Comparison of Physical Properties of Domestic Contact Lenses -Focusing on oxygen transmissibility- (국내 생산 콘택트렌즈의 물리적 특성 비교 -산소전달률을 중심으로-)

  • Kim, Ki-Sung
    • Journal of the Korea Convergence Society
    • /
    • v.9 no.1
    • /
    • pp.393-403
    • /
    • 2018
  • Although the use of silicone hydrogel contact lenses which are known to have high oxygen transmissibility is increasing, they are being sold without any product labeling of physical properties such as water content and oxygen transmissibility. To analyze the physical properties such as the water content and oxygen transmissibility of approved silicone hydrogel contact lenses, this study collected and analyzed the approval information published on the KFDA website. Of 68 cases of domestic silicone hydrogel contact lenses analyzed in this study, 61 cases (89.7%) did not meet the international standard for oxygen permeability. This is because lenses that are not different from hydrogel contact lenses were submitted for approval as silicone hydrogel contact lenses because there is no domestic standard for silicone hydrogel contact lenses. In future, besides the information published on the website, analysis of the physical properties of a wide variety of actual silicone hydrogel contact lenses on the market is required.

Understanding of Protein Adsorption to Contact Lens Hydrogels with Varying Surface Energy (콘택트렌즈용 하이드로젤 계면에너지에 따른 단백질 흡착현상의 이해)

  • Jeon, So-Ha;Noh, Hye-Ran
    • Polymer(Korea)
    • /
    • v.36 no.3
    • /
    • pp.338-343
    • /
    • 2012
  • Interfacial properties of commercially available soft contact lens hydrogels were studied to understand thermodynamic phenomena of protein adsorption. Hydrogel particles ($1{\times}1mm^2$) with varying water wettability were exposed to bovine serum albumin solutions for an hour. The remained albumin solutions were analyzed with Bradford assay method. The amount of protein adsorbed to hydrogels increased with protein solution concentrations following Langmuir isotherm. The partition coefficient ($P$) and Gibbs free energy cost of dehydrating the surface region by protein displacement upon adsorption increased with increasing hydrophilicity of contact lens. Understanding of physical chemistry in protein adsorption to contact lens materials enabled elucidating relationships between surface energy and albumin adsorption capacity.

Comparison of Corneal Edema Induced by Material of Contact Lens (콘택트렌즈의 재질별 각막부종의 비교)

  • Kim, Ki-Sung;Kim, Sun-Kyung;Kim, Tae-Hun;Kim, Hyo-Jin
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.20 no.2
    • /
    • pp.151-156
    • /
    • 2015
  • Purpose: This study has been compared the degree of corneal edema arising from the material of the lens after wearing the recommended wearing time for the contact lens. Methods: For the study, 43 adults of 77 eyes who did not use drugs and have not any disease participated. Three types of lenses including narafilcon A, HEMA, and silicone hydrogel material regular replaceable lenses were used. Central corneal thickness was measured before and after 8 hours from wearing lenses using Pentacam. The degree of corneal edema was determined by the difference before and after wearing. Results: The average corneal edema of narafilcon A, HEMA material lens, and silicone hydrogel material regular replaceable lens were $2.36{\pm}6.15{\mu}m(Mean{\pm}SD)$, $23.61{\pm}10.71{\mu}m$, $18.25{\pm}8.64{\mu}m$, respectively. The central corneal thickness after wearing narafilcon A was not statistically significant with the central corneal thickness before wearing the lens. Central corneal thickness before and after wearing HEMA material lens and silicone hydrogel material regular replaceable lens were statistically significant. Conclusions: The amount of corneal edema induced by silicone hydrogel material regular replaceable lens was no statistically significant difference to the amount of corneal edema induced by HEMA material lens, but there was significant difference to narafilcon A. Therefore, it is judged to be careful not to exceed the recommended wearing time depending on the composition of the contact lens material.

Understanding of Protein Adsorption Kinetics to Contact Lens Hydrogels (콘택트렌즈용 하이드로젤로의 단백질 흡착 반응속도 이해)

  • Kim, Hyun-Jae;Kim, Mira;Noh, Hyeran
    • Polymer(Korea)
    • /
    • v.38 no.2
    • /
    • pp.220-224
    • /
    • 2014
  • Protein adsorption kinetics was studied with the amount of proteins adsorbed to contact lens hydrogels over time scales. Hydroxyethylmethacrylate (HEMA) and silicone hydrogels were dipped in protein solutions (albumin or IgG) and adsorption amounts were measured over time scales. The amount of protein adsorbed to both hydrogel types increased rapidly in 10 min, and remained consistently in 90 min. Decreasing interfacial energetics was taken slowly up to an hour in spite of rapid diffusion of protein molecules. This is due to the fact that water deprivation from three dimensional interphase initially formed by protein diffusion took over an hour. Interpretation of adsorption kinetics on contact lens hydrogels was discussed with understanding of relationship between surface energy and protein adsorption capacity.

