monitoring.
Proceedings of the Korean Institute Of Construction Engineering and Management
/
2008.11a
/
pp.93-98
/
2008
Haeundae Doosan We've The Zenith project is adjacent to Suyoung-bay, now it is in the process of excavation and foundation work. The main use of the tower is residence which height is 300m and 80 floor, the highest residential reinforced concrete building through the Orient. It is comprised of 3 high- rised buildings and 1 low-rised building, the basement is 230m wide and 200m length sized mass structure. The lateral resistance system is acted effectively against the lateral load and satisfactorily against the wind vibration by the 4 direction extension of the center core wall($700{\sim}800mm$ thickness) and reinforced concrete column set around the slab. Flat-plate slab system(250mm thickness) is adjusted for the slab system and it enables effective work process and shortening the working term by minimizing the ceiling height and not needing to install perimeter beam and drop panel. The strength and serviceability of the structure is able to be monitored and estimated constantly through the health monitoring system during the construction and after the construction.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.