The Fludity and Compressive Strength Properties of Mortar Using Peronikel Slag Powder and Mixed Slag Aggregates (페로니켈슬래그 미분말 및 혼합슬래그 골재를 사용한 모르타르의 유동성 및 압축강도 특성)

  • Bae, Sunh-Ho;Jung, Yong-Jae;Lee, Jae-In;Kim, Ji-Hwan;Choi, Se-Jin
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2021.05a
    • /
    • pp.78-79
    • /
    • 2021
  • This study compared and analyzed the fluidity and compressive strength characteristics of mortar using ferronikel slag powder and mixed slag fine aggregate as part of the study to reduce environmental load and increase recycling rate of industrial by-products.

  • PDF

Characterization of Flowable Fill with Ferro-Nickel Slag Dust (페로니켈 슬래그 미분말을 이용한 유동성 뒤채움재 특성)

  • Lee, Kwan-Ho
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.5
    • /
    • pp.16-21
    • /
    • 2017
  • The aim of this study was to utilize ferronickel slag produced in the manufacture of stainless steel as a flowable backfill material for underground use using crushed fine powder. Experimental combinations were made using two components: Case A (sand) and Case B (soil). The optimal mixing ratio of Case A was sand (58.4%), ferronickel slag fine powder (21.6%), cement (1.8%), and water (18.2%). In the case of B, the optimal mixing ratio was determined to be soil (53.0%), ferronickel slag fine powder (20.0%), cement (1.7%), and water (25.3%). The uniaxial compressive strength of case A, which is a mixture of ordinary sand and ferronickel slag powder, was relatively larger than that of case B using soil. In addition, the strength of the specimen increased with increasing curing time. The uniaxial compressive strength tended to increase with increasing curing time. In addition, the unconfined compression strength of the fluid backfill material using common sand as the main material was relatively larger than that of the mixed material using soil as the main material. In case A, the uniaxial compressive strength ranged from 0.17-0.33 MPa, 0.21-0.39 MPa, and 0.19-0.40 MPa, respectively, at curing times of 7, 14, and 28 days. From the experimental results, it was concluded that the ratio of FNS powder and cement mixture was the most appropriate for Case A3. Case B, which used soil as the main material, showed a similar tendency to Case A. As a result of the dissolution test for evaluating the environmental harm of the FNS fine powder, there was no dissolution of substances harmful to the environment.

A Study on Strength and Durability of Vibrated and Rolled Method Mortar Mixed with Desulfurized Gypsum and Ferronickel Slag Fine Powder (탈황석고와 페로니켈슬래그 미분말을 혼합한 진동전압방식 모르타르의 강도 및 내구성에 관한 연구)

  • Yoo, Jeong-Hwan;Park, Sang-Soon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.4
    • /
    • pp.545-552
    • /
    • 2021
  • In this study, strength and durability evaluations are performed on vibrated-rolled method mortar mixtures containing desulfurized gypsum and ferronickel slag powder. Desulfurized gypsum and ferronickel slag fine powders were substituted for 25% limestone fine powders u sed in the manu factu re of VR tu bes, and mortar specimens were prepared u sing vibrated-rolled method. Accordingly, flexural and compressive strengths were performed to evaluate the strength, and chlorine ion penetration resistance and sulfuric acid resistance tests were performed to evaluate durability. Flexural and compressive strength were improved in the range 20 to 60% of desu lfu rized gypsu m among admixtu res, and the amou nt of passing charge decreased in the choride ion penetration resistance test in the range of 20 to 80% of desulfurized gypsum. As for the resistance to su lfu ric acid, when the proportion of desu lfu rized in the admixtu re was 40%, the strength and weight change rate according to the immersion period was reduced. Appropriate use of desulfurized gypsum and ferronickel slag powder is expected to improve performance in terms of strength and durability.