Characterization of Hydrogel Tinted Contact Lens Containing 4-iodoaniline using Titanium Silicon Oxide Nanoparticles as Additive (티타늄 실리콘 옥사이드 나노입자를 첨가제로 사용한 4-iodoaniline을 포함한 하이드로젤 착색 콘택트렌즈의 특성)

  • Cho, Seon-Ahr;Sung, A-Young
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.19 no.3
    • /
    • pp.315-322
    • /
    • 2014
  • Purpose: The physical and optical characteristics of hydrophilic tinted contact lens containing titanium silicon oxide nanoparticles and the basic hydrogel contact lens material containing 4-iodoaniline were examined. In this study, the utility of titanium silicon oxide nanoparticles as a UV-blocking material for ophthalmologic devices were investigated by measuring the UV transmittance of the produced polymer. Also, titanium silicon oxide nanoparticles only without the addition of 4-iodoaniline in primary contact lens materials by copolymerizing two groups were compared. Methods: For manufacturing hydrogel lens, HEMA, MA, MMA, 4-iodoaniline and a cross-linker EGDMA were copolymerized in the presence of AIBN as an initiator. Also, the titanium silicon oxide nanoparticles was used as additive. After polymerization the physical properties such as water content, refractive index, contact angle and spectral transmittance of produced contact lenses were measured. Results: Measurement of the physical properties of the copolymerized material showed that the water content, refractive index, UV-B transmittance and contact angle were in the range of 35.01~38.60%, 1.4350~1.4418, $34.15{\sim}57.25^{\circ}$ and 1.0~10.0%, respectively. Titanium silicon oxide nanoparticles is not used as an additive in the experimental group, the results of the measurement showed that the water content, refractive index, contan angle and UV-B transmittance of the hydrogel lens polymer was 34.00~36.80%, 1.4378~1.4420, $40.15{\sim}60.16^{\circ}$ and 1.8~25.0%, respectively. Conclusions: Also, the transmittance for UV light was reduced significantly in combinations containing titanium oxide nanoparticles.

Influence of Artificial Tear Containing Carboxymethyl Cellulose Component on Physical Properties of Hydrogel Contact lens (카르복시메칠 셀룰로오스 성분이 포함된 인공누액이 하이드로젤 콘택트렌즈의 물성에 미치는 영향)

  • Cho, Seon-Ahr;Sung, A-Young
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.18 no.4
    • /
    • pp.457-463
    • /
    • 2013
  • To determine the impact of artificial tears which include carboxymethyl cellulose on a hydrogel contact lenses. Methods: A contact lenses made of the cross-linking agent, EGDMA (ethylene glycol dimethacrylate) and HEMA (2-hydroxyethyl methacrylate) and with added NVP (n-vinyl-2-pyrrolidone) and MMA (methyl methacrylate) was evaluated for water content, refractive index, spectral transmittance and contact angle of produced contact lens. Results: The physical properties of the sampled copolymerized polymers showed that water content, refractive index, visible ray transmittance and contact angle were in the range of 26.61%~48.58%, 1.422~1.455, 80.8%~91.4% and $33.93^{\circ}{\sim}65.70^{\circ}$, respectively. In addition, after soaking with artificial tears, the water content, refractive index and contact angle were in the range of 24.46%~48.25%, 1.422~1.457, 77.0%~91.0% and $37.25^{\circ}{\sim}77.33^{\circ}$, respectively. The changes of the physical property depending on hydration time and showed an increase of refractive index and contact angle, decrease of water content and visible ray transmittance. Conclusions: Artificial tears which include carboxymethyl cellulose sodium which is used as a wetting agent influenced water content, refractive index, contact angle and spectral transmittance of a hydrogel contact lenses.

Polymerization of Hydrogel Contact Lens with High Oxygen Transmissibility (산소투과성이 뛰어난 Hydrogel 콘택트렌즈 합성)

  • Sung, A-Young;Kim, Tae-Hun;Kong, Jung-Il
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.11 no.1
    • /
    • pp.49-53
    • /
    • 2006
  • Acrylate -PDMS(Polydimethylsiloxane)-Urethane Prepolymer is synthesized through treating diisocynate, HEMA(2-hydroxyethylmethacrylate) and bis(hydroxyalkyl)terminated Poly(dimethylsiloxane) having high oxygen permeability under the DBTDL(Dibutylitin dilaurate) catalyst. Modification of HEMA on bis(hydroxyalkyl)terminated Poly(dimethylsiloxane) is to be able to polymerize with other contact lens materials. And modification of urethane on bis(hydroxyalkyl)terminated Poly(dimethylsiloxane) is to increase elastic property and oxygen transmissibility. This material is analyzed by FT-IR and also will be used to make hydrogel contact lens.