Consideration on the Application of Low-Heat Concrete with Ferronickel Slag Aggregate to LNG Storage Tank (페로니켈슬래그 골재를 활용한 저발열 콘크리트의 LNG 저장탱크 적용성 검토)

  • Sang Hyeon Cheong;Sukhoon Pyo;Hyeong-Ki Kim
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.12 no.1
    • /
    • pp.17-24
    • /
    • 2024
  • The characteristics of low-heat concrete, mixed with ground blast furnace slag and ferronickel slag aggregate, were analyzed. Moreover, the applicability of this concrete for mass concrete in LNG storage tanks was examined. Initially, the study investigated the characteristics of fresh and hardened concrete. Subsequently, the temperature rising curve was obtained. Utilizing the obtained parameters from the curves, a series of thermal stress analyses for the LNG storage tank were conducted to assess the risk of cracking. The results confirmed that concrete mixtures incorporating ground blast furnace slag and ferronickel slag aggregate not only exhibited sufficient workability but also achieved a compressive strength of approximately 40 MPa within 28 days. Furthermore, the concrete demonstrated a lower terminal heat rise and a faster heat generation rate compared to low-heat Portland cement concrete. An analysis of thermal stress in various sections of the LNG tank validated a low risk of cracking.

A Fluidity and Compressive Strength Properties of Blast Furnace Slag Based Non-Cement Paste Containing Ferronickel Slag Powder (페로니켈슬래그 미분말 혼입에 따른 고로슬래그 기반 무시멘트 페이스트의 유동성 및 압축강도 특성)

  • Kim, Young-Uk;Lee, Kyung-Su;Oh, Tae-Gue;Jeong, Su-Bin;Choi, Se-Jin
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.05a
    • /
    • pp.205-206
    • /
    • 2019
  • This study investigated the fluidity and compressive strength properties of blast furnace slag based non-cement paste containing ferronickel slag powder to evaluate the possibility of use in for cement replacement materials. As a result, the fluidity of non-cement paste showed a higher flow as the mixing ratio of ferronickel slag powder increased. The compressive strengths similar to those of the non-cement paste using only blast furnace slag powder were obtained when 5 and 10% of ferronickel slag powder were used.

  • PDF

Phosphorus Adsorption Characteristic of Ferronickel and Rapid Cooling Slags (페로니켈슬래그와 제강급랭슬래그의 인 흡착특성)

  • Park, Jong-Hwan;Seo, Dong-Cheol;Kim, Seong-Heon;Park, Min-Gyu;Kang, Byung-Hwa;Lee, Sang-Won;Lee, Seong-Tae;Choi, Ik-Won;Cho, Ju-Sik;Heo, Jong-Soo
    • Korean Journal of Environmental Agriculture
    • /
    • v.33 no.3
    • /
    • pp.169-177
    • /
    • 2014
  • BACKGROUND: The ferronickel and rapid cooling slags used in present study are industrial wastes derived from a steel factory in Korea. These slags are used as almost road construction materials after magnetic separation. However, the use of slag to remove phosphorus from wastewater is still a relatively less explored. The objective of this work was to evaluate the feasibility of ferronickel slag (FNS) and rapid cooling slag (RCS) as sorbents for phosphorus removal in wastewater. METHODS AND RESULTS: Adsorption experiments were conducted to determine the adsorption characteristics of the FNS and RCS for the phosphorus. Adsorption behaviour of the phosphorus by the FNS and RCS was evaluated using both the Freundlich and Langmuir adsorption isotherm equations. FNS and RCS were divided into two sizes as effective sizes. Effective sizes of FNS and RCS were 0.5 and 2.5 mm, respectively. The adsorption capacities (K) of the phosphorus by the FNS and RCS were in the order of RCS 0.5 (0.5105) > RCS 2.5 (0.3572) ${\gg}$ FNS 2.5 (0.0545) ${\fallingdotseq}$ FNS 0.5 (0.0400) based on Freundlich adsorption isotherm. The maximum adsorption capacities (a; mg/kg) of the phosphorus determined by the Langmuir isotherms were in the order of RCS 0.5 (3,582 mg/kg) > RCS 2.5 (2,983 mg/kg) > FNS 0.5 (320 mg/kg) ${\fallingdotseq}$ FNS 2.5 (187 mg/kg). RCS 0.5 represented the best sorbent for the adsorption of phosphorus. In the experiment, the Langmuir model showed better fit with our data than the Freundlich model. CONCLUSION: This study indicate that the use of RCS in constructed wetlands or filter beds is a promising solution for phosphorus removal via adsorption and precipitation mechanisms.