  • PDF

A Study on the Measurement of Water Content in Hydrogel Contact Lens by Gravimetric Method (중량측정법에 의한 하이드로젤 콘택트렌즈의 함수율 측정에 관한 연구)

  • Kim, Tae-Hun;Ye, Ki-Hun;Sung, A-Young
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.13 no.4
    • /
    • pp.59-63
    • /
    • 2008
  • Purpose: The purpose of this study is to understand a relation of water content measurement with two different method, water removal method and dry method. Methods: 72 hydrogel contact lens containing various water content (ranged from 47% to 58%) were measured by the gravimetric method at 20$^{\circ}C$and 21% of the humidity. We weighed the dried test specimen at room temperature for 30 min after cooling. Results: In dry blotting method, the water content was measured to 47.43${\pm}$8.48%. The water contents was measured to 48.15${\pm}$8.36% with wet blotting condition. It was found that wet blotting method showed the higher water content of about 7% than dry blotting method. In water content with two dry methods, each of results was measured by 47.89${\pm}$8.06% and 49.56${\pm}$7.06%. In case of microwave method, the water content was measured significantly higher water content of about 1.67% than vacuum oven method. However, no statistical difference was found (p>0.05). Conclusions: In water removal method (Dry blotting method and Wet blotting method) to weigh hydrated test specimen, wet blotting method showed significantly higher water content than dry blotting method. Also in case of dry methods (vacuum oven and microwave) to weigh dry test specimen, water content of microwave method showed higher water content than vacuum oven method, but it should be noted that microwave oven method must be used carefully to measure accurateness on the specimen position and wave power.

  • PDF

Opto-Physical Properties of Ophthalmic Lens Polymer Containing σ, m, p-Substituted Difluoroaniline as Additives (σ, m, p-위치로 치환된 Difluoroaniline을 첨가제로 사용한 안의료용 렌즈 고분자의 물리·광학적 특성)

  • No, Jung-Won;Sung, A-Young
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.19 no.1
    • /
    • pp.69-77
    • /
    • 2014
  • Purpose: The functional ophthalmic lenses containing fluorine-substituted aniline group (2,4-difluoroaniline, 2,6-difluoroaniline, 3,4-difluoroaniline) were manufactured and the physical and optical characteristics of copolymerized ophthalmic lens were investigated. Methods: HEMA (2-hydroxyethylmethacrylate), NVP (N-vinyl pyrrolidone), MA (methacrylic acid), the cross-linker EGDMA (ethylene glycol dimethacrylate) and the initiator AIBN (azobisisobutyronitrile) were used as a basic combination and fluorine-substituted aniline group (2,4-difluoroaniline, 2,6-difluoroaniline, 3,4-difluoroaniline) were used as additives for preparing the hydrogel soft contact lenses. The hydrogel ophthalmic lens was manufactured by cast mould method and the ophthalmic lenses were stored in a 0.9% NaCl normal saline for 24 hrs. Results: The optical transmittance of the sample with addition 2,4-difluoroaniline showed that the UV-B(9.8~51.4%), UV-A(58.8~79.2%) and visible transmittance(87.0~90.4%). In the case of 2,6-difluoroaniline were measured the UV-B(80.2~83.2%), UV-A(85.8~86.4%), and visible transmittance(90.8~91.4%). Also, the optical transmittance of ophthalmic lens containing 3,4-difluoroaniline were measured the UV-B transmittance of 3.8~30.4%, UV-A transmittance of 47.8%~74.4% and the visible transmittance of 86.2~91.0% respectively. Conclusions: Based on the results of this study, 2,4-difluoroaniline and 3,4-difluoroaniline can be used effectively as additive for UV-blocking ophthalmic contact lenses.

Physical Properties Assessment of Soft Contact Lens with Halogen and Carboxylic Substituted Pyridine as Additive (할로겐과 카르복시산으로 치환된 피리딘 첨가제를 사용한 소프트 콘택트렌즈의 물성 평가)

  • Kim, Duck-Hyun;Sung, A-Young
    • Journal of Korean Ophthalmic Optics Society
    • /
    • v.20 no.4
    • /
    • pp.437-443
    • /
    • 2015
  • Purpose: This study evaluated the optical and physical and characteristics of soft contact lens polymerized with addition of 3-chloropyridine-4-carboxylic acid and 3-fluoropyridine-4-carboxylic acid in the basic hydrogel contact lens material. In particular, the utility of 3-chloropyridine-4-carboxylic acid and 3-fluoropyridine- 4-carboxylic acid as a hydrogel contact lens material was investigated. Methods: In this study, 3-chloropyridine-4-carboxylic acid and 3-fluoropyridine-4-carboxylic acid were used as additives. Also, 2-hydroxyethyl methacrylate, acrylic acid, methyl methacrylate and a cross-linker EGDMA were co-polymerized in the presence of AIBN as an initiator. Results: The physical properties of the produced polymers were measured as followings. The water content of 34.54~37.15%, refractive index of 1.4320~1.4342, tensile strength of 0.2872~0.3608 kgf and contact angle of $57.82{\sim}79.57^{\circ}$, UV-B transmittance of 76.8~82.4% and UV-A transmittance of 84.6~86.6% were obtained respectively. Conclusions: Based on the results of this study, contact lens material containing 3-chloropyridine-4-carboxylic acid and 3-fluoropyridine-4-carboxylic acid is expected to be able to used as a material for high wettability and UV-block hydrogel contact lens.