A Study on the Properties of Hwangto Permeable Block Using Ferro Nickel Slag (페로니켈슬래그를 혼입한 황토투수블럭 물성에 관한 연구)

  • Kim, Soon-Ho
    • Journal of the Korea Institute of Building Construction
    • /
    • v.22 no.6
    • /
    • pp.607-618
    • /
    • 2022
  • This study involves the development of a Hwangto permeable block for rainwater storage tanks. The permeable products that form continuous voids between Hwangto binders and aggregates are fine milled slag powder, which is an industrial by-product generated during the production of Hwangto and iron, and ferro nickel slag. The properties of Hwangto permeable blocks were studied using recycled resource aggregates. The target quality is based on KSF 2394. The Hwangto permeable block for a rainwater storage tank is made of water-permeable material, and the permeability of the Hwangto permeable block itself is 0.1mm/sec or higher, with a physical performance of over 5.0MPa in flexural strength and over 20.0MPa in compressive strength. The physical properties of Hwangto permeable block for rainwater storage tanks were researched and developed. In order to prevent flooding due to heavy rain in summer and the urban heat island phenomenon due to depletion of ground water, continuous pores are formed in the block to secure a permeability function to prevent rainwater from accumulating in the pavement of the floor, and to prevent slippage for comfortable and safe storage.

Analysis of the influence of combined use of ferronickel slag fine powder and admixture on VR sewage pipe strength development (페로니켈슬래그 미분말 및 혼화재의 복합사용이 VR 하수관 강도발현에 미치는 영향분석)

  • Nam, Sang-Koo;Chung, Tae-Jun;Jo, Seol-Ah;Yoo, Jeong-Hwan;Park, Sang-Soon
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.3
    • /
    • pp.214-221
    • /
    • 2018
  • In this paper, the effects of ferronickel slag powder and admixture on the strength of VR sewer pipe were analyzed. the substitution rate was tested as a variable, and the strength development was studied through the flexural strength, compressive strength and using SEM microscopic analysis. bending strength, compressive strength results and micro analysis using SEM showed the correlation in each case. the substitution rates were 20% and 30% relative to the mass of the OPC respectively, and were substituted according to a constant ratio of ferronickel slag fine powder and mixture. when the substitution ratio was 20%, the strength development was excellent. also, bending strength and compressive strength were the best when the ferronickel slag fine powder, quicklime, gypsum and calcium chloride were used as the admixture, dense microstructural patterns appeared. the possibility of progressive strength development is shown after 28 days.

Fluidity and strength characteristics of no-cement composite applied with ferronickel slag powder according to curing temperature (양생온도에 따른 페로니켈슬래그 미분말 적용 무시멘트 복합체의 유동성 및 강도특성)

  • Kim, Chae-Young;Yoon, Joo-Ho;Park, Jeong-Yeon;Park, Gwan-Hong;Lee, Jae-In;Choi, Se-Jin
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2023.11a
    • /
    • pp.193-194
    • /
    • 2023
  • Recently, research is being conducted on geopolymers using industrial by-products as a cement substitute to reduce carbon dioxide emissions from the construction industry. Since geopolymers use industrial by-products, their performance varies depending on the type of alkali activator used, curing temperature, etc. Therefore, as part of a study to reduce carbon dioxide emissions from the construction industry, this study mixed blast furnace slag powder and ferronickel slag powder as cement substitutes, and compared and analyzed the fluidity and compressive strength of no-cement composites according to curing temperature.

  • PDF

Applicability of Ferro-nickel Slag Sand for Dry Mortar in Floor (페로니켈슬래그 잔골재의 바닥용 건조모르타르 적용성 평가)

  • Cho, Bong-Suk;Kim, Won-Ki;Hwang, Yin-Seong;Koo, Kyung-Mo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.19 no.2
    • /
    • pp.105-112
    • /
    • 2019
  • Fine aggregate made of ferronickel slag(FNS) is similar to natural fine aggregates and is used in concrete structures both domestically and abroad, but its applications and research areas are limited. In this research, in order to expand the availability of FNS and improve the performance of cement mortar products, the applicability of FNS on dry mortar for floor was examined. Experimental results show that FNS improves flow of cement mortar because it has low absorption rate, spherical shape, and glassy surface. Also, the high stiffness of the FNS aggregate itself is considered to contribute to the improvement of cement mortar quality such as crack reduction by improving the compressive strength and shrinkage reducing. In addition, when FNS fine aggregate is applied, it was possible to secure the impact sound insulation performance equal to or higher than that of mortar using natural fine aggregate.